5 Werkstofftechnik
Filtern
Dokumenttyp
- Vortrag (476)
- Posterpräsentation (117)
- Beitrag zu einem Tagungsband (71)
- Zeitschriftenartikel (63)
- Forschungsdatensatz (27)
- Buchkapitel (11)
- Dissertation (10)
- Forschungsbericht (7)
- Sonstiges (5)
- Sammelband (Herausgeberschaft für den kompletten Band) (3)
- Beitrag zu einem Sammelband (2)
- Monografie (1)
- Video (1)
- Preprint (1)
Sprache
- Englisch (630)
- Deutsch (159)
- Mehrsprachig (4)
- Französisch (2)
Referierte Publikation
- nein (795) (entfernen)
Schlagworte
- Additive Manufacturing (53)
- Corrosion (45)
- Additive manufacturing (41)
- Ontology (35)
- Glass (33)
- Microstructure (31)
- Creep (25)
- Fatigue (23)
- Transmission electron microscopy (18)
- Crack growth (16)
Organisationseinheit der BAM
- 5 Werkstofftechnik (795)
- 5.2 Metallische Hochtemperaturwerkstoffe (211)
- 5.1 Mikrostruktur Design und Degradation (205)
- 5.4 Multimateriale Fertigungsprozesse (155)
- 5.6 Glas (109)
- 5.3 Polymere Verbundwerkstoffe (96)
- 5.5 Materialmodellierung (74)
- 8 Zerstörungsfreie Prüfung (74)
- 7 Bauwerkssicherheit (61)
- 9 Komponentensicherheit (60)
Manipulating ceramic powder compacts and ceramic suspensions (slurries) within their volume with light requires a minimum transparency of the materials. Compared to polymers and metals, ceramic materials are unique as they offer a wide electronic band gap and thus a wide optical window of transparency. The optical window typically ranges from below 0.3 µm up to 5µm wavelength. Hence, to penetrate with laser light into the volume of a ceramic powder compound its light scattering properties need to be investigated and tailored. In the present study we introduce the physical background and material development strategies to apply two-photon-polymerization (2PP) for the additive manufacture of filigree structures within the volume of ceramic slurries.
The Binder Jetting BJ process is one of the most versatile additive manufacturing technologies in use. In this process a binder is locally jetted into a powder bed for the consolidation of a 3D structure, layer by layer. Basically, all materials which can be provided as a flowable powder and, thus, spreadable to a thin layer, can be processed. Metals, ceramics and polymers are processable, but also materials from nature, such as sand, wood sawdust and insect frass. Moreover, the BJ technology is adapted to large building volumes of some cubic meters easily. Besides these striking advantages, the manufacture of ceramic parts by BJ is still challenging, as the packing density of the powder bed is generally too low and the particle size of a flowable powder too large for a successful densification of printed parts in a subsequent sintering step to an advanced ceramic product. After an introduction of binder jetting in general and highlighting some examples, strategies for obtaining dense ceramic parts by BJ will be introduced.
In order to be able to manipulate ceramic powder compacts and ceramic suspensions (slurries) within their volume with light, a minimum transparency of the materials is required. Compared to polymers and metals, ceramic materials are characterized by the fact that they have a wide electronic band gap and therefore a wide optical window of transparency. The optical window generally ranges from less than 0.3 µm to 5 µm wavelength. In order to focus light into the volume of a ceramic powder compact, its light scattering properties must therefore be tailored. In this study, we present the physical background and material development strategies for the application of two-photon polymerization (2PP) and selective volumetric sintering for the additive manufacturing of structures in the volume of ceramic slips and green compacts.
Many of the most successful and precise additive manufacturing (AM) technologies are based on the deposition layer-by-layer of a flowable powder. Since the first pioneering work at the end of the 1980th many developments have been introduced, greatly extending the use of different materials, improving the physical properties of the components built and enhancing the accuracy of the process. Still very important issues remain nowadays, hampering a completely autonomous production of parts and even restricting the freedom of design by means of these technologies. One of the major issues is the low density and stability of the parts during the building process, which implies the need of support structures: The powder bed surrounding the part has an essential role, since it should support the structure during building, until it’s ready for removal. Moreover, the microstructure of the powder bed is a template for the microstructure of the part produced. In this context, the use of submicron ceramic powders is still a challenge. Three approaches for the stabilization and densification of powder beds will be presented: The Layerwise Slurry Deposition process LSD, the gas flow assisted powder deposition and the Laser Induced Slipcasting (LIS) of ceramic powder compacts.
Are we ready for putting a human footprint on Mars? Obviously, it is possible to send technologically challenging missions to our earth neighbors with a high level of complexity, such as enabling autonomous planetary mobility. As humanity contemplates mounting manned missions to Mars, strategies need to be developed for the design and operation of hospitable environments safely working in space for years. Humans require water and air provided by complicated equipment. Its safe operation is a great challenge and implies being prepared for all eventualities. Instead of foreseeing and preparing for all possible scenarios of machine failures and accidents, it appears logic taking advantage of the flexibility of humans and providing essential equipment for the reaction on critical situations. The supply of spare parts for repair and replacement of lost equipment would be one key pillar of such a strategy. Bearing in mind the absolute distance and flight trajectories for manned missions to Mars, supplying spare parts from Earth is impossible. Thus, in space manufacturing remains the only option for a timely supply. With a high flexibility in design and the ability to manufacture ready to use components directly from a computer aided model, additive manufacturing technologies appear extremely attractive. For metal parts manufacturing the Laser Beam Melting process is the most widely used additive manufacturing process in industrial application. However, envisioning the handling of metal powders in the absence of gravitation is one prerequisite for its successful application in space. A gas flow throughout the powder bed has been successfully applied to compensate for missing gravitational forces in micro gravity experiments. The so-called Gas Flow Assisted Powder Deposition is based on a porous building platform acting as a filter for the fixation of metal particles in a gas flow driven by a pressure difference maintained by a vacuum pump.
Are we ready for putting a human footprint on Mars? Obviously, it is possible to send technologically challenging missions to our earth neighbors with a high level of complexity, such as enabling autonomous planetary mobility. As humanity contemplates mounting manned missions to Mars, strategies need to be developed for the design and operation of hospitable environments safely working in space for years. Humans require water and air provided by complicated equipment. Its safe operation is a great challenge and implies being prepared for all eventualities. Instead of foreseeing and preparing for all possible scenarios of machine failures and accidents, it appears logic taking advantage of the flexibility of humans and providing essential equipment for the reaction on critical situations. The supply of spare parts for repair and replacement of lost equipment would be one key pillar of such a strategy. Bearing in mind the absolute distance and flight trajectories for manned missions to Mars, supplying spare parts from Earth is impossible. Thus, in space manufacturing remains the only option for a timely supply. With a high flexibility in design and the ability to manufacture ready to use components directly from a computer aided model, additive manufacturing technologies appear extremely attractive. For metal parts manufacturing the Laser Beam Melting process is the most widely used additive manufacturing process in industrial application. However, envisioning the handling of metal powders in the absence of gravitation is one prerequisite for its successful application in space. A gas flow throughout the powder bed has been successfully applied to compensate for missing gravitational forces in micro gravity experiments. The so-called Gas Flow Assisted Powder Deposition is based on a porous building platform acting as a filter for the fixation of metal particles in a gas flow driven by a pressure difference maintained by a vacuum pump.
At the Workshop "Neutron and Synchrotron Monitoring in Aerospace Advanced Manufacturing" at the Institute of Materials Physics in Space, German Aerospace Center (DLR) in Cologne, we presented on the opportunities and our experiences of using a powder based additive manufacturing process for in-space manufacturing applications in microgravity.
Charakterisierung von Hochtemperaturwerkstoffen durch Zug- und Ermüdungsversuche an Kleinproben
(2019)
Die Verwendung von miniaturisierten Probengeometrien in der mechanischen Prüfung ermöglicht die Entnahme des Probenmaterials direkt aus kritischen Bereichen wie Fügeverbindungen und ermöglicht die Prüfung von kleinen Bauteilen wie additiv gefertigten Strukturen. In der vorliegenden Arbeit werden exemplarisch die Ergebnisse von vergleichenden Zug- und niederzyklischen Schwing-versuchen (LCF) an dem austenitischen Stahl AISI 316L und der Nickelbasislegierung IN718 vorgestellt. Die Prüfergebnisse der Kleinproben aus AISI 316L weisen die charakteristischen Eigenschaften des Werkstoffs auf, und die Analyse der Zug- und Ermüdungsdaten führt zu Werten, die den Literaturdaten weitgehend entsprechen. Der direkte Vergleich mit Standardprobendaten zeigt jedoch systematische Abweichungen bei Zugfestigkeit, Dehngrenze und Gleichmaßdehnung, die in diesem Beitrag diskutiert werden.
Charakterisierung von Hochtemperaturwerkstoffen durch Zug- und Ermüdungsversuche an Kleinproben
(2019)
Die Verwendung von miniaturisierten Probengeometrien in der mechanischen Prüfung ermöglicht die Entnahme des Probenmaterials direkt aus kritischen Bereichen wie Fügeverbindungen und ermöglicht die Prüfung von kleinen Bauteilen wie additiv gefertigten Strukturen. In der vorliegenden Arbeit werden exemplarisch die Ergebnisse von vergleichenden Zug- und niederzyklischen Schwingversuchen (LCF) an dem austenitischen Stahl AISI 316L und der Nickelbasislegierung IN718 vorgestellt. Die Prüfergebnisse der Kleinproben aus AISI 316L weisen die charakteristischen Eigenschaften des Werkstoffs auf, und die Analyse der Zug- und Ermüdungsdaten führt zu Werten, die den Literaturdaten weitgehend entsprechen. Der direkte Vergleich mit Standardprobendaten zeigt jedoch systematische Abweichungen bei Zugfestigkeit, Dehngrenze und Gleichmaßdehnung, die in diesem Beitrag diskutiert werden.
In Germany spent nuclear fuel and high level radioactive waste is stored in interim storage containers with double lid systems. Those lids are equipped with metal seals (e.g. Helicoflex®) that ensure the safe enclosure of the inventory. The used metal seals consist of three components as can be seen in the cross-sectional view in Figure 1. The innermost part is a helical spring that is surrounded by an inner jacket made of stainless steel. The outer jacket that is made of a softer material which in case of assembly in the aforementioned storage containers is silver or aluminum (i.e. Al 99.5). During application the seal is compressed and due to the restoring force of the helical spring, the outer jacket is plastically deformed and adapts to the sealing surface. Hence, leakage paths are closed and the sealing function is generated. In Germany the above-mentioned containers are licensed for up to 40 years of interim storage, which in case extended storage becomes necessary before a final repository is available will have to be extended to even longer periods. Therefore, the evaluation of the long-term behavior of the seals is necessary, taking into account storage conditions, decay heat and possible mechanical loads as well.
At Bundesanstalt für Materialforschung und –prüfung (BAM) long-term investigations are being conducted in which seals are assembled in test flanges and aged at temperatures ranging from room temperature to 150°C for accelerated aging. The aged seals are tested semi-annually (after the first 6 months in which the seals are tested more frequently) regarding the sealing performance, the remaining seal force, and the useable resilience upon decompression. Results of these investigations have been published over the past years (e.g. Grelle, Wolff, Probst, Jaunich, & Völzke, 2017; Völzke, Wolff, Probst, Nagelschmidt, & Schulz, 2014). It was found that the seal force and the useable resilience decrease with time and temperature, which is in agreement with the result of other studies (Sassoulas et al., 2006; Wataru et al., 2016) as well. Geometry change of the outer jacket has been identified as the main reason for this seal behavior. At the prevailing operating temperatures and stresses the aluminum is subjected to creep deformation leading to a thinning of the outer jacket. Since the seal groove depth remains unchanged the helical spring expands, which in turn leads to a decrease of the generated spring and seal force.
Although the main reason for the change of seal parameters over time and temperature is known, a detailed characterization of the seal behavior and a reliable prediction of the parameter development for aging times that exceed the experimental time frame have not been possible, yet.
For deeper understanding of the aging processes, an Investigation program, which is covered in this contribution, is conducted at Bundesanstalt für Materialforschung und –prüfung (BAM) that focusses on the behavior of the aluminum jacket and its influence on the long-term sealing performance. The program investigates properties of material samples as well as the behavior of the seal as a component.
Original sheet material of the same aluminum that is used for manufacturing of the seals is investigated in compression creep tests. For this, a DMA (dynamic mechanical analysis) machine is employed (here used for static tests) that allows for a measurement of the specimens deformation under forces of up to 500 N. The advantage of this method is that the original material can be tested in the same shape as used for the seals which is 0.5 mm thick sheet material. For investigation of tensile creep standard specimens are used, that were machined from surrogate material of the same composition and annealing condition.
Furthermore, aluminum seals that are cut into smaller segments are assembled in flanges and placed in heating chambers at temperatures ranging from 23°C to 150°C. After different periods of time from 3 days to 300 days the segments are taken out of the flanges and are investigated, thus giving information on different states of aging. Measurements of the development of the seal contact width and the aluminum jacket thickness are done with an optical microscope. Further investigations on the segments will include metallography and hardness measurements.
From the detailed material and component behavior including the results of the long-term seal force and useable resilience investigations a better understanding of the overall seal behavior can be gained. The aim is to contribute to the development of material models and analytical approaches for the prediction of the sealing behavior in dependence of time and temperature.
In Germany spent nuclear fuel (SNF) and high level radioactive waste (HLW) are stored in interim storage containers with double lid systems. Those lids are equipped with metal seals (e.g. Helicoflex®) that ensure the safe enclosure of the inventory. Being licensed for up to 40 years of interim storage the evaluation of the long-term behavior of the seals is necessary, taking into account storage conditions, decay heat and possible mechanical loads.
The process of viscous flow sintering is a phenomenon that is closely linked to the surface properties of the glass particles. In this work, we studied the extreme case of acid-leaching of soda-lime-silicate glass beads of two different particle size distributions and its effects on non-isothermal viscous sintering of powder compacts. Depth profiling of the chemical composition after leaching revealed a near-surface layer depleted in alkali and alkaline earth ions, associated with concurrent hydration as mass loss was detected by thermogravimetry. Heating microscopy showed that acid treatment of glasses shifted the sinter curves to higher temperatures with increasing leaching time. Modelling of the shrinkage with the cluster model predicted a higher viscosity of the altered surface layer, while analysis of the time scales of mass transport of mobile species (Na+, Ca2+ and H2O) during isochronous sintering revealed that diffusion of Na+ can compensate for concentration gradients before sintering begins. Also, exchanged water species can diffuse out of the altered layer, but the depletion of Ca2+ in the altered surface layer persists during the sinter interval, resulting in a glass with higher viscosity, which causes sintering to slow down.
The presence of large quantities of plastic waste and its fragmentation in various environmental compartments are an important subject of current research. In the environment, (photo ) oxidation processes and mechanical abrasion lead to the formation of microplastics. However, until now, there are no established quality assurance concepts for the analysis of microplastic (<5 mm) in environmental compartments, including sampling, processing and analysis.
The aim of the present work is the development of suitable examination methods and protocols (sampling, sample preparation and detection) to qualify and quantify microplastic in urbane water management systems. At first a fractional filtration system for sampling and the analytical tool, the so-called TED-GC-MS (thermal desorption gas chromatography mass spectrometry) were developed. The TED-GC-MS method is a two-step analytical procedure which consists of a thermal extraction where the sample is annealed and characteristic decomposition products of the polymers are collected on a solid phase. Afterwards these products are analysed using GC-MS. The developed fractional filtration for sampling and the TED-GC-MS for detection were used for quantitative analysis to screen the waste water influent and effluent of a Berlin waste water treatment plant for the most relevant polymers, polyethylene (PE), polypropylene (PP), polystyrene (PS), polyethylene terephthalate (PET) and polyamide (PA).
The results of the study revealed that the polymeres PE, PS and PP were detected in the effluent, and PE and PS were find in the raw waste water of the sewage treatment plant in Ruhleben, Berlin. Differences in polymer types and amounts were detected at different sampling dates and within different sieve fractions. Much higher amounts of polymers were observed in the raw waste water. The peak areas of the decomposition products, used for quantification of the polymers, were adjusted using so-called response factors since the TED-GC-MS method is more sensitive for PP and PS than for PE. It has been shown that PE is the most dominant polymer in the samples. Comparing the masses of polymers in the effluent and in the raw sewage, a removal of 99 % of the polymers in the water treatment plant can be assumed. These results are consistent with the literature where removal rates between 98-99 % were described.
Fully-reversed fatigue behavior of scarf joint repairs for wind turbine blade shell applications
(2022)
To enable a quick and cost-effective return to service for wind turbine blades, localized repairs can be executed by technicians in the field. Scarf repairs, shown to be highly efficient with a smooth load transition across angled joint walls and a restored aerodynamic profile, are the focus of this work. The failure mechanisms of these structures were examined under quasi-static tensile and fully-reversed cyclic loading. While the scarf ratio was held constant at 1:50, the repair layup was varied between large-to-small and small-to-large. The effect of the presence of resin pockets and the fiber orientation mismatch between parent and repair material on the restored strength of BIAX ±45° glass fiber reinforced polymer scarf joint structures was studied.
Localized patches are a cost- and time-effective method for repairing fiber-reinforced polymer (FRP) sandwich wind turbine rotor blade shells. To increase the understanding of their effect on the fatigue of the blades, this study examines the effect of various layup methods of localized repair patches on the structural integrity of composite sandwich structures. Manufactured with the vacuum-assisted resin infusion (VARI) process, the shell test specimens are produced as a curved structure with glass fiber reinforced polymer (GFRP) sandwiching a polyvinyl chloride (PVC) foam core. Patch repairs are then introduced with varying layup techniques, and material properties are examined with cyclic fatigue tests. The transition region between patch and parent material is studied in greater detail with finite element method (FEM) simulations, with a focus on the effect of fiber orientation mismatch. Damage onset, crack development, and eventual failure are monitored with in-situ non-destructive testing methods to develop a robust understanding of the effects of repair concepts on material stiffness and strength.
Wind turbine rotor blades, made of fiber reinforced polymers (FRP), often fail before their projected 20-year lifespan, largely due to defects that originate during manufacturing and are propagated by operational fatigue and environmental conditions. The cost-intensive replacement outcomes lead to a high loss of earnings, and are one of the inhibitors of wind turbine production [1]. A potential repair alternative is to locally patch these areas of the blades with adhesively bonded structural repairs. However, the effects of such repair methods of the outer shell region on the structural integrity of the rotor blades are still largely unknown, and are thus investigated in this project.
The shell components of rotor blades are made of FRP composite material sandwiching a lightweight core, often a rigid foam or Balsa wood. The repair methods involve replacing the lost load path with a new material that is joined to the parent structure [2]. Repairs in this project focus on the scarf method, which allow for a smoother load distribution across the joint, aiming to study the damage mechanism of glass FRP scarf repairs for wind turbine blade shell applications. Namely, the source and path of the damage initiation and propagation, role of the interface between parent and patch material, and the role of the fiber orientation mismatch at this interface are examined. Biaxial ±45° and 0/90° FRP specimens are produced with the vacuum-assisted resin infusion (VARI) process using E-glass non-crimp fabric. The patch layers are then joined using VARI with a scarf ratio of 1:50, using glass FRP fabric with half the areal weight of the parent side to allow for better drapability. The methods and practices in specimen production are based on common industry practice in rotor blade shell manufacturing and repairs.
The specimens are tested under uniaxial tensile load, during which they are periodically monitored for damage onset. A comparison of the ±45° and 0/90° specimens allows for an understanding of the role of a highly mismatching fiber orientation in the transition zone between parent and patch material on the failure mechanism of the scarf joint. Although failure in both orientations begins as delamination at the joint edge, the difference in the mechanisms at play in the two different specimen types leads ultimately to different fracture paths. Namely, in the inter fiber failure mechanism of the ±45° specimens, the higher interlaminar strength compared to the intralaminar strength of the laminate leads to intralaminar failure of the ±45° scarf joint specimens. Alternatively, the competition in the 0/90° specimens lies between the interlaminar strength and fiber failure strength, and here we experience failure primarily across the scarf joint length. The scarf joint in the 0/90° specimens disrupts the continuity of the load-carrying 0° layers, directing the failure path to remain primarily along the scarf joint. Experimental results are compared to finite element analyses of scarf patch repairs on glass FRP sandwich specimens with the same respective layup orientations, where the damage initiation regions are identified and correlated to fiber orientation, serving as a bridge to future work which will experimentally examine the scarf repair patches on sandwich shell specimens.
Hochleistungsverbundwerkstoffe, bzw. Glasfaser-Kunststoff-Verbunde (GFK), haben sich als Leichtbauwerkstoffe für Leichtflugzeuge und Rotorblätter von Windkraftanlagen etabliert. Die hohe spezifische Festigkeit und Steifigkeit qualifizieren sie besonders für diese Anwendung. Während der Fertigung werden Imperfektionen häufig in die Blattschalen eingebracht. Durch Witterungseinflüsse kommt es zum Schadensfortschritt. Infolgedessen treten Schäden in der Blattschale, die den sicheren Betrieb gefährden können, weit vor der projektierten Lebensdauer von 20 Jahren auf. Da der Austausch von ganzen Blättern sehr kostintensiv ist, ist eine lokale Reparatur des geschädigten Bereichs zur Wiederherstellung der strukturellen Integrität, viel preisgünstiger. Die Reparatur von Rotorblättern ist in den letzten Jahren zu einem wichtigen Thema geworden. Derzeit werden verschiedenste Reparaturkonzepte angewendet. Eine einheitliche Reparaturvorgabe gibt es bisher nicht. Die Auswirkungen der angewendeten Reparaturkonzepte auf die Betriebsfestigkeit der Reparaturstelle sind weitestgehend unbekannt und sollen deshalb in diesem Projekt untersucht werden. Gekrümmte Voll-Laminat sowie Sandwich Prüfkörper werden mit dem Vacuum-Assisted-Resin-Infusion-Prozess (VARI) produziert. Um einen Teil einer Rotorblattschale darzustellen, sind sie als GFK aufgebaut, beziehungsweise die Sandwich Strukturen mit einem Polyvinylchlorid-Schaumkern (PVC) Kern, wie im Original. Schalenreparaturen in verschiedenen Layup-Techniken und Geometrie werden eingebracht und die Materialeigenschaften mit zyklischen Ermüdungstests untersucht. Im Projekt werden ideal im Labor erzeugte Reparaturstellen mit in der Praxis angewendeten Ausführungstechniken eines Industriepartners experimentell verglichen. Für die in-situ Detektion der Schadensentwicklung während des Ermüdungsversuches kommt ein kombiniertes Felddehnungs- und Thermografie-Kamerasystem zum Einsatz. Das mechanische Verhalten und die Schadensentwicklung in den verschiedenen reparierten Prüfkörper wird miteinander sowie mit den Referenzproben ohne Reparaturstellen verglichen. Zudem wird in numerischen Modellen für die verschiedenen Reparaturtechniken eine Spannungsanalyse durchgeführt um hinsichtlich der Betriebsbeanspruchung eine Bewertung angeben zu können.
High-performance composites, including glass-fiber reinforced plastic (GFRP) materials, are favored as a construction material for wind turbine rotor blades due to their high specific strength and stiffness properties. During the manufacturing process, however, imperfections are often introduced, then further propagated due to harsh environmental conditions and a variety of loads. This leads to failure significantly before their projected 20-year lifespan. As replacement of entire blades can be a costly potential outcome, localized repair of the damaged region to restore structural integrity and thus lengthen its lifespan has become an important issue in recent years. Rotor blades are often repaired using a common technique for composite laminates: adhesively bonded structural repair patches. These methods involve replacing the lost load path with a new material that is joined to the parent structure, and include scarf or plug repairs. However, there currently do not exist any standardized repair procedures for wind turbine rotor blades, as comparisons of blade properties repaired with the existing methods have not been studied in depth. Namely, there is a lack of understanding about the effects of various repair methods on the fatigue life of the shells of rotor blades. This study therefore aims to begin to fill this knowledge gap by testing the influence of different repair patches on the blades’ mechanical properties. Manufactured with the vacuum-assisted resin infusion process, the test specimens are produced as a curved structure with GFRP sandwiching a polyvinyl chloride foam core to best represent a portion of a rotor blade shell. Scarf repairs are then introduced with varying layup techniques, and material properties are examined with cyclical fatigue tests. Crack growth and development is monitored during fatigue testing by various non-destructive testing methods, including passive thermography with an infrared camera system, and a 3D deformation analysis system with ARAMIS. Large deformation fields and detection of in- and out-of-plane deformations is thus possible in-situ. The mechanical behavior and development of defects in the various repaired specimens is compared to each other as well as to reference test specimens with no repair patches. In-situ test data is combined with further non-destructive testing methods, including laminography, and active thermography, to develop a robust understanding of the effects of repair concepts.
Wind turbine rotor blades commonly fail before their projected 20-year lifespan largely due to defects that originate during manufacturing and are propagated by operational fatigue and environmental conditions. The cost-intensive replacement outcomes lead to a high loss of earnings, and are one of the inhibitors of wind turbine production. A potential repair alternative to restoring the mechanical properties of such lightweight fiber reinforced polymer (FRP) structures is to locally patch these areas with scarf joints. This type of repair allows for a smoother load distribution across the joint, and is favored especially on structures where minor aerodynamic contour changes are key. The effects of such repairs on the structural integrity, however, is still largely unknown. Building upon an understanding of the static load failure mechanism of GFRP scarf joints, presented at the ICCS23 Joint Event in 2020, the influence of the fiber orientation mismatch between parent and repair materials of 1:50 scarf joints on the failure mechanism of monolithic glass FRP specimens under cyclic fatigue load were examined in this study. Specimens with various layups were produced with the vacuum-assisted resin infusion (VARI) process using biaxial E-glass non-crimp fabric (NCF). The patch layers were then joined directly to the parent structure with the VARI using biaxial E-glass NCF with half the areal weight of the parent side to allow for better drapability. This mimics the soft-to-hard patch style utilized in wind turbine blade shell field repairs. The specimens were tested under uniaxial fatigue load, during which they were periodically monitored for damage onset. A comparison of the +45/-45° and 0/90° layups allowed for an understanding of the role of a highly mismatching fiber orientation in the transition zone between parent and patch material on the failure mechanism of the scarf joint. In addition to the tensile strength and stiffness property recovery assessment, a grayscale analysis using in-situ camera images determined the damage state leading to failure in each region across the scarf joint, which varied in the parent material versus scarf joint region, providing insight to the critical regions in this composite structure under cyclic loading.
As a type of high-performance composite material, glass-fiber reinforced plastics (GFRP) are favored for the construction of wind turbine rotor blades due to their high specific strength and stiffness properties (Grasse et al, 2010). During the blade manufacturing process, however, imperfections are often introduced, then further propagated due to harsh environmental conditions and a variety of loads (Caminero et al, 2013; Trappe et al, 2018). This leads to failure significantly before their designed lifespan. Since replacement of entire blades can be a costly potential outcome, localized repairs of the damaged region to restore structural integrity and thus lengthen its lifespan can executed in the field by technicians accessing the blades directly by suspended roping. These methods involve replacing the lost load path with a new material that is joined to the parent structure. In recent years, considerable studies have been conducted to investigate the influence of different repair parameters on the stress distribution, ultimate strength, impact behavior, and residual stresses of bonded repaired structures [Caminero et al, 2013; Trappe et al, 2018; Shufeng et al, 2014; Harman and Rider, 2011; Ahn and Springer, 2000; Lekou and Vionis, 2002). However, there currently do not exist any standardized repair procedures for wind turbine rotor blades. Namely, there is a lack of understanding about the effects of the layup of various repair methods, especially on the damage mechanism and fatigue life of the shells of rotor blades (Caminero et al, 2013; Trappe et al, 2018).
This work therefore aims to begin to enrich this knowledge gap by testing the influence of different variables among repair patches on the mechanical properties of sandwich composite structures. Manufactured with the vacuum-assisted resin infusion (VARI) process, the test specimens are produced as a GFRP structure to represent the outer shell portion of a wind turbine blade, then repaired with a scarf joint. Scarf repairs are favored as the most efficient of the common structural joints, as the removal of the damaged area with angled walls leads to a nearly uniform shear stress distribution along the bond surface and no eccentricity in the load distribution (Caminero et al, 2013; Lekou and Vionis, 2002; Siener, 1992).
The performance of specific layup methods of repair patches, namely a large-to-small versus small-to-large scheme of repair layers, is studied with static and load-controlled fatigue testing, then compared to pristine test specimens as well as to each other in terms of mechanical property restoration. The transition layer between repair and parent material is especially of interest in the performance of the structure. Damage onset, crack development and eventual failure are monitored in-situ with non-destructive testing methods, including thermography with an infrared camera system and a 3D deformation analysis system, to develop a more robust understanding of the effects of these repair concept variables on wind turbine blade shell structures.
Fully-reversed fatigue behavior of scarf joint repairs for wind turbine blade shell applications
(2022)
Due to manufacturing imperfections which can propagate to damage under in-service loads, wind turbine rotor blades, made primarily of glass fiber reinforced polymers (GFRP), often fail significantly before their design life. To enable a quick and cost-effective return to service, localized repairs can be executed by technicians in the field, directly accessing the blades by suspended roping. Scarf joint repairs, shown to be highly efficient with a smooth load transition across angled joint walls and a restored aerodynamic profile, are the focus of this study. The damage mechanisms of these structures were examined under fully-reversed mechanical cyclic loading with a load ratio R = -1, which was made possible on the coupon scale by a custom designed anti-buckling support. The number of cycles to failure were compared across load levels. While the scarf joint ratio was held constant at 1:50, known from industry and literature to be a good compromise between restored mechanical properties and repair size, the layup sequence was varied between small-to-large and large-to-small. Hereby the effect of the presence of resin pockets and fiber orientation mismatch between the parent and repair structure on the failure mechanism as well as fatigue strength of ±45° GFRP scarf joint repair structures was studied. Strain development across the joint length was measured to assess stiffness degradation in addition to the fatigue strength recovery of scarf joint structures with respect to pristine reference specimens. Grayscale analysis was used to monitor the damage state leading to fracture across the specimens. Post-mortem fractography analysis with light microscopy described the global failure mechanisms as well as local damage distribution within the structure, all of which provided insight to critical variables in scarf joint GFRP structures under fully-reversed mechanical cyclic loading, allowing for the tailoring of such repairs on wind turbine blade shells for maximum restoration of service life.
Wind turbine rotor blade shells are manufactured as sandwich structures with fiber-reinforced polymer (FRP) due to the material’s high specific stiffness and strength. With a growing renewable energy industry and thereby a spread of wind energy farms, especially in offshore applications, the need to fully utilize turbines through their designed lifespan is becoming increasingly essential. However, due to imperfections during manufacturing, which are then propagated by harsh environmental conditions and a variety of loads, blades often fail before their projected lifespan. Thus, the need for localized repair patch methods for the outer shell portions of the blades has become of greater interest in recent years, as it is crucial to the optimal compromise between continuation of wind energy production, cost efficiency, and restoration of structural performance. To increase the understanding of the effect on the fatigue life of the rotor blades, this study tests localized repair patch methods and compares them to each other as well as to reference, non-repaired specimens. Manufactured with the vacuum-assisted resin infusion process, the shell test specimens are produced as a curved structure with glass FRP sandwiching a polyvinyl chloride foam core to best represent a portion of a rotor blade shell. Patch repairs are then introduced with varying layup techniques, and material properties are examined with cyclic fatigue tests. The intermediate scale test specimens allow for the observation of material as well as structural variables, namely of interest being the stiffness and strength restoration due to the repair patches. Damage onset, crack development, and eventual failure are monitored with in-situ non-destructive testing methods to develop a robust understanding of the effects of repair concepts.
The introduction of the 5G technology and automotive radar applications moving into higher frequency ranges trigger further miniaturization of LTCC technology (low temperature co-fired ceramics). To assess dimensional tolerances of inner metal structures of an industrially produced LTCC multilayer, computer tomography (CT) scans were evaluated by machine learning segmentation.
The tested multilayer consists of several layers of a glass ceramic substrate with low resistance silver-based vertical interconnect access (VIA). The VIAs are punched into the LTCC green tape and then filled with silver-based pastes before stacking and sintering. These geometries must abide by strict tolerance requirements to ensure the high frequency properties.
This poster presents a method to extract shape and size specific data from these VIAs. For this purpose, 4 measurements, each containing 3 to 4 samples, were segmented using the trainable WEKA segmentation, a non-commercial machine learning tool. The dimensional stability of the VIA can be evaluated regarding the edge-displacement as well as the cross-sectional area. Deviation from the ideal tubular shape is best measured by aspect ratio of each individual layer. The herein described method allows for a fast and semi-automatic analysis of considerable amount of structural data. This data can then be quantified by shape descriptors to illustrate 3-dimensional information in a concise manner. Inter alia, a 45 % periodical change of cross-sectional area is demonstrated.
Die Steigerung der Leistung und des thermodynamischen Wirkungsgrades von Verbrennungsmotoren führt zu erhöhten Anforderungen an die Festigkeit abgasführender Komponenten wie z. Bsp. Abgasturbolader. Als Folge erhöhter thermomechanischer Wechselbeanspruchungen (TMF) im Betrieb kommt es an den mechanisch und/oder thermisch höchst beanspruchten Stellen der Bauteile zur Bildung von Rissen, wodurch die Lebensdauer der Komponenten begrenzt wird. Derzeit werden bei Turboladern heißgehende Bauteile mit detektierten Rissen zumeist prophylaktisch ersetzt, da die weitere Ausbreitung der Risse während des Betriebs nicht vorhergesagt werden kann. Um diese aufwändige und un- ökonomische Praxis zu vermeiden, wurde im vorliegenden Forschungsvorhaben eine rechnerische Bewertungsmethode auf Basis der experimentellen und numerischen Bruchmechanik erarbeitet, mit deren Hilfe bereits in der Auslegungsphase oder während des Betriebs die (restliche) Lebensdauer der abgasführenden Komponenten vorhergesagt werden kann. Damit wird erstmalig die quantitative Vorhersage der Rissentwicklung bei TMF-Beanspruchungsbedingungen unter Berücksichtigung großer zyklischer viskoplastischer Verformungen ermöglicht.
Zentrales Ergebnis des Vorhabens ist eine automatisierte Berechnungsprozedur auf der Basis spezieller Finite-Elemente-Techniken (FEM), womit sowohl der Pfad als auch die Größe eines Risses als Funktion der Anzahl der Lastwechsel in Bauteilen unter TMF-Bedingungen berechnet werden kann. Als geeigneter Beanspruchungsparameter zur Bewertung des Rissfortschritts unter TMF wurde die zyklische Rissöffnungsverschiebung ΔCTOD verwendet. Das Werkstoffverhalten des betrachteten austenitischen Gusseisens Ni-Resist D-5S wurde mit einem validierten viskoplastischen, temperaturabhängigen Materialmodell modelliert, das zur Berücksichtigung große Verzerrungen und Rotationen am Riss erweitert wurde. Für die genaue Berechnung des ΔCTOD bei TMF wurden effiziente FEM-Techniken erarbeitet. Zur Simulation der Rissausbreitung wurde ein automatischer FEM-Algorithmus mit inkrementeller adaptiver Neuvernetzung entwickelt, bei dem die Verformungen und inelastischen Zustandsvariablen jeweils vom alten auf das neue Netz übertragen werden. Dieser Algorithmus wurde im Software-Paket ProCrackPlast implementiert, das in Verbindung mit dem kommerziellen FEM-Code Abaqus zur Lösung dreidimensionaler Rissprobleme zur Verfügung steht. Ziel der umfangreichen experimentellen Arbeiten war es, an isothermen LCF und anisothermen TMF-Versuchen mit gekerbten Flachzugproben (SENT) das Risswachstum im Temperaturbereich von 20 °C bis 700 °C zu ermitteln. Mit Hilfe begleitender 2D FEM Simulationen wurden anhand dieser Datenbasis die Rissfortschrittskurven des Werkstoffs unter Anwendung des ΔCTOD-Konzepts bestimmt und in geeigneter, parametrisierter Form den Nutzern zur Verfügung gestellt. Die Versuche an SENT-Proben wurden mit der entwickelten Software ProCrackPlast als 3D Modell simuliert. Der Vergleich der 2D und 3D Simulationen ergab einen systematischen Unterschied im CTOD und CTOD, der mit Hilfe eines Übertragungsfaktors korrigiert wurde. Der Vergleich der 3D Berechnungen mit den Experimenten zeigte eine zufriedenstellende Übereinstimmung der er- reichten Risslänge mit der Zahl der Lastzyklen im gesamten Temperaturbereich, wobei die numerische Prognose meist auf der konservativen / sicheren Seite lag. Die Übertragbarkeit der Ergebnisse der 2D Parameteridentifikation auf 3D Risskonfigurationen mit Mixed-Mode Beanspruchung ist mit zusätzlichen Versagenshypothesen verbunden, die aufgrund fehlender Versuchsdaten im Vorhaben nicht endgültig geklärt werden konnten. Zur Validierung des Gesamtkonzeptes wurden LCF-Proben mit einem bauteil- typischen Oberflächenriss experimentell und numerisch untersucht. In der Simulation konnte die komplexe Form und Größe der Rissentwicklung zufriedenstellend (richtig) vorhergesagt werden. Die Leis- tungsfähigkeit der erarbeiteten rechnerische Bewertungsmethode wurde an weiteren TMF-Beispielen vorgestellt und diskutiert. Die Software ProCrackPlast und die viskoplastische Materialroutine wurden dem Anwenderkreis des Vorhabens zusammen mit einem Nutzer-Handbuch und Verifikationsbeispielen zur Verfügung gestellt.
Das Ziel des Forschungsvorhabens ist erreicht worden.
Due to combined cyclic mechanical and thermal loading during operation, the material of exhaust gas conducting components of combustion engines is exposed to thermomechanical fatigue (TMF). This leads to formation and growth of cracks, especially at the most highly stressed points of these components. In order to better predict the service life of cracked components before failure, it is necessary to identify a crack propagation law for the material used. Isothermal crack propagation tests have been carried out at several temperatures with a typical cast iron to identify such a law. The crack length is measured by the potential drop method. The compliance method, fractography and thermographic camera measurements have been used to validate and calibrate the potential drop measurements. Each of the isothermal tests has been simulated using a specially developed FEM-algorithm based on remeshing and remapping. This algorithm has been implemented in python and ABAQUS. Thereby, the crack tip region is modeled by collapsed Quad8 elements. From the individual simulations, the cyclic crack tip opening displacement (ΔCTOD) is extracted and regarded as a potential fracture mechanics parameter which controls the crack growth rate. By combining the data from the experiments and the simulations, the crack propagation law has been identified. Finally, anisothermal crack propagation tests have been performed for validation of the crack growth law.
The cyclic crack tip opening displacement ΔCTOD is a promising loading Parameter to quantify the crack propagation under thermomechanical fatigue (TMF). In this work, suitable techniques are investigated and compared for an accurate calculation of ΔCTOD under TMF loading using a viscoplastic temperature dependent material model.
It turned out that collapsed special crack tip elements give the best results. An efficient FEM-technique is developed to simulate the incremental crack growth by successive remeshing, whereby the deformations and internal state variables are mapped from the old mesh onto the new one. The developed techniques are demonstrated and discussed for two-dimensional examples like TMF-specimens. Recommendations are made regarding important numerical control parameters like optimal size of crack tip elements, length of crack growth increment in relation to plastic zone size and ΔCTOD value.
The cyclic crack tip opening displacement ΔCTOD is a promising loading Parameter to quantify the crack propagation under thermomechanical fatigue (TMF). In this work, suitable techniques are investigated and compared for an accurate calculation of ΔCTOD under TMF loading using a viscoplastic temperature dependent material model.
It turned out that collapsed special crack tip elements give the best results. An efficient FEM-technique is developed to simulate the incremental crack growth by successive remeshing, whereby the deformations and internal state variables are mapped from the old mesh onto the new one. The developed techniques are demonstrated and discussed for two-dimensional examples like TMF-specimens. Recommendations are made regarding important numerical control parameters like optimal size of crack tip elements, length of crack growth increment in relation to plastic zone size and ΔCTOD value.
The cyclic crack tip opening displacement ΔCTOD is a promising loading Parameter to quantify the crack propagation under thermomechanical fatigue (TMF). In this work, suitable techniques are investigated and compared for an accurate calculation of ΔCTOD under TMF loading using a viscoplastic temperature dependent material model.
It turned out that collapsed special crack tip elements give the best results. An efficient FEM-technique is developed to simulate the incremental crack growth by successive remeshing, whereby the deformations and internal state variables are mapped from the old mesh onto the new one. The developed techniques are demonstrated and discussed for two-dimensional examples like TMF-specimens. Recommendations are made regarding important numerical control parameters like optimal size of crack tip elements, length of crack growth increment in relation to plastic zone size and ΔCTOD value.
The finite element software ProCrackPlast is developed for the automated simulation of fatigue crack growth in arbitrarily loaded three-dimensional components with large scale plastic deformations, in particular under cyclic thermomechanical (TMF) loading.
ProCrackPlast is developed by extending the software Procrack, created at TU Freiberg for linear-elastic crack growth simulations. The pre-processing, FEM analysis, and the post-processing in ProCrackPlast are done by the commercial software ABAQUS. ProCrackPlast resorts to a crack growth procedure which adaptively updates the crack in finite increments based on the fracture-mechanical parameter, cyclic crack tip opening displacement ΔCTOD . Features of this software along with two application examples of fatigue crack growth in a typical cast steel, Ni-Resist, are presented in this paper to show its capability and performance.
Recently, detection and conversion of high energy radiation such as ultraviolet and X-rays has gained renewed attention. In part, technological applications in radioimaging and tomography have developed considerably as to allow lower dosages and higher resolutions, which require optimized scintillators and dosimeters. On the other hand, the increasing effort to reduce carbon footprint in energy production has triggered an intensive search for materials that can be excited with sunlight, ranging from photocatalysts to solar concentrators. At LEMAF – Laboratory of Spectroscopy of Functional Materials at IFSC/USP, we have been developing bulk glasses, polycrystalline and composite materials designed to target both challenges and, in this work an overview of recent progresses and of the state of art of these materials will be given.
For instance, the few available comercial scintillators are crystalline materials with costly and time consuming growth which hinders the development of new compositions. Glasses and glass ceramics, such as the NaPGaW composition developed in our lab, present high density, very good optical properties and high chemical stability which allow them radioluminescent response when doped with low concentrations of Ce3+, Eu3+ and Tb3+ offering a promise as alternatives to crystal scintillators. On the other hand, phosphor in glass (PiG) composites based on the persistent luminescent polycrystalline material Sr2MgSi2O7:Eu2+,Dy3+ (SMSO) embedded into NaPGa glasses offer interesting perspectives for the of UV light into visible, useful for white light generation (lighting), improved harvesting and conversion of solar light when coupled to c-Si PV cells and photocatalysis. These and other examples will be discussed.
The glasses are prepared through the conventional melt quenching technique, followed by controlled heating when glass ceramics are desired. The persistent luminescent phosphor is prepared by the microwave assisted technique (MAS) much faster and with considerable energy consumption reduction than in the usual solid state synthesis. The materials are characterized from the structural, morphological and spectroscopic (optical – UV-Vis, PL, PLE, and structural – NMR, EPR) points of view such that structure-property correlations are constantly sought to feedback synthesis and processing. Fig. 1, illustrates two examples of scintillator glasses doped with Tb3+ and PiG composites doped with Eu2+ and Dy3+.
The glass system (50NaPO3–20BaF2–10CaF2–20GdF3)-xTbCl3 with x = 0.3, 1, 3, 5, and 10 wt % was investigated. We successfully produced transparent glass ceramic (GC) scintillators with x = 1 through a melt-quenching process followed by thermal treatment. The luminescence and crystallization characteristics of these materials were thoroughly examined using various analytical methods. The nanocrystallization of Tb3+-doped Na5Gd9F32 within the doped fluoride-phosphate glasses resulted in enhanced photoluminescence (PL) and radioluminescence (RL) of the Tb3+ ions. The GC exhibited an internal PL quantum yield of 33 % and the integrated RL intensity across the UV-visible range was 36 % of that reported for the commercial BGO powder scintillator. This research showcases that Tb-doped fluoridephosphate GCs containing nanocrystalline Na5Gd9F32 have the potential to serve as efficient scintillators while having lower melting temperature compared to traditional silicate and germanate glasses.
The main deference between high entropy alloys and conventional alloys is the solid solution strengthening effect, which moves from a single element to a multi-element matrix. Little is known about the effectiveness of this effect at high temperatures. Investigation of temperature dependent solid solution strengthening in single phase multicomponent alloys with medium and high entropy using creep testing was performed. Creep tests carried out on single phase SX CrCoNi , CrMnFeCoNi and pure Ni from 700 to 1200 °C excluding oxidation, grain boundaries and multiphase effects. It was found that the influence of solid solution strengthening of CrCoNi and CrMnFeCoNi increases by decreasing temperature (1200 to 700 °C), and dislocation forests occur in CrCoNi and CrMnFeCoNi in comparison to pure Ni.
AbstractGallium fluoride phosphate glasses feature low refractive index, high energy radiation resistance, wide transmission range, and favorable emission characteristics of rare‐earth dopants. For the development of optimized glass compositions, a fundamental understanding of these properties in terms of glass structure is sought. We report nuclear magnetic resonance (NMR) structural studies of glasses in the system xGa(PO3)3–(40 − x)GaF3–20BaF2–20ZnF2–20SrF2 (x = 5, 10, 15, 20, and 25 mol%). 31P NMR results with 71Ga recoupling show that the network structure is dominated by P–O–Ga linkages, and no P–O–P linkages exist. 71Ga NMR results show that Ga is mainly six‐coordinated featuring a mixed fluoride/phosphate coordination. Quantitative estimates of this ligand distribution around gallium were obtained by 71Ga{31P} spin echo double resonance (REDOR) measurements. Photophysical properties suggest changes in the Eu(III) ligand distribution toward a fluoride‐dominated environment at low P/F ratio while the glass network is largely sustained by bridging oxygen atoms via P–O–Ga linkages.
Um den sicheren Betrieb von Windkraftanlagen zu gewährleisten, werden Rotorblätter nach der Fertigung und nach Reparatur mit verschiedenen zerstörungsfreien Verfahren auf Schaden untersucht. Bei der Fertigung von Blattschalen, die in einer Sandwich-Schalenbauweise gefertigt werden, entstehen Imperfektionen, die unter Belastung zu großen Rissen führen können. Zur Prüfung von Blattschalen wird unter anderem Ultraschallprüfung in Kontakttechnik eingesetzt. Um den Wartungsaufwand von Ultraschallanlagen zu reduzieren und um manche Kompositstrukturen vor Koppelmittel zu schützen, wird die Anwendung von Luftultraschall erforscht. Insbesondere große Fortschritte gibt es im Bereich der Entwicklung neuer Wandler.
In diesem Beitrag berichten wir über die Luftultraschallprüfung von Schalen für Rotorblätter. Es wurden typische Sandwichschalenstrukturen hergestellt und mit einem eigenentwickelten Schalenprüfstand unter simulierter Betriebsbeanspruchung belastet. Die in den Schalenprüfkörpern entstandenen Schäden wurden außerhalb des Prüfstandes mit Luftultraschall in Durchschallung untersucht. Es wurden fokussierende Wandler auf Basis von Ferroelektreten entwickelt und für diese Prüfungen eingesetzt. Mit zusätzlicher elektrischer Vorspannung konnte die Empfindlichkeit der Empfänger deutlich erhöht werden. Die nach dem Lastwechsel entstandenen Schäden in den Rotorblattschalen waren eindeutig zu detektieren.
Common air-coupled transducers for non-destructive testing consist of a piezocomposite material and several matching layers. Better acoustical matching to air is achieved by transducers based on charged cellular polypropylene (PP). This material has about hundred times lower acoustic impedance than any piezocomposite, having about the same piezoelectric coefficient. The piezoelectric properties of cellular PP are caused by the polarization of air cells. Alternatively, a ferroelectret receiver can be understood as a capacitive microphone with internal polarization creating permanent internal voltage. The sensitivity of the receiver can be increased by applying additional bias voltage. We present an ultrasonic receiver based on cellular PP including a high-voltage module providing bias voltage up to 2 kV. The application of bias voltage increased the signal by 12 to 15 dB with only 1 dB increase of the noise.
This receiver was combined with a cellular PP transmitter in through transmission to inspect several test specimens consisting of glass-fiber-reinforced polymer face sheets and a porous closed-cell PVC core. These test specimens were inspected before and after load. Fatigue cracks in the porous PVC core and some fatigue damage in the face sheets were detected. These test specimens were originally developed to emulate a rotor blade segment of a wind power plant. Similar composite materials are used in lightweight aircrafts for the general aviation. The other inspected test specimen was a composite consisted of glass-fiber-reinforced polymer face sheets and a wooden core. The structure of the wooden core could be detected only with cellular PP transducers, while commercial air-coupled transducers lacked the necessary sensitivity. Measured on a 4-mm thick carbon-fiber-reinforced polymer plate, cellular PP transducers with additional bias voltage achieved a 32 dB higher signal-to-noise ratio than commercial air-coupled transducers.
Um den sicheren Betrieb von Windkraftanlagen zu gewährleisten, werden Rotorblätter nach der Fertigung und nach Reparatur mit verschiedenen zerstörungsfreien Verfahren auf Schaden untersucht. Bei der Fertigung von Blattschalen, die in einer Sandwich-Schalenbauweise gefertigt werden, entstehen Imperfektionen, die unter Belastung zu großen Rissen führen können. Zur Prüfung von Blattschalen wird unter anderem Ultraschallprüfung in Kontakttechnik eingesetzt. Um den Wartungsaufwand von Ultraschallanlagen zu reduzieren und um manche Kompositstrukturen vor Koppelmittel zu schützen, wird die Anwendung von Luftultraschall erforscht. Insbesondere große Fortschritte gibt es im Bereich der Entwicklung neuer Wandler.
In diesem Beitrag berichten wir über die Luftultraschallprüfung von Schalen für Rotorblätter. Es wurden typische Sandwichschalenstrukturen hergestellt und mit einem eigenentwickelten Schalenprüfstand unter simulierter Betriebsbeanspruchung belastet. Die in den Schalenprüfkörpern entstandenen Schäden wurden außerhalb des Prüfstandes mit Luftultraschall in Durchschallung untersucht. Es wurden fokussierende Wandler auf Basis von Ferroelektreten entwickelt und für diese Prüfungen eingesetzt. Mit zusätzlicher elektrischer Vorspannung konnte die Empfindlichkeit der Empfänger deutlich erhöht werden. Die nach dem Lastwechsel entstandenen Schäden in den Rotorblattschalen waren eindeutig zu detektieren.
Common air-coupled transducers for non-destructive testing consist of a piezocomposite material and several matching layers. Better acoustical matching to air is achieved by transducers based on charged cellular polypropylene (PP). This material has about hundred times lower acoustic impedance than any piezocomposite, having about the same piezoelectric coefficient. The piezoelectric properties of cellular PP are caused by the polarization of air cells. Alternatively, a ferroelectret receiver can be understood as a capacitive microphone with internal polarization creating permanent internal voltage. The sensitivity of the receiver can be increased by applying additional bias voltage. We present an ultrasonic receiver based on cellular PP including a high-voltage module providing bias voltage up to 2 kV. The application of bias voltage increased the signal by 12 to 15 dB with only 1 dB increase of the noise.
This receiver was combined with a cellular PP transmitter in through transmission to inspect several test specimens consisting of glass-fiber-reinforced polymer face sheets and a porous closed-cell PVC core. These test specimens were inspected before and after load. Fatigue cracks in the porous PVC core and some fatigue damage in the face sheets were detected. These test specimens were originally developed to emulate a rotor blade segment of a wind power plant. Similar composite materials are used in lightweight aircrafts for the general aviation. The other inspected test specimen was a composite consisted of glass-fiber-reinforced polymer face sheets and a wooden core. The structure of the wooden core could be detected only with cellular PP transducers, while commercial air-coupled transducers lacked the necessary sensitivity. Measured on a 4-mm thick carbon-fiber-reinforced polymer plate, cellular PP transducers with additional bias voltage achieved a 32 dB higher signal-to-noise ratio than commercial air-coupled transducers.
Recently, additive manufacturing of ceramics has achieved the maturity to be transferred from scientific laboratories to industrial applications. At the same time, research is progressing to expand the boundaries of this field into the territory of novel materials and applications. This feature issue addresses current progress in all aspects of additive manufacturing of ceramics, from parts design to feedstock selection, from technological development to characterization of printed components.
Fresnoite glass with excess SiO2 exhibits oriented surface crystallization, in contrast to the stoichiometric glass composition. Recent EBSD studies documented that the crystals in BTS (2BaO-TiO2-xSiO2, x=0-3) can occur in a distinct [101]-orientation perpendicular to the surface and claimed that this orientation is not a result of growth selection. During these previous studies, however, the effect of surface preparation and surrounding atmosphere during the crystallization experiments were not considered. As these parameters may influence crystal orientation, we studied the surface crystallization of a BTS glass (2BaO-TiO2–2.75SiO2) under controlled conditions with the help of light, electron and polarisation microscopy as well as EBSD. Heat treatments for one hour at 840°C of fractured BTS glass surfaces in air resulted in a large number of not-separable surface crystals. This large number of crystals can be caused by dust particles, which act as nucleation agents. As crystal growth velocity could further be influenced by humidity, our experiments are performed in a filtered and dried air atmosphere. The crystal morphology and orientation will be analysed in dependence of the sample preparation and a differing surrounding atmosphere.
Inconel 718 (IN718) is a traditional age-hardenable nickel-based alloy that has been increasingly processed by additive manufacturing (AM) in recent years. In the as-solidified condition, IN718 exhibits chemical segregation and the undesired Laves phase, requiring a solution annealing (SA) prior to aging. The material produced by AM does not respond to the established thermal routines in the same way as conventionally produced IN718, and there is still no consensus on which routine yields optimal results. This work aims to provide a fundamental understanding of the heat treatment (HT) response by continuously monitoring the microstructural evolution during SA via time-resolved synchrotron x-ray diffraction, complemented by ex-situ scanning electron microscopy (SEM). The samples were produced by laser powder bed fusion to a geometry of 10x20x90 mm³, from which Ø1x5 mm³ cylindric specimens were extracted. Two different scanning strategies – incremental 67° rotations, Rot, and alternating 0°/67° tracks, Alt – were used, leading to two different as-built conditions. 1-hour SAs were carried out in the beamline ID22 of the ESRF at 50 KeV. Two SA temperatures, SA1 = 1020 °C, and SA2 = 1080 °C were tested for each scanning strategy. Data were processed using the software PDIndexer. In the as-built state, all samples showed typical subgrain columnar cell structures with predominant Nb/Mo segregation and Laves phase at the cell walls, as seen by SEM. The Alt scan induced higher intensity on the Laves peaks than the Rot scan, suggesting a greater content of Laves. Chemical homogenization in the SA was largely achieved during the heating ramp (Fig. 1). SA2 eliminated the Laves peaks just before reaching 1080 °C, and mitigated differences between Rot and Alt samples. On the other hand, SA1 induced the precipitation of the generally detrimental δ phase, also observed by SEM. Furthermore, the Rot scan showed higher δ peak intensities than the Alt scan, indicating a higher content of δ in the latter. No signs of recrystallization were observed in any of the investigated SAs.
In this work we instigated the fragmentation of Au microparticles supported on a thin amorphous carbon film by irradiating them with a gradually convergent electron beam inside the Transmission Electron Microscope. This phenomenon has been generically labeled as “electron beam-induced fragmentation” or EBIF and its physical origin remains contested. On the one hand, EBIF has been primarily characterized as a consequence of beam-induced heating. On the other, EBIF has been attributed to beam-induced charging eventually leading to Coulomb explosion. To test the feasibility of the charging framework for EBIF, we instigated the fragmentation of Au particles under two different experimental conditions. First, with the magnetic objective lens of the microscope operating at full capacity, i.e. background magnetic field B = 2 T, and with the magnetic objective lens switched off (Lorenz mode), i.e. B = 0 T. We observe that the presence or absence of the magnetic field noticeably affects the critical current density at which EBIF occurs. This strongly suggests that magnetic field effects play a crucial role in instigating EBIF on the microparticles. The dependence of the value of the critical current density on the absence or presence of an ambient magnetic field cannot be accounted for by the beam-induced heating model. Consequently, this work presents robust experimental evidence suggesting that Coulomb explosion driven by electrostatic charging is the root cause of EBIF.
Mit Hilfe des HIP-Verfahrens („Hot Isostatic Pressing“) werden Poren in der einkristallinen Nickel-Basis Superlegierung CMSX-4 kontinuierlich geschrumpft und dadurch die nach der Erstarrung und der Wärmebehandlung vorhandene Porosität stark reduziert. In diesem Beitrag werden experimentelle und numerische Untersuchungen zu den Mechanismen der Porenschrumpfung zusammengefasst. Es zeigt sich, dass das Verformungsverhalten während Kriechversuchen bei der HIP-Temperatur durch Versetzungsgleitung auf oktaedrischen Ebenen dominiert wird.
Dagegen zeigen Messungen der Porositätsabnahme und Simulationen des Porenschließens, dass die Kinetik der Porenschrumpfung durch das Phänomen der Leerstellendiffusion zwischen Poren und Kleinwinkelkorngrenzen („Low Angle Boundary“, LAB) bestimmt wird. Im Gegensatz führt die klassische Kristallviskoplastizität zu einer systematischen Überschätzung dieser Kinetik. Der scheinbare Widerspruch lässt sich auflösen, wenn man bedenkt, dass auf der Skala der Poren Versetzungsquellen nicht gleichmäßig verteilt sind, wie in der konventionellen Kristallplastizität implizit angenommen wird. Stattdessen wird in einem weiterführenden Modell davon ausgegangen, das Kleinwinkelkorngrenzen (LABs) als Versetzungsquellen fungieren, während die Scherspannungen sehr stark in der Nähe der Poren lokalisiert sind, was die Emission von Versetzungen deutlich reduziert.
The elastic constants are the most basic mechanical properties of a material and are needed for any structural analysis of a component. For example, they have a major influence on the eigenfrequencies of vibrating parts. Single crystals of Ni-base superalloys are strongly anisotropic, which means that the observed properties are orientation dependent. Tensor algebra is then required to mathematically formulate the elastic properties and their relations to the crystal orientation. Hence, this chapter first summarizes some basic definitions and calculation rules for Rotation matrices, including the definition of the Euler angles, which are most commonly used to define the relative orientations of the crystal and the component. Parts of this chapter closely follow the lines of the excellent exposition of the topic by Olschewski.
The large number of TEM investigations and the regular microstructure
of single-crystal nickel-base superalloys has boosted the development of a number of physically motivated constitutive laws. In contrast to the more phenomenological models discussed in the next chapter, these models use dislocation densities as internal variables. Obvious advantages are that the computed densities can be compared to TEM observations and the Deformation mechanisms can be easier translated into mathematical equations.
Mit Hilfe des HIP-Verfahrens („Hot Isostatic Pressing“) werden Poren in der einkristallinen Nickel-Basis Superlegierung CMSX-4 kontinuierlich geschrumpft und dadurch die nach der Erstarrung und der Wärmebehandlung vorhandene Porosität stark reduziert. In diesem Beitrag werden experimentelle und numerische Untersuchungen zu den Mechanismen der Porenschrumpfung zusammengefasst. Es zeigt sich, dass das Verformungsverhalten während Kriechversuchen bei der HIP-Temperatur durch Versetzungsgleitung auf oktaedrischen Ebenen dominiert wird.
Dagegen zeigen Messungen der Porositätsabnahme und Simulationen des Porenschließens, dass die Kinetik der Porenschrumpfung durch das Phänomen der Leerstellendiffusion zwischen Poren und Kleinwinkelkorngrenzen („Low Angle Boundary“, LAB) bestimmt wird. Im Gegensatz führt die klassische Kristallviskoplastizität zu einer systematischen Überschätzung dieser Kinetik. Der scheinbare Widerspruch lässt sich auflösen, wenn man bedenkt, dass auf der Skala der Poren Versetzungsquellen nicht gleichmäßig verteilt sind, wie in der konventionellen Kristallplastizität implizit angenommen wird. Stattdessen wird in einem weiterführenden Modell davon ausgegangen, das Kleinwinkelkorngrenzen (LABs) als Versetzungsquellen fungieren, während die Scherspannungen sehr stark in der Nähe der Poren lokalisiert sind, was die Emission von Versetzungen deutlich reduziert.