Recently developed fibre lasers provide multi-kilowatt beam power with high quality at impressive energy efficiency. Combined with gas metal arc welding (GMAW) equipment these lasers can be used in a hybrid process to weld thick-walled constructions single-pass, that are currently welded using multi-pass techniques. The main benefits are a reduction of heat induced distortions, due to the low heat input, as well as savings in filler material and process time. Probable applications can be found in power generation, ship building and pipeline constructions. An orbital (girth) laser-hybrid process using a 20 kW fibre laser and a GMAW torch is currently examined at the BAM, Berlin. The aim of this research is to obtain a stable and crack free girth welding process and to demonstrate its application in pipeline construction. The experiments are carried out on 16 mm thick plates as well pipe rings with 36" (914 mm) pipe diameter of X65. Particular welding parameters, such as welding speed, GMAW power, arc length are varied and their influence on the appearance of the weld in the different welding positions is analyzed. Even though issues remain that demand further research it could already be shown that the rings can be welded using a girth hybrid process that is divided into two half girth processes in downward direction.
The aim of the present work was to investigate the possibilities of hybrid laser arc welding regarding reliable production of longitudinal welds of high strength pipe steels X80 and X120 and to evaluate achievable mechanical properties of laser hybrid welds. The study focused on weld toughness examination in low temperature range up to -60 °C. SЮТЭКЛХО ПТХХОЫ ЦКЭОЫТКХЬ were identified in the context of this task. It could be shown that metal cored electrodes guaranteed sufficient Charpy impact toughness at low temperature for both investigated materials. Modern arc welding technologies such as modified pulsed spray arc were used to promote deeper Penetration of the filler material into the narrow laser welding gap. Edge preparation with a 14 mm deep root face was considered as optimum, because no penetration of the filler material could be detected beyond this depth limit and therefore any metallurgical influences on the weld metal properties through the welding wire could be excluded.
Unusual Corrosion Behavior of 1.4542 Exposed a Laboratory Saline Aquifer Water CCS-Environment
(2017)
Differently heat treated coupons of 1.4542 were kept at T=60 °C and ambient pressure as well as p=100 bar for 700 h - 8000 h in an a) water saturated supercritical CO2 and b) CO2-saturated synthetic aquifer environment similar to on-shore CCS-sites in the Northern German Basin. Surface corrosion layers are homogeneous but unusually discontinuously ellipsoidal. After 8000 h at 100 bar maximum corrosion rate in the liquid phase is approximately 0.014 mm/year, with normalizing providing best corrosion resistance and approximately 0.003 mm/year in the supercritical phase where hardening+tempering at 670 °C leads to lowest corrosion rates.