Process optimisation for realisation of crack-free Ni-based wear protection coatings and assessment of machinability by subsequent milling processes to produce defined surfaces

  • Reducing CO2 emissions to 62 percent up to 2030 and achieving greenhouse neutrality up to 2050 are the key goals of the EU's climate protection legislation. The expansion of technologies for climate-neutral energy generation is not the only important contribution to reducing greenhouse gases, the efficient use of material systems is also a key factor. In the area of plant engineering, steel components are provided with a wear-protection coating for efficient use to protect them against corrosive, tribological, thermal and mechanical stresses. The wear-protection coatings are primarily made of Co alloys, which are to be replaced by alternative materials, such as nickel alloys, because of the poor working conditions regarding the extraction of the cobalt and because of the health risks. In terms of corrosion behavior, many applications require a crack-free wear protection layer and additional machining. Machining by milling is not economical for wear materials, especially for SME becauseReducing CO2 emissions to 62 percent up to 2030 and achieving greenhouse neutrality up to 2050 are the key goals of the EU's climate protection legislation. The expansion of technologies for climate-neutral energy generation is not the only important contribution to reducing greenhouse gases, the efficient use of material systems is also a key factor. In the area of plant engineering, steel components are provided with a wear-protection coating for efficient use to protect them against corrosive, tribological, thermal and mechanical stresses. The wear-protection coatings are primarily made of Co alloys, which are to be replaced by alternative materials, such as nickel alloys, because of the poor working conditions regarding the extraction of the cobalt and because of the health risks. In terms of corrosion behavior, many applications require a crack-free wear protection layer and additional machining. Machining by milling is not economical for wear materials, especially for SME because of the high tool wear, but it is essential to produce defined surfaces with high quality. Alloy modifications of the filler metals for nickel-based plasma deposition welded wear protection coatings and the use of innovative ultrasonic-assisted milling processes are examined to determine how more favorable machinability can be achieved without reducing the wear protection potential. The focus is on the NiCrSiFeB alloy, which is intended to replace CoCr alloys in the area of screw machines. The modification of hard facing layers in terms of microstructure and precipitation morphology as well as suitability for machining is investigated and compared with the CoCr alloy. In this aspect, the alloy modifications are generated by a PTA process by systematically adjusting the preheating and interpass temperatures, a crack-free wear-resistant layer can be generated, which is subsequently machined by a milling process. In addition to the crack-free properties, the microstructure, the bonding as well as the mixing between the NiCrFeB alloy and a 1.8550 as well as between the CoCr alloy and a 1.4828 are analyzed and compared in the joining areas. In addition, heating and cooling rates are determined and a chemical analysis of the weld metals is performed. This study provides important knowledge about the differences between NiCrFeB alloy and CoCr alloys in terms of microstructure morphology, bonding and mixing behavior in the joining zones to the basic material.zeige mehrzeige weniger

Volltext Dateien herunterladen

  • Graebner_Giese_ISAF_BAM_AJP23.pdf
    eng

Metadaten exportieren

Weitere Dienste

Teilen auf Twitter Suche bei Google Scholar Anzahl der Zugriffe auf dieses Dokument
Metadaten
Autor*innen:Maraike Gräbner
Koautor*innen:Marcel Giese, Dirk Schröpfer, Thomas Kannengießer, Kai Treutler, Volker Wesling
Dokumenttyp:Vortrag
Veröffentlichungsform:Präsentation
Sprache:Englisch
Jahr der Erstveröffentlichung:2023
Organisationseinheit der BAM:9 Komponentensicherheit
9 Komponentensicherheit / 9.2 Versuchsanlagen und Prüftechnik
9 Komponentensicherheit / 9.4 Integrität von Schweißverbindungen
DDC-Klassifikation:Technik, Medizin, angewandte Wissenschaften / Ingenieurwissenschaften / Ingenieurwissenschaften und zugeordnete Tätigkeiten
Freie Schlagwörter:Auftragschweißen; Legierungsmodifikation; Ultraschallunterstütztes Fräsen; Zerspankräfte
Themenfelder/Aktivitätsfelder der BAM:Material
Material / Degradation von Werkstoffen
Veranstaltung:3rd International Conference on Advanced Joining Processes
Veranstaltungsort:Braga, Portugal
Beginndatum der Veranstaltung:19.10.2023
Enddatum der Veranstaltung:20.10.2023
Verfügbarkeit des Dokuments:Datei im Netzwerk der BAM verfügbar ("Closed Access")
Datum der Freischaltung:12.12.2023
Referierte Publikation:Nein
Eingeladener Vortrag:Nein
Einverstanden
Diese Webseite verwendet technisch erforderliche Session-Cookies. Durch die weitere Nutzung der Webseite stimmen Sie diesem zu. Unsere Datenschutzerklärung finden Sie hier.