Fiber reinforced polymers (FRPs) are a well established material in lightweight applications, e.g. in automotive, aerospace or wind energy. The FRP components are subjected to multiaxial mechanical as well as hygrothermal loads. Common operation temperatures are in the range of 213 K and 373 K (-60 °C and 100 °C) at a relative humidity of 10% to 90%. In spacecraft applications, the environmental conditions are even more extreme. However, the correlation between multiaxial mechanical loading and harsh environment conditions have to-date not been investigated in detail. The project aims to investigate the fatigue behavior of FRPs dependent on multiaxial mechanical loading, temperature, and humidity. Extensive experimental testing is performed on flat plate and cylindrical tube specimens, accompanied by numerical and analytical calculations.
Partially crystalline glasses are predominantly used as solid oxide fuel cell (SOFC) sealants due to their superior long term durability. However, cracks caused by thermal cycling still remain a substantial bottleneck in developing durable SOFC sealants inasmuch as, in contrast to crystal free glasses, large crystal volume fractions can retard healing. Hence, the basic understanding of crack healing in glassy crystalline materials and the effects of micro structure are important for finding optimum micro structures for both, durability and crack healing.
For studying these effects, several model glass matrix composites (GMC), for which simultaneous crystal growth and crack healing can be excluded, have been synthesized. Sodium calcium silicate glass – zirconia GMC turned out to provide sufficiently homogeneous, dense and durable model GMC for our studies. The microstructure of this GMC shows large crystal free glassy regions embedded in network of finely dispersed ZrO2 nanoscale crystals. Whereas the glassy regions allow easy local crack healing, the network of dispersed crystals increases the effective viscosity on a global scale. This effect substantially retards crack broadening during later healing stages, which often ends up in large pores. Therefore, this type of microstructure seems to be an interesting candidate for crack healing optimized sealants.