The fluorescence quantum yield (QY) of CdSe dot/CdS rod (DR) nanoparticle ensembles is dependent on the Shell growth and excitation wavelength. We analyze the origin of this dependency by comparing the optical properties of DR ensembles to the results obtained in single-particle experiments. On the Ensemble level, we find that the QY of DRs with shell lengths shorter than 40 nm exhibits no dependence on the excitation wavelength, whereas for DRs with shell lengths longer than 50 nm, the QY significantly decreases for excitation above the CdS band gap. Upon excitation in the CdSe core, the ensemble QY, the fluorescence wavelength, and the fluorescence blinking behavior of individual particles are only dependent on the radial CdS shell thickness and not on the CDs shell length. If the photogenerated excitons can reach the CdSe core region, the fluorescence properties will be dependent only on the surface passivation in close vicinity to the CdSe core. The change in QY upon excitation above the band gap of CdS for longer DRs cannot be explained by nonradiative particles because the ratio of emitting DRs is found to be independent of the DR length. We propose a model after which the decrease in QY for longer CdS shells is due to an increasing fraction of nonradiative exciton recombination within the elongated shell. This is supported by an effective-mass-approximation-based calculation, which suggests an optimum length of DRs of about 40 nm, to combine the benefit of high CdS absorption cross section with a high fluorescence QY.
We assessed the influence of Yb3+ and Er3+ dopant concentration on the relative spectral distribution, quantum yield ( UC), and decay kinetics of the upconversion luminescence (UCL) and particle brightness (BUC) for similarly sized (33 nm) oleate-capped -NaYF4:Yb3+,Er3+ upconversion (UC) nanoparticles (UCNPs) in toluene at broadly varied excitation power densities (P). This included an Yb3+ series where the Yb3+ concentration was varied between 11%–21% for a constant Er3+ concentration of 3%, and an Er3+ series, where the Er3+ concentration was varied between 1%–4% for a constant Yb3+ concentration of 14%. The results were fitted with a coupled rate equation model utilizing the UCL data and decay kinetics of the green and red Er3+ emission and the Yb3+ luminescence at 980 nm. An increasing Yb3+ concentration favors a pronounced triphotonic population of 4F9/2 at high P by an enhanced back energy transfer (BET) from the 4G11/2 level. Simultaneously, the Yb3+-controlled UCNPs absorption cross section overcompensates for the reduction in UC with increasing Yb3+ concentration at high P, resulting in an increase in BUC. Additionally, our results show that an increase in Yb3+ and a decrease in Er3+ concentration enhance the color tuning range by P. These findings will pave the road to a deeper understanding of the energy transfer processes and their contribution to efficient UCL, as well as still debated trends in green-to-red intensity ratios of UCNPs at different P.
Applications of luminescent nanomaterials like semiconductor nanocrystals (QDs) and lanthanide-based upconversion nanocrystals (UCNPs) in the life sciences such as bioimaging studies or their use as reporter in assays call for a correlation of the photoluminescence (PL) properties of these nanomaterials on ensemble and single particle levels. This is particularly relevant within the context of continuously decreasing detection limits. Aiming at optimum nanomaterials for spectroscopic and microscopic applications, we examine the optical properties of QDs like II/VI QDs and cadmium-free AgInS2/ZnS QDs (AIS/ZnS) and UCNPs of different chemical composition, size, and particle architecture for ensembles and single particles. This includes PL spectra, PL quantum yields (ΦF), brightness values, blinking behavior, and PL decay kinetics. For UCNPs with their nonlinear spectrally converted PL excited by sequential multiphoton absorption, these measurements were also done as a function of excitation power density (P). Special emphasis is dedicated to the performance parameters ΦF and brightness, that determine signal size and provide a measure for nanocrystal quality.[1-5]
Systematic studies of the excitation energy dependence (EED) [6] of the PL properties of II/VI and ternary AgInS2/ZnS QDs reveal the potential of this relatively simple method for providing insights into the electronic energy structure of QDs. The intrinsic nature of the inhomogeneous broadening of the PL bands of AIS/ZnS QDs was confirmed by single particle spectroscopy.[5] By combining P-dependent integration spectroscopy and single particle measurements of UCNPs, using a new custom-made setup, consisting of different lasers, an inverted microscope, different detectors, and an AFM, we could study the P-dependent optical properties of these nonlinear emitters from ~10 W/cm2 up to ~105 W/cm2. These results provide optimum dopant ion concentrations for bioanalytical, spectroscopic, and microscopic applications of UCNP.
Acknowledgement. Financial support by grants RE1203/12-3 and RE1203/20-1 (support of F. Weigert, L. Dhamo, and F. Frenzel) from German Research Council (DFG) is acknowledged.
The fast and accurate detection of disease-related biomarkers and potentially harmful analytes in different matrices is one of the main challenges in the life sciences. In order to achieve high signal-to-background ratios with frequently used photoluminescence techniques, luminescent reporters are required that are either excitable in the first diagnostic window or reveal luminescence lifetimes exceeding that of autofluorescent matrix components. Here, we demonstrate a reporter concept relying on broad band emissive ternary quantum dots (QDs) with luminescence lifetimes of a few hundred nanoseconds utilized for prolongating the lifetimes of organic or inorganic emitters with lifetimes in the order of a very few 10 ns or less through fluorescence resonant energy transfer. Using spectrally resolved and time-resolved measurements of the system optical response we demonstrate the potential of lifetime multiplexing with such systems exemplarily for AgInS2/ZnS and CdSe/ZnS QDs.