The triaxial distribution of the residual stress in laser powder bed fused austenitic steel 316L was determined by X-ray and neutron diffraction. The residual stress analysis results were linked to the thermal history of the specimens, which were manufactured with varying inter-layer-times and scanning velocities. A clear link between the in-process temperature of the specimens and the residual stress was found, based on in-situ monitoring data.
The influence of the inter-layer-time and the scanning velocity on the surface and bulk residual stress in laser powder bed fused 316L specimens was investigated. This study combines X-ray and neutron diffraction results with the thermal history of the specimens acquired through in-situ process monitoring. The process parameter variations were observed to directly influence the thermal history, which gave new insights in the assessment of the residual stress results.
The laser powder bed fusion of 316L leads to the formation of large residual stress. In this presentation, different stress relieve treatments were employed to assess their potential to relax the residual stress. The residual stress was determined by X-ray and neutron diffraction. The results give insights on the range of relaxation one can obtain by employing low and high temperature heat treatments and relates the relaxation to changes in the microstructure.