The study deals with the determination of the influence of an externally applied oscillating magnetic field on the melt pool dynamics in high power laser beam and hybrid laser arc welding processes. An AC magnet was positioned under the workpiece which is generating an upward directed electromagnetic force to counteract the formation of the droplets. To visualise the melt flow characteristics, several experiments were carried out using a special technique with mild steel from S355J2 with a plate thickness of up to 20 mm and a quartz glass in butt configuration. The profile of the keyhole and the melt flow were recorded with a highspeed camera from the glass side. Additionally, the influence of the magnetic field orientation to the welding direction on the filler material dilution on laser hybrid welding was studied with variating oscillation frequency. The element distribution over the whole seam thickness was measured with X-ray fluorescence (XRF). The oscillation frequency demonstrated a great influence on the melt pool dynamics and the mixing of the elements of the filler wire. The highspeed recordings showed, under the influence of the magnetic field, that the melt is affected under strong vortex at the weld root, which also avoids the formation of droplets.
The stability of the keyhole decreases for deep penetrated high-power laser beam welding. The keyhole tends to collapse with increasing laser power and e.g. keyhole induced porosity can occur. This study deals with the observation of the keyhole during high-power laser beam welding in partial penetration mode by means of a high-speed camera. A butt configuration of 25 mm thick structural steel and transparent quartz glass was used for the experiments. An oscillating magnetic field was applied perpendicular to the welding direction on the root side of the steel plate. The keyhole was highlighted with a coaxial diode laser. It was ascertained that the stability of the keyhole and the weld penetration depth were increased by applying an oscillating magnetic field with an oscillating frequency of 1.2 kHz and a magnetic flux density of 50 mT.
Through experimental observation and auxiliary numerical simulation, this investigation studies the different types of grain refinement of 5754 aluminum alloy laser beam welding by applying a transverse oscillating magnetic field. Scanning electron microscope results have proved that the application of a magnetic field can reduce the average crystal branch width and increase its number. The interaction between the induced eddy current generated by the Seebeck effect and the applied external magnetic field produces a Lorentz force, which is important for the increase of the number of crystal branches. Based on the theory of dendrite fragmentation and the magnetic field-induced branches increment, the grain size reduction caused by the magnetic field is studied. Furthermore, the effects of the magnetic field are analyzed by combining a phase field method model and simulations of nucleation and grain growth. The grain distribution and average grain size after welding verifies the reliability of the model. In addition, the introduction of a magnetic field can increase the number of periodic three-dimensional solidification patterns. In the intersection of two periods of solidification patterns, the metal can be re-melted and then re-solidified, which prevents the grains that have been solidified and formed previously from further growth and generates some small cellular grains in the new fusion line. The magnetic field increases the building frequency of these solidification structures and thus promotes this kind of grain refinement.
Through experimental observation and auxiliary numerical simulation, this investigation studies the different types of grain refinement of 5754 aluminum alloy laser beam welding by applying a transverse oscillating magnetic field. Scanning electron microscope results have proved that the application of a magnetic field can reduce the average crystal branch width and increase its number. The interaction between the induced eddy current generated by the Seebeck effect and the applied external magnetic field produces a Lorentz force, which is important for the increase in the number of crystal branches. Based on the theory of dendrite fragmentation and the magnetic field-induced branches increment, the grain size reduction caused by the magnetic field is studied. Furthermore, the effects of the magnetic field are analyzed by combining a phase field method model and simulations of nucleation and grain growth. The grain distribution and average grain
size after welding verify the reliability of the model. In addition, the introduction of a magnetic field can increase the number of periodic three-dimensional solidification patterns. In the intersection of two periods of solidification patterns, the metal can be re-melted and then re-solidified, which prevents the grains, that have been solidified and formed previously, from further growth and generates some small cellular grains in the new fusion line. The magnetic field increases the building frequency of these solidification structures and thus promotes this kind of grain refinement.
Through experimental observation and auxiliary numerical simulation, this investigation studies the different types of grain refinement of 5754 aluminum alloy laser beam welding by applying a transverse oscillating magnetic field. Scanning electron microscope results have proved that the application of a magnetic field can reduce the average crystal branch width and increase its number. The interaction between the induced eddy current generated by the Seebeck effect and the applied external magnetic field produces a Lorentz force, which is important for the increase in the number of crystal branches. Based on the theory of dendrite fragmentation and the magnetic field-induced branches increment, the grain size reduction caused by the magnetic field is studied. Furthermore, the effects of the magnetic field are ana lyzed by combining a phase field method model and simulations of nucleation and grain growth. The grain distribution and average grain size after welding verify the reliability of the model. In addition, the introduction of a magnetic field can increase the number of periodic three-dimensional solidification patterns. In the intersection of two periods of solidification patterns, the metal can be re-melted and then re-solidified, which prevents the grains, that have been solidified and formed previously, from further growth and generates some small cel lular grains in the new fusion line. The magnetic field increases the building frequency of these solidification structures and thus promotes this kind of grain refinement.
Electromagnetic stirring is known to promote material flow, reduce porosity, uniform elements distribution, and refine grain in laser beam welding (LBW), which enhances the applicability of LBW in various industries. In this study, a phase-field model of dendrite growth in AA5754 Al alloy electromagnetic stirring laser beam welding was established. The model considered the thermal electromagnetic Lorentz force resulting from the interaction between the electric field generated by the Seebeck effect and the magnetic field, as well as the temperature gradient and solidification rate of the solidification interface obtained from the computational fluid dynamics electromagnetic stirring LBW model. The variation rules of dendrite growth with different magnetic parameters and effects are analyzed. Comprehensively, the magnetic field promotes the solidification rate, thus promoting interfacial instability and a large magnetic flux density leads to a faster interface instability. The solidification rate as well as the temperature gradient affect the growth rate, and the accelerated growth caused by the so lidification rate with a high frequency and a large magnetic flux density effectively inhibits the slow growth caused by the temperature gradient. The thermal electromagnetic Lorentz force is the main factor for the branch increment at low frequencies, while both thermal electromagnetic Lorentz force and temperature gradient in crease the number of branches at high frequencies. The calculated average branch numbers considering various factors in the stable stage under different magnetic parameters were consistent with the results of the scanning electron microscope tests.
The development of high energy laser sources enables single-pass welds of thick plates up to 30 mm, but often additional materials are needed to influence the properties of the weld seams. However, the homogenous distribution of filler materials in form of e.g. electrodes is only possible up to 7 mm while the elements are only traceable up to a depth of 14 mm. To overcome this problem a two-step process is used where first the edges of the weld partners are coated with the filler material by laser metal deposition (LMD) and afterwards are welded by laser beam. Single-pass welds with electromagnetic weld pool support of 30 mm thick S355 J2+N-plates with austenitic AISI 316L-coatings were investigated as well as the influence of the coatings to the penetration depth of the laser beam without electromagnetic weld pool support in double-sided joints. The weld seams were tested by X-ray inspection and cross sections.
AISI 2205 duplex stainless steel is used in a variety of industries, including the chemical and petrochemical industries. This is due to its high tensile strength combined with good ductility and corrosion resistance. However, in laser beam welding, these properties are negatively afected by the high cooling rates typical of the welding process. The resulting higher ferrrite content in the weld metal than in the base material leads to a reduction in the ductility and corrosion resistance of the welded joint. To overcome this problem, in this study, thick plates were coated by direct energy deposition (DED) prior to laser beam welding, whereas a duplex powder mixture containing a higher nickel concentration was used as a coating material. To improve the weld quality for the proposed two-step process, a method of additional material deposition instead of conventional tack weld was investigated. The resulting welded joints showed a well-balanced austenite to ferrite ratio and their properties and microstructure were verifed by metallographic analysis, electron backscatter difraction and Charpy impact testing. Using the standard ASTM G48 test method, it was found that the corrosion resistance of the welds was improved by a factor of four in average compared to the conventionally welded joints. The resulting properties, such as good ductility and corrosion resistance, of the welds with pre-coated edges showed good agreement with those of the base metal and confrmed the proposed two-step process as a promising alternative to the conventional approaches for welding thick duplex stainless steel plates.
Duplex stainless steels combine the positive properties of its two phases, austenite and ferrite. Due to its good corrosion resistance, high tensile strength, and good ductility, it has multiple applications. But laser beam welding of duplex steels changes the balanced phase distribution in favor of ferrite. This results in a higher vulnerability to corrosion and a lower ductility. Herein, different powder combinations consisting of duplex and nickel for coating layers by laser metal deposition (LMD) are investigated. Afterward, laser tracks are welded, and the temperature cycles are measured. The ferrite content of the tracks is analyzed by feritscope, metallographic analysis, and electron backscatter diffraction. The goal is the development of a powder mixture allowing for a duplex microstructure in a two-step process, where first the edges of the weld partners are coated with the powder mixture by LMD and second those edges are laser beam welded. The powder mixture identified by the pretests is tested in the two-step process and analyzed by metallographic analysis, energy-dispersive X-ray spectroscopy, and
Vickers hardness tests. The resulting weld seams show a balanced duplex microstructure with a homogenous nickel distribution and a hardness of the weld seam similar to the base material.
The development of high energy laser sources enables single-pass welds of thick plates up to 30 mm, but often additional materials are needed to influence the properties of the weld seams. However, the homogenous distribution of filler materials in form of e.g. electrodes is only possible up to 7 mm while the elements are only traceable up to a depth of 14 mm. To overcome this problem a two-step process is used where first the edges of the weld partners are coated with the filler material by laser metal deposition (LMD) and afterwards are welded by laser beam. Single-pass welds with electromagnetic weld pool support of 30 mm thick S355 J2+N-plates with austenitic AISI 316L-coatings were investigated as well as the influence of the coatings to the penetration depth of the laser beam without electromagnetic weld pool support in double-sided joints. The weld seams were tested by X-ray inspection and cross sections.
In recent years, it was shown that the introduction of additional oscillating and permanent magnetic fields to laser beam and laser-arc hybrid welding can bring several beneficial effects.
Examples are a contactless weld pool support for metals of high thickness suffering from severe drop-out when being welded conventionally or an enhanced stirring to improve the mixing of added filler material in the depth of the weld pool to guarantee homogeneous resulting mechanical properties of the weld. The latest research results show the applicability to various metal types over a wide range of thicknesses and welding conditions. The observations made were demonstrated in numerous experimental studies and a deep understanding of the interaction of the underlying physical mechanisms was extracted from numerical calculations.
Notch impact toughness of laser beam welded thick sheets of cryogenic nickel alloyed steel X8Ni9
(2020)
This research work deals with the investigations of the impact toughness of laser beam welded 14.5 mm thick sheets made of cryogenic steel X8Ni9 as a function of preheating. This 9% nickel alloyed steel is widely used in the liquefied natural gas (LNG) industry. An application of highly efficient welding processes such as high-power laser beam welding (LBW) in LNG sector requires an understanding of the interactions between the LBW process parameters and weld properties, in particular the impact toughness. The results show that the original fine-grained martensitic microstructure of the base metal (BM) is significantly changed by melting and crystallization during the LBW, what can lead to a decrease in the impact toughness of the weld metal (WM) below the required level. An optimal preheating temperature range leads to the favorable thermal welding cycle and is of remarkable importance for maintaining the notch impact toughness of laser beam welded joints of these thick steel sheets. A parameter window was identified in which V-notch impact toughness comparable to that of the BM at -196 °C was achieved.
The present work deals with the recently confirmed widening of the weld pool interface, known as a bulging effect, and its relevance in high power laser beam welding. A combined experimental and numerical approach is utilized to study the influence of the bulge on the hot cracking formation and the transport of alloying elements in the molten pool. A technique using a quartz glass, a direct-diode laser illumination, a high-speed camera, and two thermal imaging cameras is applied to visualize the weld pool geometry in the longitudinal section. The study examines the relevance of the bulging effect on both, partial and complete penetration, as well as for different sheet thicknesses ranging from 8 mm to 25 mm. The numerical analysis shows that the formation of a bulge region is highly dependent on the penetration depth and occurs above 10 mm penetration depth. The location of the bulge correlates strongly with the cracking location. The obtained experimental and numerical results reveal that the bulging effect increases the hot cracking susceptibility and limits the transfer of alloying elements from the top of the weld pool to the weld root.
The present work deals with the recently confirmed widening of the weld pool interface, known as a bulging effect, and its relevance in high power laser beam welding. A combined experimental and numerical approach is utilized to study the influence of the bulge on the hot cracking formation and the transport of alloying elements in the molten pool. A technique using a quartz glass, a direct-diode laser illumination, a high speed camera, and two thermal imaging cameras is applied to visualize the weld pool geometry in the longitudinal section. The study examines the relevance of the bulging effect on both, partial and complete penetration, as well as for different sheet thicknesses ranging from 8 mm to 25 mm. The numerical analysis shows that the formation of a bulge region is highly dependent on the penetration depth and occurs above 10 mm penetration depth. The location of the bulge correlates strongly with the cracking location. The obtained experimental and numerical results reveal that the bulging effect increases the hot cracking susceptibility and limits the transfer of alloying elements from the top of the weld pool to the weld root
The present work deals with the development of a strategy for the prevention of end crater defects in high-power laser welding of thick-walled circumferential welds. A series of experiments were performed to understand the influence of the welding parameters on the formation of end crater defects such as pores, cracks, excessive root-side drop-through and shrinkage cavities in the overlap area. An abrupt switch-off of the laser power while closing the circumferential weld leads to a formation of a hole which passes through the whole welded material thickness. A laser power ramp causes solidification cracks which are initiated on the transition from full-penetration mode to partial penetration. Strategies with a reduction of the welding speed shows a creation of inadmissible root sagging. Defocusing the laser beam led to promising results in terms of avoiding end crater defects. Cracks and pores in the overlap area could be effectively avoided by using defocusing techniques. A strategy for avoiding of end crater imperfections was tested on flat specimens of steel grade S355J2 with a wall thickness of 10 mm and then transferred on the 9.5 mm thick pipe sections made of high-strength steel X100Q.
Die Wärmeverteilung des Lasers beim Laserstrahltiefschweißen ist für die Formgebung der Dampfkapillare und für die Schweißbaddynamik entscheidend. In dieser Arbeit werden die Laserwärmeverteilung und deren Einflüsse auf die Schweißbadtiefe sowie -breite numerisch anhand des Ray-Tracing-Verfahrens analysiert. Hierbei wird der La-serstrahl in mehreren Strahlenbündeln bzw. Subrays unterteilt. Diesbezüglich soll der Pfad der Subrays präzis be-rechnet werden, um die Dynamik der Dampfkapillare und des Schweißbades eines realen Schweißprozesses rich-tig abzubilden. Zu diesem Zweck beschäftigt sich die vorliegende Arbeit mit der Genauigkeitsverbesserung der Kontaktposition und der Reflexionsrichtung der Subrays auf der freien Oberfläche anhand der Level-Set-Methode. Um die Güte dieses Simulationsansatzes zu gewährleisten, wurde eine Gegenüberstellung mit den zwei klassischen Ray-Tracing-Verfahren mittels drei verschiedenen Benchmark-Testreihen durchgeführt. Anschließend wurden die Versuchsergebnisse zur Validierung der implementierten numerischen Ansätze verwendet. Im Rahmen dieser Arbeit kann es gezeigt werden, dass unterschiedliche Wärmeverteilung aufgrund der verschiedenen Ray-Tracing-Verfahren deutlich zu erkennen ist, welche wiederum die Schweißbaddynamik sowie die lokalisierte Dampfkapil-lardynamik stark beeinflussen. Ferner wurde es bestätigt, dass die implementierte Level-Set-Methode zu einer ge-naueren Ermittlung der Kontaktposition und der Reflexionsrichtung der Subrays und somit zu einer Verbesserung der simulierten Schmelzkontur führt.
Der Absorptionsgrad metallischer Werkstoffe spielt bei Fügeprozessen mit einer Strahlungsquelle wie dem Hochleistungslaserstrahltiefschweißen eine bedeutende Rolle. Dieser beeinflusst die Menge der absorbierten Laserenergie, welche zum Aufschmelzen sowie zur lokalen Verdampfung des zu verbindenden Materials führt. Eine der wichtigsten Eigenschaften der Laserstrahlabsorption ist die Temperaturabhängigkeit. Dennoch wird sie in vielen Simulationsarbeiten häufig ignoriert und stattdessen ein angepasster Parameter zur Kalibrierung der Ergebnisse implementiert. Diese Vorgehensweise wirkt sich negativ auf die Zuverlässigkeit sowie die Genauigkeit des numerischen Modells sowie auf die Vorhersagbarkeit der Simulationsergebnisse aus. In der vorliegenden Arbeit wird die Temperaturabhängigkeit der Laserabsorption in ein selbstkonsistentes zweiphasiges Modell unter Berücksichtigung der gekoppelten 3D-Fluidströmung und Wärmeübertragung einbezogen. Die berechnete Laserstrahlabsorption wird durch die temperaturabhängigen Materialeigenschaften, die Lasercharakteristik und den Einfallswinkel des Laserstrahls bestimmt. Die freie Oberfläche jeder Phase wird mithilfe der volume-of-fluid Methode, kurz VOF, berechnet und die Laser-Material-Wechselwirkung wird durch ein neulich implementiertes Ray-Tracing-Verfahren modelliert, die auf einem lokalisierten Level-Set-Algorithmus basiert. Anschließend wird die transiente Wärmeeinbringung und die Geometrie der Schweißnaht analysiert und mit dem temperaturunabhängigen Absorptionsmodell verglichen. Es wurde festgestellt, dass die Temperaturabhängigkeit der Laserabsorption entscheidend für die genaue Bestimmung der Wärmeeinbringung und der Schmelzbadgeometrie ist. Das entwickelte Modell wurde anhand der experimentellen Untersuchungen validiert und die Bedeutung der Temperaturabhängigkeit bei der Laserstrahlabsorption wurde für die Simulation des Laserstrahltiefschweißens aufgeklärt.
Die Wärmeverteilung des Lasers beim Laserstrahltiefschweißen ist für die Formgebung der Dampfkapillare und für die Schweißbaddynamik entscheidend. In dieser Arbeit werden die Laserwärmeverteilung und deren Einflüsse auf die Schweißbadtiefe sowie -breite numerisch anhand des Ray-Tracing-Verfahrens analysiert. Hierbei wird der La-serstrahl in mehreren Strahlenbündeln bzw. Subrays unterteilt. Diesbezüglich soll der Pfad der Subrays präzis berechnet werden, um die Dynamik der Dampfkapillare und des Schweißbades eines realen Schweißprozesses richtig abzubilden. Zu diesem Zweck beschäftigt sich die vorliegende Arbeit mit der Genauigkeitsverbesserung der Kontaktposition und der Reflexionsrichtung der Subrays auf der freien Oberfläche anhand der Level-Set-Methode. Um die Güte dieses Simulationsansatzes zu gewährleisten, wurde eine Gegenüberstellung mit den zwei klassi-schen Ray-Tracing-Verfahren mittels drei verschiedenen Benchmark-Testreihen durchgeführt. Anschließend wur-den die Versuchsergebnisse zur Validierung der implementierten numerischen Ansätze verwendet. Im Rahmen dieser Arbeit kann es gezeigt werden, dass unterschiedliche Wärmeverteilung aufgrund der verschiedenen Ray-Tracing-Verfahren deutlich zu erkennen ist, welche wiederum die Schweißbaddynamik sowie die lokalisierte Dampfkapillardynamik stark beeinflussen. Ferner wurde es bestätigt, dass die implementierte Level-Set-Methode zu einer genaueren Ermittlung der Kontaktposition und der Reflexionsrichtung der Subrays und somit zu einer Ver-besserung der simulierten Schmelzkontur führt.
The high amount of resource consumption of fusion welding processes offers the potential to reduce their environmental impact. While the driving forces are known froma qualitative perspective, the quantitative assessment of the crucial parameters is not a trivial task. Therefore, herein, a welding-specific methodology to utilize life cycle assessment as a tool for evaluating the environmental impact of fusion welding processes is presented. In this context, two welding processes, resistance spot welding and laser beam welding, are analyzed for two different use cases.
These comprise the welding of shear test specimens and a cap profile made of electrogalvanized sheets of DC 05þ ZE (1.0312) as representative of an automotive application. For both welding processes, the main influences on the resulting environmental impact categories are evaluated and compared. The requirements for ecological efficient welding processes are discussed and implemented.
The spatial laser energy absorption inside the keyhole is decisive for the dynamic molten pool behaviors and the resultant weld properties in high-power laser beam welding (LBW). In this paper, a numerical simulation of the LBW process, considering the 3D transient heat transfer, fluid flow, and keyhole dynamics, is implemented, in which the free surface is tracked by the volume-of-fluid algorithm. The underlying laser-material interactions i.e., the multiple reflections and Fresnel absorption, are considered by an advanced ray-tracing method based on a localized Level-Set strategy and a temperature-dependent absorption coefficient. The laser energy absorption is analyzed from a time-averaged point of view for a better statistical representation. It is found for the first time that a noticeable drop of the time-averaged laser energy absorption occurs at the focus position of the laser beam, and the rest region of the keyhole has relatively homogenous absorbed energy. This unique absorption pattern may lead to a certain keyhole instability and have a strong correlation with the detrimental bulging and narrowing phenomena in the molten pool. The influence of the different focus positions of the laser beam on the keyhole dynamics and molten pool profile is also analyzed and compared. The obtained numerical results are compared with experimental measurements to assure the validity of the proposed model.
The spatial laser energy absorption inside the keyhole is decisive for the dynamic molten pool behaviors and the resultant weld properties in high-power laser beam welding (LBW). In this paper, a numerical simulation of the LBW process, considering the 3D transient heat transfer, fluid flow, and keyhole dynamics, is implemented, in which the free surface is tracked by the volume-of-fluid algorithm. The underlying laser-material interactions, i.e., the multiple reflections and Fresnel absorption, are considered by an advanced ray-tracing method based on a localized level-set strategy and a temperature-dependent absorption coefficient. The laser energy absorption is analyzed from a time-averaged point of view for a better statistical representation. It is found for the first time that a significant drop in the time-averaged laser energy absorption occurs at the focus position of the laser beam and that the rest of the keyhole region has relatively homogeneous absorbed energy. This unique absorption pattern may lead to a certain keyhole instability and have a strong correlation with the detrimental bulging and narrowing phenomena in the molten pool. The influence of different focus positions of the laser beam on the keyhole dynamics and molten pool profile is also analyzed. The obtained numerical results are compared with experimental measurements to ensure the validity of the proposed model.
The spatial laser energy absorption inside the keyhole is decisive for the dynamic molten pool behaviors and the resultant weld properties in high-power laser beam welding (LBW). In this paper, a numerical simulation of the LBW process, considering the 3D transient heat transfer, fluid flow, and keyhole dynamics, is implemented, in which the free surface is tracked by the volume-of-fluid algorithm. The underlying laser-material interactions i.e., the multiple reflections and Fresnel absorption, are considered by an advanced ray-tracing method based on a localized Level-Set strategy and a temperature-dependent absorption coefficient. The laser energy absorption is analyzed from a time-averaged point of view for a better statistical representation. It is found for the first time that a noticeable drop of the time-averaged laser energy absorption occurs at the focus position of the laser beam, and the rest region of the keyhole has relatively homogenous absorbed energy. This unique absorption pattern may lead to a certain keyhole instability and have a strong correlation with the detrimental bulging and narrowing phenomena in the molten pool. The influence of the different focus positions of the laser beam on the keyhole dynamics and molten pool profile is also analyzed and compared. The obtained numerical results are compared with experimental measurements to assure the validity of the proposed model.
An accurate and efficient description of the spatial distribution of laser energy is a crucial factor for the modeling of laser material processing, e.g., laser welding, laser cutting, or laser-based additive manufacturing. In this study, a 3D heat transfer and fluid flow model coupled with the volume-of-fluid algorithm for free surface tracking is developed for the simulation of molten pool dynamics in high-power laser beam welding. The underlying laser-material interactions, i.e., the multiple reflections and Fresnel absorption, are considered by a raytracing method. Two strategies of free surface reconstruction used in the ray-tracing method are investigated: a typical piecewise linear interface calculation (PLIC)-based method and a novel localized level-set method. The PLIC-based method is discrete, resulting in noncontinuous free surface reconstruction. In the localized level-set method, a continuous free surface is reconstructed, and, thus, the exact reflection points can be determined. The calculated spatial laser energy distribution and the corresponding molten pool dynamics from the two methods are analyzed and compared. The obtained numerical results are evaluated with experimental measurements to assure the validity of the proposed model. It is found that distinct patterns of the beam multiple reflections are obtained with the different free surface reconstructions, which shows significant influence not only on the molten pool behaviors but also on the localized keyhole dynamics.
An accurate and efficient description of the spatial distribution of laser energy is a crucial factor for the modeling of laser material processing, e.g., laser welding, laser cutting, or laser-based additive manufacturing. In this study, a 3D heat transfer and fluid flow model coupled with the volume-of-fluid algorithm for free surface tracking is developed for the simulation of molten pool dynamics in high-power laser beam welding. The underlying laser-material interactions, i.e., the multiple reflections and Fresnel absorption, are considered by a ray-tracing method. Two strategies of free surface reconstruction used in the ray-tracing method are investigated: a typical piecewise linear interface calculation (PLIC)-based method and a novel localized Level-Set method. The PLIC-based method is discrete, resulting in non-continuous free surface reconstruction. In the localized Level-Set method, a continuous free surface is reconstructed, and thus the exact reflection points can be determined. The calculated spatial laser energy distribution and the corresponding molten pool dynamics from the two methods are analyzed and compared. The obtained numerical results are evaluated with experimental measurements to assure the validity of the proposed model. It is found that distinct patterns of the beam multiple reflections are obtained with the different free surface reconstructions, which shows significant influence not only on the molten pool behaviors but also on the localized keyhole dynamics.
Advantages such as element homogenization and grain refinement can be realized by introducing electromagnetic stirring into laser beam welding. However, the involved weld pool behavior and its direct role on determining the final microstructure have not been revealed quantitatively. In this paper, a 3D transient heat transfer and fluid flow model coupled with element transport and magnetic induction is developed for wire feed laser beam welding with electromagnetic stirring. The magnetohydrodynamics, temperature profile, velocity field, keyhole evolution and element distribution are calculated and analyzed. The model is well tested against the experimental results. It is suggested that a significant electromagnetic stirring can be produced in the weld pool by the induced Lorentz force under suitable electromagnetic parameters, and it shows important influences on the thermal fluid flow and the solidification parameter. The forward and downward flow along the longitudinal plane of the weld pool is enhanced, which can bring the additional filler wire material to the root of the weld pool. The integrated thermal and mechanical impacts of electromagnetic stirring on grain refinement which is confirmed experimentally by electron backscatter diffraction analysis are decoupled using the calculated solidification parameters and a criterion of dendrite fragmentation.
The weld quality and the possible defect formation are directly determined by the weld pool shape and the thermo-fluid dynamics therein. In this paper, an untypical weld pool profile, i.e., elongated at its top and bottom but narrowed at the middle, is found experimentally and numerically in the wire feed laser beam welding. The detrimental influence of the weld pool narrowing on the element transport is analyzed and discussed. A magnetohydrodynamic technique is utilized to suppress the narrowing, aiming at a more homogenous element distribution. It is found that a low-temperature region is formed in the middle of the weld pool due to the interaction of the two dominant circulations from the top and bottom regions. The weld pool is significantly narrowed due to the untypical growth of the mushy zone in the low-temperature region, which results in a direct blocking effect on the downward flow and the premature solidification in the middle region. The Lorentz force produced by a transverse oscillating magnetic field shows the potential to change the flow pattern into a single-circulation type and the low-temperature-gradient region is mitigated.
Therefore, the downward transfer channel is widened, and its premature solidification is prevented. The numerical results are well validated by experimental measurements of metal/glass observation and X-ray fluorescence element mapping.
The transport phenomena in the wire feed laser beam welding are investigated numerically. A three-dimensional transient heat transfer and fluid flow model coupled with free surface tracing and element transport is developed. A ray-tracing method with local grid refinement algorithm is used to calculate the multiple reflections and Fresnel absorption on the keyhole wall. The filler material flows backward along the lateral side of the weld pool, and subsequently flows forward along the longitudinal plane. The occurrence of the bulging phenomenon may further prevent the downward transfer of the additional elements to the root of the weld pool.
The additional element from the filler wire in the laser beam welding is usually distributed inhomogeneously in the final weld due to the high solidification rate of weld pool. It has been found that the electromagnetic stirring produced by an external oscillating magnetic field can enhance the material mixing in the weld pool to achieve a more uniform element distribution. However, the magnetic field has a highly nonlinear and multicoupled interaction with the weld pool behavior, which makes the quantitative explanation of the physical mechanism difficult. In this study, the effect of electromagnetic stirring on the transport phenomena in the wire feed laser beam welding is investigated by a numerical modeling. A 3D transient multiphysical model considering the magnetohydrodynamics, heat transfer, fluid flow, keyhole dynamics, and element transport is developed. The multiple reflections and the Fresnel absorption of the laser on the keyhole wall are calculated using the ray tracing method. The numerical results show that a Lorentz force produced by the oscillating magnetic field and its induced eddy current gives significant influence on the transport phenomena in the molten pool. The forward and downward flow is enhanced by the electromagnetic stirring, which homogenizes the distribution of the additional elements from a nickel-based filler wire in a steel weld pool. The numerical results show a good agreement with the high-speed images of the molten pool, the fusion line from the optical micrograph, and the element distribution from the energy dispersive x-ray spectroscopy. This work provides a physical base for the electromagnetic-controlled laser beam welding and some guidance for the selection of electromagnetic parameters.
The introduction of electromagnetic stirring to laser beam welding can bring several beneficial effects e.g. element homogenization and grain refinement. However, the underlying physics has not been fully explored due to the absence of quantitative data of heat and mass transfer in the molten pool. In this paper, the influence of electromagnetic stirring on the thermo-fluid flow and element transport in the wire feed laser beam welding is studied numerically and experimentally. A three-dimensional transient heat transfer and fluid flow model coupled with dynamic keyhole, magnetic induction and element Transport is developed for the first time. The results suggest that the Lorentz force produced by an oscillating magnetic field and its induced eddy current shows an important influence on the thermo-fluid flow and the keyhole stability. The melt flow velocity is increased by the electromagnetic stirring at the rear and lower regions of molten pool. The keyhole collapses more frequently at the upper part. The additional Elements from the filler wire are significantly homogenized because of the enhanced forward and downward flow. The model is well verified by fusion line shape, high-speed images of molten pool and measured element distribution. This work provides a deeper understanding of the transport phenomena in the laser beam welding with magnetic field.
The additional element from the filler wire in the laser beam welding is usually distributed inhomogeneously in the final weld due to the high solidification rate of weld pool. It has been found that the electromagnetic stirring produced by an external oscillating magnetic field can enhance the material mixing in the weld pool to achieve a more uniform element distribution. However, the magnetic field has a highly non-linear and multi-coupled interaction with the weld pool behavior, which makes the quantitative explanation of the physical mechanism difficult. In this study, the effect of electromagnetic stirring on the transport phenomena in the wire feed laser beam welding is investigated by a numerical modelling. A 3D transient multi-physical model considering the magnetohydrodynamics, heat transfer, fluid flow, keyhole dynamics and element transport is developed. The multiple reflections and the Fresnel absorption of the laser on the keyhole wall are calculated using the ray tracing method. The numerical results show that a Lorentz force produced by the oscillating magnetic field and its induced eddy current gives significant influence on the transport phenomena in the molten pool. The forward and downward flow is enhanced by the electromagnetic stirring, which homogenizes the distribution of the additional elements from a nickel-based filler wire in a steel weld pool. The numerical results show a good agreement with the high-speed images of the molten pool, the fusion line from the optical micrograph and the element distribution from the energy dispersive X-ray spectroscopy. This work provides a physical base for the electromagnetic-controlled laser beam welding and some guidance for the selection of electromagnetic parameters.
The additional element from the filler wire in the laser beam welding is usually distributed inhomogeneously in the final weld due to the high solidification rate of weld pool. It has been found that the electromagnetic stirring produced by an external oscillating magnetic field can enhance the material mixing in the weld pool to achieve a more uniform element distribution. However, the magnetic field has a highly non-linear and multi-coupled interaction with the weld pool behavior, which makes the quantitative explanation of the physical mechanism difficult. In this study, the effect of electromagnetic stirring on the transport phenomena in the wire feed laser beam welding is investigated by a numerical modelling. A 3D transient multi-physical model considering the magnetohydrodynamics, heat transfer, fluid flow, keyhole dynamics and element transport is developed. The multiple reflections and the Fresnel absorption of the laser on the keyhole wall are calculated using the ray tracing method. The numerical results show that a Lorentz force produced by the oscillating magnetic field and its induced eddy current gives significant influence on the transport phenomena in the molten pool. The forward and downward flow is enhanced by the electromagnetic stirring, which homogenizes the distribution of the additional elements from a nickel-based filler wire in a steel weld pool. The numerical results show a good agreement with the high-speed images of the molten pool, the fusion line from the optical micrograph and the element distribution from the energy dispersive X-ray spectroscopy. This work provides a physical base for the electromagnetic-controlled laser beam welding and some guidance for the selection of electromagnetic parameters.
An accurate and efficient description of the spatial distribution of laser energy is a crucial factor for the modeling of laser material processing, e.g., laser welding, laser cutting, or laser-based additive manufacturing. In this study, a 3D heat transfer and fluid flow model coupled with the volume-of-fluid algorithm for free surface tracking is developed for the simulation of molten pool dynamics in high-power laser beam welding. The underlying laser-material interactions, i.e., the multiple reflections and Fresnel absorption, are considered by a ray-tracing method. Two strategies of free surface reconstruction used in the ray-tracing method are investigated: a typical piecewise linear interface calculation (PLIC)-based method and a novel localized Level-Set method. The PLIC-based method is discrete, resulting in non-continuous free surface reconstruction. In the localized Level-Set method, a continuous free surface is reconstructed, and thus the exact reflection points can be determined. The calculated spatial laser energy distribution and the corresponding molten pool dynamics from the two methods are analyzed and compared. The obtained numerical results are evaluated with experimental measurements to assure the validity of the proposed model. It is found that distinct patterns of the beam multiple reflections are obtained with the different free surface reconstructions, which shows significant influence not only on the molten pool behaviors but also on the localized keyhole dynamics.
The weld quality and the possible defect formation are directly determined by the weld pool shape and the thermo-fluid dynamics therein. In this paper, an untypical weld pool profile, i.e., elongated at its top and bottom but narrowed at the middle, is found experimentally and numerically in the wire feed laser beam welding. The detrimental influence of the weld pool narrowing on the element transport is analyzed and discussed. A magnetohydrodynamic technique is utilized to suppress the narrowing, aiming at a more homogenous element distribution. It is found that a low-temperature region is formed in the middle of the weld pool due to the interaction of the two dominant circulations from the top and bottom regions. The weld pool is significantly narrowed due to the untypical growth of the mushy zone in the low-temperature region, which results in a direct blocking effect on the downward flow and the premature solidification in the middle region. The Lorentz force produced by a transverse oscillating magnetic field shows the potential to change the flow pattern into a single-circulation type and the low-temperature-gradient region is mitigated. Therefore, the downward transfer channel is widened, and its premature solidification is prevented. The numerical results are well validated by experimental measurements of metal/glass observation and X-ray fluorescence element mapping.
The deep penetration laser beam welding (LBW) has developed to one of the most promising metal joining methods in the modern manufacturing industry. It has well-known advantages of good penetration capacity, low heat input, high reachable welding speed and low welding distortion in comparison to conventional arc welding techniques. However, there are still challenges in LBW making the realization of the advantages difficult, such as porosity or inhomogeneous element distribution when using filler material. The magnetohydrodynamics technique is a promising way to solve these issues by introducing a suitable electromagnetic field, and correspondingly Lorentz force, to control the Transport phenomena in the weld pool.
The underlying physics in wire feed laser beam welding with electromagnetic stirring were investigated numerically and experimentally. A three-dimensional transient heat transfer and fluid flow model coupled with dynamic keyhole, magnetic induction and element transport was developed for the first time. The electromagnetic behaviour as well as the temperature and velocity profiles, solidification parameters, keyhole evolution and element transport are calculated.
The model is well tested against the experimental results. The beneficial effects from electromagnetic stirring (element homogenization and grain refinement) are explained quantitatively using the numerical data and the results from high-speed imaging, OM, EDX and EBSD.
The distribution of the alloying elements from the filler wire in laser beam welding plays an important role on the property of the final weld. In this study, the transport phenomena in the wire feed laser beam welding are investigated numerically. A three-dimensional transient heat transfer and fluid flow model coupled with free surface tracing and element transport is developed. A ray-tracing method with local grid refinement algorithm is used to calculate the multiple reflections and Fresnel absorption on the keyhole wall. The filler material flows backward along the lateral side of the weld pool, and subsequently flows forward along the longitudinal plane to bring the additional alloying elements to the forepart of the weld pool. The occurrence of the bulging phenomenon may further prevent the downward transfer of the additional elements to the root of the weld pool. The numerical results show a good agreement with the experimental fusion line and element distribution.
It is proposed to model the experimentally observed weld pool boundary with superellipses (Lamé curves) and to find the unknown parameters of the curves using optimization methods. It has been shown experimentally that during laser welding of austenitic stainless steel with a thickness of 2 mm at a speed of 20 mm/s, the rear weld pool part has a shape close to triangular which can be accurately approximated by a superellipse. Analytical dependences of the trajectory and growth rate of the crystal and its cross-sectional area on the geometry of the rear weld pool part are obtained.
Among the various welding technologies, resistance spot welding (RSW) and laser beam welding (LBW) play a significant role as joining methods for the automobile industry. The application of RSW and LBW for the automotive body alters the microstructure in the welded areas. It is necessary to identify the mechanical properties of the welded material to be able to make a reliable statement about the material behavior and the strength of welded components. This study develops a method by which to determine the mechanical properties for the weldment of RSW and LBW for two dual phase (DP) steels, DP600 and DP1000, which are commonly used for the automotive bodies. The mechanical properties of the resistance spot weldment were obtained by performing tensile tests on the notched tensile specimen to cause an elongation of the notched and welded area in order to investigate its properties. In order to determine the mechanical properties of the laser beam weldment, indentation tests were performed on the welded material to calculate its force-penetration depth-curve. Inverse numerical simulation was used to simulate the indentation tests to determine and verify the parameters of a nonlinear isotropic material model for the weldment of LBW. Furthermore, using this method, the parameters for the material model of RSW were verified. The material parameters and microstructure of the weldment of RSW and LBW are compared and discussed. The results show that the novel method introduced in this work is a valid approach to determine the mechanical properties of welded high-strength steel structures. In addition, it can be seen that LBW and RSW lead to a reduction in ductility and an increase in the amount of yield and tensile strength of both DP600 and DP1000.
The strain field can reflect the initiation time of solidification cracks during the welding process. The traditional strain measurement is to first obtain the displacement field through digital image correlation (DIC) or optical flow and then calculate the strain field. The main disadvantage is that the calculation takes a long time, limiting its suitability to real-time applications. Recently, convolutional neural networks (CNNs) have made impressive achievements in computer vision.
To build a good prediction model, the network structure and dataset are two key factors. In this paper, we first create the training and test sets containing welding cracks using the controlled tensile weldability (CTW) test and obtain the real strain fields through the Lucas–Kanade algorithm. Then, two new networks using ResNet and DenseNet as encoders are developed for strain prediction, called StrainNetR and StrainNetD. The results show that the average endpoint error (AEE) of the two networks on our test set is about 0.04, close to the real strain value. The computation time could be reduced to the millisecond level, which would greatly improve efficiency.
To save weight without affecting the functional properties of vehicles, heavy materials must be replaced with lighter alternatives.Modern lightweight concepts have therefore been developed, featuring multi-material designs that require the joining of dissimilar materials.One new possible approach for the joining of dissimilar metals is based on laser welding and melt displacement by contactless induced electromagnetic forces.
In order to reduce weight of vehicles, the interest in multi-material-design has been growing within the last few years. For vehicles the combination of steel and aluminium alloys offers the most promising compromise between weight, strength and formability. Thermal joining of these dissimilar materials is still a challenge to overcome. A possible approach is a new joining technology, whereby a combination of laser beam welding and contactless induced electromagnetic forces are used to displace the generated melt of one joining partner into a notch of the other. This paper presents the working principle and shows numerical analyses to improve the understanding of this joining process. The simulations help to calculate the thermal development of the joining partners, which is important for the formation of intermetallic phases. Furthermore, the calculation of the time required for a complete displacement is possible. The numerical results are validated by experimental results.
In order to reduce CO2 emissions, an increasing interest in lightweight construction exists in the automotive industry, especially the multi-material-design approach. The main construction materials here are steels and aluminium alloys. Due to their different physical material properties and limited mutual solubility, these two materials cannot be joined thermally without difficulty. This paper presents a new joining approach for dissimilar materials. It uses electromagnetic displacement of a laser-generated melt pool to produce overlap joints between 1 mm steel (1.0330) and 2 mm aluminium alloy (EN AW 5754). Contactless induced Lorentz forces are generated by an alternating current (AC) magnet system. The controlled displacement of the aluminium alloy melt into the hole of the overlying steel sheet is investigated through numerical and experimental studies. The numerical results are compared with cross sections and thermocouple measurements. For the first time, it is possible to achieve a reproducible controlled melt pool displacement on thin sheets to produce overlap joints between dissimilar materials.
In order to reduce weight of vehicles, the interest in multi-material-design has been growing within the last few years. For vehicles the combination of steel and aluminium alloys offers the most promising compromise between weight, strength and formability. Thermal joining of these dissimilar materials is still a challenge to overcome. A possible approach is a new joining technology, whereby a combination of laser beam welding and contactless induced electromagnetic forces are used to displace the generated melt of one joining partner into a notch of the other. This paper presents the working principle and shows numerical analyses to improve the understanding of this joining process. The simulations help to calculate the thermal development of the joining partners, which is important for the formation of intermetallic phases. Furthermore, the calculation of the time required for a complete displacement is possible. The numerical results are validated by experimental results.
In this contribution, we present a physically motivated heat source model for the numerical modeling of laser beam welding processes. Since the calibration of existing heat source models, such as the conic or Goldak model, is difficult, the representation of the heat source using so-called Lamé curves has been established, relying on prior Computational Fluid Dynamics (CFD) simulations.
Lamé curves, which describe the melting isotherm, are used in a subsequent finite-element (FE) simulation to define a moving Dirichlet boundary condition, which prescribes a constant temperature in the melt pool. As an alternative to this approach, we developed a physically motivated heat source model, which prescribes the heat input as a body load directly. The new model also relies on prior CFD simulations to identify the melting isotherm. We demonstrate numerical results of the new heat source model on boundary-value problems from the field of laser beam welding and compare it with the prior CFD simulation and the results of the Lamé curve model and experimental data.
The study deals with the determination of the influence of an externally applied oscillating magnetic field on the melt pool dynamics in high power laser beam and hybrid laser arc welding processes. An AC magnet was positioned under the workpiece which is generating an upward directed electromagnetic force to counteract the formation of the droplets. To visualise the melt flow characteristics, several experiments were carried out using a special technique with mild steel from S355J2 with a wall thickness of up to 20 mm and a quartz glass in butt configuration. The profile of the keyhole and the melt flow were recorded with a high-speed camera from the glass side. Additionally, the influence of the magnetic field orientation to the welding direction on the filler material dilution on laser hybrid welding was studied with variating oscillation frequency. The element distribution over the whole seam thickness was measured with X-ray fluorescence (XRF). The oscillation frequency demonstrated a greater influence on the melt pool dynamics and the mixing of the elements of the filler wire. The high-speed recordings showed, under the influence of the magnetic field, that the melt is affected under strong vortex at the weld root, which also avoids the formation of droplets
Because of its excellent corrosion resistance, high tensile strength and
high ductility, duplex stainless steel 2205 offers many areas of application. Though laser beam welding accompanied by high cooling rates, duplex steels tend to perform higher ferrite contents in weld metal as the base metal, which leads to a reduction of ductility and corrosion resistance of the weld joint. To overcome this problem, a solution, based on buttering the plate edges by laser metal deposition (LMD) with material containing higher Ni concentrations prior to laser welding was suggested.
In this context different process parameters for LMD and different mixtures of duplex and nickel powder, were investigated. In a second step the possibility of welding those edges defect free while achieving balanced austenite-ferrite ratio was verified with metallographic analysis, Electron Backscatter Diffraction (EBSD) and impact testing according to Charpy. The improved corrosion resistance was observed with ASTM G48 standard test method.
One of the challenges of the high-power hybrid laser welding of thick steels is the sensitivity of the process of the process to manufacturing tolerances. This usually leads to a time-consuming preparation of the welding edges, such as milling. The study deals with the influence of the edge quality of milled and plasma-cut steel made of S355J2 with a wall thickness of 20 mm on the laser hybrid welded seam quality. Furthermore, the gap bridgeability and the tolerances towards edge misalignment was investigated. An AC magnet was used as backing support to prevent sagging and positioned under the workpiece, to generate an upwards directed electromagnetic pressure. The profiles of the edges and the gap on the top and root side were measured using a digital camera. Single-pass laser hybrid welds of plasma-cut edges could be welded using a laser beam power of just 13.7 kW. A gap bridgeability up to 2 mm and misalignment of edges up to 2 mm could be achieved successful. Additionally, the independence of the cutting side and the welding side was shown, so that samples were welded to the opposite side to their cutting. For evaluation of internal defects or irregularities, X-ray images were carried out. Charpy impact strength tests were performed to determine the toughness of the welds.
High power laser beam welding has been already introduced in ship building industry since last two decades and is characterized by higher performance as conventional arc welding technologies through its higher welding speed, penetration depth and therefore higher productivity. Moreover, high quality weld joints are achievable thanks to a stronger automatization degree and better repeatability of the process. A further advantage of the laser beam welding is a manufacturing of parts with very low distortion according to much lower heat input, so that rework amount can be reduced significantly. Nevertheless, there are still some unresolved problems limiting the range of application of the technology in part manufacturing within ship building industry, restricted by development and application of new materials or new design of ship vessels.
The present contribution deals with some novel aspects of laser beam welding technology allowing to widen this range significantly. One of the possibilities is to increase the weld seam thickness for single pass laser or laser-hybrid welding is to apply contactless EM-support system based on generation of the Lorentz force counteracting the liquid metal drop out. Also, application of laser-hybrid welding technology for welding novel materials like cold resistant steel X8Ni9 used for construction of LNG tanks brings technological and design advantages comparing to conventional welding technologies by using of a similar alloyed filler wire instead of expensive Ni-based filler material. Finally, it is shown how the application of computational techniques can be used to helps to improve the quality of laser welded joints and avoid the critical weld failure by optimization of the welding process parameters.
This paper presents investigation results of a process for defect-free hybrid laser arc welding (HLAW) of closed circumferential welds. The process aims to avoid weld imperfections in the overlap area of a HLAW circumferential weld. A process control strategy for closing the circumferential weld was developed to achieve a defect-free overlap region by controlling the solidification conditions at the end of the weld. The controlled heat flow is achieved by adjusting the parameters of both welding processes involved, the laser beam as well as gas metal arc welding (GMAW) process. Experimental investigations were carried out on 12 mm to 15 mm thick tube sections. The influence of process parameters such as the laser ramp time, the change in magnification scale and the defocusing of the laser beam on the solidifi-cation conditions at the end of the circumferential weld was investigated to find an optimum strategy for ramping out the process energy. Within the framework of the experimental studies, it was demonstrated that defocusing the laser beam in the range between 60 mm and 100 mm over a short run-out area of the weld of approximately 15 mm led to a significantly better weld formation in the overlap area. A favourable cup-shaped weld shape could be achieved without a tendency to crack. The laser optics with a motor-driven lens system made it possible to increase the laser beam diameter without changing the position of the GMAW arc relative to the component surface.
The present work deals with the development of a strategy for the prevention of end crater defects in high-power laser welding of thick-walled circumferential welds. A series of experiments were performed to understand the influence of the welding Parameters on the formation of end crater defects such as pores, cracks, root excess weld metal and shrinkage cavities in the overlap area. An abrupt switch-off of the laser power while closing the circumferential weld leads to a formation of a hole which passes through the whole welded material thickness. A laser power ramp-down causes solidification cracks which are initiated on the transition from full-penetration mode to partial penetration. Defocusing the laser beam led to promising results in terms of avoiding end crater defects. Cracks and pores in the overlap area could be effectively avoided by using defocusing techniques.
A strategy for avoiding of end crater imperfections was tested on flat specimens of steel grade S355J2 with a wall thickness of between 8 mm and 10 mm and then transferred on the 10 mm thick pipe sections made of high-strength pipeline steel API5L-X100Q.
In diesem Beitrag werden Ergebnisse der Untersuchungen eines Verfahrens zum fehlerfreien Laserstrahl-MSG-Hybridschweißen von geschlossenen Rundnähten vorgestellt. Das Verfahren zielt auf die Vermeidung von Schweißnahtunregelmäßigkeiten im Überlappbereich einer hybridgeschweißten Rundnaht. Eine Strategie der Prozessführung beim Schließen der Rundnaht wurde entwickelt, mit der ein fehlerfreier Überlappbereich durch die Kontrolle der Erstarrungsbedingungen am Schweißnahtende erreicht wird. Die kontrollierte Wärmeführung wird durch eine Anpassung der Parameter von beiden beteiligten Schweißprozessen, dem Laserstrahl sowie dem Metallschutzgas (MSG)-Schweißprozess, realisiert. Experimentelle Untersuchungen wurden an 12 bis 15 mm dicken Rohrabschnitten durchgeführt. Der Einfluss von Prozessparametern wie der Veränderung des Abbildungsmaßstabs und der Defokussierung des Laserstrahls auf die Erstarrungsbedingungen am Ende der Rundnaht wurde untersucht, um eine optimale Strategie zum Herausführen der Prozessenergie zu finden.
Im Rahmen der experimentellen Untersuchungen konnte gezeigt werden, dass eine Defokussierung des Laserstrahls im Bereich zwischen 60 mm und 100 mm über einen kurzen Auslaufbereich der Naht von etwa 15 mm zu einer deutlich besseren Nahtausbildung im Überlappbereich führt. Es konnte eine günstige kelchförmige Schweißnaht ohne eine Tendenz zur Rissbildung erzielt werden. Die Laseroptik mit motorisch angesteuertem Linsensystem ermöglichte dabei eine Vergrößerung des Laserstrahldurchmessers ohne eine Veränderung der Position des MSG-Lichtbogens relativ zur Bauteiloberfläche.