Practical breakdown voltage calculations using dielectric breakdown strength reference values
- Dielectric breakdown is a catastrophic failure of ceramic substrates and insulators. The use of dielectric breakdown strength (DBS) reference values for the dimensioning of such components is not straightforward, as the DBS depends on sample thickness and electrode area. This fact also hampers a valid comparison of data taken from different literature sources. Based on the empirically confirmed proportionality of DBS to the reciprocal square root of sample thickness and an approach to account for the influence of electrode area on the failure probability, a practical equation is derived to calculate the breakdown voltage for arbitrary sample thickness and electrode area from one set of DBS reference data. To validate the equation, the AC DBS of commercial alumina substrates with thicknesses ranging from 0.3 mm to 1.0 mm was performed using different printed electrodes with varying areas. The breakdown voltages comprise a range from 18 kV for thick samples to 8.5 kV for thin samples,Dielectric breakdown is a catastrophic failure of ceramic substrates and insulators. The use of dielectric breakdown strength (DBS) reference values for the dimensioning of such components is not straightforward, as the DBS depends on sample thickness and electrode area. This fact also hampers a valid comparison of data taken from different literature sources. Based on the empirically confirmed proportionality of DBS to the reciprocal square root of sample thickness and an approach to account for the influence of electrode area on the failure probability, a practical equation is derived to calculate the breakdown voltage for arbitrary sample thickness and electrode area from one set of DBS reference data. To validate the equation, the AC DBS of commercial alumina substrates with thicknesses ranging from 0.3 mm to 1.0 mm was performed using different printed electrodes with varying areas. The breakdown voltages comprise a range from 18 kV for thick samples to 8.5 kV for thin samples, resulting in DBS values from 17 kV/mm for 1.0 mm thick samples to 29 kV/mm for 0.3 mm thin samples, all made from the same material. The influence of electrode area is comparatively smaller. The results calculated with the proposed equation are in reasonable accordance with the measured data. Thus, the equation can be applied for a proper comparison of literature DBS data measured in different setups and for a reasonable estimation of breakdown voltages in DBS tests and applications based on reference data.…
Autor*innen: | Björn MiellerORCiD |
---|---|
Dokumenttyp: | Vortrag |
Veröffentlichungsform: | Präsentation |
Sprache: | Englisch |
Jahr der Erstveröffentlichung: | 2020 |
Organisationseinheit der BAM: | 5 Werkstofftechnik |
5 Werkstofftechnik / 5.4 Multimateriale Fertigungsprozesse | |
Freie Schlagwörter: | Ceramics; Dielectric breakdown; Weibull distribution |
Themenfelder/Aktivitätsfelder der BAM: | Material |
Veranstaltung: | Electroceramics Conference XVII |
Veranstaltungsort: | Online meeting |
Beginndatum der Veranstaltung: | 24.08.2020 |
Enddatum der Veranstaltung: | 28.08.2020 |
Verfügbarkeit des Dokuments: | Datei im Netzwerk der BAM verfügbar ("Closed Access") |
Datum der Freischaltung: | 07.09.2020 |
Referierte Publikation: | Nein |
Eingeladener Vortrag: | Nein |