Filtern
Erscheinungsjahr
Dokumenttyp
Sprache
- Englisch (35)
- Deutsch (3)
- Mehrsprachig (1)
Schlagworte
- Weathering (39) (entfernen)
Organisationseinheit der BAM
On the basis of a lot of investigation on the spectral sensitivity of photo degradation of plastics and on the underestimated influence of temperature and relative humidity on degradation processes a new type of weathering device was presented at the end of the seventies:
It was a combination of a radiation source with fluorescent UV lamps and a precise climatic cabinet.
The radiation emission from a combination of four different types of fluorescent UV lamps was superimposed on the specimen surfaces in the climatic cabinet to match the UV part of solar radiation as closely as possible. Air temperature was controlled to within ± 1 °C, and relative humidity to within ± 5 %RH.
As the lamps’ emission is focussed on the UV range almost no radiation heating of the sample occurs. Therefore, the temperature of the sample, which is the quantity of consideration for the degradation, is nearly identical with the chamber’s air temperature, which is the quantity to be controlled. Also, therefore, high humidity can be obtained on the sample surface. The limitation of the emission to the UV range is sufficient for the study of the polymer matrix.
This type of weathering device offers an exactness of microclimatic control of the sample’s surface, which should be a standard for weathering devices. Even now it is the only weathering device which generates pure relative humidity (without aerosol).
A systematic approach was used to investigate the weathering-induced degradation of a common water–based intumescent coating. In this study, the coatings are intended for humid indoor applications on steel substrates. The coating contains ammonium polyphosphate, pentaerythritol, melamine, and polyvinyl acetate. By replacing each ingredient with a less water-soluble substance, the most vulnerable substances, polyvinyl acetate and pentaerythritol, were identified. Furthermore, the weathering resistance of the system was improved by exchanging the ingredients. The coatings were stressed by artificial weathering tests and evaluated by fire tests. Thermogravimetry and Fourier-transform infrared spectroscopy were used to study the thermal decomposition. This study lays the foundation for the development of a new generation of water-based intumescent coatings.
A new irradiation device for the exposure of plastic products is presented. Developed in the BAM division 3.1 "Dangerous Goods Packaging" it can be used for artificial UV irradiation of plastic Containers filled with hazardous liquids.
Present regulations and tests only investigate the exposure effects of UV and of media separately, but as the damaging effect is expected to be synergistic for at least some media, a combined test was looked for.
A chamber of 60 cm by 60 cm base area and 1 m height gives space for up to 40 cm wide objects. Two fluorescent UV lamp arrays are arranged on opposite walls, separated from the chamber by quartz glass panes. By continuously rotating the exposure object by means of a rotary disc that the object is placed on, spatial irradiation homogeneity is achieved over the exposure duration. The spectral irradiance of the chosen UVA 340 nm lamps gives the best match of global solar radiation in the short wavelength ränge. The close arrangement of the UVA lamps (15 each side) results in 60 W m'2 UV irradiance.
Constant temperature is adjusted to typically 40 °C by the control of the fan speed. This temperature is chosen, as it is the required temperature for three week storage of filled polyethylene Containers, for proving Chemical compatibility in the field of dangerous goods. To ensure homogeneity, an interiorfan provides for air circulation.
Chemiluminescence for the early detection of weathering effects of coatings - Part I: Fundamentals
(2010)
Combined impact of ultraviolet and chemical fluids on high-density polyethylene packaging material
(2012)
To investigate the ageing behaviour of filled plastic containers outdoors, square cuts of the wall of two high-density polyethylene (HDPE) types were exposed to ultraviolet (UV) radiation at their front side and to specific liquid chemicals (de-ionized water, surfactant or White Spirit) at their back. The UV radiant exposure at the front side was 80 MJ/m².
To compare the actions of the different exposures, separate dark backside fluid exposures were performed, in parallel. Besides, UV weathering was carried out until a UV radiant exposure of 325 MJ/m², being roughly comparable to outdoor exposure of one year in Northern Australia.
An unpigmented HDPE included in the investigation gave no sufficient protection for the White Spirit. In addition, it showed clear degradation after several of these exposures. In combination with the White Spirit, an increase of carbonyl bonds was measured, presumably assignable to degradation products of the White Spirit.
For a pigmented HDPE material, with the implemented combined exposures, no relevant damage was observed, within applied the exposure period.