Ingenieurwissenschaften und zugeordnete Tätigkeiten
Filtern
Dokumenttyp
- Zeitschriftenartikel (135)
- Beitrag zu einem Tagungsband (69)
- Vortrag (27)
- Forschungsbericht (4)
- Posterpräsentation (1)
Schlagworte
- Laser beam welding (56)
- Additive manufacturing (13)
- Laser metal deposition (12)
- Microstructure (11)
- Numerical simulation (11)
- Solidification cracking (11)
- DED (10)
- Laserstrahlschweißen (10)
- Mechanical properties (10)
- Additive Manufacturing (9)
- Hybrid laser-arc welding (8)
- Laser welding (8)
- Numerical modeling (8)
- Thick-walled steel (8)
- Weld pool shape (8)
- Additive Fertigung (7)
- Porosity (7)
- Resistance spot welding (7)
- Element transport (6)
- Hybrid laser arc welding (6)
- Laserhybridschweißen (6)
- Magnetohydrodynamics (6)
- AM (5)
- Artificial neural network (5)
- Directed Energy Deposition (5)
- Gründungsstrukturen (5)
- Hochfester Stahl (5)
- Hybrid Laser Arc Welding (5)
- Liquid metal embrittlement (5)
- Magnetic field (5)
- Solidification (5)
- Widerstandspunktschweißen (5)
- Crack (4)
- Critical strain (4)
- Deep penetration (4)
- Deep penetration laser beam welding (4)
- Directed energy deposition (4)
- Endkrater (4)
- Grain refinement (4)
- High power laser beam welding (4)
- Inconel 718 (4)
- Laser Metal Deposition (4)
- Laser hybrid welding (4)
- Liquid Metal Embrittlement (4)
- Offshore Windenergieanlagen (4)
- Simulation (4)
- Weld pool dynamics (4)
- 9%Ni steel (3)
- Automatisierte Fertigung (3)
- Bulging effect (3)
- Cryogenic steel (3)
- Crystal branch development (3)
- Electromagnetic Weld Pool Support (3)
- Elektromagnetische Schmelzbadunterstützung (3)
- End crater (3)
- Equivalent heat source (3)
- Full Penetration (3)
- Gap bridgeability (3)
- Heat conduction (3)
- Künstliche Intelligenz (3)
- Laser energy distribution (3)
- Laser-Pulver-Auftragschweißen (3)
- Laserimplantation (3)
- Leichtbau (3)
- Mathematical modeling (3)
- Mechanical mismatching (3)
- Molten pool dynamics (3)
- Multi-physical modelling (3)
- Numerical modelling (3)
- Numerical process simulation (3)
- Partial penetration (3)
- Periodic solidification pattern (3)
- Process simulation (3)
- Quality assurance (3)
- Ray tracing (3)
- Rundnaht (3)
- Thick Materials (3)
- Welding simulation (3)
- AISI D2 (2)
- Advanced high strength steel (2)
- Advanced high strength steels (2)
- Auftragschweißen (2)
- Automatisierte schweißtechnische Fertigung (2)
- Bulge effect (2)
- Bulge formation (2)
- Charpy impact toughness (2)
- Circumferential weld (2)
- DED-EB (2)
- Data preparation (2)
- Defokussierung (2)
- Digitalisierung (2)
- Dimensional accuracy (2)
- Directed Enery Deposition (2)
- Dissimilar metal weld overlays (2)
- Dual phase steel (2)
- Duplex AISI 2205 (2)
- EBAM (2)
- Edge quality (2)
- Electromagnetic backing (2)
- Electromagnetic support (2)
- Electromagnetic weld pool support (2)
- Electron beam welding (2)
- Elektronenstrahlschweißen (2)
- FGM (2)
- Flüssigmetallinduzierte Rissbildung (2)
- Full penetration (2)
- Grain size (2)
- Hardness (2)
- Heat treatment (2)
- High-power laser beam welding (2)
- Hot crack (2)
- Hot cracking (2)
- Hybrid welding (2)
- In situ strain (2)
- Keyhole collapse (2)
- Keyhole mode welding (2)
- LME (2)
- Laser-Hybridschweißen (2)
- Laser-metal-deposition (2)
- Matching ferritic welding electrode (2)
- Melt pool dinamics (2)
- Melt pool dynamics (2)
- Metal mixing (2)
- Neuronales Netz (2)
- Nickel (2)
- Optical measurement (2)
- Oscillating magnetic field (2)
- Oscillating vapor plume (2)
- Path planning (2)
- Pipe manufacturing (2)
- Preheating (2)
- Process monitoring (2)
- RSW (2)
- Refill friction stir spot welding (2)
- SMAW (2)
- Schweißnahtbewertung (2)
- Selective Laser Melting (2)
- Single pass welding (2)
- Stainless Steel (2)
- Strain rate (2)
- Submerged arc welding (2)
- Superellipse (2)
- Testing method (2)
- Thermal cycles (2)
- Thermo-fluid flow (2)
- Ti-6Al-4V (2)
- TiB2 (2)
- Transient heat transfer (2)
- Umweltwirkungen (2)
- Verfahrensvergleich (2)
- WAAM (2)
- Weld defects (2)
- Welding thermal cycle (2)
- Wire arc additive manufacturing (2)
- Wire electron beam additive manufacturing (2)
- Zinc coated steel (2)
- Zink (2)
- Ökobilanzierung (2)
- Überlappbereich (2)
- 316L (1)
- 9%Ni steel, (1)
- AC magnetic field (1)
- AGIL (1)
- AHSS (1)
- AM feature integration (1)
- Adaptive control (1)
- Adaptive welding beam oscillation (1)
- Advanced High-Strength Steel (AHSS) (1)
- Advanced high-strength steel (1)
- Advanced high-strength steels (1)
- Al-Mg-Si-Legierungen (1)
- Al/Mg alloys (1)
- AlMg0.7SiTiB filler wire (1)
- Alloy 247 (1)
- Aluminium-Druckguss (1)
- Aluminum alloys (1)
- Aluminum bronze (1)
- Analytical model (1)
- Artificial Intelligence (1)
- Artungleiche Werkstoffe (1)
- As-shielded arc welding (1)
- Aufgelöste Tragstrukturen (1)
- Auftriebskräfte (1)
- Austenitic welding electrode (1)
- Automated manufacturing (1)
- Automated welding (1)
- Automatisierte schweißtechniche Fertigung (1)
- Automobilindustrie (1)
- Automotive application (1)
- Bending test (1)
- Bewegtes Gitter (1)
- Bionik (1)
- Boundary element method (1)
- Build-up strategy (1)
- Bulging (1)
- Bulging effects (1)
- CFD model (1)
- CFD-model (1)
- Calculation time (1)
- Carbon dioxide footprint (1)
- Cimensional Accuracy (1)
- Circumferential welds (1)
- Clad steels (1)
- Clustering (1)
- Coarse grained heat affected zone (1)
- Coarse-grained heat-affected zone (1)
- Columnar crystal growth (1)
- Computer vision (1)
- Condition monitoring (1)
- Conventional Ni-based austenitic welding electrode (1)
- Convolutional neural network (1)
- Cracking (1)
- Crater (1)
- Cryogenic Steel (1)
- CuSn1 (1)
- DED-LB (1)
- DIC (1)
- Damage prediction (1)
- Deep learning (1)
- Deformed geometry (1)
- Dendrite growth (1)
- Density measurement (1)
- Deposition rate (1)
- Deposition welding (1)
- Design of experiments (1)
- Dickblech (1)
- Die-cast aluminum (1)
- Die-casted aluminum (1)
- Digital Image Correlation (1)
- Digitalization (1)
- Digitization (1)
- Direct Energy Deposition (1)
- Direct Laser Metal Deposition (1)
- Direct energy deposition (1)
- Directed Energy Depositio (1)
- Dissimilar joints (1)
- Distortion (1)
- Distortion simulation (1)
- Duplex (1)
- Duplex steels (1)
- EBSD (1)
- Edge effects (1)
- Efficient modelling (1)
- Eindringprüfung (1)
- Electro-thermomechnical model (1)
- Electrode geometry (1)
- Electromagnetic (1)
- Electromagnetic influence (1)
- Electromagnetic stirring (1)
- Electromagnetic supported degassing (1)
- Electromagnetic weld pool support system (1)
- Electron beam (1)
- Elektonenstrahlschweißen (1)
- Elektromagnetische Badstütze (1)
- Elektromagnetische Porenreduktion (1)
- Elektromagnetische Schmelzbadbeeinflussung (1)
- Elektromagnetische Schmelzbadsicherung (1)
- Elektromagnetische Schmelzbadstütze (1)
- Embedded electronics (1)
- End-crater (1)
- Energy parameters of the arc (1)
- Environmental impact categories (1)
- Equivalent stress concentration factors (1)
- FE-model (1)
- FEM (1)
- Fatigue tests (1)
- Ferritic welding electrode (1)
- Ferromagnetic steels (1)
- Ferromagnetischer Stahl (1)
- Fiber laser (1)
- Filler material distribution (1)
- Filler wire (1)
- Filler wire mixing (1)
- Fine-grained Steel (1)
- Finite Element Method (1)
- Finite element method (1)
- Finite element method (FEM) (1)
- Finite element simulation (1)
- Flange width (1)
- Flüssigmetallversprödung (1)
- Forschungsdatenmanagement (1)
- Fresnel reflection (1)
- Friction stir welding (1)
- Functionally Graded Materials (1)
- Funktionally Graded Material (1)
- Fusion zone (1)
- Fusion zone profile (1)
- Fusion zone size (1)
- Fusion zone, nickel alloys (1)
- Fügequalität (1)
- Fügetechnologie (1)
- GMA welding (1)
- GTAW (1)
- Galvanized steel (1)
- Gap bridging (1)
- Gas shielded arc welding (1)
- General analytical solutions (1)
- Gleeble (1)
- Gleeble testing (1)
- Grade S960QL steel (1)
- Grain structure (1)
- Greens function method (1)
- HSLA (1)
- Hardly separable problem (1)
- Heat Input (1)
- Heat Treatment (1)
- Heat flow (1)
- Heat input (1)
- Heissrisse (1)
- Heißrisse (1)
- Heißzug (1)
- High brightness (1)
- High power (1)
- High process speeds (1)
- High speed laser cladding (1)
- High strength steels (1)
- High-Power Welding (1)
- High-power fibre laser (1)
- High-power laser (1)
- High-power laser beam (1)
- High-strength fine-grained steels (1)
- High-strength low-alloy steel (1)
- High-strength steel sheets (1)
- Highspeed-plasma-laser-cladding (1)
- Hochleistungslaserstrahlschweißen (1)
- Hochleistungsschweißen (1)
- Hohlprofilknoten (1)
- Hold time (1)
- Hot Cracks (1)
- Hot cracking test (1)
- Hybrid Laser-Arc Welding (1)
- Hybrid components (1)
- Hybrid-laser-arc welding (1)
- Hybridschweißen (1)
- Hydrostatic and arc pressure exceed the Laplace pressure (1)
- Impact absorbed energy (1)
- Implementierung (1)
- Inconel 625 (1)
- Inconel 939 (1)
- Industrial and Manufacturing Engineering (1)
- Instumented indentation test (1)
- Integrated alignment features (1)
- KI (1)
- Kaltzähe Stähle (1)
- Kerbspannungskonzept (1)
- Keyhole mode laser beam welding (1)
- Keyhole stability (1)
- Kl (1)
- Knotenweise Zwangsbedingungen (1)
- Körperschall (1)
- Künstliche Neuronale Netze (1)
- L-PBF (1)
- LMD (1)
- LPA (1)
- Lamé curves (1)
- Lamé curves approximation (1)
- Laser (1)
- Laser Beam Welding (1)
- Laser Metal Deposition (LMD) (1)
- Laser Metal Deposition; Laser Beam Welding; Duplex; Stainless Steel (1)
- Laser Powder Bed Fusion (1)
- Laser cutting (1)
- Laser implantation (1)
- Laser keyhole welding (1)
- Laser melting (1)
- Laser metal deposition (LMD) (1)
- Laser powder bed fusion (1)
- Laser powder-based directed energy deposition (1)
- Laser surfacing (1)
- Laser- und Lichtbogenenergie (1)
- Laser-Pulver-Auftragschweißen (LPA) (1)
- Laser-Pulver-Auftragschweißen; Laserstrahlschweißen, Duplex, Pufferschichten (1)
- Laser-beam welding, (1)
- Laser-hybrid welding (1)
- Laser-plasma hybrid (1)
- Laserdispergieren (1)
- Laserpulverauftragschweißen (1)
- Leichtbauprinzipien (1)
- Lichtbogensensorik (1)
- Life Cycle Assessment (LCA) Fusion welding (1)
- Life Cycle Assessment (LCA) Impact categories (1)
- Life Cycle Assessment (LCA) Schweißprozesse (1)
- Life Cycle Assessment (LCA) Umweltwirkungen (1)
- Life cycle assessment (1)
- Lightweight principles (1)
- Liquid Metal Embrittlement (LME) (1)
- Local critical strain (1)
- Local fatigue spproaches (1)
- Low Temperature Toughness (1)
- Low feed rates (1)
- Low heat input GMA welding (1)
- Low heat input Gma welding (1)
- MAG Prozesssteuerung (1)
- MHD (1)
- MSG-Engspaltschweißen (1)
- MSG-Schweißen (1)
- Magnesium Alloy (1)
- Magnesium alloy (1)
- Magnetic bath support (1)
- Maritime Components (1)
- Matching ferritic filler metal (1)
- Material modeling (1)
- Mechanical Properties (1)
- Mechanical properties of the joints (1)
- Mechanical property (1)
- Mechanical-technological properties (1)
- Mechanisch technologische Kennwerte (1)
- Metallic vapour plume (1)
- Microstructure Tensile strength (1)
- Misalignment of edges (1)
- Misalignment of the edges (1)
- Mittelrippendefekt (1)
- Model calibration (1)
- Model order reduction (1)
- Modellierung (1)
- Molten pool behaviour (1)
- Moving mesh (1)
- Multi - physical modeling (1)
- Multi-materials joining (1)
- Multiple reflections (1)
- Narrow gap welding (1)
- Neural networks (1)
- Ni-based austenitic filler metal (1)
- Ni-based austenitic welding electrode (1)
- Ni-based superalloy (1)
- NiCrBSi (1)
- Nickel alloys (1)
- Nickel-based superalloy (1)
- Nickelbasis-Superlegierungen (1)
- Notch stress approach (1)
- Novel metrology (1)
- Numerical Simulation (1)
- Numerical analysis (1)
- Numerical simulations (1)
- Numerical welding simulation (1)
- Numerical welding simulations (1)
- Numerische ISmulation (1)
- Offshore Windenergie (1)
- Offshore wind turbines (1)
- Open science (1)
- Open source (1)
- OpenScience (1)
- Optical flow (1)
- Optical measurment technique (1)
- Optische Emissionsspektroskopie (OES) (1)
- Partial penetration welding (1)
- Pearlitic microstructure (1)
- Penetration depth (1)
- Phase field method (1)
- Pipe Welding (1)
- Pipe weld preparation (1)
- Pipeline (1)
- Pipeline steel X120 (1)
- Pipeline steel of grade X120 (1)
- Plane crystalization (1)
- Plasma cutting (1)
- Plasma-Transferred-Arc (1)
- Plasma-cut samples (1)
- Plasma-cutting (1)
- Plasma-transferred-arc (1)
- Plastic deformation (1)
- Plume heating (1)
- Porosity reduction (1)
- Porosität (1)
- Post-weld heat treatment (1)
- Powder Analysis (1)
- Precipitation hardening aluminum alloys (1)
- Preheatin (1)
- Process chain (1)
- Profilvermessung (1)
- Proper generalized decomposition (1)
- Prozesskette (1)
- Prozesssimulation (1)
- Prozessüberwachung (1)
- Prüfverfahren (1)
- Pufferschichten (1)
- Pulsed laser beam welding (1)
- Qualität (1)
- Qualitätssicherung (1)
- Rail tracks (1)
- Ray teacing (1)
- Ray tracing method (1)
- Ray-tracing (1)
- Ray-tracing methods (1)
- Recycling (1)
- Research data management (1)
- Residual stress (1)
- Resistance Spot Welding (RSW) (1)
- Rundnähte (1)
- SLM printed plasma torch (1)
- Schallemissionsanalyse (SEA) (1)
- Schutzgas (1)
- Schutzgasschweißen (1)
- Schweißeignung (1)
- Schweißen von kaltzähen Stählen (1)
- Schweißnahtgeometrie (1)
- Schweißprozesse (1)
- Schweißsimulation (1)
- Schweißstruktursimulation (1)
- Schweißtechnik (1)
- Schweißunregelmäßigkeiten (1)
- Seam geometry (1)
- Secondary heat source (1)
- Selektive-laser-melting (1)
- Sensor (1)
- Sensorik (1)
- Ship building (1)
- Shipbuilding steel (1)
- Single-pass welding (1)
- Software (1)
- Solidification behaviour (1)
- Solidification craking (1)
- Stahl und Aluminium (1)
- Stainless steels (1)
- Steady-state weld pool (1)
- Steel (1)
- Steel and Al (1)
- Strain fields prediction (1)
- Strain measurement (1)
- Strain-rate (1)
- Stress-strain behavior (1)
- Superalloy (1)
- Superelliptic Lamé curves (1)
- Support structures (1)
- Surface cracks (1)
- Surface texturing (1)
- TIG welding (1)
- Technical crack detection (1)
- Temperature behavior (1)
- Temperature distribution (1)
- Tensile properties (1)
- Tensile resistance spot welding experiment (1)
- Tensile strength (1)
- Texture (1)
- Thermo-capillary convection (1)
- Thermo-fluid dynamics (1)
- Thermographie (1)
- Thermography (1)
- Thick materials (1)
- Thick plate welding (1)
- Thick plates (1)
- Thick steel plates (1)
- Thick-Walled Steel (1)
- Thick-plate welding (1)
- Thick-walled Structures (1)
- Thin steel plates (1)
- Three-dimensional crystallization (1)
- Titanium alloy (1)
- Toughness (1)
- Transformable steels (1)
- Tubular X-joints (1)
- Tubular joints (1)
- Tungsten carbide (1)
- Turbine components (1)
- Turbulence (1)
- Two-dimensional solidification (1)
- Two-run welding technique (1)
- Ultrasonic vibration (1)
- Unterpulverschweißen (1)
- V-notch impact toughness (1)
- Vapor recondensation (1)
- Vaporization (1)
- Verzug (1)
- Viscoplasticity (1)
- WEBAM (1)
- Wear resistance (1)
- Weld end crater (1)
- Weld imperfections (1)
- Weld pool (1)
- Weld pool behavior (1)
- Weld pool geometry (1)
- Weld pool modeling (1)
- Weld pool shape approximation (1)
- Weld root (1)
- Weld seam geometry (1)
- Weldability (1)
- Welding (1)
- Welding Current (1)
- Welding Simulation (1)
- Welding parameter (1)
- Welding process simulation (1)
- Weldx (1)
- Widerstandpunktschweißen (1)
- Windkraftanlagen (1)
- Wineglass shape (1)
- Wire Electron Beam Additive Manufacturing (1)
- Wire feed laser beam welding (1)
- Wire-based additive manufacturing (1)
- Wärmenachbehandlung (1)
- X8Ni9 (1)
- Zinc (1)
- Zinkbeschichtung (1)
- deposition welding (1)
- digital image correlation (1)
- dual phase steel (1)
- highspeed plasma laser cladding (1)
- laser energy distribution (1)
- laser hybrid welding (1)
- resistance spot welding (1)
- thermal cycles (1)
- thick plate welding (1)
- Äquivalente Spannungskonzentrationsfaktoren (1)
- Äquivalente Wärmequelle (1)
- Ökonomische und ökologische Vorteile (1)
- ГИДРОДИНАМИКА (1)
- КОНВЕКЦИЯ (1)
- ЛАЗЕРНАЯ СВАРКА (1)
- МЕТОД КОНЕЧНЫХ ЭЛЕМЕНТОВ (1)
- СВАРОЧНАЯ ВАННА (1)
- ТЕМПЕРАТУРНОЕ ПОЛЕ (1)
- ТЕПЛОПРОВОДНОСТЬ (1)
- ЧИСЛЕННОЕ МОДЕЛИРОВАНИЕ (1)
Organisationseinheit der BAM
- 9.3 Schweißtechnische Fertigungsverfahren (236) (entfernen)
Eingeladener Vortrag
- nein (27)
Hybrid laser-arc welding of thick-walled ferromagnetic steels with electromagnetic weld pool support
(2018)
The hybrid laser-arc welding (HLAW) process provides many advantages over laser welding and arc welding alone, such as high welding speed, gap bridgeability, and deep penetration. The developments in hybrid laser-arc welding technology using modern high-power lasers allow single-pass welding of thick materials. This technology can be used for the heavy metal industries such as shipbuilding, power plant fabrication, and line-pipe manufacturing. The obvious problem for single-pass welding is the growth of the hydrostatic pressure with increasing thickness of materials leading to drop-out of molten metal. This phenomenon is aggravated at slow welding velocities because of increasing weld seam width followed by a decrease of Laplace pressure compensating the hydrostatic pressure. Therefore, weld pool support is necessary by welding of thick materials with slow welding velocities. The innovative electromagnetic weld pool support system is contactless and has been used successfully for laser beam welding of aluminum alloys and austenitic and ferromagnetic steels. The support system is based on generating Lorentz forces within the weld pool. These are produced by an oscillating magnetic field orientated perpendicular to the welding direction. The electromagnetic weld pool support facilitates a decrease in the welding speed without a sagging and drop-out of the melt thus eliminating the limitations of weldable material thickness.
The study deals with the application of the high-power hybrid-laser arc welding process on up to 15 mm thick pipe segments with the intention to avoid end crater imperfections during closing of the circumferential welds, where the pipes were turned during welding in 1G- and 2Gpositions.
Different techniques such as laser power ramp-down, abrupt switch-off of the laser power and change of the magnification of the laser spot diameter and defocusing of the laser beam relative to the workpiece were tested to remove the laser energy from the process. It could be shown that a high defocusing of the optic system above 40 mm with a resulting beam diameter > 2.9 mm in a short overlap length of approx.
20 mm leads to the formation of a cup-shaped weld seam, which is preferred for avoidance of cracks and pores in the end crater. A laser optics with motor-driven lens system was used for the welding experiments to defocuse the laser beam without changing the position of the arc.
Diese Arbeit zeigt erstmals die Anwendung einer elektromagnetischen Schmelzbadsicherung beim einlagigen MSG-Schweißen von dickwandigen Stählen. Die innovativen Entwicklungen im Bereich des Lichtbogenschweißverfahrens ermöglichen eine Erhöhung der Abschmelzleistung, um die Einschweißtiefe zu steigern. Somit kann die Lagenanzahl reduziert und die Produktivität gesteigert werden. Allerdings besteht insbesondere beim einlagigen Schweißen von dickwandigen Bauteilen in PA-Position ein erhöhtes Risiko für das gravitationsbedingte Austropfen der Schmelze an der Wurzel. Zur Verhinderung werden Badsicherungen eingesetzt, die mechanisch angebracht und nach dem Schweißen entfernt werden müssen, was zeit- und kostenintensiv ist.
Die im Rahmen dieser Studie eingesetzte elektromagnetische Schmelzbadsicherung wirkt dem gravitationsbedingten Austropfen der Schmelze entgegen und kompensiert den hydrostatischen Druck. Sie wirkt kontaktlos, was im Gegensatz zu herkömmlichen Badsicherungen vorteilhaft ist, so dass auf eine zeit- und kostenintensive Nachbearbeitung der Schweißnahtwurzel verzichtet werden kann. Das auf extern angelegten oszillierenden Magnetfeldern beruhende Verfahren wird dabei unterhalb des zu schweißenden Bauteils positioniert. Die Magnetfeldlinien sind quer zur Schweißrichtung ausgerichtet, sodass längs zur Schweißrichtung Wirbelströme im Werkstück und eine stets nach oben gerichtete Lorentzkraft generiert werden. Mit Hilfe der elektromagnetischen Badsicherung konnten beim einlagigen MSG-Schweißen von bis zu 10 mm dicken Blechen die Tropfenbildung vermieden werden. Die innovative Technologie ermöglicht es, dickwandige Bauteile einlagig zu schweißen und reduziert die Nachbearbeitungszeiten und -kosten deutlich.
The study deals with the influence of the heat input and the resulting cooling times on the microstructure and Charpy impact toughness of single-pass laser hybrid welded 20-mm thick high-strength steel S690QL. The main focus is on the change of the mechanical properties over the entire seam thickness. The cooling times were measured in-situ using a pyrometer and an optical fibre in three different depths of the seam where Charpy impact test specimens were also later taken. Thereby, three different heat inputs from 1.3 kJ/mm to 2 kJ/mm were investigated. Despite the observed decreased values of both t8/5-cooling time and the Charpy impact toughness in the root part of the seam, the required impact toughness of 38 J/cm2 could be reached in dependance on applied heat input, especially at the heat input of 1.6 kJ/mm.
Die technischen Entwicklungen in der Lasertechnologie in den letzten Jahrzehnten haben eine neue Generation von Hochleistungslasersystemen im Leistungsbereich bis zu 100 kW auf den Markt gebracht. Dennoch ist die industrielle Anwendung des Hochleistungslaserstrahlschweißens auf bis zu 15 mm dicke Bleche beschränkt. Mögliche Ursachen der Einschränkungen des Verfahrens sind z.B. die Sensibilität des Verfahrens auf Fertigungstoleranzen wie Spalt und Kantenversatz, die erhöhte Tropfenbildung bei höheren Blechdicken und eine inhomogene Verteilung des Zusatzwerkstoffes beim Laserhybridschweißen. In dieser Studie wird ein auf extern angelegte Magnetfelder basierte elektromagnetische Schmelzbadstütze eingesetzt, um die Grenzen des Verfahrens zu erweitern und die Herausforderungen zu minimieren. Der wesentliche Vorteil der elektromagnetischen Schmelzbadstütze ist, dass sie berührungslos arbeitet. Mit Hilfe der elektromagnetischen Schmelzbadstütze konnten bei 20 mm dicken Proben aus S355J2 die Tropfenbildung an der Wurzel vermieden werden. Zudem wurde der Einfluss der Kantenqualität auf die Schweißnahtqualität untersucht, wobei verschiedene Schneidverfahren zur Kantenvorbereitung eingesetzt wurden, wie z.B. Plasma-, Brenn- oder Laserschneiden. Es konnte gezeigt werden, dass auch bei schlechteren Kantenvorbereitung im Gegensatz zu gefrästen Bauteilen die Werkstoffe einlagig mittels Laserhybridschweißen bei einer hohen Schweißnahtqualität gefügt werden konnten. Bei plasmageschnittenen Proben wurden zudem eine Spaltüberbrückbarkeit bzw. Kantenversatz von bis zu 2 mm sicher überbrückt. Des Weiteren war es mit Hilfe der externen Magnetfelder möglich, die Durchmischung des Zusatzwerkstoffes über die gesamte Schweißnahttiefe deutlich zu homogenisieren.
The study deals with the influence of the heat input on the thermal cycles and Charpy impact toughness for hybrid laser-arc welding of 25 mm thick structural steel S355J2 using a 20-kW high-power laser in combination with an electromagnetic weld pool support. The main focus is on the change of the mechanical properties over the entire seam thickness. The cooling times were measured using a pyrometer in combination with an optical fibre in three different locations near to fusion lines corresponding to different heights of the seam. Also, Charpy impact specimens were taken from different parts of the weld joint corresponding to the different heights. The influence of the heat input was investigated for 1.8 kJ mm-1 and 3.2 kJ mm-1. Despite the observed decreased values of both t8/5-cooling time and the Charpy impact toughness in the root part of the seam, the required values could be reached in dependance on applied heat input.
The study deals with the determination of the influence of an externally applied oscillating magnetic field on the melt pool dynamics in high power laser beam and hybrid laser arc welding processes. An AC magnet was positioned under the workpiece which is generating an upward directed electromagnetic force to counteract the formation of the droplets. To visualise the melt flow characteristics, several experiments were carried out using a special technique with mild steel from S355J2 with a plate thickness of up to 20 mm and a quartz glass in butt configuration. The profile of the keyhole and the melt flow were recorded with a highspeed camera from the glass side. Additionally, the influence of the magnetic field orientation to the welding direction on the filler material dilution on laser hybrid welding was studied with variating oscillation frequency. The element distribution over the whole seam thickness was measured with X-ray fluorescence (XRF). The oscillation frequency demonstrated a great influence on the melt pool dynamics and the mixing of the elements of the filler wire. The highspeed recordings showed, under the influence of the magnetic field, that the melt is affected under strong vortex at the weld root, which also avoids the formation of droplets.
One of the challenges of the high-power hybrid laser welding of thick steels is the sensitivity of the process of the process to manufacturing tolerances. This usually leads to a time-consuming preparation of the welding edges, such as milling. The study deals with the influence of the edge quality of milled and plasma-cut steel made of S355J2 with a wall thickness of 20 mm on the laser hybrid welded seam quality. Furthermore, the gap bridgeability and the tolerances towards edge misalignment was investigated. An AC magnet was used as backing support to prevent sagging and positioned under the workpiece, to generate an upwards directed electromagnetic pressure. The profiles of the edges and the gap on the top and root side were measured using a digital camera. Single-pass laser hybrid welds of plasma-cut edges could be welded using a laser beam power of just 13.7 kW. A gap bridgeability up to 2 mm and misalignment of edges up to 2 mm could be achieved successful. Additionally, the independence of the cutting side and the welding side was shown, so that samples were welded to the opposite side to their cutting. For evaluation of internal defects or irregularities, X-ray images were carried out. Charpy impact strength tests were performed to determine the toughness of the welds.
The stability of the keyhole decreases for deep penetrated high-power laser beam welding. The keyhole tends to collapse with increasing laser power and e.g. keyhole induced porosity can occur. This study deals with the observation of the keyhole during high-power laser beam welding in partial penetration mode by means of a high-speed camera. A butt configuration of 25 mm thick structural steel and transparent quartz glass was used for the experiments. An oscillating magnetic field was applied perpendicular to the welding direction on the root side of the steel plate. The keyhole was highlighted with a coaxial diode laser. It was ascertained that the stability of the keyhole and the weld penetration depth were increased by applying an oscillating magnetic field with an oscillating frequency of 1.2 kHz and a magnetic flux density of 50 mT.
It is already known that the laser beam welding (LBW) or hybrid laser-arc welding (HLAW) processes are sensitive to manufacturing tolerances such as gaps and misalignment of the edges, especially at welding of thick-walled steels due to its narrow beam diameter. Therefore, the joining parts preferably have to be milled. The study deals with the influence of the edge quality, the gap and the misalignment of edges on the weld seam quality of hybrid laser-arc welded 20-mm-thick structural steel plates which were prepared by laser and plasma cutting. Single-pass welds were conducted in butt joint configuration. An AC magnet was used as a contactless backing. It was positioned under the workpiece during the welding process to prevent sagging. The profile of the edges and the gap between the workpieces were measured before welding by a profile scanner or a digital camera, respectively. With a laser beam power of just 13.7 kW, the single-pass welds could
be performed. A gap bridgeability up to 1 mm at laser-cut and 2 mm at plasma-cut samples could be reached respectively.
Furthermore, a misalignment of the edges up to 2 mm could be welded in a single pass. The new findings may eliminate the need for cost and time-consuming preparation of the edges.
The application of hybrid laser-arc welding (HLAW) for joining closed circumferential welds is a challenge due to the high risk of forming a defective overlap area with a shrinkage void or solidification cracks in the material thickness. A series of HLAW experiments were performed to understand the development of a faulty overlap area when closing the circumferential weld. Welding trials on flat specimens and pipe segments were supported by numerical analyses in which the thermomechanical behavior of the welds in the overlap area was investigated. Different process control strategies were tested, including variations in defocusing levels and the overlap length. The newly developed HLAW head, including laser optics with a motor-driven collimation system, made it possible to defocus the laser beam during welding without disturbing the stability of the welding process. High-level defocusing of the laser beam of more than 40 mm relative to the specimen surface with a resulting beam diameter of > 2.9 mm, and in combination with a short overlap length of 15 mm, was promising with respect to the formation of a desired cup-shaped weld profile that is resistant to solidification cracks.
Bislang kommt das Laserstrahlschweißen bzw. Laserhybridschweißen hauptsächlich bei Dickblechen mit einer Wandstärke von bis zu 15 mm zum Einsatz. Für Anwendungen über 20 mm war dieses Verfahren aufgrund einiger Herausforderungen bisher nur bedingt realisierbar. Eine von der Bundesanstalt für Materialforschung und -prüfung (BAM) entwickelte elektromagnetische Schmelzbadunterstützung ermöglicht nun ein einlagiges Schweißen von bis zu 30 mm Wandstärke.
Laserstrahlhybridschweissen von Türmen für Windkraftanlagen Ökonomische und ökologische Vorteile
(2022)
Das Laserstrahlhybridschweißen ist beim Schweißen von Türmen für Windkraftanlagen eine Alternative zum Unterpulverschweißen von Dickblechen in Mehrlagentechnik und bietet hier ökonomische und ökologische Vorteile. Der industrielle Einsatz des Verfahrens ist jedoch durch prozessspezifische Herausforderungen eingeschränkt. Die im Beitrag beschriebene kontaktlose elektromagnetische Badstütze dient zur Erweiterung des Verfahrenspotenzials im Dickblechbereich >15 mm.
Single-pass Hybrid Laser Arc Welding of Thick Materials Using Electromagnetic Weld Pool Support
(2019)
Hybrid laser-arc welding process allows single-pass welding of thick materials, provides good quality formation of joints with minimal thermal deformations and a high productivity in comparison with arc-based welding processes. Nevertheless, thick-walled steels with a thickness of 20 mm or more are still multi-pass welded using arc welding processes, due to increased process instability by increasing laser power. One limitation factor is the inadmissible formation of gravity drop-outs at the root. To prevent this, an innovative concept of electromagnetic weld pool support is used in this study. With help of such system a stable welding process can be established for 25 mm thick steel plates and beyond. Sound welds could be obtained which are tolerant to gaps and misalignment of the welded parts. The adaptation of this system to laser and hybrid laser-arc welding process can dramatically increase the potential field of application of these technologies for real industrial implementation.
The presented study deals with the performing and mechanical testing of single pass hybrid laser-arc welds (HLAW) on 25 mm thick plates made of steel grade S355J2. One of the challenges have to be solved at full penetration HLAW of thick plates is the drop formation occurring due to the disbalances of the forces acting in the keyhole and on the melt pool surface. Such irregularities mostly limit the use of high-power laser beam welding or HLAW of thick-walled constructions. To overcome this problem, an innovative concept of melt pool support based on generating Lorentz forces in the weld pool is used in this work. This method allows to perform high quality welds without sagging even for welding of 25 mm thick plates in flat position at a welding speed of 0.9 m min-1. For the obtain of full penetrated welds a laser beam power of 19 kW was needed. A high V-impact energy of up to 160 J could be achieved at the test temperature of 0 °C. Even at the most critical part in the weld root an impact energy of 60 J in average could be reached. The tensile strength of the weld reaches that of the base material. An introduce of the HLAW process with electromagnetic support of the melt pool in the industrial practice is an efficient alternative to the time- and cost-intensive arc-based multi-layer welding techniques which are established nowadays for joining of thick-walled constructions.
With global increases in clean energy demand, the natural gas is gaining in importance. Pipelines are the safest and most cost-effective way of transporting natural gas. Due to high transport volume and resulting high operation pressure, the demand for ultra-high strength steel grades such as X120 is very strong. As a result of the fact that these steels are produced by thermo-mechanical controlled processing, the welding process must be selected accordingly. Based on investigations, a high heat input such as by submerged arc welding process leads to softening in the weld metal and loss of strength whereas pure laser beam welding results in high cooling rates and deteriorate toughness of the weld metal. The objective of this research is to investigate the influence of heat input to mechanical properties of hybrid laser-arc welded pipeline steels of grade X120. Test specimens with a thickness of 20 mm could be welded without preheating in a single-pass with different welding velocities to observe the largest possible parameter window of the heat input. The achieved V-notch impact energy for hybrid laser-arc welded samples was 144±37 J at a testing temperature of -40 °C. With a tensile strength of 930±4 MPa the requirements of API 5L was achieved. To prevent gravity drop-outs at the slow welding speeds, an electromagnetic weld pool support system was used, which works contactless and is based on generating Lorentz forces. It was therefore possible to control the cooling rate in order to meet the requirements of the mechanical properties. By adapting the electromagnetic weld pool support to the laser and laser hybrid welding process, the application potential of these technologies for industrial implementation can be drastically increased.
The influence of heat input and welding speed on the microstructure and mechanical properties of single-pass hybrid laser arc welded 20mm thick plates of high-strength pipeline steel X120 were presented. The heat Input was varied in the range of 1.4 kJ mm−1 to 2.9 kJ mm−1, while the welding speed was changed between 0.5m min−1 and 1.5m min−1. A novel technique of bath support based on external oscillating electromagnetic field was used to compensate the hydrostatic pressure at low welding velocities. A major advantage of this technology is, that the welding speed and thus the cooling time t8/5 can be variated in a wide parameter window without issues regarding the weld root quality. The recommended welding thermal cycles for the pipeline steel X120 can be met by that way. All tested Charpy-V specimens meet the requirements of API 5 L regarding the impact energy. For higher heat inputs the average impact energy was 144 ± 37 J at a testing temperature of −40 °C. High heat Input above 1.6 kJ mm−1 leads to softening in the weld metal and heat-affected-zone resulting in loss of strength. The minimum tensile strength of 915 MPa could be achieved at heat inputs between 1.4 kJ mm−1 and 1.6 kJ mm−1.
The hybrid laser arc welding (HLAW) process provides many advantages such as improved gap bridgeability, deep penetration and misalignment of edges, that is why the process is used increasingly in industrial applications e.g. shipbuilding, power plant industry and line-pipe manufacturing. The obvious encountered problem for single pass welding in flat position is the gravity drop-out at low welding velocities. With the usage of an electromagnetic weld pool support system, which is based on generating Lorentz forces within the weld pool, wide seams followed by reduced welding velocities could be achieved in this study leading to the realization of a gap bridgeability up to 1 mm, misalignment of edges up to 2 mm and a single pass weld up to 28 mm thickness with a 20-kW fibre laser. These developments expand the boundaries of the HLAW process for different industrial applications. As a result, less accurate preparation of the edges would be sufficient, which saves time for manufacturing.
Hybrid laser-arc welding offers many advantages, such as deep penetration, good gap bridge-ability, and low distortion due to reduced heat input. The filler wire which is supplied to the process is used to influence the microstructure and mechanical properties of the weld seam.
A typical problem in deep penetration high-power laser beam welding with filler wire and hybrid laser-arc welding is an insufficient mixing of filler material in the weld pool, leading to a non-uniform element distribution in the seam. In this study, oscillating magnetic fields were used to form a non-conservative component of the Lorentz force in the weld pool to improve the element Distribution over the entire thickness of the material. Full penetration hybrid laser-arc welds were performed on 20-mm-thick S355J2 steel plates with a nickel-based wire for different arrangements of the oscillating magnetic field. The Energy-dispersive X-ray spectroscopy (EDS) data for the distribution of two tracing elements (Ni and Cr) were used to analyze the homogeneity of dilution of the filler wire.
With a 30° turn of the magnetic field to the welding direction, a radical improvement in the filler material distribution was demonstrated. This would lead to an improvement of the mechanical properties with the use of a suitable filler wire.
The laser hybrid welding process offers many advantages regarding deep penetration, increased welding velocity and with the help of the supplied filler wire an improved bridgeability to gap and misalignment tolerances. High power laser systems with a power of approx. 30 kW are already available on the market. Nevertheless, multi-layer technology with an arc process is still used for welding of plates from a thickness from 20 mm. A potential cause is the process instability with increasing laser power. It is inevitable that gravity drop-out due to the high hydrostatic pressure at increasing wall thickness especially at welding in flat position and with a low welding speed. The surface tension decreases with increasing root width resulting from low welding velocities. To prevent such inadmissible defects of the seam a use of weld pool support is required. Usual weld pool support systems such as ceramic or powder supports require a mechanical detachment which is time-consuming. The electromagnetic weld pool support system described in this work shows an alternative weld pool support which works contactless. It is based on generating Lorentz forces in the weld pool due to oscillating magnetic field and induced eddy currents. This innovative technology offers single pass welds up to 28 mm in flat position and reduced welding velocity with a laser power of just 19 kW. It also leads to improved mechanical-technological properties of the seams because of the slow cooling rate. With usage of an electromagnetic weld pool support the limitation of the hybrid laser arc welding process in the thick sheet metal will be extend.
Characterization of Ti-6Al-4V fabricated by multilayer laser powder-based directed energy deposition
(2022)
Laser powder-based directed energy deposition (DED-L) is increasingly being used in additive manufacturing (AM). As AM technology, DED-L must consider specific challenges. It must achieve uniform volume growth over hundreds of layers and avoid heat buildup of the deposited material. Herein, Ti–6Al–4V is fabricated using an approach that addresses these challenges and is relevant in terms of transferability to DED–L applications in AM. The assessment of the obtained properties and the discussion of their relationship to the process conditions and resulting microstructure are presented. The quality of the manufacturing process is proven in terms of the reproducibility of properties between individual blanks and with respect to the building height. The characterization demonstrates that excellent mechanical properties are achieved at room temperature and at 400 °C.
Liquid metal embrittlement (LME) cracking is a phenomenon observed during resistance spot welding (RSW) of zinccoated advanced highstrength steels (AHSS) in automotive manufacturing. In this study, severe cracks are observed at the edge of the sheet under reduced flange widths. These cracks, traversing the AHSS sheet, culminate at the edge with a width of approximately 1.2 mm.
Through combined numerical and experimental investigations, and material testing, these cracks are identified and validated as a new type of LME crack. The mechanism behind this crack formation is attributed to unique geometric conditions that, when compared to center welding, amplify radial material flow by ninefold to 0.87 mm. The resultant tangential tensile stresses approximate 760 MPa, which exceed the yield strength of the examined advanced highstrength steel (AHSS) under heightened temperature conditions, and when combined with liquid zinc, promote the formation of this new type of LME crack.
The effect of the oscillating metal vapor plume on the keyhole and molten pool behavior during the laser beam welding of AlMg3 aluminum alloys is investigated by experimental and numerical methods. The real-time height of the metal vapor plume is measured by high-speed camera observation. The obtained experimental results are used to evaluate the additional heating source and laser beam attenuation caused by the scattering and absorption based on the Beer–Lambert theory. Furthermore, the dynamic behavior of the metal vapor plume is incorporated into a 3D transient heat transfer and fluid flow model, coupled with the ray tracing method, for the laser beam welding of the AlMg3 alloy. It is found that additional heating resulting from the scattered and absorbed laser beam energy by the metal vapor plume significantly expands the shape of the molten pool on the top region. Moreover, the oscillating metal vapor plume caused the fluctuation of the high-temperature region in the molten pool. The probability of keyhole collapse at the bottom increases 17% due to the oscillating laser power induced by the laser beam attenuation. The internal interplay between the metal vapor plume, molten pool shape, and keyhole collapse is obtained. The developed model has been validated by experiments, which shows a good agreement.
The effect of the oscillating metal vapor plume on the keyhole and molten pool behavior during the laser beam welding of AlMg3 aluminum alloys is investigated by the experimental and numerical method. The real-time height of the metal vapor plume is measured by high-speed camera observation. The obtained experimental results are used to evaluate the additional heating source and laser beam attenuation caused by the scattering and absorption based on the Beer-Lambert theory. Furthermore, the dynamic behavior of the metal vapor plume is incorporated into a 3D transient heat transfer and fluid flow model, coupled with the ray tracing method, for the laser beam welding of the AlMg3 alloy. It is found that the additional heating resulting from the scattered and absorbed laser beam energy by the metal vapor plume significantly expands the shape of the molten pool on the top region. Moreover, the oscillating metal vapor plume caused the fluctuation of the molten pool shape. The probability of keyhole collapse at the bottom increases significantly to 72% due to the oscillating laser power induced by the laser beam attenuation. The internal interplay between the metal vapor plume, molten pool shape, and the keyhole collapse are obtained. The developed model has been validated by the experiments, which shows a good agreement.
The contactless magnetohydrodynamic technology has been considered as a potential and promising method to improve the weld qualities of deep penetration laser beam welding. In this paper, numerical investigations are conducted to study the influence of the auxiliary oscillating magnetic field on the porosity suppression in laser beam welding of 5754 aluminum alloy. To obtain a deeper insight into the suppression mechanism, a three-dimensional transient multi-physical model is developed to calculate the heat transfer, fluid flow, keyhole dynamic, and magnetohydrodynamics. A ray tracing algorithm is employed to calculate the laser energy distribution on the keyhole wall. A time-averaged downward Lorentz force is produced by an oscillating magnetic field. This force acts in the molten pool, leading to a dominant downward flow motion in the longitudinal section, which blocks the bubble migration from the keyhole tip to the rear part of the molten pool. Therefore, the possibility for the bubbles to be captured by the solidification front is reduced. The electromagnetic expulsive force provides an additional upward escaping speed for the bubbles of 1 m/s ~ 5 m/s in the lower and middle region of the molten pool. The simulation results are in a good agreement with experimental measurements. Based on the results obtained in this study, a better understanding of the underlying physics in laser beam welding enhanced by an auxiliary oscillating magnetic field can be provided and thus the welding process can be further optimized reducing the porosity formation.
Through experimental observation and auxiliary numerical simulation, this investigation studies the different types of grain refinement of 5754 aluminum alloy laser beam welding by applying a transverse oscillating magnetic field. Scanning electron microscope results have proved that the application of a magnetic field can reduce the average crystal branch width and increase its number. The interaction between the induced eddy current generated by the Seebeck effect and the applied external magnetic field produces a Lorentz force, which is important for the increase of the number of crystal branches. Based on the theory of dendrite fragmentation and the magnetic field-induced branches increment, the grain size reduction caused by the magnetic field is studied. Furthermore, the effects of the magnetic field are analyzed by combining a phase field method model and simulations of nucleation and grain growth. The grain distribution and average grain size after welding verifies the reliability of the model. In addition, the introduction of a magnetic field can increase the number of periodic three-dimensional solidification patterns. In the intersection of two periods of solidification patterns, the metal can be re-melted and then re-solidified, which prevents the grains that have been solidified and formed previously from further growth and generates some small cellular grains in the new fusion line. The magnetic field increases the building frequency of these solidification structures and thus promotes this kind of grain refinement.
Through experimental observation and auxiliary numerical simulation, this investigation studies the different types of grain refinement of 5754 aluminum alloy laser beam welding by applying a transverse oscillating magnetic field. Scanning electron microscope results have proved that the application of a magnetic field can reduce the average crystal branch width and increase its number. The interaction between the induced eddy current generated by the Seebeck effect and the applied external magnetic field produces a Lorentz force, which is important for the increase in the number of crystal branches. Based on the theory of dendrite fragmentation and the magnetic field-induced branches increment, the grain size reduction caused by the magnetic field is studied. Furthermore, the effects of the magnetic field are analyzed by combining a phase field method model and simulations of nucleation and grain growth. The grain distribution and average grain
size after welding verify the reliability of the model. In addition, the introduction of a magnetic field can increase the number of periodic three-dimensional solidification patterns. In the intersection of two periods of solidification patterns, the metal can be re-melted and then re-solidified, which prevents the grains, that have been solidified and formed previously, from further growth and generates some small cellular grains in the new fusion line. The magnetic field increases the building frequency of these solidification structures and thus promotes this kind of grain refinement.
Through experimental observation and auxiliary numerical simulation, this investigation studies the different types of grain refinement of 5754 aluminum alloy laser beam welding by applying a transverse oscillating magnetic field. Scanning electron microscope results have proved that the application of a magnetic field can reduce the average crystal branch width and increase its number. The interaction between the induced eddy current generated by the Seebeck effect and the applied external magnetic field produces a Lorentz force, which is important for the increase in the number of crystal branches. Based on the theory of dendrite fragmentation and the magnetic field-induced branches increment, the grain size reduction caused by the magnetic field is studied. Furthermore, the effects of the magnetic field are ana lyzed by combining a phase field method model and simulations of nucleation and grain growth. The grain distribution and average grain size after welding verify the reliability of the model. In addition, the introduction of a magnetic field can increase the number of periodic three-dimensional solidification patterns. In the intersection of two periods of solidification patterns, the metal can be re-melted and then re-solidified, which prevents the grains, that have been solidified and formed previously, from further growth and generates some small cel lular grains in the new fusion line. The magnetic field increases the building frequency of these solidification structures and thus promotes this kind of grain refinement.
Electromagnetic stirring is known to promote material flow, reduce porosity, uniform elements distribution, and refine grain in laser beam welding (LBW), which enhances the applicability of LBW in various industries. In this study, a phase-field model of dendrite growth in AA5754 Al alloy electromagnetic stirring laser beam welding was established. The model considered the thermal electromagnetic Lorentz force resulting from the interaction between the electric field generated by the Seebeck effect and the magnetic field, as well as the temperature gradient and solidification rate of the solidification interface obtained from the computational fluid dynamics electromagnetic stirring LBW model. The variation rules of dendrite growth with different magnetic parameters and effects are analyzed. Comprehensively, the magnetic field promotes the solidification rate, thus promoting interfacial instability and a large magnetic flux density leads to a faster interface instability. The solidification rate as well as the temperature gradient affect the growth rate, and the accelerated growth caused by the so lidification rate with a high frequency and a large magnetic flux density effectively inhibits the slow growth caused by the temperature gradient. The thermal electromagnetic Lorentz force is the main factor for the branch increment at low frequencies, while both thermal electromagnetic Lorentz force and temperature gradient in crease the number of branches at high frequencies. The calculated average branch numbers considering various factors in the stable stage under different magnetic parameters were consistent with the results of the scanning electron microscope tests.
Numerical analysis of ultrasonic vibration enhanced friction stir welding of dissimilar Al/Mg alloys
(2023)
The ultrasonic vibration enhanced friction stir welding (UVeFSW) process has unique advantages in joining dissimilar Al/Mg alloys. While there are complex coupling mechanisms of multi-fields in the process, it is of great significance to model this process, to reveal the influence mechanism of ultrasonic vibration on the formation of Al/Mg joints.
In this study, the acoustic-plastic constitutive equation was established by considering the influence of both ultrasonic softening and residual hardening on the flow stress at different temperatures and strain rates. And the ultrasonic induced friction reduction (UiFR) effect on friction coefficient in different relative directions at the FSW tool-workpiece interface was quantitatively calculated and analyzed.
The Al/Mg UVeFSW process model was developed through introducing the above acoustic effects into the model of Al/Mg friction stir welding (FSW). The ultrasonic energy is stronger on the aluminum alloy side. In the stirred zone, there is the pattern distribution of ultrasonic sound pressure and energy. The heat generation at the tool-workpiece contact interface and viscous dissipation were reduced after applying ultrasonic vibra-tion. Due to the UiFR effect, the projection of friction coefficient and heat flux distributions at the tool-workpiece interface present a "deformed" butterfly shape. The calculated results show that ultrasonic vibra-tion enhanced the material flow and promoted the mixing of dissimilar materials.
Die lichtbogenbasierte, additive Fertigung ist dank hoher erreichbarer Aufbauraten und nahezu uneingeschränktem Bauraum zur Fertigung großvolumiger Bauteile prädestiniert. Die Kombination etablierter Maschinenkomponenten aus Robotertechnik, Schweißtechnik und Sensorik ermöglicht den präzisen schichtweisen Materialauftrag. Die Wirkmechanismen zwischen Prozessparametern und den daraus resultierenden mechanisch-technologischen Eigenschaften der additiv gefertigten Bauteile stellen eine Herausforderung dar. Dies gilt insbesondere auch für dickwandige Bauteile. Bei der Fertigung von Bauteilen aus höherfesten Al-Mg-Si-Aluminiumlegierungen ist aufgrund der hohen Anfälligkeit für Erstarrungsrisse und der Neigung zu wasserstoffinduzierter Porosität im besonderen Maße auf das Temperaturregime und die gewählte Aufbaustrategie zu achten.
Der Einfluss der Prozessparameter auf die Bauteilqualität wurde durch die Analyse der Größe und Verteilung von Poren sowie der resultierenden Festigkeit untersucht. Darüber hinaus wurde der Einfluss einer Wärmenachbehandlungsstrategien auf das Festigkeitsverhalten analysiert. Es konnte gezeigt werden, dass dickwandige Strukturen aus höherfesten Al-Mg-Si-Aluminiumlegierungen mit mechanischen Kennwerten im Bereich des Referenzmaterials mittels MSGLichtbogenverfahren additiv gefertigt werden können.
Wire arc additive manufacturing enables the production of near-net shape large-volume metallic components leveraging an established industrial base of welding and cladding technology and adapting it for layer-wise material deposition. However, the complex relationship between the process parameters and resulting mechanical properties of the components still remains challenging. In case of high-strength Al-Mg-Si aluminum alloys, no commercial filler wires are yet available due the high susceptibility of solidification cracking as well as the necessary efforts to obtain acceptable mechanical properties. To address this need, we evaluated a novel filler wire based on AlMg0.7Si doped with a Ti5B1 master alloy to foster fine equiaxed grains within the deposited metal. The correlation between the process parameters and component quality was examined by analyzing the size and distribution of pores as well as the grain morphology. Furthermore, we evaluated the influence of different post-weld heat treatment strategies to achieve mechanical properties corresponding to the reference wrought material. We demonstrated that fine equiaxed grains in the weld metal reduced the susceptibility of solidification cracking significantly. The novel AlMg0.7Si-TiB (S Al 6063-TiB) filler wire facilitated wire arc additive manufacturing of high-strength aluminum components with mechanical properties that were almost as superior as the corresponding wrought base material.
Der Einsatz von Aluminiumlegierungen als Konstruktionswerkstoff hat in den letzten Jahren stetig zugenommen. Insbesondere höherfeste Aluminiumlegierungen, wie die Vertreter der 6000’er Aluminiumgruppe, rücken Aufgrund ihres hervorragenden Festigkeits- / Gewichtsverhältnisses immer mehr in den Fokus.
Vertreter dieser Aluminiumklasse, die als Hauptlegierungselemente Magnesium und Silizium beinhalten, weisen neben der bei allen Aluminiumlegierungen präsenten Affinität zur Porenbildung zusätzlich eine ausgeprägte Heißrissanfälligkeit auf. Die additive Verarbeitung von Al-Mg-Si-Legierungen mittels MSG Verfahren gestaltet sich daher herausfordernd.
Neben der Schweißeignung ist die geometrische Gestalt der Schweißraupe für die additive Fertigung von entscheidender Bedeutung. Spurbreite und Spurhöhe sind maßgebliche Größen, die bei der Pfadgenerierung im Hinblick auf Endkonturnähe und der Vermeidung von Ungänzen, Poren und Bildefehlern zu beachten sind.
Dieser Beitrag zeigt am Beispiel des Wire Arc Additive Manufacturing von Al-Mg-Si-Legierungen einen Ansatz, mit dem es möglich ist, zeit- und kostenintensive vollfaktorielle Parameterstudien zum Erhalt von Spurgeometrie und Schweißqualität durch dynamische Parameterstudien zu ersetzen.
The combination of laser powder bed fusion (LPBF), known for its geometrical freedom and accuracy, and the nozzle-based laser metal deposition process (LMD), known for its high build-up rates, has great potential to reduce the additive manufacturing times for large metallic parts. For the industrial application of the LPBF-LMD hybrid process chain, it is necessary to investigate the infuence of the LMD process on the LPBF substrate. In addition, the build plate material also has a signifcant impact on the occurrence of distortion along the additive manufacturing process chain. In the literature, steel build plates are often used in laser-based additive manufacturing processes of Inconel 718, since a good metallurgical Bonding can be assured whilst reducing costs in the production and restoration of the build plates. This paper examines the distortion caused by LMD material deposition and the infuence of the build plate material along the hybrid additive manufacturing process chain. Twin cantilevers are manufactured by LPBF and an additional layer is subsequently deposited with LMD. The distortion is measured in the as-built condition as well as after heat treatment. The efect of diferent LMD hatch strategies on the distortion is determined. The experiments are conducted using the nickel-base alloy Inconel 718. The results show a signifcant infuence of LMD path strategies on distortion, with shorter tool paths leading to less distortion. The remaining distortion after heat treatment is considerably dependent on the material of the build plate.
Additive manufacturing is no longer just used for the production of prototypes but already found its way into the industrial production. However, the fabrication of massive metallic parts with high geometrical complexity is still too time-consuming to be economically viable. The combination of the powder bed-based selective laser melting process (SLM), known for its geometrical freedom and accuracy, and the nozzle-based laser metal deposition process (LMD), known for its high build-up rates, has great potential to reduce the process duration. For the industrial application of the SLM-LMD hybrid process chain it is necessary to investigate the interaction of the processes and its effect on the material properties to guarantee part quality and prevent component failure. Therefore, hybrid components are manufactured and examined before and after the heat treatment regarding the microstructure and the hardness in the SLM-LMD transition zone. The experiments are conducted using the nickel-based alloy Inconel 718.
Despite the advances in hardware and software techniques, standard numerical methods fail in providing real-time simulations, especially for complex processes such as additive manufacturing applications. A real-time simulation enables process control through the combination of process monitoring and automated feedback, which increases the flexibility and quality of a process. Typically, before producing a whole additive manufacturing structure, a simplified experiment in the form of a beadon-plate experiment is performed to get a first insight into the process and to set parameters suitably. In this work, a reduced order model for the transient thermal problem of the bead-on-plate weld simulation is developed, allowing an efficient model calibration and control of the process. The proposed approach applies the proper generalized decomposition (PGD) method, a popular model order reduction technique, to decrease the computational effort of each model evaluation required multiple times in parameter estimation, control, and optimization. The welding torch is modeled by a moving heat source, which leads to difficulties separating space and time, a key ingredient in PGD simulations. A novel approach for separating space and time is applied and extended to 3D problems allowing the derivation of an efficient separated representation of the temperature.
The results are verified against a standard finite element model showing excellent agreement. The reduced order model is also leveraged in a Bayesian model parameter estimation setup, speeding up calibrations and ultimately leading to an optimized real-time simulation approach for welding experiment using synthetic as well as real measurement data.
The development of high energy laser sources enables single-pass welds of thick plates up to 30 mm, but often additional materials are needed to influence the properties of the weld seams. However, the homogenous distribution of filler materials in form of e.g. electrodes is only possible up to 7 mm while the elements are only traceable up to a depth of 14 mm. To overcome this problem a two-step process is used where first the edges of the weld partners are coated with the filler material by laser metal deposition (LMD) and afterwards are welded by laser beam. Single-pass welds with electromagnetic weld pool support of 30 mm thick S355 J2+N-plates with austenitic AISI 316L-coatings were investigated as well as the influence of the coatings to the penetration depth of the laser beam without electromagnetic weld pool support in double-sided joints. The weld seams were tested by X-ray inspection and cross sections.
AISI 2205 duplex stainless steel is used in a variety of industries, including the chemical and petrochemical industries. This is due to its high tensile strength combined with good ductility and corrosion resistance. However, in laser beam welding, these properties are negatively afected by the high cooling rates typical of the welding process. The resulting higher ferrrite content in the weld metal than in the base material leads to a reduction in the ductility and corrosion resistance of the welded joint. To overcome this problem, in this study, thick plates were coated by direct energy deposition (DED) prior to laser beam welding, whereas a duplex powder mixture containing a higher nickel concentration was used as a coating material. To improve the weld quality for the proposed two-step process, a method of additional material deposition instead of conventional tack weld was investigated. The resulting welded joints showed a well-balanced austenite to ferrite ratio and their properties and microstructure were verifed by metallographic analysis, electron backscatter difraction and Charpy impact testing. Using the standard ASTM G48 test method, it was found that the corrosion resistance of the welds was improved by a factor of four in average compared to the conventionally welded joints. The resulting properties, such as good ductility and corrosion resistance, of the welds with pre-coated edges showed good agreement with those of the base metal and confrmed the proposed two-step process as a promising alternative to the conventional approaches for welding thick duplex stainless steel plates.
Vor allem in den letzten Jahren ist das Interesse der Industrie an der additiven Fertigung deutlich gestiegen. Die Vorteile dieser Verfahren sind zahlreich und ermöglichen eine ressourcenschonende, kundenorientierte Fertigung von Bauteilen, welche zur stetigen Entwicklung neue Anwendungsbereiche und Werkstoffe führen. Aufgrund der steigenden Anwendungsfälle, nimmt auch der Wunsch nach Betriebssicherheit unabhängig von anschließenden kostenintensiven zerstörenden und zerstörungsfreien Prüfverfahren zu. Zu diesem Zweck werden im Rahmen des von der BAM durchgeführten Themenfeldprojektes „Prozessmonitoring in Additive Manufacturing“ verschiedenste Verfahren auf ihre Tauglichkeit für den in-situ Einsatz bei der Prozessüberwachung in der additiven Fertigung untersucht. Hier werden drei dieser in-situ Verfahren, die Thermografie, die optische Emissionsspektroskopie und die Schallmissionsanalyse für den Einsatz beim Laser-Pulver-Auftragschweißen betrachtet.
Duplex stainless steels combine the positive properties of its two phases, austenite and ferrite. Due to its good corrosion resistance, high tensile strength, and good ductility, it has multiple applications. But laser beam welding of duplex steels changes the balanced phase distribution in favor of ferrite. This results in a higher vulnerability to corrosion and a lower ductility. Herein, different powder combinations consisting of duplex and nickel for coating layers by laser metal deposition (LMD) are investigated. Afterward, laser tracks are welded, and the temperature cycles are measured. The ferrite content of the tracks is analyzed by feritscope, metallographic analysis, and electron backscatter diffraction. The goal is the development of a powder mixture allowing for a duplex microstructure in a two-step process, where first the edges of the weld partners are coated with the powder mixture by LMD and second those edges are laser beam welded. The powder mixture identified by the pretests is tested in the two-step process and analyzed by metallographic analysis, energy-dispersive X-ray spectroscopy, and
Vickers hardness tests. The resulting weld seams show a balanced duplex microstructure with a homogenous nickel distribution and a hardness of the weld seam similar to the base material.
Duplex stainless steels combine the positive properties of its two phases, austenite and ferrite. Due to its good corrosion resistance, high tensile strength and good ductility it has multiple applications. But laser beam welding of duplex steels changes the balanced phase distribution in favor of ferrite. This results in a higher vulnerability to corrosion and a lower ductility. In this study different powder combinations consisting of duplex and nickel for coating layers by laser metal deposition are investigated. Afterwards laser tracks are welded, and the temperature cycles measured. The ferrite content of the tracks are analyzed by feritscope, metallographic analysis and Electron Backscatter Diffraction. The goal is the development of a powder mixture allowing for a duplex microstructure in a two-step process, where firstly the edges of the weld partners are coated with the powder mixture by LMD and secondly those edges are laser beam welded. The powder mixture identified by the pretests is tested in the two-step process and analyzed by metallographic analysis, energy dispersive X-ray spectroscopy and Vickers hardness tests. The resulting weld seams show a balanced duplex microstructure with a homogenous nickel distribution and a hardness of the weld seam similar to the base material.
Duplexstähle finden aufgrund ihrer Eigenschaften, wie der guten Korrosionsbeständigkeit, einer hohen Festigkeit bei gleichzeitig guter Duktilität häufig industrielle Anwendung. Durch die hohen Abkühlraten beim Laserstrahlschweißen weisen Schweißnähte jedoch anstelle eines ausgeglichenen Duplexgefüges einen deutlich erhöhten Ferritanteil, im Vergleich zum Basiswerkstoff, auf. Dies führt zu einer verringerten Duktilität sowie Korrosionsbeständigkeit. Um dieses Problem zu lösen, wurde ein Prozess entwickelt, der auf einer Kantenbeschichtung mit nickelhaltigem Zusatzmaterial der zu fügenden Bleche mittels Laser-Pulver-Auftragschweißen (LPA) basiert.
Die resultierenden Schweißnähte wurden zerstörend anhand von Schliffbildern, EDX-Aufnahmen, Härtemessungen und Kerbschlagbiegeversuchen geprüft.
Duplexstähle finden in vielen industriellen Bereichen Anwendung, dies ist nicht zuletzt ihren hervorragenden Eigenschaften, wie einer guten Korrosionsbeständigkeit, einer guten Duktilität bei trotzdem hoher Festigkeit, zuzuschreiben. Diese Eigenschaften werden jedoch durch das Schweißen, vor allem das Laserstrahlschweißen, beeinträchtigt, da die hohen Abkühlraten zu erhöhten Ferritanteilen im Schweißgut führen. Mit Hilfe eines zweistufigen Prozesses, bei dem die Kanten der Fügepartner vor dem Schweißen mit nickelhaltigem Pulver beschichtet werden, soll dieses Problem für dickwandige Bleche gelöst werden.
In diesem Zusammenhang wurden verschiedene Prozessparameter für den Laser-Pulver-Auftragschweiß-Prozess untersucht sowie die defektfreie Schweißung dieser beschichteten Kanten mit unterschiedlichen Prozessgasen.
Because of its excellent corrosion resistance, high tensile strength and high ductility, duplex stainless steel 2205 offers many areas of application. Though laser beam welding accompanied by high cooling rates, duplex steels tend to perform higher ferrite contents in weld metal as the base metal, which leads to a reduction of ductility and corrosion resistance of the weld joint. To overcome this problem, a solution, based on buttering the plate edges by laser metal deposition (LMD) with material containing higher Ni concentrations prior to laser welding was suggested.
In this context different process parameters for LMD process were investigated. In a second step the possibility of welding those edges defect free while achieving balanced austenite-ferrite ratio was verified with metallographic analysis, Electron Backscatter Diffraction (EBSD) and impact testing according to Charpy.
Laser metal deposition (LMD) as an additive manufacturing technique became increasingly important in recent years and thus the demand for component safety. This is the reason, for the need for reliable in-situ defect detection techniques. For laser beam weld seams an optical measurement technique based on an optical flow algorithm was successfully used to define the critical straining conditions that lead to hot cracking. This algorithm was adapted for bead-on-plate weld seams on LMD deposited layers of IN718 alloy while performing external strain on the specimen in an externally loaded hot cacking test facility. The resulting transversal hot cracks along the weld seam were localized via X-Ray inspection and the type of cracking confirmed by Scanning Electron Microscopy (SEM). The strain distribution was measured in the vicinity of the solidification front and correlated to the detected hot cracks. Based on the results this technique could be adopted for LMD experiments.
The shape of the parts, created by the technology of direct laser metal deposition (DLMD), is influenced by various parameters, for example, the power and diameter of the laser source spot. The contribution of energy from the laser affects the temperature distribution in the formed layers. The changing temperature in the working area entails a Change in the geometry of the layers and affects the stability of the process. In this paper, experiments on the measurement of temperature cycles in the DLMD process with different directions of the filling track are carried out. An infrared camera was used to measure thermal cycles. The calibration of the acquired data (i.e. correspondence table between the intensity of thermal radiation of the material and the absolute temperature) was done with help of two-color pyrometer ex situ and in situ measurements. The experiments are carried out on two materials 316L and Inconel 718. The effect of the maximum temperature on the layer height is shown, and thermal cycles in the formation of layers for different filling strategies are presented.
New developments in nickel-based superalloys and production methods, such as the use of additive manufacturing (AM), can result in innovative designs for turbines. It is crucial to understand how the material behaves during the AM process to advance industrial use of these techniques. An analytical model based on reaction-diffusion formalism is developed to better explain the solidification behavior of the material during laser metal deposition (LMD). The well-known Scheil-Gulliver theory has some drawbacks, such as the assumption of equilibrium at the solid-liquid interface, which is addressed by this method. The solidified fractions under the Scheil model and the pure equilibrium model are calculated using CALPHAD simulations. Differential scanning calorimeter is used to measure the heat flow during the solid-liquid phase transformation, the result of which is further converted to solidified fractions. The analytical model is compared with all the other models for validation.
Die Laserimplantation erlaubt die Herstellung verschleißbeständiger, erhabener Mikrostrukturen (Implants) auf Stahloberflächen durch ein diskontinuierliches Dispergieren von keramischen Partikeln mittels gepulster Laserstrahlung. Durch die flexible Anordnung separierter Implants zu komplexen Mustern erlaubt das Verfahren eine gezielte Oberflächenstrukturierung zur Beeinflussung des Reibungs- und Verschleißverhaltens. Insbesondere erwies sich Titandiborid (TiB2) als Implantationsmaterial für geeig-net, da eine Manipulation der Implantgeometrie in einem breiten Bereich vorgenommen werden konnte, ohne dass Materialdefekte wie Risse oder Poren auftraten.
Ziel der Untersuchungen war es, den Einfluss implantierter TiB2-Partikel auf die Materialeigenschaften von X153CrMoV12 zu ermitteln. Hierfür wurden im Rahmen der Arbeit die Laserparameter (Pulsleistung und -dauer) in einem breiten Parameterfeld variiert und vergleichende Untersuchungen an TiB2 implan-tierten Zonen sowie an punktuell umschmelzstrukturierten Zonen durchgeführt. Die Ergebnisse zeigen, dass eine reine Umschmelzstrukturierung zu einer deutlichen Reduktion der Oberflächenhärte aufgrund erhöhter Restaustenitgehalte (γR) führt. Im Gegensatz dazu führt das Laserimplantieren von TiB2-Partikeln zu einer deutlichen Härtesteigerung in den kuppel- oder ringförmigen Implants. Härtewerte von bis zu 1800 HV1 resultieren aus dispergierten TiB2-Primärpartikeln sowie in-situ ausgeschiedenen Se-kundärphasen, durch die der Restaustenitanteil zudem deutlich reduziert wird.
In einer Vielzahl technischer Anwendungen spielt die Aufrechterhaltung eines definierten Reibungs- und Verschleißverhaltens zwischen bewegten Oberflächen für die Sicherheit und Funktionalität eine entscheidende Rolle. Die Oberflächentechnik versucht durch geeignete Verfahren die Randschichten zu ertüchtigen, um Reibung und Verschleiß zu kontrollieren. Eine Verbesserung der Materialeigenschaften kann durch flächige Beschichtungen erreicht werden. Zusätzlich ermöglichen Oberflächenstrukturierungen breite Möglichkeiten zur Beeinflussung des Schmierungszustandes bzw. der Kontaktbedingungen. Neben Negativstrukturen bieten ebenfalls erhabene Mikrostrukturen großes Potenzial zur Beeinflussung des tribologischen Verhaltens. Ihr Einsatz ist aber aufgrund der besonderen Verschleißproblematik erhabener Strukturen momentan limitiert, so dass in der Regel zusätzliche verschleißreduzierende Beschichtungen notwendig werden.
In diesem Beitrag wurde das Verfahren der Laserimplantation angewandt, mit dem erhabene und separierte Oberflächenstrukturen hoher Verschleißfestigkeit in einem Fertigungsschritt erzeugbar sind. Das Verfahren basiert auf einem lokalisierten Dispergieren von Hartstoffpartikeln. Hierfür wurde erstmalig ein gepulster Faserlaser mit hoher Strahlqualität zur Erzeugung punkt- und linienförmiger Mikrostrukturen angewandt. Versuche wurden auf dem Kaltarbeitsstahl X153CrMoV12 unter Anwendung von Titandiborid als Hartstoff durchgeführt. Anhand von Härtemessungen konnte gezeigt werden, dass sowohl punkt- als auch linienförmige Strukturen mit Härten über 1000 HV1 und einer feinkörnigen Mikrostruktur mit feinverteilten Hartstoffpartikeln herstellbar sind. Des Weiteren war es möglich, die Implantgeometrien, welche an Querschliffen und durch Weißlichtinterferometeraufnahmen erfasst wurden, durch die Pulsleistung und Pulsdauer zu steuern.
In einer Vielzahl technischer Anwendungen spielt die Aufrechterhaltung eines definierten Reibungs- und Verschleißverhaltens zwischen bewegten Oberflächen für die Sicherheit und Funktionalität eine ent-scheidende Rolle. Die Oberflächentechnik versucht durch geeignete Verfahren die Randschichten zu ertüchtigen, um Reibung und Verschleiß zu kontrollieren. Eine Verbesserung der Materialeigenschaften kann durch flächige Beschichtungen erreicht werden. Zusätzlich ermöglichen Oberflächenstrukturierun-gen breite Möglichkeiten zur Beeinflussung des Schmierungszustandes bzw. der Kontaktbedingungen. Neben Negativstrukturen bieten ebenfalls erhabene Mikrostrukturen großes Potenzial zur Beeinflussung des tribologischen Verhaltens. Ihr Einsatz ist aber aufgrund der besonderen Verschleißproblematik er-habener Strukturen momentan limitiert, so dass in der Regel zusätzliche verschleißreduzierende Be-schichtungen notwendig werden.
In diesem Beitrag wurde das Verfahren der Laserimplantation angewandt, mit dem erhabene und sepa-rierte Oberflächenstrukturen hoher Verschleißfestigkeit in einem Fertigungsschritt erzeugbar sind. Das Verfahren basiert auf einem lokalisierten Dispergieren von Hartstoffpartikeln. Hierfür wurde erstmalig ein gepulster Faserlaser mit hoher Strahlqualität zur Erzeugung punkt- und linienförmiger Mikrostrukturen angewandt. Versuche wurden auf dem Kaltarbeitsstahl X153CrMoV12 unter Anwendung von Titandibo-rid als Hartstoff durchgeführt. Anhand von Härtemessungen konnte gezeigt werden, dass sowohl punkt- als auch linienförmige Strukturen mit Härten über 1000 HV1 und einer feinkörnigen Mikrostruktur mit feinverteilten Hartstoffpartikeln herstellbar sind. Des Weiteren war es möglich, die Implantgeometrien, welche an Querschliffen und durch Weißlichtinterferometeraufnahmen erfasst wurden, durch die Puls-leistung und Pulsdauer zu steuern.