Molecular dynamics of Janus Polynorbornenes: Glass Transitions and Nanophase separation

  • For the first time, dielectric and calorimetric investigations of a homologous series of Janus polynorbornenes with rigid main backbones and flexible −Si(OR)3 side groups of differing length alkyl chains (R = propyl, butyl, hexyl, octyl, and decyl) is reported. Generally, this class of polymers has some potential for applications in the field of gas separation membranes. Two dielectrically active processes are observed at low temperatures, denoted as β- and α-relaxation. The former can be assigned to localized fluctuations, while the latter is related to the glassy dynamics of the flexible −Si(OR)3 side groups, creating a nanophase separation in both the alkyl chain-rich and backbone-rich domains. This is confirmed through temperature-modulated differential scanning calorimetry (TMDSC) measurements and X-ray scattering experiments. The glass transition temperatures of the backbone rich domains, which are beyond or near to their degradation temperatures in terms of conventional DSC, areFor the first time, dielectric and calorimetric investigations of a homologous series of Janus polynorbornenes with rigid main backbones and flexible −Si(OR)3 side groups of differing length alkyl chains (R = propyl, butyl, hexyl, octyl, and decyl) is reported. Generally, this class of polymers has some potential for applications in the field of gas separation membranes. Two dielectrically active processes are observed at low temperatures, denoted as β- and α-relaxation. The former can be assigned to localized fluctuations, while the latter is related to the glassy dynamics of the flexible −Si(OR)3 side groups, creating a nanophase separation in both the alkyl chain-rich and backbone-rich domains. This is confirmed through temperature-modulated differential scanning calorimetry (TMDSC) measurements and X-ray scattering experiments. The glass transition temperatures of the backbone rich domains, which are beyond or near to their degradation temperatures in terms of conventional DSC, are determined for the first time using fast scanning calorimetry employing both fast heating and cooling rates. This is complemented with scattering experiments that show how the size of the alkyl chain-rich domains increases with the side chain length. Alongside these results, a significant conductivity contribution was observed for all poly(tricyclononenes) with −Si(OR)3 side groups, which is interpreted in terms of a percolation model.zeige mehrzeige weniger

Volltext Dateien herunterladen

  • janus_poster.pdf
    eng

Metadaten exportieren

Weitere Dienste

Teilen auf Twitter Suche bei Google Scholar Anzahl der Zugriffe auf dieses Dokument
Metadaten
Autor*innen:Mohamed Aejaz KolmangadiORCiD
Koautor*innen:Paulina Szymoniak, Martin Böhning, Andreas Schönhals
Dokumenttyp:Posterpräsentation
Veröffentlichungsform:Präsentation
Sprache:Englisch
Jahr der Erstveröffentlichung:2021
Organisationseinheit der BAM:6 Materialchemie
6 Materialchemie / 6.6 Physik und chemische Analytik der Polymere
DDC-Klassifikation:Technik, Medizin, angewandte Wissenschaften / Ingenieurwissenschaften / Ingenieurwissenschaften und zugeordnete Tätigkeiten
Freie Schlagwörter:Conductivity; Dynamics; Glass transition
Themenfelder/Aktivitätsfelder der BAM:Material
Veranstaltung:DPG Online Spring Conference 2021
Veranstaltungsort:Online meeting
Beginndatum der Veranstaltung:22.03.2021
Enddatum der Veranstaltung:24.03.2021
Verfügbarkeit des Dokuments:Datei im Netzwerk der BAM verfügbar ("Closed Access")
Datum der Freischaltung:25.03.2021
Referierte Publikation:Nein
Einverstanden
Diese Webseite verwendet technisch erforderliche Session-Cookies. Durch die weitere Nutzung der Webseite stimmen Sie diesem zu. Unsere Datenschutzerklärung finden Sie hier.