Filtern
Erscheinungsjahr
Dokumenttyp
- Zeitschriftenartikel (69) (entfernen)
Schlagworte
- Neutron imaging (9)
- Tomography (9)
- Radiography (8)
- Fuel cell (7)
- Water transport (7)
- Electron tomography (6)
- Neutron tomography (6)
- Polymer electrolyte membrane fuel cell (PEMFC) (6)
- Computed tomography (5)
- Reconstruction algorithm (5)
Organisationseinheit der BAM
Paper des Monats
- ja (1)
Coarsening of grain-refined semi-solid Al-Ge32 alloy: X-ray microtomography and in situ radiography
(2007)
Rocks are commonly very heterogeneous materials. Randomly distributed micro-flaws inside the rock are believed to initiate tensile cracks from which shear fractures develop and coalescence through en echelon interactions leads to fracture. In this paper, we describe the results of applying high-resolution X-ray tomography to samples of greywacke and limestone experimentally deformed under unconfined axial shortening at various loads equivalent to different fractions of the sample strength. Mineral grains, pores, micro-cracks and other voids were imaged with a resolution of 10 µm. 3D image analysis enabled us to monitor the initial state of the samples and the changes in them due to compression. Crack morphology is characterized and compared to the micro-structure of the sample before and after deformation. In the greywacke, formation of a macro-crack ~10° oblique to the stress direction is observed. It initiated in fine intergranular material at the top tip of the sample and is composed of tensile fractures connected by wing cracks. None of the voids defined in the initial state fractured, and the crack is interpreted to have started either as a micro-crack which was smaller than the resolution of the tomography, or, as a completely new crack. In the limestone, cracks are observed to initiate in features that are too small to be imaged by the tomography, or also in newly created cracks.
Ein effektives Wassermanagement ist ein wichtiger Aspekt in der Entwicklung von Brennstoffzellen hinsichtlich Langzeitstabilität und Optimierung der Leistungsfähigkeit. Eine zentrale Rolle spielt dabei die Gasdiffusionslage, die für die gleichmäßige Verteilung der Reaktionsgase auf die elektrochemisch aktive Schicht (Katalysator) sorgen soll. In diesem Beitrag werden gemeinsame Forschungsaktivitäten des Helmholtz-Zentrums Berlin für Materialien und Energie (Entwicklung bildgebender Verfahren) sowie des Zentrums für Sonnenenergie- und Wasserstoff-Forschung (ZSW, Entwicklung von Brennstoffzellen) vorgestellt. Im Rahmen dieser Kooperation werden die Entstehung, die Verteilung und der Transport von flüssigem Wasser, kurz das Wassermanagement, unter Betriebsbedingungen untersucht. Mittels Synchrotronradiografie und -tomografie werden kleinste Wassercluster in der Gasdiffusionslage detektiert. Die gewonnenen Erkenntnisse dienen der Modifikation und einer gezielten Auswahl der eingesetzten Materialien.
In-situ-Neutronenradiografie wird erfolgreich eingesetzt, um flüssiges Wasser in Niedertemperatur-PEM-Brennstoffzellen während des Betriebs zerstörungsfrei abzubilden und das sogenannte Wassermanagement eine der größten Herausforderungen der Entwicklung durch Anpassung der Materialeigenschaften zu optimieren. Dabei werden die besonderen Eigenschaften der Neutronen genutzt, die metallische Bauteile relativ leicht durchdringen, während selbst kleine Wassermengen durch ihre starke Streuung leicht nachweisbar sind. Die relativ langen Messzeiten für die Neutronentomografie werden durch den Betrieb der Zelle im angehaltenen Zustand realisierbar, sodass die dreidimensionale Wasserverteilung darstellbar wird.
The carbon dioxide evolution and bubble formation in an operating fuel has been studied by means of synchrotron X-ray radiography. Two different observation directions have been chosen: a through-plane insight has been employed to track the formation of bubbles starting at the corner of the lands of the flow field; a depth profile of the carbon dioxide evolution has been derived from cross sectional studies describing an affected area of up to 100 µm. The dynamics of the bubble formation and detachment of the bubbles from the position of formation is strongly correlated with the current density. Cracks and breaks in the catalyst layer which result from the preparation process are visible under operating conditions and a possible swelling of the catalyst layer does not reach a complete vanishing of the cracks.
Water transport in an operating PEM fuel cell was investigated with synchrotron X-ray radiography with a spatial resolution of 3 µm and a temporal resolution of 5 s. This method allows for the detection of water accumulations with less than 10 µm diameter. We demonstrate that synchrotron X-ray imaging can dramatically expand the possibilities of imaging with high spatial and time resolution, especially as a complement to neutron radiography. Water transport processes from the first appearance of small water accumulations in the gas diffusion layer to their transport into the channel system were analysed in situ. Correlations between local effects such as water formation and operating conditions of the whole system, e.g. power variations, were found. A recently described eruptive water transport mechanism is analysed in detail.
Die Aufklärung spezifischer Fragestellungen zur Funktionalität von PEM(polymer electrolyte membrane)- und DMFC(Direct Methanol)-Brennstoffzellen bedarf der 3D-Abbildung der spezifischen Komponenten mit unterschiedlichen Strahlungsarten: des Wassergehalts in den Flow Fields mit Neutronen, der Katalysator-Alterung in der MEA (membrane electrode assembly) mit Synchrotronstrahlung und der freien (reaktiven) Katalysator-Oberfläche von Nano-Partikeln mit TEM-Elektronen-Tomografie. Diese Messungen im Bereich der mm- bis nm-Skala unterliegen dabei erheblichen Restriktionen: einer ortsabhängigen Verschmierung der Neutronenradiogramme, Manipulatorinstabilitäten der Synchrotronmessungen sowie einer Kombination von Limited-View-Datensätzen, wenigen Projektionswinkeln und teilweiser Nichtdurchstrahlbarkeit in der Elektronen-CT. Die Vorteile eines fortentwickelten Directt-Algorithmus für die Bewältigung dieser Randbedingungen gegenüber gefilterten Rückprojektionen werden aufgezeigt.
Charakterisierung von Katalysatormaterialien für Brennstoffzellen mittels Elektronentomografie
(2010)
Zur Optimierung moderner Katalysatoren für Brennstoffzellen werden diese elektronen-tomografisch charakterisiert. Die Elektronentomografie ermöglicht einzigartige Einblicke in die Nanometer-Strukturen der metallischen Katalysatorpartikel, die auf einem elektrisch leitenden, inerten Kohlenstoffträger abgeschieden werden. Die dreidimensional bildgebende Methode ermöglicht über qualitative Untersuchungen hinaus detaillierte quantitative Form- und Strukturanalysen der Katalysatormaterialien. So werden beispielsweise die Positionen der Katalysatorpartikel relativ zum Trägermaterial analysiert. Ihre Form und Einbettung in den Träger, welche die für die katalytische Reaktion maßgebliche "freie Oberfläche" definieren, werden bestimmt. Die Elektronentomografie ermöglicht somit quantitative Vergleiche zwischen verschiedenen Katalysatormaterialien und Herstellungsverfahren. Sie erweitert die Möglichkeiten der Korrelation gewünschter elektrochemischer Eigenschaften mit der Nanostruktur dieser Materialien und macht so weitere Optimierungen der Katalysatormaterialien möglich.
Magnetic domains have been the subject of much scientific investigation since their theoretical existence was first postulated by P.-E. Weiss over a century ago. Up to now, the three-dimensional (3D) domain structure of bulk magnets has never been observed owing to the lack of appropriate experimental methods. Domain analysis in bulk matter thus remains one of the most challenging tasks in research on magnetic materials. All current domain observation methods are limited to studying surface domains or thin magnetic films. As the properties of magnetic materials are strongly affected by their domain structure, the development of a technique capable of investigating the shape, size and distribution of individual domains in three dimensions is of great importance. Here, we show that the novel technique of Talbot-Lau neutron tomography with inverted geometry enables direct imaging of the 3D network of magnetic domains within the bulk of FeSi crystals.
In contrast to classical low temperature polymer electrolyte fuel cells (LT-PEFCs), the membrane conductivity in high temperature polymer electrolyte fuel cells (HT-PEFCs) (operating temperature ~ 160 °C) is based on proton transport within phosphorus-oxygen acids at different levels of hydration, orthophosphoric acid (H3PO4) being the simplest example. We present for the first time in-situ synchrotron X-ray radiography measurements applied to a HT-PEFC to gain insight into the local composition of the membrane electrode assembly (MEA) under dynamic operating conditions. Transmission changes during the radiographic measurements exhibit a clear influence of the formation of product water on the membrane composition.
Synchrotron X-ray absorption edge imaging was used to investigate the ruthenium distribution in both fresh and aged Pt/Ru-based membrane electrode assemblies (MEA) of direct methanol fuel cells. MEAs aged in different ways were analyzed: artificially aged by MeOH depletion and aged for 1700 h in an operating fuel cell stack. An element sensitive tomographic technique – differential X-ray absorption edge tomography – was applied allowing for a 3D-visualization of the ruthenium distribution within the MEA. We found a markedly changed Ru distribution after aging which is correlated to the GDL structure, the flow field geometry, and CO2 transport in the methanol solution.
The three-dimensional water distribution and water transport paths in the gas diffusion layer (GDL) and the adjacent micro-porous layer (MPL) of a polymer electrolyte membrane fuel cell (PEMFC) were analyzed during cell operation. The technique of quasi in-situ X-ray tomography was used for a 3D visualization of the water distribution and the structure of the GDL at different operating conditions. Based on findings from in-situ radiographic measurements water transport paths were detected and subsequently examined by tomography. The combination of these 2D and 3D techniques allows for a fully three-dimensionally resolved visualization of transport paths through the GDL.
The 3-dimensional spatial distribution of liquid water in different gas diffusion layer (GDL) materials was analyzed using synchrotron X-ray tomography. The capability of the method was demonstrated by virtually separating the GDL components in order to facilitate individual analysis of fiber material, liquid water and gas filled pore spaces. The influence of hydrophobic surface treatment on the water distribution in the GDL was illustrated by analyzing three GDL materials with different degrees of hydrophobicity. In the least hydrophobic sample, liquid water tends to form larger clusters which stretch out about several hundred µm inside the porous GDL. In contrast, only small water clusters were found in the strongly hydrophobic material with high Polytetrafluoroethylene (PTFE)-content as the liquid is partially pressed out of the GDL. Additionally, the influence of fiber orientation on the water distribution in the felt material was demonstrated.
We present transmission electron microscope (TEM) tomography investigations of ruthenium-based fuel cell catalyst materials as employed in direct methanol fuel cells (DMFC). The digital three-dimensional representation of the samples not only enables detailed studies on number, size, and shape but also on the local orientation of the ruthenium particles to their support and their freely accessible surface area. The shape analysis shows the ruthenium particles deviate significantly from spherical symmetry which increases their surface to volume ratio. The morphological studies help to understand the structure formation mechanisms during the fabrication as well as the high effectiveness of these catalysts in the oxygen reduction reaction at the cathode side of fuel cells.
CT (computed tomography) reconstructions of fuel cell components of a yet unrivaled spatial resolution and quality are presented. This is achieved by application of the novel DIRECTT (Direct Iterative Reconstruction of Computed Tomography Trajectories) algorithm. We focus on two different key issues which essentially rule the fuel cell's durability on different length scales and physical interactions. On the resolution scale of some 100 µm agglomerations of condensed water in flow-field channels are detected by means of quasi-in situ neutron CT (after operation). Five orders of magnitude below nanometer sized Ru catalyst particles on carbon black support are visualized by electron tomography. Both types of experiments are especially adapted to the type of material involved but they are accompanied by severe deviations from ideal CT measuring conditions, as well. In order to overcome the tremendous reconstruction artifacts of standard algorithms, we employ DIRECTT which is described in detail. Comparisons of DIRECTT reconstructions to the conventional filtered back projection, prove the significant improvements in both experimental methods.
We present transmission electron microscope (TEM) tomography investigations of ruthenium-based fuel cell catalyst materials as employed in direct methanol fuel cells (DMFC). The digital three-dimensional representation of the samples not only enables detailed studies on number, size, and shape but also on the local orientation of the ruthenium particles to their support and their freely accessible surface area. The shape analysis shows the ruthenium particles deviate significantly from spherical symmetry which increases their surface to volume ratio. The morphological studies help to understand the structure formation mechanisms during the fabrication as well as the high effectiveness of these catalysts in the oxygen reduction reaction at the cathode side of fuel cells.
Neutron tomography was applied to study the 3D water distribution in full polymer electrolyte membrane fuel cell (PEMFC) stacks. The water distribution after switch-off of the fuel cell was analyzed over a period of 36 h. We found a slowly increasing water amount in the fuel cell, but only few changes within a time period of 5 h, which is about the time necessary for neutron tomography. In this way, the requirement for successful tomography was obtained. It is demonstrated how the quasi in-situ tomography technique enables us to study the water content in individual flow field channels of three-fold stacks. Flow field as well as stack design issues are addressed by this visualization method showing weak points due to a non-uniform water distribution that can be identified by means of neutron imaging.
Synchrotron X-ray radiography and tomography investigations of a custom-made polymer electrolyte membrane fuel cell optimised for visualisation purposes are presented. The 3D water distribution and transport pathways in the porous carbon fibre gas diffusion layers (GDLs) were investigated. The authors found that water is not only moving from the GDL into the channel, but can also take the opposite way, that is, from the channel into free pore space of the GDL. Such movement of water into the opposite direction has been subject of speculations but has so far not yet been reported and might bring new insights into the general water transport behaviour, which might give new aspects to the general description of water transport processes and influence modelling assumptions to describe the process taking place in the GDL.
A new high-resolution detector setup for neutron imaging has been developed based on infinity-corrected optics with high light collection, combined with customized mounting hardware. The system can easily be installed, handled and fitted to any existing facility, avoiding the necessity of complex optical systems or further improved electronics (CCD). This is the first time optical magnification higher than 1:1 has been used with scintillator-based neutron detectors, as well as the first implementation of infinity corrected optics for neutron imaging, achieving the smallest yet reported effective pixel size of 3.375 µm. A novel transparent crystal scintillator (GGG crystal) has been implemented with neutrons for the first time to overcome limitations of traditional powder scintillators (Li6/ZnS, Gadox). The standardized procedure for resolution measurements with the Modulation Transfer Function (MTF) is summarized to facilitate comparison between instruments and facilities. Using this new detector setup, a resolution of 14.8 µm with a field of view of 6 mm × 6 mm has been achieved while maintaining reasonable count times. These advances open a wide range of new possible research applications and allow the potential for additional future developments.
Perforated gas diffusion layers (GDLs) of polymer electrolyte membrane fuel cells (PEMFCs) were investigated by means of in-situ synchrotron X-ray radiography during operation. We found a strong influence of perforations on the water distribution and transport in the investigated Toray TGP-H-090 GDL. The water occurs mainly around the perforations, while the holes themselves show varying water distributions. Some remain dry, while most of them fill up with liquid water after a certain period or might serve as drainage volume for effective water transport.
Aufgrund des hohen Wirkungsgrades und der vielfältigen Einsatzmöglichkeiten können Brennstoffzellen einen wichtigen Beitrag zur zukünftigen Energieversorgung leisten. Für die Optimierung der Brennstoffzellentechnik ist es erforderlich, die während des Zellbetriebs ablaufenden Prozesse zu verstehen und exakt zu charakterisieren. Ein ausbalanciertes Wassermanagement ist die Grundlage für die optimale Leistungsfähigkeit einer wasserstoffbetriebenen Zelle. Das während des Betriebs entstehende Wasser muss die Membran ausreichend befeuchten, um deren Protonenleitfähigkeit aufrechtzuerhalten. Andererseits behindern zu große Wasseransammlungen in der Zelle die Gaszufuhr durch die porösen Materialien sowie in den Kanälen der Gasverteilerstrukturen. Alterungsphänomene einzelner Zellkomponenten können die Verteilung der Wasseransammlungen und somit das Wassermanagement empfindlich stören und so die Leistungsfähigkeit der Brennstoffzelle herabsetzen. Zur Analyse der Wasserverteilung werden zerstörungsfreie, bildgebende Methoden, wie die Ex-situ-Neutronentomografie und die In-situ-Synchrotronradiografie, eingesetzt. Diese Methoden können während des Brennstoffzellenbetriebs mit weiteren Messverfahren, beispielsweise der ortsaufgelösten Stromdichtemessung, kombiniert werden. Auf diese Weise werden einzelne Komponenten, wie zum Beispiel die Gasdiffusionsschichten, charakterisiert.
Synchrotron X-ray absorption edge imaging with high energy resolution was applied to study aging of fuel cell catalyst materials. The combination of an imaging and a high X-ray energy resolution set-up allows acquiring spatially resolved XAS (XANES and EXAFS) spectra. We analyzed the two-dimensional distribution of Pt and Ru in fresh and aged fuel cell catalysts. Spatially resolved XAS images were taken at the RuK edge and at the PtL3 edge. Taking radiographs above and below the absorption edges provides quantitative information about the thickness of the catalytic materials and additional chemical information. A strong influence of the flow field channels and the structure of the gas diffusion layers on the thicknesses of the catalytic elements were found: a thinner catalyst layer was found below the ribs of the flow field geometries as well as under crossing points of fiber bundles of the woven gas diffusion layers.
Investigation of fuel cell materials and liquid water transport by means of synchrotron imaging
(2013)
Synchrotron imaging allows addressing various important issues in fuel cell research, for example water distribution and transport. The water distribution in polymer electrolyte membrane fuel cells (PEMFCs) was observed quasi in-situ directly after operation by means of synchrotron tomography. The 3D data set was compared with the tomogram of a dry cell in order to separate the water distribution from cell materials. Engineered transport pathways realized by perforating holes through the gas diffusion layer (GDL) are a recent approach to optimize water transport and cell performance. For some parameter sets a cell performance increase and an improvement of stabilization have already been proven. We present high resolution investigations of the water distribution in perforated GDLs of operating PEMFCs by means of in-situ synchrotron radiography. The surrounding areas of the holes exhibited a distinct hydrophilic character.
Water evolution in the gas diffusion layer of a polymer electrolyte membrane fuel cell was visualized in situ by means of synchrotron X-ray radiography. Cracks in the microporous layer were identified as start points of efficient liquid water transfer paths through the gas diffusion layer. Quantitative analysis of the water flow rate through those arbitrarily distributed cracks into the gas channel revealed that they have a strong influence on the overall liquid water transport. This could find entry into future material design and simulation.
We present a synchrotron X-ray tomographic study on the morphology of carbon fiber-based gas diffusion layer (GDL) material under compression. A dedicated compression device is used to provide well-defined compression conditions. A flat compression punch is employed to study the fiber geometry at different degrees of compression. Transport relevant geometrical parameters such as porosity, pore size and tortuosity distributions are calculated. The geometric properties notably change upon compression which has direct impact on transport conditions for gas and fluid flow. The availability of broad 3D paths, which are most important for the transport of liquid water from the catalyst layer through the GDL, is markedly reduced after compression. In a second experiment, we study the influence of the channel-land-pattern of the flow-field on shape and microstructure of the GDL. A flow-field compression punch is employed to reproduce the inhomogeneous compression conditions found during fuel cell assembly. While homogenously compressed underneath the land the GDL is much less and inhomogeneously compressed under the channel. The GDL material extends far into the channel volume where it can considerably influence gas and fluid flow. Loose fiber endings penetrate deeply into the channel and form obstacles for the discharge of liquid water droplets.
Typische 'Missing Wedge'(MW)-Artefakte in Rekonstruktionen der Computertomografie können mit dem iterativen DIRECTT-Algorithmus (Direkte iterative Rekonstruktion computertomografischer Trajektorien) unterdrückt werden. Die durch fehlende Projektionswinkel bedingten MW-Restriktionen betreffen bisher nur Sonderapplikationen der Röntgen- und Neutronentomografie, müssen in der Nanometer auflösenden Elektronentomografie jedoch als Standard akzeptiert werden. Die MW-Artefakte werden besonders effektiv mit einer spezifischen DIRECTT-Prozedur partiell diskreter Zwischenlösungen beseitigt. Für die Beurteilung der Abbildungsqualität werden Rekonstruktionen von vollständigen und unvollständigen Mess- und Modell-Datensätzen erzeugt und mit Ergebnissen anderer Algorithmen (gefilterte Rückprojektion (FBP) und ART-Methoden) verglichen. Die Fourier-Transformierten der Rekonstruktionen demonstrieren die erfolgreiche Ergänzung der fehlenden Information im MW-Bereich. Die quantitative Bewertung der lokalen Rekonstruktionsqualität mit Methoden der räumlichen Statistik ergibt auch für unterschiedliche Signal-Rausch-Verhältnisse signifikante Vorteile gegenüber FBP und ART.
We investigated the hydrogen distribution spatially and temporally in technical iron at room temperature. Samples were charged electrochemically and subsequently analysed by means of neutron radiography and tomography. The radiographic images allowed for a time-resolved analysis of hydrogen fluxes. The three-dimensional distribution of hydrogen measured by neutron tomography delivered valuable information for the damage analysis of hydrogen-induced cracks. For the first time hydrogen concentration gradients inside the material could be detect directly together with the cracks. The neutron radiography and tomography results were gained at the Research Reactor BER II of the HZB in Berlin.
We investigated hydrogen embrittlement and blistering in electrochemically hydrogen-charged technical iron samples at room temperature. Hydrogen-stimulated cracks and blisters and the corresponding hydrogen distributions were observed by neutron tomography. Cold neutrons were provided by the research reactor BER II to picture the sample with a spatial resolution in the reconstructed three-dimensional model of ~25 µm. We made the unique observation that cracks were filled with molecular hydrogen and that cracks were surrounded by a 50 µm wide zone with a high hydrogen concentration. The zone contains up to ten times more hydrogen than the bulk material. The hydrogen enriched zone can be ascribed to a region of increased local defect density. Hydrogen also accumulated at the sample surface having the highest concentration at blistered areas. The surfaces of the brittle fractured cracks showed micropores visualized by scanning electron microscopy. The micropores were located at grain boundaries and were surrounded by stress fields detected by electron backscattered diffraction. The cracks clearly originated from the micropores.
Influence of artificial aging of gas diffusion layers on the water management of PEM fuel cells
(2014)
The influence of artificial aging of gas diffusion layers (GDL) on the water management within the GDL was investigated in-operando by synchrotron X-ray radiography. One GDL was subjected to an accelerated aging procedure in 30% H2O2 solution, while another GDL was pristine. Radiographic measurements were combined with temporally resolved electrical analyzes. Significant differences in cell voltage and water accumulation were observed during cell operation at steady-state conditions. The cell which contained the aged GDL featured a higher water amount especially at the anode side and a lower cell voltage.
We present an experimental approach to study the three-dimensional microstructure of gas diffusion layer (GDL) materials under realistic compression conditions. A dedicated compression device was designed that allows for synchrotron-tomographic investigation of circular samples under well-defined compression conditions. The tomographic data provide the experimental basis for stochastic modeling of nonwoven GDL materials. A plain compression tool is used to study the fiber courses in the material at different compression stages. Transport relevant geometrical parameters, such as porosity, pore size, and tortuosity distributions, are exemplarily evaluated for a GDL sample in the uncompressed state and for a compression of 30 vol.%. To mimic the geometry of the flow-field, we employed a compression punch with an integrated channel-rib-profile. It turned out that the GDL material is homogeneously compressed under the ribs, however, much less compressed underneath the channel. GDL fibers extend far into the channel volume where they might interfere with the convective gas transport and the removal of liquid water from the cell.
Neutron tomography has been applied to investigate the mechanism of hydrogen assisted cracking in technical iron and supermartensitic steel. Rectangular technical iron block samples showed blistering due to intense hydrogen charging and the tomographic method revealed in situ the spatial distribution of hydrogen and cracks. Hydrogen accumulated in a small region around cracks and the cracks are filled with hydrogen gas. Cracks close to the surface contained no hydrogen. Hydrogenous tensile test samples of supermartensitic steel were pulled until rupture and showed hydrogen accumulations at the notch base and in the plastically deformed region around the fracture surface.
This paper gives a brief overview on3D imaging of magnetic domains with shearing grating neutron tomography. We investigated the three-dimensional distribution of magnetic domain walls in the bulk of a wedge-shaped FeSi single crystal. The width of the magnetic domains wasanalyzed at different locations within the crystal. Magnetic domains close to the tip of the wedge are much smaller than in the bulk. Furthermore, the three-dimensional shape of individual domains wasinvestigated. We discuss prospects and limitations of the applied measurement technique.
The potentials of incoherent X-ray scattering (Compton) computed tomography (CT) are investigated. The imaging of materials of very different atomic number or density at once is generally a perpetual challenge for X-ray tomography or radiography. In a basic laboratory set-up for simultaneous perpendicular Compton scattering and direct beam attenuation tomography are conducted by single channel photon counting line scans. This results in asymmetric distortions of the projection profiles of the scattering CT data set. In a first approach, corrections of Compton scattering data by taking advantage of rotational symmetry yield tomograms without major geometric artefacts. A cylindrical sample composed of PE, PA, PVC, glass and wood demonstrates similar Compton contrast for all the substances, while the conventional absorption tomogram only reveals the two high order materials. Comparison to neutron tomography
reveals astonishing similarities except for the glass component (without hydrogen). Therefore, Compton CT offers the potential to replace neutron tomography, which requires much more efforts.
Carbon fiber based felt materials are widely used as gas diffusion layer (GDL) in fuel cells. Their transport properties can be adjusted by adding hydrophobic agents such as polytetrafluoroethylene (PTFE). We present a synchrotron X-ray tomographic study on the felt material Freudenberg H2315 with different PTFE finishing. In this study, we analyze changes in microstructure and shape of GDLs at increasing degree of compression which are related to their specific PTFE load. A dedicated compression device mimicking the channel-land pattern of the flowfield is used to reproduce the inhomogeneous compression found in a fuel cell. Transport relevant geometrical parameters such as porosity, pore size distribution and geometric tortuosity are calculated and consequences for media transport discussed. PTFE finishing results in a marked change of shape of compressed GDLs: surface is smoothed and the invasion of GDL fibers into the flow field channel strongly mitigated. Furthermore, the PTFE impacts the microstructure of the compressed GDL. The number of available wide transport paths is significantly increased as compared to the untreated material. These changes improve the transport capacity liquid water through the GDL and promote the discharge of liquid water droplets from the cell.
A strategy to mitigate typical reconstruction artefacts in missing wedge computed tomography is presented. These artefacts appear as elongations of reconstructed details along the mean direction (i.e. the symmetry centre of the projections). Although absent in standard computed tomography applications, they are most prominent in advanced electron tomography and also in special topics of X-ray and Neutron tomography under restricted geometric boundary conditions. We investigate the Performance of the DIRECTT (Direct Iterative Reconstruction of Computed Tomography Trajectories) algorithm to reduce the directional artefacts in standard procedures. In order to be sensitive to the anisotropic nature of missing wedge artefacts, we investigate isotropic substructures of metal foam as well as circular disc models. Comparison is drawn to filtered backprojection and algebraic techniques. Reference is made to reconstructions of complete data sets. For the purpose of assessing the reconstruction Quality, Fourier transforms are employed to visualize the missing wedge directly. Deficient reconstructions of disc models are evaluated by a length-weighted boundary orientations. The DIRECTT results are assessd at different signal-to-noise ratios by means of local and integral evaluation Parameters.
Neutron Bragg-edge imaging was applied for the visualization of a γ-Austenite to α'-martensite phase transformation. In the present study, a super martensitic
stainless steel sample was heated until complete austenitization and was subsequently cooled down to room temperature. The martensitic phase Transformation started at Ms = 190 °C. Using a monochromatic neutron beam with λ = 0.390 nm, the transmitted intensity was significantly reduced during cooling below Ms, since the emerging martensitic phase has a higher attenuation coefficient than the austenitic phase at this wavelength. The phase Transformation process was visualized by filming the transmission images from a scintillator screen with a CCD camera with a temporal resolution of 30 s and a spatial
resolution of 100 µm.
In this investigation, synchrotron X-ray imaging was used to investigate the water distribution inside newly developed gas diffusion media in polymer electrolyte membrane fuel cells. In-situ radiography was used to reveal the relationship between the structure of the microporous layer (MPL) and the water flow in a newly developed MPL equipped with randomly arranged holes. A strong influence of these holes on the overall water transport was found. This contribution provides a brief overview to some of our recent activities on this research field.
The water management in proton exchange membrane fuel cells (PEMFC) is strongly influenced by the design of the gas diffusion layers (GDL). Limiting current measurements in small-scale cells operating at high stoichiometries are useful to determine the oxygen transport resistance. The oxygen transport resistance increases, once water condenses inside the GDL. In this study a new electrochemical method for voltage loss estimation of GDL induced oxygen transport losses are presented. This new method, referred to as “transient limiting current” (TLC), is compared with the literature method. TLC allows a direct estimation of oxygen transport resistance at an arbitrarily conditioned state. This study also presents a case study of liquid water visualization of a PEM fuel cell with varying GDLs types.
With the help of quasi in-situ synchrotron X-ray computed tomography and time resolved radiography measurements we investigate appearance and distribution of liquid water inside the GDLs under limiting current conditions.
Die Computer-gestützte Laminografie (CL) wurde als komplementäre Methode zur Computertomografie für die dreidimensionale Bildgebung von lateral ausgedehnten Objekten entwickelt. Ursprünglich für medizinische Zwecke verwendet, wurde diese Methode kürzlich als zerstörungsfreie nicht-invasive Methode nicht nur in der Materialforschung, sondern auch mit steigendem Interesse für kunsthandwerkliche und historische Objekte eingesetzt. Hier wird die Computer-gestützten Laminografie mit polychromatischer Neutronenstrahlung an einer historischen Tsuba eingesetzt, einem Stichblatt eines japanischen Schwerts. Eine Analyse der Lötstellen gibt Rückschlüsse auf das Herstellungsverfahren. Zudem wurden unterschiedliche Materialsysteme gefunden, vermutlich um dem Tsuba lokal eine höhere Stabilität zu verleihen. Die Messungen wurden an der Imaging-Beamline CONRAD-2 an der Neutronenquelle BER 2 des Helmholtz-Zentrums Berlins (HZB) durchgeführt.
In various kinds of radiography, deficient transmission imaging may occur due to backlighting inside the detector itself arising from light or radiation scattering. The related intensity mismatches barely disturb the high resolution contrast, but its long range nature results in reduced attenuation levels which are often disregarded. Based on X-ray observations and an empirical formalism, a procedure is developed for a first order correction of detector backlighting. A backlighting factor is modeled as a function of the relative detector coverage by the sample projection. Different cases of sample transmission are regarded at different backlight factors and detector coverage. The additional intensity of backlighting may strongly affect the values of materials’ attenuation up to a few 10%. The presented scenario provides a comfortable procedure for corrections of X-ray or neutron transmission imaging data.
The ability to track electrode degradation, both spatially and temporally, is fundamental to understand performance loss during operation of lithium batteries. X-ray computed tomography can be used to follow structural and morphological changes in electrodes; however, the direct detection of electrochemical processes related to metallic lithium is difficult due to the low sensitivity to the element. In this work, 4-dimensional neutron computed tomography, which shows high contrast for lithium, is used to directly quantify the lithium diffusion process in spirally wound Li/SOCl2 primary cells. The neutron dataset enables the quantification of the lithium transport from the anode and the accumulation inside the SOCl2 cathode to be locally resolved. Complementarity between the collected neutron and X-ray computed tomographies is shown and by applying both methods in concert we have observed lithium diffusion blocking by the LiCl protection layer and identified all cell components which are difficult to distinguish using one of the methods alone.
Herein, we present a detailed investigation of the electrochemically triggered formation and dissolution processes of α- and β-sulfur crystals on a monolithic carbon cathode using operando high-resolution synchrotron radiography (438 nm/pixel).
The combination of visual monitoring with the electrical current response during cyclic voltammetry provides valuable insights into the sulfur formation and dissolution mechanism. Our observations show that the crystal growth process is mainly dictated by a rapid equilibrium between long-chain polysulfides on one side and solid sulfur/short-chain polysulfides on the other side, which is consistent with previous studies in this field. The high temporal and spatial resolution of synchrotron imaging enables the observation of different regimes during the sulfur formation and dissolution process. The appearance of short-chain polysulfides after the first anodic CV peak initiates a rapid dissolution process of α-sulfur crystals on the cathode. The increase in the long-chain lithium polysulfide concentration at the cathode surface during charge results in an increased crystal growth rate, which in turn produces imperfections in α- and β-sulfur crystals. There are strong indications that these defects are fluid inclusions, which may trap dissolved polysulfides and therefore reduce the electrochemical cell capacity.
The understanding of dynamic processes in Li-metal batteries is an important consideration to enable the full capacity of cells to be utilised. These processes, however, are generally not directly observable using X-ray techniques due to the low attenuation of Li; and are challenging to visualise using neutron imaging due to the low temporal resolution of the technique. In this work, complementary X-ray and neutron imaging are combined to track the dynamics of Li within a primary Li/SOCl2 cell. The temporal challenges posed by neutron imaging are overcome using the golden ratio imaging method which enables the identification of Li diffusion in operando. This combination of techniques has enabled an improved understanding of the processes which limit rate performance in Li/SOCl2 cells and may be applied beyond this chemistry to other Li-metal cells.
Phosphoric acid as the electrolyte in high-temperature polymer electrolyte membrane fuel cell plays an essential role in ist performance and lifetime. Maldistribution of phosphoric acid in the catalyst layer (CL) may result in performance degradation. In the present study, pore-scale simulations were carried out to investigate phosphoric acid’s multiphase flow in a cathode CL. A reconstructed CL model was built using focused ion beam-SEM images, where distributions of pore, carbon support, binder, and catalyst particles can be identified. The multi-relaxation time lattice Boltzmann method was employed to simulate phosphoric Acid invading and leaching from the membrane into the CL during the membrane electrode assembly fabrication process. The predicted redistribution of phosphoric acid indicates that phosphoric acid of low viscosity or low wettability is prone to leaching into the CL.
The effective transport properties and the active electrochemical active surface area (ECSA) were computed using a pore-scale model. They were subsequently used in a macroscopic model to evaluate the cell performance. A parametric study shows that cell performance first increases with increasing phosphoric acid content due to the increase of ECSA. However, further increasing phosphoric acid content results in performance degradation due to mass transfer limitation caused by acid flooding.
The mechanical compression of metal foam flow-field based polymer electrolyte fuel cells (PEFCs) is critical in determining the interfacial contact resistance with gas diffusion layers (GDLs), reactant flow and water management.
The distinct scale between the pore structure of metal foams and the entire flow-field warrant a multilength scale characterization that combines ex-situ tests of compressed metal foam samples and in-operando analysis of operating PEFCs using X-ray computed tomography (CT) and neutron radiography. An optimal ‘medium’ compression was found to deliver a peak power density of 853 mW/cm². The X-ray CT data indicates that the compression process significantly decreases the mean pore size and narrows the pore size distribution of metal foams. Simulation results suggest compressing metal foam increases the pressure drop and gas velocity, improving the convective liquid water removal. This is in agreement with the neutron imaging results that demonstrates an increase in the mass of accumulated liquid water with minimum compression compared to the medium and maximum compression cases. The results show that a balance between Ohmic resistance, water removal capacity and parasitic power is imperative for the optimal performance of metal foam based PEFCs.
While X-ray based darkfield imaging with grating interferometers is already widely used, darkfield imaging with neutrons has still a relatively small user community focused mostly on magnetic materials. Here, we demonstrate the application of neutron darkfield imaging byTalbot-Lau type grating interferometry to fiber reinforced plastics. Common carbon and glass fiber composites have been investigated including characteristic damage structures. The darkfield images show a strong signal response caused by fiber delamination, suitable fiber direction, particles, pores and cracks. The basic principles of neutron darkfield imaging applied to fiber composites are highlighted.