Laser Welding of SLM-Manufactured Tubes Made of IN625 and IN718
- The advantage of selective laser melting (SLM) is its high accuracy and geometrical flexibility. Because the maximum size of the components is limited by the process chamber, possibilities must be found to combine several parts manufactured by SLM. An application where this is necessary, is, for example, the components of gas turbines, such as burners or oil return pipes, and inserts, which can be joined by circumferential welds. However, only a few investigations to date have been carried out for the welding of components produced by SLM. The object of this paper is, therefore, to investigate the feasibility of laser beam welding for joining SLM tube connections made of nickel-based alloys. For this purpose, SLM-manufactured Inconel 625 and Inconel 718 tubes were welded with a Yb:YAG disk laser and subsequently examined for residual stresses and defects. The results showed that the welds had no significant influence on the residual stresses. A good weld quality could be achieved inThe advantage of selective laser melting (SLM) is its high accuracy and geometrical flexibility. Because the maximum size of the components is limited by the process chamber, possibilities must be found to combine several parts manufactured by SLM. An application where this is necessary, is, for example, the components of gas turbines, such as burners or oil return pipes, and inserts, which can be joined by circumferential welds. However, only a few investigations to date have been carried out for the welding of components produced by SLM. The object of this paper is, therefore, to investigate the feasibility of laser beam welding for joining SLM tube connections made of nickel-based alloys. For this purpose, SLM-manufactured Inconel 625 and Inconel 718 tubes were welded with a Yb:YAG disk laser and subsequently examined for residual stresses and defects. The results showed that the welds had no significant influence on the residual stresses. A good weld quality could be achieved in the seam circumference. However, pores and pore nests were found in the final overlap area, which meant that no continuous good welding quality could be accomplished. Pore formation was presumably caused by capillary instabilities when the laser power was ramped out.…
Autor*innen: | T. Jokisch, A. Marko, S. Gook, Ö. Üstündag, Andrey GumenyukORCiD, Michael RethmeierORCiD |
---|---|
Dokumenttyp: | Zeitschriftenartikel |
Veröffentlichungsform: | Verlagsliteratur |
Sprache: | Englisch |
Titel des übergeordneten Werkes (Englisch): | Materials |
Jahr der Erstveröffentlichung: | 2019 |
Organisationseinheit der BAM: | 9 Komponentensicherheit |
9 Komponentensicherheit / 9.3 Schweißtechnische Fertigungsverfahren | |
Veröffentlichende Institution: | Bundesanstalt für Materialforschung und -prüfung (BAM) |
Verlag: | Multidisciplinary Digital Publishing Institute |
Verlagsort: | Basel |
Jahrgang/Band: | 12 |
Ausgabe/Heft: | 18 |
Erste Seite: | 2967, 1 |
Letzte Seite: | 15 |
DDC-Klassifikation: | Technik, Medizin, angewandte Wissenschaften / Ingenieurwissenschaften / Ingenieurwissenschaften und zugeordnete Tätigkeiten |
Freie Schlagwörter: | Inconel 718; Laser Powder Bed Fusion; Laser welding; Selective Laser Melting |
Themenfelder/Aktivitätsfelder der BAM: | Material |
DOI: | 10.3390/ma12182967 |
URN: | urn:nbn:de:kobv:b43-489679 |
ISSN: | 1996-1944 |
Verfügbarkeit des Dokuments: | Datei für die Öffentlichkeit verfügbar ("Open Access") |
Lizenz (Deutsch): | Creative Commons - CC BY - Namensnennung 4.0 International |
Datum der Freischaltung: | 16.09.2019 |
Referierte Publikation: | Ja |
Datum der Eintragung als referierte Publikation: | 27.09.2019 |
Schriftenreihen ohne Nummerierung: | Wissenschaftliche Artikel der BAM |