Multi-principal element alloys (MPEAs) are innovative materials that have attracted extensive research attention within the last decade. MPEAs are characterized by a solid solution of equiatomic metallic elements. Depending on the number of elements, they are also referred as high entropy alloys (HEAs with n ≥ 4 elements like CoCrFeMnNi) and medium-entropy alloys (MEA with n = 3 elements CoCrNi). Depending on the alloy concept, MPEAs show exceptional properties in terms of mechanical performance or corrosion resistance at extreme environments. In that connection, hydrogen and its challenges for the most metallic materials gets more and more important. MPEAs are candidate materials for the substitution of conventional materials like austenitic stainless steels e.g., at very high-pressure up to 1000 bar. Those pressures are typically reached in valves or compressors for refueling of tanks with operational pressure of 700 bar. So far, the susceptibility of HEA/MEAs to hydrogen assisted cracking (if any) and the especially the underlying hydrogen uptake and diffusion was not within the scientific scope and not investigated in detail yet. For that reason, we focused on the hydrogen absorption the characterization of the hydrogen diffusion and trapping at elevated temperatures in a CoCrFeMnNi-HEA (each element with 20 at.-%) and CoCrNi-MEA, each element with 33.3 at.-%). As reference grade, the commercially available austenitic stainless steel AISI 316L was investigated. High-pressure hydrogen charging was conducted at different pressures in autoclave environment with maximum value of 1,000 bar. Thermal desorption analysis (TDA) via carrier gas hot extraction with coupled mass spectrometry was used with a max. heating rate of 0.5 K/s up to 650 °C. The measured desorption spectra of the different samples were deconvoluted into a defined number of individual peaks. The individually calculated peak temperatures allowed the definition of activation energies for predominant trap sites in the respective materials as well as the percentage share of the totally absorbed hydrogen concentration. The results present for the first time the complex interaction of both MPEAs and high-pressure hydrogen charging. A deconvolution of four peaks was selected and a main desorption peak was identified the dominant hydrogen trap containing the biggest share of the absorbed hydrogen concentration. The chemical composition an austenitic phase of both MPEAs is responsible for delayed hydrogen diffusion and strong, but mostly reversible, trapping. The comparison with the 316L samples showed significantly higher activation energies in the MPEAs, whereas hydrogen was also trapped at very high extraction temperatures. The absorbed maximum hydrogen concentration at 1,000 bar was 130 ppm for the CoCrFeMnNi-HEA, 50 ppm for the CoCrNi-MEA and 80 ppm for the 316L. It is interesting that the CoCrFeMnNi-HEA has obviously a way higher trapping capability compared to the conventional austenitic 316L, which could be a major advantage in terms of resistance to hydrogen assisted cracking.
High-entropy alloys (HEAs) are innovative high-performance materials that have attracted more and more research attention. HEAs are characterized by a solid solution of typically five equiatomic metallic elements. In addition, medium-entropy alloys (MEA, with three elements) are of interest and become more and more important. Depending on the alloy concept, HEAs and MEAs show exceptional mechanical properties, especially high-strength and ductility combinations at both cryogenic and elevated temperatures combined with excellent corrosion resistance. Future structural HEA/MEA components can be exposed to potential applications with hydrogen containing environments like high-temperature water in pressurized nuclear reactors or aerospace structures. Other potential applications could be in materials for vessel walls in the field of cryogenic and high-pressure hydrogen storage. So far, the susceptibility of HEAs/MEAs to hydrogen assisted cracking (if any) and the hydrogen diffusion is not investigated in detail yet and can limit or extend possible applications of HEA/MEA as structural materials. In our work, we focused on the hydrogen absorption, diffusion, and distribution in a HEA (CoCrFeMnNi the original Cantor-alloy) and a MEA (CoCrNi). Cathodic hydrogen charging was carried out for the hydrogen ingress, and thermal desorption analysis (TDA) revealed complex hydrogen trapping in both alloy types up to 300 °C. The absorbed total hydrogen concentrations were > 100 ppm for the HEA and > 40 ppm for MEA. In addition, the assessment of the peak deconvolution is not trivial and must consider both experimental and microstructure influences.
Future structural components made of the novel high-entropy (HEA) or medium-entropy alloys (MEA) components can be potentially exposed to hydrogen containing environments like high-temperature water in pressurized nuclear reactors or aerospace structures. Further applications are vessels wall materials for cryogenic or high-pressure hydrogen storage. So far, the susceptibility of HEA/MEAs to hydrogen assisted cracking (if any) and the hydrogen diffusion is not investigated in detail yet and can limit or extend possible applications of HEA/MEA as structural materials. In our work, we focused on the hydrogen absorption, diffusion, and distribution in a HEA (Co20Cr20Fe20Mn20Ni20, the original Cantor-alloy) and a MEA (Co33.3Cr33.3Ni33.3). Conventional cathodic hydrogen charging was carried out for the hydrogen ingress in the materials. Thermal desorption analysis (TDA) via carrier gas hot extraction with coupled mass spectrometry revealed complex hydrogen trapping in both alloy types up to 300 °C. The absorbed total hydrogen concentrations were ≥ 70 ppm for the HEA and approximately 40 ppm for the MEA-type. Although both materials have different chemical composition, the TDA spectra were comparable. In addition, it was shown that the consideration of the sample geometry is an important influence on the sample temperature. It decreases the effective applied heating rate, which must be anticipated for each hydrogen peak after deconvolution of the spectra. This increases the activation energy and shifts the peak to lower temperatures. As a result, microstructure effects can be separated from experimental boundary conditions like the concentration gradient due to the charging process and later thermal activation.
Hochentropie-Legierungen (HEAs) zeichnen sich durch einen Mischkristall-System aus mindestens fünf und Mittelentropie-Legierungen (MEAs) durch mindestens drei Hauptlegierungselemente aus, in äquiatomarer Zusammensetzung. Sie zeigen außergewöhnliche Anwendungseigenschaften, wie z.B. hohe Festigkeit, Duktilität oder Korrosionsbeständigkeit. Zukünftige HEA/MEA-Komponenten aufgrund ihrer Eigenschaften für wasserstoffhaltige Umgebungen (wie Behälter für kryogene oder Hochdruckspeicherung) von Interesse. Daher ist die Bewertung der Wasserstoffabsorption und die Diffusion in diesen Materialien von großer Bedeutung. Dazu wurden in unserer Studie eine CoCrFeMnNi-HEA und eine CoCrNi-MEA untersucht. Die Proben wurden elektrochemisch mit Wasserstoff beladen. Für die Ermittlung des Wasserstoffdiffusionsverhaltens wurde die thermische Desorptionsanalyse (TDA) mit unterschiedlichen Heizraten bis zu 0,250 K/s angewandt. Die nachfolgende Peakentfaltung der Signale führte zu Hochtemperatur-Desorptionsspitzen und Wasserstofftrapping auch über 280°C. Eine resultierende Gesamtwasserstoffkonzentration > 40 ppm wurde für den MEA ermittelt und > 100 ppm für den HEA. Dies deutet auf zwei wichtige Effekte hin:
(1) verzögerte Wasserstoffdiffusion und (2) eine beträchtliche Menge an getrapptem Wasserstoff auch bei hoher Temperatur. Beide Effekte können hinsichtlich einer wasserstoffunterstützten Rissbildung kritisch werden, dies erfordert jedoch weitere Untersuchungen. Zusätzlich erfolgte die Bestimmung des lokalen Volta-Potentials mittels hochauflösender Kelvin-Sonden-Kraft-Mikroskopie (SKPFM). Die ermittelten Scans zeigen einen bestimmten Einfluss der Wasserstoffbeladung auf die Potentiale.
Hydrogen-assisted cracking is a critical combination of local microstructure, mechanical load and hydrogen concentration. Welded microstructures of low-alloyed creep-resistant Cr-Mo-V steels show different hydrogen trapping kinetics. This influences the adsorbed hydrogen concentration as well as the diffusion by moderate or strong trapping. A common approach to describe hydrogen traps is by their activation energy that is necessary to release hydrogen from the trap. In the present study, Cr-Mo-V steel T24 (7CrMoVTiB10-10) base material and TIG weld metal were investigated. Electrochemically hydrogen charged specimens
were analyzed by thermal desorption analysis (TDA) with different linear heating rates. The results show two different effects. At first, the microstructure effect on trapping is evident in terms of higher hydrogen concentrations in the weld metal and increased activation energy for hydrogen release. Secondly, it is necessary to monitor the real specimen temperature. A comparison between the adjusted heating rate and the real specimen temperature shows that the calculated activation energy varies by factor two. Thus, the trap character in case of the base material changes to irreversible at decreased temperature. Hence, the effect of the experimental procedure must be considered as well if evaluating TDA results. Finally, realistic temperature assessment is mandatory for calculation of activation energy via TDA.