Biomaterials for bone replacement and grafting should possess sufficient strength, be bioresorbable and demonstrate osteoconductive and osteoinductive properties. However, resorption of modern materials for bone grafting (hydroxyapatite (HA) and tricalcium phosphate (TCP)) is reported, in some cases, to be not enough, this is why the search for more soluble compounds compared to HA and TCP looks very perspective. A possible way to increase ceramics solubility leads to partial substitution of Ca2+ -ions in Ca3(PO4)2 by alkali cations, like Na+ or/and K+. Improvement of solubility stems from decreasing lattice energy of a substituted phase, as well as the increase in hydration energy of the ions releasing from the phase to ambient solution. From this viewpoint, bioceramics based on compositions from Ca3(PO4)2 - CaKPO4 - CaNaPO4 ternary system seems to be prospective for bone replacement and grafting in the sense of resorption properties. At the same time, one should bear in mind that solubility level (resorbability) is governed not only by reduction of lattice energy but also by microstructure features. Grain sizes and porosity contribute much to dissolution rate making the study of sintering of the ceramics mentioned above highly important.
To control Ca3(PO4)2 - CaKPO4 - CaNaPO4 based ceramic microstructure it is necessary to know possible phase transformations in the system and the way to manage microstructure by sintering schedule or sintering process.
In this work, an isothermal section for phase diagram of Ca3(PO4)2 - CaKPO4 - CaNaPO4 ternary system is studied with several techniques. According to the XRD of quenched samples, this phase triangle has four single-phase areas at 1200˚C (Figure 1). It was shown that single-phase CaK0.6Na0.4PO4 cannot be sintered to full-dense ceramics by conventional sintering regardless time-temperature schedule. Two-step sintering technique, beneficial in the case of HA-ceramics, was unsuccessful in all cases of calcium-alkali phosphate compositions. However, field-assisted sintering techniques like, e.g. Spark Plasma Sintering (SPS), can overcome this problem due to significant impact on grain boundary diffusion. In connection with this fact, grains grow much slower retaining sintering process in a pore control regime. In this work CaK0.6Na0.4PO4 low-porous ceramics was also fabricated by FAST-methods of sintering. Moreover, other alternative sintering techniques, such as reaction sintering, may be useful in accelerating ions diffusion but stopping excessive grain growth.Strength properties of ceramics were evaluated by B3B-testing, micro- and nanoindentation techniques. Fracture toughness also becomes higher with potassium content increase, guiding porosity level.
Resorption properties of sintered ceramics were studied in different solutions with pH=5 and 7.4.
Acknowledgements. The research of sintering processes in calcium phosphate materials were funded by RFBR according to the research project № 18-33-00974.
An investigation of the two-component phase diagram of the CaNaPO4- CaKPO4system performed using various analysis techniques is reported. The continuous solid solution series of α-CaMPO4 existing above 700 °C undergoes eutectoid decomposition during cooling to β-CaMPO4-based solid solutions enriched with Na and K, and to an intermediate nonstoichiometric compound with an ideal composition of CaK0.6Na0.4PO4. All three compounds exhibit significant volumetric effects associated with first-order phase transitions, with positive volume changes under cooling for the intermediate compound. Increased K content in ceramics based on CaKyNa1-yPO4 compositions enhances the strength properties of those ceramics, including their fracture toughness, which is associated with increased density. Increased K content also has a smaller effect of inducing phase transformations accompanied by strong volume changes.
Accelerator magnets that can reach magnetic fields well beyond the Nb-Ti performance limits are presently being built and developed, using Nb3Sn superconductors. This technology requires reaction heat treatment (RHT) of the magnet coils, during which Nb3Sn is formed from its ductile precursor materials (a “wind and react” approach). The Nb3Sn microstructure and microchemistry are strongly influenced by the conductor fabrication route, and by the Phase changes during RHT. By combining in situ differential scanning calorimetry, high Energy synchrotron x-ray diffraction, and micro-tomography experiments, we have acquired a unique data set that describes in great detail the phase and microstructure changes that take place during the processing of restacked rod process (RRP), powder-in-tube (PIT), and internal tin (IT) Nb3Sn wires. At temperatures below 450 ° the phase evolutions in the three wire types are similar, with respectively solid state interdiffusion of Cu and Sn, Cu6Sn5 formation, and Cu6Sn5 peritectic transformation. Distinct differences in phase evolutions in the wires are found when temperatures exceed 450 °C. The volume changes of the conductor during RHT are a difficulty in the production of Nb3Sn accelerator magnets. We compare the wire diameter changes measured in situ by dilatometry with the phase and void volume evolution of the three types of Nb3Sn wire. Unlike the Nb3Sn wire length changes, the wire diameter evolution is characteristic for each Nb3Sn wire type. The strongest volume increase, of about 5%, is observed in the RRP wire, where the main diameter increase occurs above 600 °C upon Nb3Sn formation.