Investigation of Elastic Properties of the Single-Crystal Nickel-Base Superalloy CMSX-4 in the Temperature Interval between Room Temperature and 1300 °C
- The elastic properties of the single-crystal nickel-base superalloy CMSX-4 used as a blade material in gas turbines were investigated by the sonic resonance method in the temperature interval between room temperature and 1300 °C. Elastic constants at such high temperatures are needed to model the mechanical behavior of blade material during manufacturing (hot isostatic pressing) as well as during technical accidents which may happen in service (overheating). High reliability of the results was achieved using specimens of different crystallographic orientations, exciting various vibration modes as well as precise measurement of the material density and thermal Expansion required for modeling the resonance frequencies by finite element method. Combining the results measured in this work and literature data the elastic constants of the gamma and gamma' phases were predicted. This prediction was supported by measurement of the temperature dependence of the gamma'fraction. All dataThe elastic properties of the single-crystal nickel-base superalloy CMSX-4 used as a blade material in gas turbines were investigated by the sonic resonance method in the temperature interval between room temperature and 1300 °C. Elastic constants at such high temperatures are needed to model the mechanical behavior of blade material during manufacturing (hot isostatic pressing) as well as during technical accidents which may happen in service (overheating). High reliability of the results was achieved using specimens of different crystallographic orientations, exciting various vibration modes as well as precise measurement of the material density and thermal Expansion required for modeling the resonance frequencies by finite element method. Combining the results measured in this work and literature data the elastic constants of the gamma and gamma' phases were predicted. This prediction was supported by measurement of the temperature dependence of the gamma'fraction. All data obtained in this work are given in numerical or analytical forms and can be easily used for different scientific and engineering calculations.…
Autor*innen: | A. Epishin, Bernard FedelichORCiD, Monika Finn, Georgia Künecke, Birgit RehmerORCiD, Gert Nolze, C. Leistner, N. Petrushin, I. Svetlov |
---|---|
Dokumenttyp: | Zeitschriftenartikel |
Veröffentlichungsform: | Verlagsliteratur |
Sprache: | Englisch |
Titel des übergeordneten Werkes (Englisch): | Crystals |
Jahr der Erstveröffentlichung: | 2021 |
Organisationseinheit der BAM: | 5 Werkstofftechnik |
5 Werkstofftechnik / 5.2 Metallische Hochtemperaturwerkstoffe | |
5 Werkstofftechnik / 5.5 Materialmodellierung | |
Veröffentlichende Institution: | Bundesanstalt für Materialforschung und -prüfung (BAM) |
Verlag: | MDPI |
Jahrgang/Band: | 11 |
Ausgabe/Heft: | 2 |
Erste Seite: | 152 |
DDC-Klassifikation: | Technik, Medizin, angewandte Wissenschaften / Ingenieurwissenschaften / Ingenieurwissenschaften und zugeordnete Tätigkeiten |
Freie Schlagwörter: | Characterization; Elastic constants; Nickel-base superalloys; Single-crystals |
Themenfelder/Aktivitätsfelder der BAM: | Material |
DOI: | 10.3390/cryst11020152 |
URN: | urn:nbn:de:kobv:b43-520972 |
Verfügbarkeit des Dokuments: | Datei für die Öffentlichkeit verfügbar ("Open Access") |
Lizenz (Deutsch): | Creative Commons - CC BY - Namensnennung 4.0 International |
Datum der Freischaltung: | 10.02.2021 |
Referierte Publikation: | Ja |
Datum der Eintragung als referierte Publikation: | 24.03.2021 |
Schriftenreihen ohne Nummerierung: | Wissenschaftliche Artikel der BAM |