Degradation effects of automotive coatings after weathering as detected by thermoluminescence
(2004)
A systematic approach was used to investigate the weathering-induced degradation of a common water–based intumescent coating. In this study, the coatings are intended for humid indoor applications on steel substrates. The coating contains ammonium polyphosphate, pentaerythritol, melamine, and polyvinyl acetate. By replacing each ingredient with a less water-soluble substance, the most vulnerable substances, polyvinyl acetate and pentaerythritol, were identified. Furthermore, the weathering resistance of the system was improved by exchanging the ingredients. The coatings were stressed by artificial weathering tests and evaluated by fire tests. Thermogravimetry and Fourier-transform infrared spectroscopy were used to study the thermal decomposition. This study lays the foundation for the development of a new generation of water-based intumescent coatings.
We report the selective ring opening copolymerisation (ROCOP) of
oxetane and phthalic thioanhydride by a heterobimetallic Cr(III)K
catalyst precisely yielding semi-crystalline alternating poly(esteralt-
thioesters) which show improved degradability due to the
thioester links in the polymer backbone.
Combined impact of ultraviolet and chemical fluids on high-density polyethylene packaging material
(2012)
To investigate the ageing behaviour of filled plastic containers outdoors, square cuts of the wall of two high-density polyethylene (HDPE) types were exposed to ultraviolet (UV) radiation at their front side and to specific liquid chemicals (de-ionized water, surfactant or White Spirit) at their back. The UV radiant exposure at the front side was 80 MJ/m².
To compare the actions of the different exposures, separate dark backside fluid exposures were performed, in parallel. Besides, UV weathering was carried out until a UV radiant exposure of 325 MJ/m², being roughly comparable to outdoor exposure of one year in Northern Australia.
An unpigmented HDPE included in the investigation gave no sufficient protection for the White Spirit. In addition, it showed clear degradation after several of these exposures. In combination with the White Spirit, an increase of carbonyl bonds was measured, presumably assignable to degradation products of the White Spirit.
For a pigmented HDPE material, with the implemented combined exposures, no relevant damage was observed, within applied the exposure period.
Jerrycans made from three different types of high-density polyethylene (HDPE) were exposed outdoors, for one Berlin summer season. They were filled with a 55 percent nitric acid solution (HN03), pure water, or air, and half of them were protected from sunlight by an UV absorbing canvas. Thus, the separate effects of UV radiation and nitric acid could be compared to the combined impact. Combined impact was mainly affected by decomposition of nitric acid, resulting in presence of reactive nitrogen oxides, increased oxygen partial pressure, and UV radiation energy, simultaneously in vapour phase.
To investigate the degradation effects after the outdoor exposure, jerrycans were exposed to a so called hydraulic internal pressure test, similar to an approval test for dangerous goods packaging. After combined impact of UV radiation and nitric acid, internal pressure tests showed very fast failures, whereas after separate impacts no remarkable deteriorations were observed, compared to unaged jerrycans.
A new irradiation device for the exposure of plastic products is presented. Developed in the BAM division 3.1 "Dangerous Goods Packaging" it can be used for artificial UV irradiation of plastic Containers filled with hazardous liquids.
Present regulations and tests only investigate the exposure effects of UV and of media separately, but as the damaging effect is expected to be synergistic for at least some media, a combined test was looked for.
A chamber of 60 cm by 60 cm base area and 1 m height gives space for up to 40 cm wide objects. Two fluorescent UV lamp arrays are arranged on opposite walls, separated from the chamber by quartz glass panes. By continuously rotating the exposure object by means of a rotary disc that the object is placed on, spatial irradiation homogeneity is achieved over the exposure duration. The spectral irradiance of the chosen UVA 340 nm lamps gives the best match of global solar radiation in the short wavelength ränge. The close arrangement of the UVA lamps (15 each side) results in 60 W m'2 UV irradiance.
Constant temperature is adjusted to typically 40 °C by the control of the fan speed. This temperature is chosen, as it is the required temperature for three week storage of filled polyethylene Containers, for proving Chemical compatibility in the field of dangerous goods. To ensure homogeneity, an interiorfan provides for air circulation.
To determine a polymer’s spectral response of photo degradation, two main methods have been established. The so-called “filter technique” uses polychromatic radiation, which is filtered by a set of various sharp cut-on filters. This procedure provides separated reading points of an activation spectrum of the investigated material. With the "spectrographic technique” a specimen is irradiated with pectrally dispersed radiation, locally quasi monochromatically, and the local property changes.are related to the radiant exposure at the respective wavelengths. A third method, the irradiation of specimens with quasi monochromatic radiation behind interference filters, is rarely used.
These methods have advantages and disadvantages and therefore, there are limits for conclusions from these spectral data. Concerning the quasi monochromatic Irradiation of specimens the development of new UV radiation sources looks promising.
With the rapid development of inexpensive UV Light-emitting diodes (LEDs), new : sources of nearly monochromatic radiation in the UV ränge are available, even down to about 250 nm. To determine the spectral response, the use of such UV-LEDs in TO-18 ) and TO-39 metal cases combines the advantages of low cost and energy efficiency, stable spectral irradiance, temperature.and humidity control, larger specimen areas, and an easy and stable analysis.
Combinations of different UV LEDs are also discussed as replacement for xenon arc ' radiation sources, see patent application EP01528388A1.
For polypropylene of varied stabilization, spectral sensitivity as well as temperature dependence of irradiation caused crack formation was determined in artificial irradiation tests. UV radiant exposure HUV necessary to generate crack formation was measured both in spectrally dispersed irradiation and artificial irradiation in a Fluorescent UV lamp device. Dependencies were fitted to a plateau function and an Arrhenius function, respectively, to describe the action of irradiation by response functions. Applied to weather data from Phoenix, the results were compared with respective outdoor exposure results.
Exposure response function for a quantitative prediction of weathering caused aging of polyethylene
(2019)
The exposure response function of the carbonyl formation over the bulk has been determined for a high-density polyethylene of a thickness of 200 μm, which was used as a weathering reference material according to ISO TR 19032. To this end, spectral sensitivity was studied by local measurement of the effect of spectrally dispersed irradiation. Both the exposure device and the methodology of determination are described.
The temperature dependency of photooxidation was determined by UV exposure at various temperatures between 23 and 80 °C. Deviations from linearity and thus reciprocity below 40 °C are discussed and assumed to be related to diffusion limitations. An Arrhenius approach –based on data of linear carbonyl formation – has been incorporated into the exposure response function. Using this exposure response function, aging in terms of the distribution of a quantitative property change over a plastic component can be predicted for a specific outdoor location with real chronologic weather data as input for the exposure. Thus, artificial and natural weathering can be linked and compared. The established exposure response function has been validated by outdoor exposure results from the literature. If an estimated diffusion limitation is taken into consideration, calculations and published data are in good agreement.
Weathering reference materials (WRMs) are used to characterize the harshness of an exposure, aiming on either reproducibility of a specific exposure or on the comparability between various kinds of natural or artificial weathering exposure.
The materials that are used as weathering reference materials differ in their sensitivities (as well as in interactions and interferences of the latter), conditioned by the different processes which lead to the respective property change. It is also essential to take into account the necessary measurement equipment for the respective property change, in order to allow timely intervention.
What are the key issues on choosing a weathering reference material?
What can be learned from the weathering reference materials, investigated so far?
Possibilities and limitations are discussed on the basis of existing weathering reference materials. Conclusions are drawn, for establishing new weathering reference materials.