7.5 Technische Eigenschaften von Polymerwerkstoffen
Filtern
Erscheinungsjahr
- 2022 (39) (entfernen)
Dokumenttyp
- Zeitschriftenartikel (18)
- Vortrag (15)
- Buchkapitel (3)
- Beitrag zu einem Tagungsband (1)
- Posterpräsentation (1)
- Forschungsbericht (1)
Schlagworte
- Elastomers (4)
- Flame retardancy (4)
- Graphene (4)
- Synergy (4)
- Brandschutz (3)
- Epoxy resin (3)
- Expandable graphite (3)
- High-density polyethylene (3)
- Nanocomposite (3)
- Nanocomposites (3)
Organisationseinheit der BAM
- 7 Bauwerkssicherheit (39)
- 7.5 Technische Eigenschaften von Polymerwerkstoffen (39)
- 6 Materialchemie (5)
- 5 Werkstofftechnik (4)
- 5.3 Polymere Verbundwerkstoffe (4)
- 6.6 Physik und chemische Analytik der Polymere (4)
- 6.5 Synthese und Streuverfahren nanostrukturierter Materialien (2)
- 7.3 Brandingenieurwesen (2)
- 3 Gefahrgutumschließungen; Energiespeicher (1)
- 3.1 Sicherheit von Gefahrgutverpackungen und Batterien (1)
Eingeladener Vortrag
- nein (15)
Im Rahmen des Forschungsprojektes IGF 20470N wurden Untersuchungen zum Alterungsverhalten von reaktiven Brandschutzsystemen (RBS) auf Stahlbauteilen durchgeführt. Mithilfe der Ergebnisse einer umfangreichen Literaturrecherche sowie experimentellen und numerischen Untersuchungen sollte ein Vorschlag für ein Prüfkonzept zum Nachweis einer Nutzungsdauer von RBS von mehr als 10 Jahren auf Basis von Kurzzeitversuchen abgeleitet werden. Dabei setzt die Bewertung des Alterungsverhaltens von RBS voraus, dass die Mechanismen der Alterung hinreichend bekannt sind.
Dafür wurden zunächst systematisch Daten von Kurz- und Langzeitversuchen von nationalen Zulassungsprüfungen der letzten Jahrzehnte ausgewertet. Anschließend wurden umfangreiche experimentelle Untersuchungen an einer wasserbasierten sowie einer epoxidharzbasierten Richtrezeptur durchgeführt. Da aus der Literatur bekannt ist, dass die Einflüsse der Bewitterung zu einer Veränderung der Konzentration der Bestandteile innerhalb der Beschichtung führen können, wurden Untersuchungen mit Mangelrezepturen durchgeführt, wobei systematisch einzelne Bestandteile reduziert wurden. Neben optischen Untersuchungen wurden thermoanalytische Verfahren (DSC-TG-, ATR-FTIR-, Elementar-, Farbanalyse) angewandt sowie Brandversuche an beschichteten Stahlplatten durchgeführt. Des Weiteren wurden die Richtrezepturen den beschleunigten Kurzzeitversuchen gemäß EAD 350402-00-1106 (2017) unterzogen, welche die Zulassung von Produkten auf europäischer Ebene regelt. Für die wasserbasierte Richtrezeptur wurden die Bewitterung für den feuchten Innenraum (Typ Z1) mehrfach wiederholt (1x, 3x, 6x). Für die epoxidharzbasierte Richtrezeptur entsprach die Bewitterung dem Zyklus für die Außenanwendung (Typ X). In Brandversuchen sowie thermoanalytischen und optischen Untersuchungen wurde das Alterungsverhalten sowie die thermische Schutzwirkung analysiert.
Anschließend wurden numerische Simulationen von Stahlbauteilen mit gealterten RBS durchgeführt und anhand der experimentellen Untersuchungen validiert. Mithilfe der numerischen Modelle kann eine Bewertung der thermischen Schutzwirkung von Stahlbauteilen mit gealterten RBS vorgenommen werden.
Mithilfe der gesammelten Erkenntnisse wurde ein Vorschlag für ein Prüfkonzept für den Nachweis einer Nutzungsdauer von mehr als 10 Jahren abgeleitet. Das Prüfkonzept besteht dabei aus einem Katalog von Möglichkeiten, die aktuellen Zulassungsprüfungen auf europäischer Ebene für eine Nutzungsdauer von 10 Jahren auf einen längeren Zeitraum zu erweitern.
Polyurethane foams (PUF) are generally flammable, so they are limited in some applications due to strict fire safety requirements. In this study, three distinct industrial benchmark polyurethane foams containing synergistic combinations of expandable graphite (EG) and phosphorous flame retardants (P-FR) were investigated one by one for their fire performance and smoke behavior. This paper aims to substantiate the hypothesis that the combination of EG and P-FR used in polyurethane foams yields a top-notch composite in terms of flame retardancy and smoke behavior by meeting the demanding requirement of low maximum average heat emission (MARHE) and smoke emission in a variety of applications, like advanced materials in construction, lightweight materials for railways, and more.
Leather is considered a luxury good when used in seating and upholstery. To improve safety, flame retardancy in leather is usually achieved through various finishing processes such as spray or roller coating. These treatments require processing steps that cost time and are laborintensive. One avenue to achieving flame retardancy in leather is to add flame retardants during the tanning process. However, the influence on flame retardancy exerted by specific intumescent additives specifically added during leather tanning has yet to be investigated. This work explores the roles played by intumescent additive compounds in flame retarding leather when they are added during tanning instead of applied as a coating. Via a systematic investigation of various compound mixtures, the flame retardant effects in the condensed and the gas phases are elucidated. The results show a strong impact of melamine in the gas phase and of polyphosphates in the condensed phase. Their impact was quantified in fire and smoke analysis, showing a 14% reduction in the peak of heat release rate, strongly reduced burning lengths, and a 20% reduction in total smoke release compared to nontreated leather. These results illuminate the key role played by specific compounds in the flame retardancy of leather, particularly when they are added specifically during the tanning process instead of being applied as a coating.
This method has great potential to reduce processing steps, lower costs, and improve material safety.
Reaktive Brandschutzsysteme finden im baulichen Brandschutz Anwendung zur Erhöhung des Feuerwiderstands von Stahlkonstruktionen. Neben den Anforderungen an die Feuerwiderstandsdauer können damit auch Ansprüche an die Ästhetik erfüllt werden. Die profilfolgende Applikation und die geringen Trockenschichtdicken der Produkte ermöglichen es, das filigrane Erscheinungsbild von Stahlkonstruktionen aufrechtzuerhalten. Neben der thermischen Schutzwirkung muss auch die Dauerhaftigkeit der Brandschutzbeschichtung sichergestellt werden. Die Bewertungsmethoden, die auf europäischer Ebene durch das EAD 350402-00-1106 zur Verfügung stehen, zielen auf eine Nutzungsdauer von zehn Jahren ab. Prüfverfahren für einen darüber hinausgehenden Zeitraum sind nicht beschrieben. In diesem Beitrag werden experimentelle Untersuchungen zum Einfluss der Bewitterung auf das Expansionsverhalten, zur thermischen Schutzwirkung und zu den während des Aufschäumens im Brandfall stattfindenden Reaktionen vorgestellt. Die Versuche wurden an einem wasserbasierten und einem epoxidharzbasierten reaktiven Brandschutzsystem durchgeführt. Die Ergebnisse wurden im Rahmen des IGF-Forschungsvorhabens 20470 N erzielt.
Composites in Fire and Flame
(2022)
Overview over the research results of the BAM in the field fire retardancy of composites. In different applications the flame retardancy of composites targets on different fire protection goals in the fire scenarios ignition, developing fire, and fully developed fire. Efficient solutions are tailored to pass a distinct fire test and to fit to a specific material. Flame inhibition as main flame retardancy mode of action combined with a minor mode of action in the condensed phase is general very efficient approach for composites. Alternatively residue design is demanded to achieve good results with only condensed phase mechanisms. Improving the fire stability asks for protective fire residues.
Investigation of the Thermal Stability of Proteinase K for the Melt Processing of Poly(L‑lactide)
(2022)
The enzymatic degradation of aliphatic polyesters offers unique opportunities for various use cases in materials science. Although evidently desirable, the implementation of enzymes in technical applications of polyesters is generally challenging due to the thermal lability of enzymes. To prospectively overcome this intrinsic limitation, we here explored the thermal stability of proteinase K at conditions applicable for polymer melt processing, given that this hydrolytic enzyme is well established for its ability to degrade poly(L-lactide) (PLLA). Using assorted spectroscopic methods and enzymatic assays, we investigated the effects of high temperatures on the structure and specific activity of proteinase K. Whereas in solution, irreversible unfolding occurred at temperatures above 75−80 °C, in the dry, bulk state, proteinase K withstood prolonged incubation at elevated temperatures. Unexpectedly little activity loss occurred during incubation at up to 130 °C, and intermediate levels of catalytic activity were preserved at up to 150 °C. The resistance of bulk proteinase K to thermal treatment was slightly enhanced by absorption into polyacrylamide (PAM) particles. Under these conditions, after 5 min at a temperature of 200 °C, which is required for the melt processing of PLLA, proteinase K was not completely denatured but retained around 2% enzymatic activity. Our findings reveal that the thermal processing of proteinase K in the dry state is principally feasible, but equally, they also identify needs and prospects for improvement. The experimental pipeline we establish for proteinase K analysis stands to benefit efforts directed to this end. More broadly, our work sheds light on enzymatically degradable polymers and the thermal processing of enzymes, which are of increasing economical and societal relevance.
Tailored crosslinking in elastomers is crucial for their technical applications. The incorporation of nanoparticles with high surface-to-volume ratios not only leads to the formation of physical networks and influences the ultimate performance of nanocomposites, but it also affects the chemical crosslinking reactions. The influence of few-layer graphene (FLG) on the crosslinking behavior of natural rubber is investigated. Four different curing systems, two sulfur-based with different accelerator-to-sulfur ratios, and two peroxide-based with different peroxide concentrations, are combined with different FLG contents. Using differential scanning calorimetry (DSC), vulcametry (MDR) and swelling measurements, the results show an accelerating effect of FLG on the kinetics of the sulfur-based curing systems, with an exothermic reaction peak in DSC shifted to lower temperatures and lower scorch and curing times in the MDR. While a higher accelerator-to-sulfur ratio in combination with FLG leads to reduced crosslinking densities, the peroxide crosslinkers are hardly affected by the presence of FLG. The good agreement of crosslink densities obtained from the swelling behavior confirms the suitability of vulcameter measurements for monitoring the complex vulcanization process of such nanocomposite systems in a simple and efficient way. The reinforcing effect of FLG shows the highest relative improvements in weakly crosslinked nanocomposites.
Überblick über den State-of-the-Art und aktuelle Trends mit den Schwerpunkten:
- nachwachsende Rohstoffe in flammgeschützten Polymerwerkstoffen (flammgeschützte Biopolymere und Biokomposite; biomass-basierte Flammschutzmittel, nachwachsende Hilfsstoffe aus Abfallströmen)
- Nachhaltigkeit und Flammschutz
- Konzepte von Analogie bis Out-of-the-Box.
Overview of the state of the art and current trends with the main topics:
- renewable sources in flame retardant polymers (flame retarded bio-polymers and biocomposites; bio-flame retardants, renewable adjuvants from industrial waste)
- flame retardancy meets sustainability
- concepts between analogy and out-of-the-box.
The fracture surface of slow and continuous crack propagation during environmental stress cracking of a semicrystalline polyethylene exhibits isotropic roughness exponents at the local scale but resolved across the macroscopic fracture surface a clear position dependence is found. The spatially resolved roughness exponent admits values in the range between 0.1 and 0.4, demonstrating nontrivial exponents in the small length-scale regime. Instead, they vary across the fracture surface according to the stress-state distribution, which suggests that the exponents are intimately linked to the locally dominating dissipation processes during craze cracking.
Especially now in times of the energy revolution, the demand for energy-efficient separation processes promotes the advancement of new high-performance materials for use as highly selective separation membranes. Polymers with intrinsic microporosity (PIMs) are of high interest in the field of gas separation membranes. Currently the application of PIMs for membrane technology is still restrained by their strong tendency to physical aging involving a significant loss of their good gas separation properties. Physical aging phenomenon is related to the molecular mobility of PIMs which was investigated by broadband dielectric spectroscopy (BDS) previously [1]. In this work, covalent phosphinine-based framework (Eto-CPSF) was used as a nanofiller (0-10 wt %) in a PIM-1 matrix to potentially enhance the gas transport properties and prevent physical aging. Since molecular mobility is a fundamental parameter determining gas transport as well as physical aging in such a material, our study includes dielectric investigations by BDS of pure PIM-1 and PIM-1/Eto-CPSF mixed matrix membranes to establish a correlation between molecular mobility and gas transport properties. In addition, gas permeability was determined by the time-lag method (0-10 bar pressure) at 35 °C for N2, O2, CH4 and CO2 for all MMMs.
The dielectric behavior of the polymeric films and their response upon heating were measured by isothermal frequency scans during different heating/cooling cycles in a broad temperature range up to 250 °C. Multiple dielectric processes following Arrhenius behavior were observed. Local fluctuations, Maxwell-Wagner-Sillars (MWS) polarization and structural relaxations were discussed correlating to structural-properties of PIM-1. As main result for MMMs, the permeability of PIM-1 for CH4 and CO2 gases were increased significantly with only 5 wt% of nanofiller within the polymer matrix. However, this is not observed for Eto-CPSF concentrations higher than ca. 7 wt% probably due to a microphase separated morphology of the nanocomposite system. Furthermore, the permselectivity of membranes for pair gases O2/N2 and CO2/N2 show enhancement up to a concentration of about 7 wt% Eto-CPSF filler.
Polymers of intrinsic microporosity (PIMs) are promising candidates for the active layer in gas separation membranes due to their high permeability and reasonable permselectivity. These appealing properties originate from a microporous structure as a result of inefficient segment packing in the condensed state due to a combination of a ladder-like rigid backbone and sites of contortion. However, this class of polymers suffers from a significant decrease in the permeability with time due to physical aging, whereby typically, the permselectivity increases. The initial microporous structures approach a denser state via local rearrangements, leading to the reduction of the permeability. Hence, a detailed characterization of the molecular mobility in such materials can provide valuable information on physical aging. In this work, the dielectric behavior of PIM-1 films and their behavior upon heating (aging) were revisited by isothermal frequency scans during different heating/cooling cycles over a broad temperature range between 133 and 523 K (−140 to 250 °C). In addition, the obtained results were compared with data of samples that were annealed at ambient temperatures over different time scales. Multiple dielectric processes were observed: several relaxation processes due to local fluctuations and a Maxwell−Wagner−Sillars polarization effect related to the microporosity. The temperature dependence of the rates of all processes follows the Arrhenius law where the estimated activation energy depends on the nature of the process. The influence of the thermal history (aging) on the processes is discussed in detail.
The phenomenon of environmental stress cracking is still a major issue in materials engineering as well as from a scientific perspective. Especially in the case of packaging materials made of high-density polyethylene, assessing the potential of premature damage due to environmental stress cracking is complex because of the large number of components in possible liquid filling goods. As a first guideline, the well-known effect of detergents and dispersants is usually considered, but the interplay with other components, such as organic solvents is often unknown. Particularly challenging in this respect are crop protection products, consisting of several different admixtures in addition to the biologically active ingredients. This study is based on two model liquids representing these admixtures that were established for testing in this context. The model liquids as well as their constituting components were used as liquid media in the Full Notch Creep Test to characterize the environmental stress cracking behavior of a typical high-density polyethylene. Complementary to the time-to failure of a notched specimen obtained from these tests, the crack opening was monitored optically, and the fracture surface was analyzed post-failure by laser scanning microscopy as well as scanning electron microscopy. Based on the results, the effect of various surfactants as well as the influence of organic solvents on environmental stress cracking are discussed.
Genormte künstliche Bewitterungstests sind häufig nicht spezifisch für die Anwendungssituation oder das Material. Das macht die Entwicklung spezifischer Tests erforderlich. Für deren Entwicklung müssen Maximalparameter der Anwendungssituation bekannt sein, womit dann der künstliche Test formuliert wird und dessen Bedingungen werden dann solange optimiert, bis die Korrelation der Effekte von natürlichem und künstlichem Test ausreichend ist.
Für Untersuchungen der Freisetzung kann der verbleibende Rest in der Probe und/oder die freigesetzte Menge in Luft, Boden, Wasser bestimmt werden.
Im ersten Beispiel der Witterungswirkung wurde die Freisetzung von Kohlenstoff-Nanoröhrchen (CNT) aus Polymer-Kompositen untersucht (unter Verwendung von empfindlich-nachweisbarer radioaktiver 14C-Markierung für einzelne CNT-Partikel), in einem zweiten die Freisetzung von anorganischen und organischen Bestandteilen aus elastomeren Bestandteilen von Sportböden (Bahnen und Kunstrasen) in Wasser.
The incorporation of nanoscale particles into elastomers enable a boost in performance and/or a distinct reduction of conventional filler loadings due to their high surface to volume ratio. 2D layered nanoparticles like graphene and graphene-related materials provide a great potential as effective fillers in rubber, especially by enhancing mechanical and barrier properties. The type and properties of the nanoparticles, their interface and the elastomeric matrix materials influence the technical behavior, and therefore the potential application fields of such rubber nanocomposites. Especially crucial for the efficiency of the nanofiller, however, is its best possible incorporation into the elastomer. The dispersing of nanoparticles without agglomerates usually constitutes a challenge when using conventional two-roll milling or internal mixing. Academic approaches for highly dispersed nanocomposites solve this problem but are often energy and time consuming with no feasible scale up possibility. Therefore, an ultrasonic assisted NR latex premixing process was established to produce highly filled masterbatches, enabling the main processing with conventional rubber processing techniques.
Two carbon-based nanoparticles with similar specific surface areas were investigated and incorporated in natural rubber as nanocomposites: A commercially available multilayer graphene (MLG) and a nanoscale carbon black (nCB). The mentioned premixed masterbatches were further processed to nanocomposites by the addition of matrix NR, two-roll milling, and hot pressing (vulcanization). By this procedure an increase in Young’s modulus of 157% (MLG) and 71% (nCB) could be obtained at a concentration level of 3 phr. As anisotropic material behavior was observable for the nanocomposites containing MLG, different measurement methods were investigated to quantify the orientation of the nanoparticles in the nanocomposites: Sorption measurements (swelling in 2 dimensions), hardness and dynamical mechanical analysis (in-plane vs. cross-plane), X-Ray diffraction and transmission and scanning electron microscopy.
A few layer/multilayer graphene (MLG) with a specific surface area of BET=250 m2/g is proposed as an efficient multifunctional nanofiller for rubbers. The preparation method, i.e., ultrasonically-assisted solution mixing of master batches followed by two-roll milling, strongly influences the dispersion in the elastomeric matrix and is fundamental for the final properties. When homogenously dispersed, single stacks of only approximately 10 graphene sheets, with an aspect ratio of 34, work at low loadings, enabling the replacement of large amounts of carbon black (CB), an increase in efficiency, and a reduction in filler load. The appropriate preparation yielded nanocomposites in which just 3 phr are sufficient to significantly improve the rheological, curing, gas barrier properties, electrical and thermal conductivity, as well as mechanical properties of different rubbers, as shown for chlorine-Isobutylene-Isoprene rubber (CIIR), nitrile-butadiene rubber (NBR), natural rubber (NR), and styrene-butadiene rubber (SBR). 3 phr of MLG tripled the Young’s modulus of CIIR, an effect equivalent to 20 phr of CB. The stronger interactions between MLG and NR or SBR also resulted in a reduction in the elongation at break by 20% and 50%, respectively, while the same parameter was hardly changed for CIIR/MLG and NBR/MLG. CIIR/MLG and NBR/MLG were stiffer but just as defomable than CIIR and NBR. The strong reinforcing effect of 3 phr MLG was confirmed by the increase of greater than 10 Shore A in hardness. MLG reduces gas permeability, increases thermal and electrical conductivities, and retards flammability, the latter shown by the reduction in heat release rate in the cone calorimeter. We investigated MLG also as a synergist for reducing the aluminium trihydrate loading in flame retardant hydrogenated acrylonitrile-butadiene (HNBR), polybutadiene chloroprene (BR/CR), and chlorosulfonated polyethylene rubber(CSM). The higher the nanofiller concentration is, the greater the improvement in the properties. For instance, the permeability decreased by 30% at 3 phr of MLG, 50% at 5 phr and 60% at 10 phr, respectively. Moreover, the MLG nanocomposites improve stability of mechanical properties against the effects of weathering. In key experiments an increase in UV-absorption and a pronounced radical scavenging were proved as stabilizing mechanisms. In a nutshell, MLG is an efficient multifunctional nanofiller ready to be used for innovative rubber development.
Due to the high flammability and smoke toxicity of polyurethane foams (PUFs) during burning, distinct efficient combinations of flame retardants are demanded to improve the fire safety of PUFs in practical applications. This feature article focuses on one of the most impressive halogen-free combinations in PUFs: expandable graphite (EG) and phosphorus-based flame retardants (P-FRs). The synergistic effect of EG and P-FRs mainly superimposes the two modes of action, charring and maintaining a thermally insulating residue morphology, to bring effective flame retardancy to PUFs. Specific interactions between EG and P-FRs, including the agglutination of the fire residue consisting of expanded-graphite worms, yields an outstanding synergistic effect, making this approach the latest champion to fulfill the demanding requirements for flame-retarded PUFs. Current and future topics such as the increasing use of renewable feedstock are also discussed in this article.
In the recent years, more and more products in construction and automotive industry are bonded by adhesive tapes instead of mechanical fasteners but there is no sufficient understanding of how these bonded, layered materials behave in fires. Our research project gives an insight of how adhesives and substrates interact with each other in different fire scenarios and how flame retardants function in pressure sensitive adhesive (PSA) tapes. A systematic investigation on the burning behavior of PSA tapes as free-standing films, as top layers on different substrates and as sandwich-like adhesive joints was performed. The burning behavior of free-standing PSA tapes and those used as a coating was significantly improved by using phosphorus-based flame retardants. Furthermore, it was shown that, depending on tape structure and substrate, the PSA tape can lower the fire risk by acting as an intermediate protection layer in bonded materials.
The crack propagation rate of environmental stress cracking was studied on high-density polyethylene compact tension specimens under static loading. Selected environmental liquids are distilled water, 2 wt% aqueous Arkopal N100 solution, and two model liquid mixtures, one based on solvents and one on detergents, representing stress cracking test liquids for commercial crop protection products. The different surface tensions and solubilities, which affect the energetic facilitation of void nucleation and craze development, are studied. Crack growth in surface-active media is strongly accelerated as the solvents induce plasticization, followed by strong blunting significantly retarding both crack initiation and crack propagation. The crack propagation rate for static load as a function of the stress intensity factor within all environments is found to follow the Paris–Erdogan law. Scanning electron micrographs of the fracture surface highlight more pronounced structures with both extensive degrees of plasticization and reduced crack propagation rate, addressing the distinct creep behavior of fibrils. Additionally, the limitations of linear elastic fracture mechanisms for visco-elastic polymers exposed to environmental liquids are discussed.
Emanating from developing flame retarded biocomposites, we have proposed renewable natural fibers (including keratin) taken from industrial waste as an authentic sustainable approach. More recently, we have investigated non-vegan flame retardant approaches. This paper loves to give you an insight into our ongoing projects on biogenic industrial wastes like leather, bone meal, and insects. Materials were characterized multi-methodically, flame retardant modes of action quantified, decomposition mechanism proposed, and synergisms explained. Considering the large quantities of leather waste (LW) in industrial-scale production, we underline LW as multifunctional bio-adjuvants. LW enhances the flame retardancy of poly(ethylene-vinyl acetate) (EVA) containing phosphorus flame retardants (P-FR). Products/by-products of the invertebrate and vertebrate farming, respectively, are promising bio-based adjuvants in flame retarded bio-epoxy thermosets. While the addition of bone meal yields the formation of an inorganic shield, protein-based powders from insects provide an intumescent behavior. In combination with a P-FR superior charring and self-extinguishing are obtained.
Acknowledgement: In part of this work was supported by the Volkswagen Foundation grant “Experiment!” No. 97437.
In a laboratory test, transparent high‐density polyethylene (HDPE) jerrycans have been exposed to both UV radiation and 55 wt‐% nitric acid solution at (41 ± 2)°C, for up to 20 days. For comparison, UV radiant exposure (21 days) and nitric acid exposure (up to 6 weeks) were performed separately, at nearly equal temperatures. The damages are compared with FTIR spectroscopy in ATR and HT‐gel permeation chromatography(GPC) on a molecular level and with hydraulic internal pressure testing as a component test. For the used jerrycans, relevant oxidation can only be found after the combined exposure. This is caused by the decomposition of nitric acid into nitrous gases by UV radiation, which is also observed at lower concentrations (28 wt‐%). After 6 days of laboratory exposure, this is rated as critical, which corresponds to about 1/10 year in Central Europe, according to the UV radiant exposure. The gradual increase in oxidative damage shows the reproducibility of the test.
Renewable alternatives for common thermoset resins are demanded to go for sustainability. The objective is to create a flame retarded epoxy resin from a commercial bio epoxy resin with halogen free inorganic and organic flame retardants, respectively. Alumina trihydrate, aluminum diethyl phosphinate, a DOPO-based phosphonamidate and ammonium polyphosphate seem to have promising performances. Properties are enhanced with different bio fillers: pyrolyzed cocoa shells and plant waste (provided by Otto A. Müller Recycling GmbH, thanks!), short fibers and nonwovens of the natural fiber kenaf, hydroxypropyl-ß-cyclodextrin and sulfobutylether-ß-cyclodextrin.
Fire performance is investigated by cone calorimeter examinations, LOI and UL-94 ratings. Thermal analysis is given by TG-FTIR and DSC measurements.
Combinations of flame retardants and bio-fillers lead to reduced PHRR and THR, reach V0 in UL-94 and have a significant increase in LOI of up to 37 vol.-%. 10 % ammonium polyphosphate with 10 % pyrolyzed cocoa shell performs best, builds a magnificent protective layer, and shows good intumescence.
Material solutions that meet both circular bioeconomy policies and high technical requirements have become a matter of particular interest. In this work, a prospectively abundant proteinrich waste resource for the manufacturing of flame-retardant epoxy biocomposites, as well as for the synthesis of biobased flame retardants or adjuvants, is introduced. Different biomass fillers sourced from the cultivation of the mealworm beetle Tenebrio molitor are embedded in a bioepoxy resin cured with tannic acid and investigated regarding the fire performance of the thermosets. By means of spectroscopic and thermal analysis (attenuated total reflectance FTIR spectroscopy, thermogravimetric analysis-coupled FTIR spectroscopy, and differential scanning calorimetry), the influence of the biomass microparticles on the curing and thermal degradation behavior is evaluated. The final performance of the biocomposites is assessed based on fire testing methodology (limited oxygen index, UL-94, and cone calorimetry). Providing a high charring efficiency in the specific tannic acid-based epoxy matrix, the protein-rich adult beetle is further investigated in combination with commercial environmentally benign flame retardants in view of its potential as an adjuvant. The results highlight a char forming effect of nonvegan fillers in the presence of tannic acid, particularly during thermal decomposition, and point toward the potential of protein-based flame retardants from industrial insect rearing for future formulations.
Brände zerstören immer wieder wichtige Kulturgüter und gefährden nationales Kulturerbe. Das Projekt BRAWA erarbeitet neue Strategien und innovative Technologien, um die Brandsicherheit historischer Gebäude zu erhöhen. Dabei basiert das Konzept auf der Vernetzung von Sensoren, die bereits beim Auftreten bestimmter Gase in der Frühphase der Brandentstehung Alarm auslösen. Durch ein neuartiges Helferkonzept soll eine frühe Branderkennung und -bekämpfung ermöglicht werden.
2D layered nanoparticles enable a distinct reduction of filler loadings in rubber compounds combined with a boost in performance due to their high surface to volume ratio. They often enable unique property profiles providing a great potential as effective fillers in rubber, especially by enhancing mechanical and barrier properties.
As the best possible incorporation into the elastomer matrix is crucial for the efficiency of the nanofiller, dispersing and exfoliation of the nanoparticles without formation of agglomerates usually constitutes an outstanding challenge - especially when using conventional processing methods. Laboratory-scale approaches for highly dispersed nanocomposites sometimes solve this problem, but these are often too energy and time consuming and provide no scale up possibility for real applications. Therefore, a latex premixing process was established to produce highly filled masterbatches, enabling the processing with conventional techniques.
The presence of nanoparticles greatly impacts the behavior of elastomeric compounds, besides affecting the properties of the final product also the processing is influenced (rheology, crosslinking).
In this study, nanocomposites of natural rubber and multilayer graphene (MLG) were prepared via a latex masterbatch route. Different strategies for masterbatch premixing are compared (stirring vs. ultrasonication, coagulation vs. drying). Dispersion and exfoliation of MLG were determined by transmission electron microscopy. The reinforcing effect of MLG affects the viscosity while the dispersed graphene layers may also act as diffusion barrier/absorbent for the crosslinking agents. In contrast to that, MLG forms physical crosslinks in the final product. Swelling measurements and differential scanning calorimetry allow a differentiation between chemical and physical network links. Different technical properties of the nanocomposites were measured with respect to mechanical and application relevant behavior.
Das langsame Risswachstum (slow crack growth, SCG) sowie der umgebungsbedingte Spannungsriss (environmental stress cracking, ESC) sind relevante Schädigungsmechanismen für teilkristalline Werkstoffe auf Basis von Polyethylen hoher Dichte (PE-HD).
Der Vortrag gibt einerseits einen Überblick über die grundlegenden Struktur-Eigenschafts-Beziehungen in diesem Kontext, andererseits werden auch verschiedene praxisorientierte Prüfverfahren vorgestellt. Letztere wurden in gemeinsamen Forschungsprojekten von BAM und LBF mit dem Schwerpunkt Gefahrgutbehälter bzw. Pflanzenschutzmittel vergleichend untersucht und durch weitergehende Analytik ergänzt.
The chapter gives a brief introduction to (nano)compositecomposite materials having the focus on polymer-based nanocomposites. The different dimensionalities of nanoparticles are introduced, along with their distribution in the matrix.
Different application fields of polymer-based nanocomposites, like flame retardancy, filled rubbers, nanofilled thermosets and thermoplastics, separation membranes and nanodielectrics, are considered in greater detail.
Brandschutz
(2022)
In den letzten Jahrzehnten wurde die Degradation der polymeren Matrix von flammgeschützten Polymeren eingehend untersucht. Erst in den letzten Jahren jedoch hat sich die Frage der Lebensdauer der Funktionalität des Flammschutzes selbst als wichtige Fragestellung herauskristallisiert, z.B. bei Kabeln. Deshalb sollte diese Fragestellung durch systematisch-variierte künstliche Klima- und Bewitterungstests an flammgeschützten Polymerwerkstoffen untersucht werden
In den letzten Jahrzehnten wurde die Degradation der polymeren Matrix von flammgeschützten Polymeren eingehend untersucht. Erst in den letzten Jahren jedoch hat sich die Frage der Lebensdauer der Funktionalität des Flammschutzes selbst als wichtige Fragestellung herauskristallisiert, z.B. bei Kabeln. Deshalb sollte diese Fragestellung durch systematisch-variierte künstliche Klima- und Bewitterungstests an flammgeschützten Polymerwerkstoffen untersucht werden.
Valorizing “non-vegan” bio-fillers: Synergists for phosphorus flame retardants in epoxy resins
(2022)
Sustainable, biogenic flame retardant adjuvants for epoxy resins are receiving increased focus. Zoological products like insects, bone meal, and eggshells are available in large quantities, but remain uninvestigated as functional fillers to epoxy resins, although they are potential synergists to flame retardants. The efficacy and flame retardancy of “non-vegan” additives in combination with flame retardants is investigated and the fire behavior and thermal decomposition of bio-sourced epoxy resin composites is characterized. By comparing the fire performance of composites containing flame retardants or fillers at varying loadings (5, 10, and 20%), their role as synergists that enhance the function of organophosphorus flame retardants in bio-epoxy composites is identified and quantified. Peak heat release rates were 44% lower in composites containing both filler and flame retardant versus those containing only flame retardants, and fire loads were reduced by 44% versus the pure resin, highlighting the ability of “non-vegan” fillers to function as synergists.
The important take home message of this chapter: When multicomponent flame retardant systems are applied to polymeric materials, it becomes possible to address multiple fire properties, increase efficiency, and minimize flame retardant use to maximize polymer property balance. Flame retardants are combined or used together with adjuvants or synergists; fibers and fillers make a crucial contribution to their fire properties. Multicomponent systems are discussed in their capacity as an overall powerful strategy for achieving and optimizing non-halogenated flame-retardant polymeric materials.
The valorization of macroalgae digestate as a secondary resource for high value chemicals and nutrients will promote the sustainability and circularity of anaerobic digestion based biorefinery. In this study, three digestates from A. nodosum C.linum and L. digitata were separated into liquid and solid fractions to investigate the production of high value added chemicals through pyrolysis using Pyrolysis Gas Chromatography Mass Spectroscopy (Py-GC/MS) while the filtered liquid fractions were tested as an alternative culture media to grow C. sorokiniana under mixotrophic conditions. The digestates showed different thermal degradation and an improvement of bio-oil profiles compared to the starter material. Pyrolyzates from raw macroalgae were characterized by a high anhydrosugar content in contrast to high aromatics observed in the case of their digestates. Toluene, benzofuran and vinylphenol, base chemicals for many industries, represented together 30–37% of the total chemicals produced during pyrolysis of the three macroalgae digestate. On the other hand, C. sorokiniana cultured on digestate-based media showed a higher lipid content with an increase in monounsaturated fatty acids and a lower poly-unsaturated fatty acid content in comparison to microalgae grown in standard tris-acetate-phosphate media. Thus, the acyl composition was shifted in a direction more suitable for biodiesel production by this process. In addition, the increase of Chemical Oxygen Demand and Volatile Fatty Acids concentration in the digestate was found to reduce ammonium toxicity. Finally, 94% of Chemical Oxygen Demand and 83% of ammonium were removed by microalgae from the digestate-based media which will reduce the pollution risk of the biorefinery. Overall, the results indicate that using macroalgae solid digestates can generate improvements in the quality of
products obtained by pyrolysis and the liquid digestate can positively influence microalgae growth and its products.
The incorporation of nanoparticles like multilayer graphene (MLG) into elastomeric composites boosts their technical performance, such as their mechanical behavior and electrical conductivity. Common filler types (carbon black (CB) and aluminum trihydroxide (ATH)) generally fulfill single, specific purposes and are often used in high loadings. CB typically reinforces rubber mechanically, while ATH increases flame retardancy. Small amounts of MLG reduce these high filler contents and maintain the multifunctional characteristics of rubber composites. In chlorosulfonated polyethylene (CSM) + ATH, an intrinsically flame-retardant rubber was designed to achieve the highest standards such as maximum average of heat emission (MARHE) <90 kW m−2, 3 phrMLG was substituted for 15 phr CB and/or 3 phr ATH via an industrially applicable processing approach. Replacing either CB or ATH resulted in a property profile that was multifunctionally improved in terms of features such as mechanical performance, reduced sorption, and flame retardance. MLG nanocomposites are reported to show promise as an industrially utilizable route to obtain multifunctional high-performance rubbers.
We report dielectric and calorimetric studies on metathesis and addition-type polytricyclononenes, both based on the same monomer bearing three pendant OSiMe3 groups. For the addition-type polymer, dielectric spectroscopy reveals a β*-process related to the microporosity, whereas for its metathesis counterpart, the segmental dynamics manifests as an α-process related to a glass transition. Besides active dielectric processes, a significant conductivity contribution is detected for both samples which for the microporous additiontype polymer is three orders of magnitude greater than for the metathesis polymer. The broadband dielectric spectroscopy is complemented by detailed calorimetric investigations, comprising DSC, FSC, and TMDSC. The calorimetric methods detected the glass transition for the metathesis polymer in agreement with the observed dielectric α-process. Furthermore, the already reported gas transport properties for both polymers are compared, setting them in correlation with the observed molecular mobility and conductivity behavior. The discussed results reflect significant differences in molecular mobility of the two polymers affecting the appearance of microporosity which strongly determines the gas transport properties.
Simulation of the burning and dripping cables in fire using the particle finite element method
(2022)
The behavior of the cable jacket in fire characterized by the tendency to melt and drip constitutes a major source of fire hazard. The reason is that the melted material may convey the flame from one point to another, expanding fire and contributing to the fire load. In this article, the capability of a new computational strategy based on the particle finite element method for simulating a bench-scale cables burning test is analyzed. The use bench-scale test has been previously used to simulate the full-scale test described in EN 50399. As the air effect is neglected, a simple combustion model is included. The samples selected are two cables consisting of a copper core and differently flame retarded thermoplastic polyurethane sheets. The key modeling parameters were determined from different literature sources as well as experimentally. During the experiment, the specimen was burned under the test set-up condition recording the process and measuring the temperature evolution by means of three thermocouples. Next, the test was reproduced numerically and compared with a real fire test. The numerical results show that the particle finite element method can accurately predict the evolution of the temperature and the melting of the jacket.
A systematic series of flexible polyurethane foams (FPUF) with different concentrations of flame retardants, bis([dimethoxyphosphoryl]methyl) phenyl phosphate (BDMPP), and melamine (MA) or expandable graphite (EG) was prepared. The mechanical properties of the FPUFs were evaluated by a universal testing machine. The pyrolysis behaviors and the evolved gas analysis were done by thermogravimetric analysis (TGA) and TGA coupled with Fourier-transform infrared (TG-FTIR), respectively. The fire behaviors were studied by limiting oxygen index (LOI), UL 94 test for horizontal burning of cellular materials (UL 94 HBF), and cone calorimeter measurement. Scanning electronic microscopy (SEM) was used to examine the cellular structure's morphology and the postfire char residue of the FPUFs. LOI and UL 94 HBF tests of all the flame retarded samples show improved flame retardancy. BDMPP plays an essential role in the gas phase because it significantly reduces the effective heat of combustion (EHC). This study highlights the synergistic effect caused by the combination of BDMPP and EG. The measured char yield from TGA is greater than the sum of individual effects. No dripping phenomenon occurs during burning for FPUF-BDMPP-EGs, as demonstrated by the result of the UL 94 HBF test. EG performs excellently on smoke suppression during burning, as evident in the result of the cone calorimeter test. MA reduces the peak heat release rate (pHRR) significantly. The synergistic effect of the combination of BDMPP and EG as well as MA offers an approach to enhance flame retardancy and smoke suppression.