The chapter gives a brief introduction to (nano)compositecomposite materials having the focus on polymer-based nanocomposites. The different dimensionalities of nanoparticles are introduced, along with their distribution in the matrix.
Different application fields of polymer-based nanocomposites, like flame retardancy, filled rubbers, nanofilled thermosets and thermoplastics, separation membranes and nanodielectrics, are considered in greater detail.
Carbon nanomembranes are synthetic two-dimensional sheets with nanometer thickness, macroscopic lateral dimensions, and high structural homogeneity. They have great application potential in various branches of nanotechnology. Because of their full carbon structure, it is not clear whether macromolecules like poly(methyl methacrylate) (PMMA) can be irreversibly adsorbed on their surface. Here, irreversible adsorption means that the polymer chains cannot be removed by a leaching process, which is assumed in technological transfer processes. However, if polar defects are present on the carbon nanomembranes (CNMs), it may occur that polymers can be irreversibly adsorbed. To address this question, PMMA was spin-coated on top of CNMs, annealed for a specific time at different temperatures, and then tried to be removed by a acetone treatment in a leaching approach. The samples were investigated in detail by atomic force microscopy, X-ray photoelectron spectroscopy, and broadband dielectric spectroscopy, where the latter method has been applied to CNMs for the first time. Unambiguously, it was shown that PMMA can be adsorbed on the surface of CNMs after annealing the sample above the glasstransition temperature of PMMA. The general occurrence of polar defects on the surface of CNMs and the adsorption of polymers open opportunities for advanced innovative hybrid materials combining the properties of the CNM with those of the polymer.
Historically, to tune the properties of a polymer or more general soft matter systems by a second phase is not a new concept and dates back to the 40s of the last century. Beside some successes, the improvement of the properties remained somehow limited. The expectations of the enhancement of the properties of composites changed by the developments of Toyota Central research in the 1990s. It was shown that the incorporation of 5 vol% exfoliated layers of a clay system into a polymer leads to a strong improvement of the mechanical and thermal properties. This discovery stimulated a broad research interest of both fundamental and applied character. Today, polymer-based nanocomposites have reached a billion-dollar global market. The corresponding applications span from components for transportation, commodity plastics with enhanced barrier and/or flame retardancy characteristics, to polymers with electrical properties for shielding, electronics, sensors, and solar cells as well as to live science. Important fields are filled rubbers, reinforced thermoplastics, or thermosets for automotive, aircraft/space and marine industries, but also membranes for separation processes as well as barrier layers, just to mention a few.
For a variety of applications, the molecular mobility in nanocomposites is of great importance. This concerns the molecular mobility needed to form a percolating filler network in rubbers used in tires or in composites employed in electric shielding applications. In general, it is also essential for processing polymer-based nanocomposites. Furthermore, separation processes in composite materials for membranes require a certain molecular mobility. This also concern nanodielectrics used in electrical applications or sensors where the mobility of charge carriers can be related to the fluctuations of molecular groups etc. Finally, the molecular mobility can be taken as probe for structure on a molecular scale.
Broadband dielectric spectroscopy is a powerful tool to investigate the molecular mobility in polymer systems. It is due to the extremely broad frequency and sensitivity range that can be covered by this technique. Information about localized and cooperative molecular fluctuations, polarization effects at interfaces, as well as charge transport processes can be deduced. Therefore, this book focusses on broadband dielectric spectroscopy of composite materials. Moreover, the dielectric studies are accompanied by mechanical spectroscopy, advanced calorimetry, NMR techniques, as well as transmission electron microscopy and X-ray scattering investigations.
Besides a brief introduction to (nano)composites, the book aims to address fundamental aspects of the molecular mobility in this innovative group of materials. Selected examples with scientific interest and some cases with high industrial impact were chosen. Due to the breadth of the subject, unfortunately not all topics could be addressed in detail, such as processing for instance.
Berlin, Andreas Schönhals
July 2021 Paulina Szymoniak
Epoxy-Based Nanocomposites—What Can Be Learned from Dielectric and Calorimetric Investigations?
(2022)
Epoxy-based nanocomposites are promisingmaterials for industrial applications (i.e., aerospace, marine, and automotive industries) due to their extraordinary mechanical and thermal properties. Regardless of the broad field of applications, there is still a considerable need to identify their structure–property relationships. Here, a detailed dielectric and calorimetric (DSC and fast scanning calorimetry) study on different epoxy-based nanocomposites was performed. Bisphenol A diglycidyl ether (DGEBA) cured with diethylenetriamine (DETA) was employed as the polymeric matrix, which was reinforced with three diverse nanofillers that exhibit different interaction strengths with the epoxy matrix (halloysite nanotubes, surface modified halloysite nanotubes, and taurine-modified layered double hydroxide). The structure, molecular mobility, and vitrification behavior are discussed in detail, focusing on the intrinsic structural and dynamic heterogeneity, as well as interfacial properties.
An immobilization of graphene oxide (GO) into a matrix of polyvinyl formaldehyde (PVF) foam as an eco-friendly, low cost, superior, and easily recovered sorbent of Pb ions from an aqueous solution is described. The relationships between the structure and electrochemical properties of PVF/GO composite with implanted Pb ions are discussed for the first time. The number of alcohol groups decreased by 41% and 63% for PVF/GO and the PVF/GO/Pb composite, respectively, compared to pure PVF. This means that chemical bonds are formed between the Pb ions and the PVF/GO composite based on the OH groups. This bond formation causes an increase in the Tg values attributed to the formation of a strong surface complexation between adjacent layers of PVF/GO composite. The conductivity increases by about 2.8 orders of magnitude compared to the values of the PVF/GO/Pb composite compared to the PVF. This means the presence of Pb ions is the main factor for enhancing the conductivity where the conduction mechanism is changed from ionic for PVF to electronic conduction for PVF/GO and PVF/GO/Pb.
This paper presents the results concerning monotropic nematic liquid crystals 4-pentylphenyl 40-alkyl benzoate (5PnB) (n = 3 or 5 carbon atoms in the alkyl chain). Their mesophase properties were supported by images of the polarized optical microscopy. Molecular dynamics in the bulk samples or in the composites prepared with aerosil A380 was investigated by broadband dielectric spectroscopy in a large temperature range, appropriately chosen. Thermo gravimetric and infrared investigations were additionally performed. The data were compared with those of structurally related nematics like cyanophenyl pentyl benzoates, which have a cyan group instead of the pentyl chain. The dielectric spectra of the bulk 3P5B and 5P5B demonstrate a dielectric behavior with several relaxation processes as expected for nematic liquid crystals. The temperature dependence of the relaxation rates (and of the dielectric strength) seems to have two distinguished regimes. Thus, in the isotropic state, at higher temperatures the data obey the Vogel–Fulcher–Tammann law, whereas an Arrhenius law is fitted at lower temperature, in a close similarity to the behavior of a constrained dynamic glass transition. Samples with a high density of silica (larger than 7 g aerosil/1 g of 5PnB) were prepared to observe a thin layer adsorbed on the particle surface; it was estimated that almost each guest 5PnB molecule interacts with the aerosil surface. For the composites only one main relaxation process is observed at frequencies much lower than those for the corresponding bulk, which was assigned to the dynamics of the molecules in the surface layer. Infrared spectroscopy shows that these molecules interact with the surface by the ester carbonyl group leading to the monolayer self-assembly at liquid–solid interface. We note once more the importance of the functional unit(s) for the interaction with the hydroxyl groups on the aerosil surface.
Hexakis(n-alkyloxy)triphenylene) (HATn) consisting of an aromatic triphenylene core and alkyl side chains are model discotic liquid crystal (DLC) systems forming a columnar mesophase. In the mesophase, the molecules of HATn self-assemble in columns, which has one-dimensional high charge carrier mobility along the columns. Here, a homologous series of HATn with different length of the alkyl chain (n = 5,6,8,10,12) is investigated using differential scanning calorimetry (DSC), broadband dielectric spectroscopy (BDS) and advanced calorimetric techniques including fast scanning calorimetry (FSC) and specific heat spectroscopy (SHS). The investigation of the phase behavior was done utilizing DSC experiments and the influence of the alkyl chain length on the phase behavior was revealed. By the dielectric investigations probing the molecular mobility, a c-relaxation due to localized fluctuations as well as two glassy dynamics, the acore- and aalkyl-relaxation, were observed in the temperature range of the plastic crystalline phase. Moreover, the observed glassy dynamics were further studied employing advanced calorimetry. All observed relaxation processes are attributed to the possible specific molecular fluctuations and discussed in detail. From the results a transition at around n = 8 from a rigid constrained (n = 5,6) to a softer system (n = 10,12) was revealed with increasing alkyl chain length. A counterbalance of two competing effects of a polyethylene-like behavior of the alkyl chains in the intercolumnar domains and self-organized confinement is discussed in the context of a hindered glass transition.
Nowadays, sensors based on polymers/nanostructured metal oxide composites have been investigated exten-sively because of their sensitivity to NO2 gas at ambient temperature. In this work, nanocomposite membranes of xanthan gum (XG) with different contents of MnO2 nanoparticles were prepared as a potential NO2 gas sensor operating at room temperature by a simple one-step oxidation-reduction reaction. The structural, morphological, thermal, and electrical properties of the composite membrane were investigated. The FT-IR results confirm the successful preparation of MnO2 through the oxidation of XG by KMnO4 and reveal further the structural changes of the XG/MnO2 nanocomposite upon its exposure to NO2 gas. The capping of the synthesized MnO2 nano-particles by XG, the surface composition of the XG/MnO2 nanocomposite membranes, and the effect of NO2 gas on the surface composition was investigated using the XPS technique. The DC conductivity and dielectric loss of nanocomposites were higher than for neat XG. The conductivities of the nanocomposites XG/MO-4, XG/MO-4/ low NO2, and XG/MO-4/high NO2 composites are half, one, and three orders of magnitude higher than that for pure XG revealing a transition from insulating to conductive properties. The results demonstrated that XG/MnO2 nanocomposite membranes are promising for potential applications in NO2 gas sensing.
Polymers of intrinsic microporosity (PIMs) are promising candidates for the active layer in gas separation membranes due to their high permeability and reasonable permselectivity. These appealing properties originate from a microporous structure as a result of inefficient segment packing in the condensed state due to a combination of a ladder-like rigid backbone and sites of contortion. However, this class of polymers suffers from a significant decrease in the permeability with time due to physical aging, whereby typically, the permselectivity increases. The initial microporous structures approach a denser state via local rearrangements, leading to the reduction of the permeability. Hence, a detailed characterization of the molecular mobility in such materials can provide valuable information on physical aging. In this work, the dielectric behavior of PIM-1 films and their behavior upon heating (aging) were revisited by isothermal frequency scans during different heating/cooling cycles over a broad temperature range between 133 and 523 K (−140 to 250 °C). In addition, the obtained results were compared with data of samples that were annealed at ambient temperatures over different time scales. Multiple dielectric processes were observed: several relaxation processes due to local fluctuations and a Maxwell−Wagner−Sillars polarization effect related to the microporosity. The temperature dependence of the rates of all processes follows the Arrhenius law where the estimated activation energy depends on the nature of the process. The influence of the thermal history (aging) on the processes is discussed in detail.
We study the molecular mobility and electrical conductivity of a homologous series of linear shaped columnar ionic liquid crystals ILCn, (n = 8, 10, 12, 14, 16) using broadband dielectric spectroscopy (BDS), specific heat spectroscopy (SHS), and X-ray scattering. We aim to understand how the alkyl chain length influences the dynamics and electric conductivity in this system. Two dielectrically active relaxation modes are observed, the γ and the αcore process, that correspond to the localized fluctuations of the alkyl chains and cooperative motions of the aromatic core in the columns, respectively. Both the γ relaxation and the αcore process slow down with increasing alkyl chain length. SHS reveals one relaxation process, the αalkyl process that has a similar temperature dependence as that of the αcore process for ILC12, 14, and 16 but shifts to higher temperature for ILC8 and 10. For ILC12, 14, and 16, the absolute values of DC conductivity increase by 4 orders of magnitude at the transition from the plastic crystalline to hexagonal columnar phase. For ILC8 and 10, the DC conductivity behavior is similar to ionic liquids, where the conductivity is coupled with structural relaxation. Small-angle X-ray investigations reveal that both the intercolumnar distance and the disorder coherence length increase with alkyl chain length; conversely, the DC conductivity decreases monotonically.
Acrylic acid-styrene copolymer films were deposited plasma-chemically more gently using the pulsed plasma mode instead of the continuous mode, with linear and some slightly branched chains and marginal crosslinking.
Then, the styrene unit of copolymers was wet-chemically sulfonated by chlorosulfuric acid. On exposure to air, the formed 4-chlorosulfonic acid groups hydrolyze to sulfonic acid groups (-SO3H).
FTIR, XPS and broadband dielectric spectroscopy were employed to characterize the composition, the structure, the functional groups, and the electrochemical performance for the copolymers. A high concentration of sulfonic acid-containing groups was obtained in the sulfonated PS sample. The values of the DC conductivity DC for the sulfonated sample of the AA/S copolymer are ca. five orders of magnitude higher than that of the not-sulfonated copolymer materials.