Spatially resolved determination of chloride content on rough surfaces using LIBS

  • The durability and the lifetime of reinforced concrete structures can be drastically reduced by the influence of damage processes. One of the most common causes is chloride-induced corrosion, which is triggered by increased chloride content near the reinforcement. In a study, the chloride content should be determined directly at corrosion areas. The LIBS system used consists of a micro-chip laser (3 mJ, 100 Hz, 1.5ins) and two compact spectrometers covering the wavelength range of 177-355 nm (UV) and 750-940 nm (NIR). The analysis of the chloride content was carried out via the atomic chlorine spectral line 837.59 nm, using helium for signal amplification. Calibrations were carried out for quantitative chlorine measurements with 15 reference samples in the working range of 0.05 to 6.00 wt% chlorine. The calibration of the LIBS system was done according to DIN 32 645 and was tested for linearity. The determination of the quantitative chlorine contents was carried out on samples whichThe durability and the lifetime of reinforced concrete structures can be drastically reduced by the influence of damage processes. One of the most common causes is chloride-induced corrosion, which is triggered by increased chloride content near the reinforcement. In a study, the chloride content should be determined directly at corrosion areas. The LIBS system used consists of a micro-chip laser (3 mJ, 100 Hz, 1.5ins) and two compact spectrometers covering the wavelength range of 177-355 nm (UV) and 750-940 nm (NIR). The analysis of the chloride content was carried out via the atomic chlorine spectral line 837.59 nm, using helium for signal amplification. Calibrations were carried out for quantitative chlorine measurements with 15 reference samples in the working range of 0.05 to 6.00 wt% chlorine. The calibration of the LIBS system was done according to DIN 32 645 and was tested for linearity. The determination of the quantitative chlorine contents was carried out on samples which were broken and thus have a high surface roughness. This requires real time correction of the focus point to compensate for the roughness of the samples. The poster shows spatially resolved element distributions and determined quantitative chloride concentrations near the corrosion Areas.zeige mehrzeige weniger

Volltext Dateien herunterladen

  • Spatially resolved determination of chloride content on rough surfaces using LIBS.pdf
    eng

Metadaten exportieren

Weitere Dienste

Teilen auf Twitter Suche bei Google Scholar Anzahl der Zugriffe auf dieses Dokument
Metadaten
Autor*innen:Tobias Günther
Koautor*innen:Tobias Völker, Steven Millar, Gerd Wilsch
Dokumenttyp:Posterpräsentation
Veröffentlichungsform:Präsentation
Sprache:Englisch
Jahr der Erstveröffentlichung:2018
Organisationseinheit der BAM:8 Zerstörungsfreie Prüfung
8 Zerstörungsfreie Prüfung / 8.2 Zerstörungsfreie Prüfmethoden für das Bauwesen
DDC-Klassifikation:Naturwissenschaften und Mathematik / Chemie / Analytische Chemie
Freie Schlagwörter:Chloride; LIBS; Rough surface
Themenfelder/Aktivitätsfelder der BAM:Chemie und Prozesstechnik
Veranstaltung:Xth international conference on Laser-Induced Breakdown Spectroscopy
Veranstaltungsort:Atlanta, GA, USA
Beginndatum der Veranstaltung:21.10.2018
Enddatum der Veranstaltung:26.10.2018
Verfügbarkeit des Dokuments:Datei im Netzwerk der BAM verfügbar ("Closed Access")
Datum der Freischaltung:03.12.2018
Referierte Publikation:Nein
Einverstanden
Diese Webseite verwendet technisch erforderliche Session-Cookies. Durch die weitere Nutzung der Webseite stimmen Sie diesem zu. Unsere Datenschutzerklärung finden Sie hier.