Grain refinement is an important opportunity to improve mechanical properties of fusion welds and the weldability (susceptibility to solidification cracking) of the base metal. In this study, grain refinement was achieved in aluminium welds through additions of grain refiner to the weld metal. Increasing grain refiner additions led to a decrease of the weld metal mean grain size (down to −86 %). The grain refinement efficiency was the highest in commercial pure Al (Alloy 1050A, Al 99.5), followed by Alloy 6082 (Al Si1MgMn) and Alloy 5083 (Al Mg4.5Mn0.7). To investigate this clear influence of alloy content on grain size, the undercooling parameters P and Q were calculated. Temperature measurements revealed that solidification parameters such as solidification growth rate or cooling rate vary significantly along the solidification front, dependent upon torch speed and alloy. On the basis of this comparison, an analytical approach was used to model the columnar to equiaxed transition (CET). Moreover, wavelength dispersive X-ray spectroscopy (WDS) and transmission electron microscopy (TEM) analyses revealed particles rich in Ti and B that are probably TiB2 particles coated by Al3Ti nucleating Al grains during solidification. Also, Ti/B contents needed in commercial filler wires to allow optimum weld metal grain refinement were calculated dependent upon base alloy and welding process.
This work addresses the fatigue strength of friction-welded joints for the drive pinion in heavy-duty trucks. Three different friction welding (FW) variants were tested for the joint between the pinion and the bevel of the shaft: (1) conventional FW using series materials, (2) conventional FW from dissimilar materials for every part, and (3) dissimilar joints by applying joint-site structure of FW. Each joint variant was compared to the series production part using a 4-point bending test. Results showed that the higher strength material slightly improved the fatigue strength of the conventional friction-welded joints. Despite the light weight of the component joined structurally at the site, the joint revealed a lower endurance limit compared to other variants. However, there has been little discussion on the weld zone position. The applied equivalent stresses on the weld zone of the joint-site structure are less similar to the position for the conventional FW. Characterization of the failure explains the extraordinary behaviors in relation to S-N curves.
The industrial demand for flexible and innovative manufacturing technologies is continuously increasing. These technologies have to be sustainable and resource-efficient, and have to allow the production of long-life capital goods. Consequently, the additive processes gain in importance as they offer an enormous potential of application, especially for the turbomachinery industry.
In order to use additive manufacturing technologies in industrial applications, it is necessary to consider the complete process chain, including all necessary pre- and postprocessing. Although additive manufacturing is increasingly covered in scientific research, the linking between this technology and conventional industrial processes is rarely described.
Life Cycle Assessment (LCA) and Social Life Cycle Assessment (SLCA) are applied in evaluating possible social and environmental impacts of the state-of-art welding technologies, such as Manual Metal Arc Welding (MMAW), Manual Gas Metal Arc Welding (GMAW), Automatic GMAW and Automatic Laser-Arc Hybrid Welding (LAHW). The LCA results indicate that for 1 meter weld seam, MMAW consumes the largest amount of resources (like filler material and coating on electrodes) and energy, which contributes to comparatively higher environmental impacts in global warming potential, acidification, photochemical ozone creation potential and eutrophication than other chosen processes. With regard to social aspects, the health issues and fair salary are under survey to compare the relative potential risk on human health caused by fumes in different welding technologies, and to indicate the sufficiency of current salary of welders in Germany. The results reflect that the wage status of welders is still fair and sufficient. The manual processes bring much higher potential risk of welders health than the automatic processes, especially MMAW.
This paper deals with the use of an adaptive control system for compensating the variation in the gap height of a fillet welded lap joint. Gap bridging requires the input of additional filler material and is related to an increased energy input. Hence, the aim was a compensation of the effect of an increased heat input, in order to maintain the weld pool and excessive penetration, which can prevent consequently root reinforcement and burn-through. The findings achieved in this work show possibilities for a real-time controlled adjustments of the welding parameters in automated metal active gas (MAG) welding for compensating a higher heat input, in particular by means of the torch offset relative to the top sheet at the fillet weld on a lap joint.
Understanding the influence of tool/pin shapes on the thermal and material flow behaviors in friction stir welding is of great significance for the optimal design of tool/pin based on a scientific principle. In this study, a numerical method based on computational fluid dynamics is employed to quantitatively analyze the thermo-physical phenomena in friction stir welding with two tools of different pin shapes (axisymmetrical conical tool and asymmetrical triflat tool). Through combining a steady state model with a transient state model, both the computation efficiency and accuracy are ensured. The boundary conditions of heat transfer and material flow are determined with considering a partial sticking/sliding contact condition at the toolworkpiece interface. The total heat generation, heat density and temperature distribution during the welding process with triflat tool are elucidated and compared with that of conical tool, and the material flow patterns and deformation regions of various pin orientations are illustrated in detail. It is found that the deformation zone caused by triflat tool is larger than that by conical tool, which is validated by the weld macrographs. The computed thermal cycles and peak temperature values at some locations are in good agreement with the experimentally measured ones.
The safety of components or constructions is of great importance in the manufacturing and processing of metallic materials. Solidification cracking as well as the weldability of materials remain still for many years a highly contentious issues, particularly with regard to the causes of the hot crack formation. Many of studies have been conducted to determine the critical condition of occurrence of the solidification cracking. In this study different digital image correlation measuring techniques in conjunction with laser diodes as the illuminating source have been employed to measure the arising strain field during the laser welding process at the surface of the workpiece directed to the laser beam in the close vicinity of the weld pool. The Controlled Tensile Weldability test (CTW) was used to apply an external tensile load during the laser beam welding in order to generate the solidification cracks. The results showed that by means of those techniques it is possible to measure the strain field without any disturbances from the intense welding light or the smoke. Additionally, the strain and the strain rate as a critical factor determining solidification crack formation can be measured and analyzed.
This paper presents an approach to reconstruct the three-dimensional transient temperature field for fusion welding processes as input data for computational weld mechanics. The methodology to solve this inverse heat conduction problem fast and automatically focuses on analytical temperature field models for volumetric heat sources and application of global optimisation. The important issue addressed here is the question which experimental data is needed to guarantee a unique reconstruction of the experimental temperature field. Different computational-experimental test cases are executed to determine the influence of various sets of discrete experimental data on the solvability of the optimisation problem. The application of energy distributions utilised for laser beam welding allows reconstructing the temperature field efficiently. Furthermore, the heat input into the workpiece determined by the simulation contributes to the evaluation of the thermal efficiency of the welding process.
Partial penetration welding with a fiber laser at a 9-kW laser power was carried out on 20-mm-thick plates at different positions and analyzed by both experimental and numerical methods. Experiments were carried out for four different angular positions at 1.5 m/min welding speed. All four cases showed a tail-like structure of molten pool on the top surface. The in-depth mechanisms of the energy input characteristics in fiber laser position welding for eight different positions were studied by numerical simulation using the volume-of-fluid (VOF) method. Experimental and numerical results were compared for four cases and showed fair agreement. Observation of flow pattern and bead shape revealed that gravity had little influence on bead shape and flow structure, but changed the pore structure considerably. Flow structure showed a periodic behavior which probably nullified the effect of gravity in position welding. Most of the laser rays reached the bottom of the keyhole without interruption and then multiple reflections started within the keyhole. The first five reflections inside the keyhole delivered around 70 % of the total energy.
Selective Laser Melting (SLM) and Laser Metal Deposition (LMD) are prominent methods in the field of additive manufacturing technology. While the powder-bed based SLM allows the manufacturing of complex structures, buildrate and part volumes are limited. In contrast, LMD is able to operate with high deposition rates on existing parts, however shape complexity is limited. Utilizing their respective strengths, a combination of these two additive technologies has the potential to produce complex parts with high deposition rates.
In this paper, a process chain consisting of additive technologies SLM and LMD is described. The experiments are conducted using the alloys Ti-6Al-4V and Inconel 718. A cylindrical test specimen is produced and the microstructure along the SLM-LMD zone is described. In addition, this process chain was tested in the manufacturing of a turbine blade. The feasibility of implementing this process chain for small batch production is discussed. The results are evaluated to show advantages and limitations of the SLM-LMD process chain. This paper is relevant for industrial or scientific users of additive manufacturing technologies, who are interested in the feasibility of a SLM-LMD process chain and its potential for increased deposition rates.