Ingenieurwissenschaften und zugeordnete Tätigkeiten
Filtern
Erscheinungsjahr
- 2019 (38) (entfernen)
Dokumenttyp
- Zeitschriftenartikel (17)
- Beitrag zu einem Tagungsband (16)
- Vortrag (5)
Sprache
- Englisch (38) (entfernen)
Schlagworte
Organisationseinheit der BAM
Eingeladener Vortrag
- nein (5)
Single-pass Hybrid Laser Arc Welding of Thick Materials Using Electromagnetic Weld Pool Support
(2019)
Hybrid laser-arc welding process allows single-pass welding of thick materials, provides good quality formation of joints with minimal thermal deformations and a high productivity in comparison with arc-based welding processes. Nevertheless, thick-walled steels with a thickness of 20 mm or more are still multi-pass welded using arc welding processes, due to increased process instability by increasing laser power. One limitation factor is the inadmissible formation of gravity drop-outs at the root. To prevent this, an innovative concept of electromagnetic weld pool support is used in this study. With help of such system a stable welding process can be established for 25 mm thick steel plates and beyond. Sound welds could be obtained which are tolerant to gaps and misalignment of the welded parts. The adaptation of this system to laser and hybrid laser-arc welding process can dramatically increase the potential field of application of these technologies for real industrial implementation.
The presented study deals with the performing and mechanical testing of single pass hybrid laser-arc welds (HLAW) on 25 mm thick plates made of steel grade S355J2. One of the challenges have to be solved at full penetration HLAW of thick plates is the drop formation occurring due to the disbalances of the forces acting in the keyhole and on the melt pool surface. Such irregularities mostly limit the use of high-power laser beam welding or HLAW of thick-walled constructions. To overcome this problem, an innovative concept of melt pool support based on generating Lorentz forces in the weld pool is used in this work. This method allows to perform high quality welds without sagging even for welding of 25 mm thick plates in flat position at a welding speed of 0.9 m min-1. For the obtain of full penetrated welds a laser beam power of 19 kW was needed. A high V-impact energy of up to 160 J could be achieved at the test temperature of 0 °C. Even at the most critical part in the weld root an impact energy of 60 J in average could be reached. The tensile strength of the weld reaches that of the base material. An introduce of the HLAW process with electromagnetic support of the melt pool in the industrial practice is an efficient alternative to the time- and cost-intensive arc-based multi-layer welding techniques which are established nowadays for joining of thick-walled constructions.
With global increases in clean energy demand, the natural gas is gaining in importance. Pipelines are the safest and most cost-effective way of transporting natural gas. Due to high transport volume and resulting high operation pressure, the demand for ultra-high strength steel grades such as X120 is very strong. As a result of the fact that these steels are produced by thermo-mechanical controlled processing, the welding process must be selected accordingly. Based on investigations, a high heat input such as by submerged arc welding process leads to softening in the weld metal and loss of strength whereas pure laser beam welding results in high cooling rates and deteriorate toughness of the weld metal. The objective of this research is to investigate the influence of heat input to mechanical properties of hybrid laser-arc welded pipeline steels of grade X120. Test specimens with a thickness of 20 mm could be welded without preheating in a single-pass with different welding velocities to observe the largest possible parameter window of the heat input. The achieved V-notch impact energy for hybrid laser-arc welded samples was 144±37 J at a testing temperature of -40 °C. With a tensile strength of 930±4 MPa the requirements of API 5L was achieved. To prevent gravity drop-outs at the slow welding speeds, an electromagnetic weld pool support system was used, which works contactless and is based on generating Lorentz forces. It was therefore possible to control the cooling rate in order to meet the requirements of the mechanical properties. By adapting the electromagnetic weld pool support to the laser and laser hybrid welding process, the application potential of these technologies for industrial implementation can be drastically increased.
Hybrid laser-arc welding offers many advantages, such as deep penetration, good gap bridge-ability, and low distortion due to reduced heat input. The filler wire which is supplied to the process is used to influence the microstructure and mechanical properties of the weld seam.
A typical problem in deep penetration high-power laser beam welding with filler wire and hybrid laser-arc welding is an insufficient mixing of filler material in the weld pool, leading to a non-uniform element distribution in the seam. In this study, oscillating magnetic fields were used to form a non-conservative component of the Lorentz force in the weld pool to improve the element Distribution over the entire thickness of the material. Full penetration hybrid laser-arc welds were performed on 20-mm-thick S355J2 steel plates with a nickel-based wire for different arrangements of the oscillating magnetic field. The Energy-dispersive X-ray spectroscopy (EDS) data for the distribution of two tracing elements (Ni and Cr) were used to analyze the homogeneity of dilution of the filler wire.
With a 30° turn of the magnetic field to the welding direction, a radical improvement in the filler material distribution was demonstrated. This would lead to an improvement of the mechanical properties with the use of a suitable filler wire.
Additive manufacturing is no longer just used for the production of prototypes but already found its way into the industrial production. However, the fabrication of massive metallic parts with high geometrical complexity is still too time-consuming to be economically viable. The combination of the powder bed-based selective laser melting process (SLM), known for its geometrical freedom and accuracy, and the nozzle-based laser metal deposition process (LMD), known for its high build-up rates, has great potential to reduce the process duration. For the industrial application of the SLM-LMD hybrid process chain it is necessary to investigate the interaction of the processes and its effect on the material properties to guarantee part quality and prevent component failure. Therefore, hybrid components are manufactured and examined before and after the heat treatment regarding the microstructure and the hardness in the SLM-LMD transition zone. The experiments are conducted using the nickel-based alloy Inconel 718.
The shape of the parts, created by the technology of direct laser metal deposition (DLMD), is influenced by various parameters, for example, the power and diameter of the laser source spot. The contribution of energy from the laser affects the temperature distribution in the formed layers. The changing temperature in the working area entails a Change in the geometry of the layers and affects the stability of the process. In this paper, experiments on the measurement of temperature cycles in the DLMD process with different directions of the filling track are carried out. An infrared camera was used to measure thermal cycles. The calibration of the acquired data (i.e. correspondence table between the intensity of thermal radiation of the material and the absolute temperature) was done with help of two-color pyrometer ex situ and in situ measurements. The experiments are carried out on two materials 316L and Inconel 718. The effect of the maximum temperature on the layer height is shown, and thermal cycles in the formation of layers for different filling strategies are presented.
To increase the competitiveness of jacket substructures compared to monopiles a changeover from an individual towards a serial jacket production based on automated manufactured tubular joints combined with standardized pipes has to be achieved. Therefore, this paper addresses fatigue tests of automatically welded tubular X-joints focusing on the location of the technical fatigue crack. The detected location of the technical crack is compared to numerical investigations predicting the most fatigue prone notch considering the structural stress approach as well as the notch stress approach. Besides, the welding process of the automated manufactured tubular X-joints is presented.
Single-pass Hybrid Laser Arc Welding of Thick Materials Using Electromagnetic Weld Pool Support
(2019)
Hybrid laser-arc welding process allows single-pass welding of thick materials, provides good quality formation of joints with minimal thermal deformations and a high productivity in comparison with arc-based welding processes. Nevertheless, thick-walled steels with a thickness of 20 mm or more are still multi-pass welded using arc welding processes, due to increased process instability by increasing laser power. One limitation factor is the inadmissible formation of gravity drop-outs at the root. To prevent this, an innovative concept of electromagnetic weld pool support is used in this study. With help of such system a stable welding process can be established for 25 mm thick steel plates and beyond. Sound welds could be obtained which are tolerant to gaps and misalignment of the welded parts. The adaptation of this system to laser and hybrid laser-arc welding process can dramatically increase the potential field of application of these technologies for real industrial implementation.
The present work deals with the development of a strategy for the prevention of end crater defects in high-power laser welding of thick-walled circumferential welds. A series of experiments were performed to understand the influence of the welding parameters on the formation of end crater defects such as pores, cracks, excessive root-side drop-through and shrinkage cavities in the overlap area. An abrupt switch-off of the laser power while closing the circumferential weld leads to a formation of a hole which passes through the whole welded material thickness. A laser power ramp causes solidification cracks which are initiated on the transition from full-penetration mode to partial penetration. Strategies with a reduction of the welding speed shows a creation of inadmissible root sagging. Defocusing the laser beam led to promising results in terms of avoiding end crater defects. Cracks and pores in the overlap area could be effectively avoided by using defocusing techniques. A strategy for avoiding of end crater imperfections was tested on flat specimens of steel grade S355J2 with a wall thickness of 10 mm and then transferred on the 9.5 mm thick pipe sections made of high-strength steel X100Q.
The presented study deals with the performing and mechanical testing of single pass hybrid laser-arc welds (HLAW) on 25 mm thick plates made of steel grade S355J2. One of the challenges have to be solved at full penetration HLAW of thick plates is the drop formation occurring due to the disbalances of the forces acting in the keyhole and on the melt pool surface. Such irregularities mostly limit the use of high-power laser beam welding or HLAW of thick-walled constructions. To overcome this problem, an innovative concept of melt pool support based on generating Lorentz forces in the weld pool is used in this work. This method allows to perform high quality welds without sagging even for welding of 25 mm thick plates in flat position at a welding speed of 0.9 m min-1. For the obtain of full penetrated welds a laser beam power of 19 kW was needed. A high V-impact energy of up to 160 J could be achieved at the test temperature of 0 °C. Even at the most critical part in the weld root an impact energy of 60 J in average could be reached. The tensile strength of the weld reaches that of the base material. An introduce of the HLAW process with electromagnetic support of the melt pool in the industrial practice is an efficient alternative to the time- and cost-intensive arc-based multi-layer welding techniques which are established nowadays for joining of thick-walled constructions.