5 Werkstofftechnik
Filtern
Erscheinungsjahr
- 2022 (13) (entfernen)
Dokumenttyp
- Vortrag (8)
- Zeitschriftenartikel (5)
Sprache
- Englisch (9)
- Deutsch (3)
- Mehrsprachig (1)
Schlagworte
- AGIL (4)
- Additive manufacturing (3)
- Laser powder bed fusion (3)
- Microstructure (3)
- Additive Fertigung (2)
- Additive Manufacturing (2)
- Diffraction (2)
- Electron backscatter diffraction (2)
- Mechanical behavior (2)
- Neutron diffraction (2)
Organisationseinheit der BAM
- 9 Komponentensicherheit (13) (entfernen)
Eingeladener Vortrag
- nein (8)
Laser powder bed fusion (PBF-LB/M) of metallic alloys is a layer wise additive manufacturing process which provides significant scope for more efficient designs of components, benefiting performance and weight, leading to efficiency improvements for various sectors of industry. However, to benefit from these design freedoms, knowledge of the high produced induced residual stress and mechanical property anisotropy associated with the unique microstructures is critical. X-ray and neutron diffraction are considered the benchmark for non-destructive characterization of surface and bulk internal residual stress. The latter, characterized by the high penetration power in most engineering alloys, allows for the use of diffraction angle close to 90° enabling a near cubic sampling volume to be specified. However, the complex microstructures of columnar growth with inherent crystallographic texture typically produced during PBF-LB/M of metallics present significant challenges to the assumptions typically required for time efficient determination of residual stress. These challenges include the selection of an appropriate set of diffraction elastic constants and a representative strain-free reference for the material of interest. In this presentation advancements in the field of diffraction-based residual stress analysis of L-PBF Inconel 718 will be presented. The choice of an appropriate set of diffraction-elastic constants depending on the underlying microstructure will be described.
Das zyklische plastische Verformungsverhalten von additiv gefertigtem Edelstahl AISI 316L wurde in dehnungsgeregelten Kurzzeitfestigkeitsversuchen (LCF-Versuchen) untersucht. Dabei wurden zwei Wärmebehandlungszustände betrachtet: Beim ersten Zustand war die fertigungsbedingte zelluläre Struktur vorhanden, während sie durch die zweite Wärmebehandlung aufgelöst wurde. Untersuchungen im Transmissions-Elektronen-Mikroskop (TEM) zeigten, dass die zyklische Verformung die Zellstruktur lokal zerstörte und Gleitbänder entstanden, was die Entfestigung in diesem Fall erklärt. Für Material ohne Zellstrukturen resultierten nach zyklischer Verformung ähnliche Versetzungsstrukturen wie in konventionell gefertigtem (warmgewalzten) Material.
Additive manufacturing methods such as laser powder bed fusion (LPBF) allow geometrically complex parts to be manufactured within a single step. However, as an aftereffect of the localized heat input, the rapid cooling rates are the origin of the large residual stress (RS) retained in as-manufactured parts. With a view on the microstructure, the rapid directional cooling leads to a cellular solidification mode which is accompanied by columnar grown grains possessing crystallographic texture. The solidification conditions can be controlled by the processing parameters and the scanning strategy. Thus, the process allows one to tailor the microstructure and the texture to the specific needs. Yet, such microstructures are not only the origin of the mechanical anisotropy but also pose metrological challenges for the diffraction-based RS determination. In that context the micromechanical elastic anisotropy plays an important role: it translates the measured microscopic strain to macroscopic stress. Therefore, it is of uttermost importance to understand the influence of the hierarchical microstructures and the texture on the elastic anisotropy of LPBF manufactured materials.
This study reveals the influence of the build orientation and the texture on the micro-mechanical anisotropy of as-built Inconel 718. Through variations of the build orientation and the scanning strategy, we manufactured specimens possessing [001]/[011]-, [001]-, and [011]/[111]-type textures. The resulting microstructures lead to differences in the macroscopic mechanical properties. Even further, tensile in-situ loading experiments during neutron diffraction measurements along the different texture components revealed differences in the microstrain response of multiple crystal lattice planes. In particular, the load partitioning and the residual strain accumulation among the [011]/[111] textured specimen displayed distinct differences measured up to a macroscopic strain of 10 %. However, the behavior of the specimens possessing [001]/[011]-and [001]-type texture was only minorly affected. The consequences on the metrology of RS analysis by diffraction-based methods are discussed.
Komponenten von Fahrrädern werden im Betrieb vorwiegend schwingend beansprucht. Typische Werkstoffe sind Stahl, Aluminiumlegierungen, Messing, CFK und thermoplastische Kunststoffe. Da es sich, unabhängig von der Preiskategorie, um konstruktiven Leichtbau handelt, werden einige Bauteile betriebsfest mehr oder weniger weit oberhalb der Dauerfestigkeit ausgelegt. Die im normalen Betrieb auftretenden Schäden sind daher weit überwiegend Schwingbrüche. Andere Schadensmechanismen wie z.B. Korrosion spielen quantitativ eine untergeordnete Rolle. Schwingbrüche treten nach einer Periode unbemerkten Risswachstums oft ohne Vorwarnung und ohne makroskopische Verformung auf. Im Falle von sicherheitsrelevanten Komponenten wie Rahmen, Gabeln, Lenkern, Sattelstützen, Kurbelarmen oder Pedalen kann dies zu erheblichen Personenschäden führen, die den Wert des ursächlichen Bauteilschadens weit überschreiten.
Über einen langjährigen Zeitraum wurden gebrochene Komponenten aus dem Alltag und aus Gerichtsverfahren analysiert. Das Hauptaugenmerk lag hierbei auf der fraktographischen Analyse, teilweise wurden die zu Grunde liegenden Schadensursachen ermittelt. Einflussfaktoren sind beispielsweise konstruktive Kerben an ungünstigen Stellen, aber auch Werkstoffwahl und Fertigungsqualität spielen eine Rolle. In den meisten Fällen wurde jedoch die konstruktive Lebensdauer überschritten. Diese wird praktisch nie mitgeteilt, und eine wiederkehrende Prüfung sicherheitsrelevanter Bauteile findet nicht statt.
Im Sinne der Vermeidung von Schäden und Unfällen könnte darauf hingewirkt werden, für sicherheitsrelevante Komponenten Lebensdauern besser abzuschätzen und von der Laufleistung abhängige Sichtprüfungen zu empfehlen.
The round robin test investigated the reliability users can expect for AlSi10Mg additive manufactured specimens by laser powder bed fusion through examining powder quality, process parameter, microstructure defects, strength and fatigue. Besides for one outlier, expected static material properties could be found. Optical microstructure inspection was beneficial to determine true porosity and porosity types to explain the occurring scatter in properties. Fractographic analyses reveal that the fatigue crack propagation starts at the rough as-built surface for all specimens. Statistical analysis of the scatter in fatigue using statistical derived safety factors concludes that at a stress of 36.87 MPa the fatigue limit of 107 cycles could be reached for all specimen with a survival probability of 99.999 %.
The presentation shows the results of high cycle fatigue (HCF) tests from the aluminium alloy EN AW-2618A. This study investigates the mean stress influence in the T61 condition and the effect of overaging. For this purpose, axial HCF tests were carried out at room temperature and different stress ratios (R=-1, R=0.1) as well as with overaged conditions (T61+10h@230°C, T61+1000h@230°C). After completion of the tests, the fracture surfaces were examined to study crack initiation.
Entwicklung der Mikrostruktur der mechanischen Eigenschaften und der Eigenspannungen in L-PBF 316L
(2022)
Die additive Fertigung (AM) metallischer Werkstoffe mittels Laser Powder Bed Fusion (L-PBF) ermöglicht einzigartige hierarchische Mikrostrukturen, die zu Verbesserungen bestimmter mechanischer Eigenschaften gegenüber konventionell hergestellten Varianten derselben Legierung führen können. Allerdings ist das L-PBF-Verfahren häufig durch das Vorhandensein hoher Eigenspannungen gekennzeichnet, die es zu verstehen und zu mindern gilt. Daher ist das Verständnis der Mikrostrukturen, der Eigenspannungen und der daraus resultierenden mechanischen Eigenschaften entscheidend für eine breite Akzeptanz bei sicherheitskritischen Anwendungen. Die BAM hat ein multidisziplinäres Forschungsprogramm gestartet, um diese Aspekte bei LPBF 316L zu untersuchen. Der vorliegende Beitrag stellt einige der wichtigsten Ergebnisse vor: der Einfluss von Prozessparametern auf die Mikrostruktur, der Einfluss von Mikrostruktur und Textur auf die Festigkeit, Kriechverhalten und Schädigung und die Stabilität von Eigenspannungen und Mikrostruktur unter Wärmebehandlungsbedingungen.
The manufacturability of metallic alloys using laser-based additive manufacturing methods such as laser powder bed fusion has substantially improved within the last decade. However, local melting and solidification cause hierarchically structured and crystallographically textured microstructures possessing large residual stress. Such microstructures are not only the origin of mechanical anisotropy but also pose metrological challenges for the diffraction-based residual stress determination. Here we demonstrate the influence of the build orientation and the texture on the microstructure and consequently the mechanical anisotropy of as-built Inconel 718. For this purpose, we manufactured specimens with [001]/[011]-, [001]- and [011]/[111]-type textures along their loading direction. In addition to changes in the Young’s moduli, the differences in the crystallographic textures result in variations of the yield and ultimate tensile strengths. With this in mind, we studied the anisotropy on the micromechanical scale by subjecting the specimens to tensile loads along the different texture directions during in situ neutron diffraction experiments. In this context, the response of multiple lattice planes up to a tensile strain of 10% displayed differences in the load partitioning and the residual strain accumulation for the specimen with [011]/[111]-type texture. However, the relative behavior of the specimens possessing an [001]/[011]- and [001]-type texture remained qualitatively similar. The consequences on the metrology of residual stress determination methods are discussed.
Laser powder-based directed energy deposition (DED-L) is a technology that offers the possibility for 3D material deposition over hundreds of layers and has thus the potential for application in additive manufacturing (AM). However, to achieve broad industrial application as AM technology, more data and knowledge about the fabricated materials regarding the achieved properties and their relationship to the manufacturing process and the resulting microstructure is still needed. In this work, we present data regarding the low-cycle fatigue (LCF) behavior of Ti-6Al-4V. The material was fabricated using an optimized DED-L process. It features a low defect population and excellent tensile properties. To assess its LCF behavior two conventionally manufactured variants of the same alloy featuring different microstructures were additionally tested. The strain-controlled LCF tests were carried out in fully reversed mode with 0.3 % to 1.0 % axial strain amplitude from room temperature up to 400°C. The LCF behavior and failure mechanisms are described. For characterization, optical microscopy (OM), scanning electron microscopy (SEM), and micro-computed tomography (µCT) were used. The low defect population allows for a better understanding of the intrinsic material’s properties and enables a fairer comparison against the conventional variants. The fatigue lifetimes of the DED-L material are nearly independent of the test temperature. At elevated test temperatures, they are similar or higher than the lifetimes of the conventional counterparts. At room temperature, they are only surpassed by the lifetimes of one of them. The principal failure mechanism involves multiple crack initiation sites.
Metal Additive Manufacturing (AM) technologies such as Laser Powder Bed Fusion (LPBF) are characterized by layer wise construction, which enable advancements of component design, with associated potential gains in performance and efficiency. However, high magnitude residual stresses (RS) are often a product of the rapid thermal cycles typical of the layerwise process. Therefore, a deep understanding of the formation of RS, the influence of process parameters on their magnitude and the impact on mechanical performance is crucial for widespread application. The experimental characterisation of these RS is essential for safety related engineering application and supports the development of reliable numerical models. Diffraction-based methods for RS analysis using neutrons and high energy X-rays enable non-destructive spatially resolved characterisation of both surface and bulk residual stresses in complex components. This presentation will provide an overview of recent research by the BAM at large scale facilities for the characterization of residual stresses in LPBF metallic alloys as a function of process parameters. In addition, the challenges posed by the textured and hierarchical microstructures of LPBF materials on diffraction-based RS analysis in AM materials will be discussed. This will include the question of the d0 reference lattice spacing and the appropriate choice of the diffraction elastic constants (DECs) to calculate the level of RS in LPBF manufactured alloys.
Characterization of Ti-6Al-4V fabricated by multilayer laser powder-based directed energy deposition
(2022)
Laser powder-based directed energy deposition (DED-L) is increasingly being used in additive manufacturing (AM). As AM technology, DED-L must consider specific challenges. It must achieve uniform volume growth over hundreds of layers and avoid heat buildup of the deposited material. Herein, Ti–6Al–4V is fabricated using an approach that addresses these challenges and is relevant in terms of transferability to DED–L applications in AM. The assessment of the obtained properties and the discussion of their relationship to the process conditions and resulting microstructure are presented. The quality of the manufacturing process is proven in terms of the reproducibility of properties between individual blanks and with respect to the building height. The characterization demonstrates that excellent mechanical properties are achieved at room temperature and at 400 °C.
Creep and creep damage behavior of stainless steel 316L manufactured by laser powder bed fusion
(2022)
This study presents a thorough characterization of the creep properties of austenitic stainless steel 316L produced by laser powder bed fusion (LPBF 316L) contributing to the sparse available data to date. Experimental results (mechanical tests, microscopy, X-ray computed tomography) concerning the creep deformation and damage mechanisms are presented and discussed. The tested LPBF material exhibits a low defect population, which allows for the isolation and improved understanding of the effect of other typical aspects of an LPBF microstructure on the creep behavior. As a benchmark to assess the material properties of the LPBF 316L, a conventionally manufactured variant of 316L was also tested. To characterize the creep properties, hot tensile tests and constant force creep tests at 600 °C and 650 °C are performed. The creep stress exponents of the LPBF material are smaller than that of the conventional variant. The primary and secondary creep stages and the times to rupture of the LPBF material are shorter than the hot rolled 316L. Overall the creep damage is more extensive in the LPBF material. The creep damage of the LPBF material is overall mainly intergranular. It is presumably caused and accelerated by both the appearance of precipitates at the grain boundaries and the unfavorable orientation of the grain boundaries. Neither the melt pool boundaries nor entrapped gas pores show a significant influence on the creep damage mechanism.
High- and medium-entropy alloys (HEAs) are a quite new class of materials. They have a high potential for applications from low to high temperatures due to the excellent combination of their structural properties.
Concerning their application as components; processing properties, such as machinability, have hardly been investigated so far. Hence, machinability analyses with a focus on the influence of the milling process and its basic parameters (cutting speed, feed per cutting edge) on the resulting surface integrity of specimens from an equiatomic high- (CoCrFeMnNi) and a medium- (CoCrNi) entropy alloy have been carried out. A highly innovative milling process with ultrasonic assistance (USAM) was compared to conventional milling processes.
Recent studies have shown that USAM has a high potential to significantly reduce the mechanical load on the tool and workpiece surface during milling. In this study, the basic machining and ultrasonic parameters were systematically varied. After machining, the surface integrity of the alloys was analyzed in terms of topography, defects, subsurface damage, and residual stresses. It was observed that USAM reduces the cutting forces and increases the surface integrity in terms of lower tensile residual stresses and defect density near the surfaces for the CoCrFeMnNi alloy. It was shown that the cutting forces and the metallurgical influence in the sub surface region are reduced by increasing the cutting speed and reducing the feed rate per cutting edge. With the CoCrNi alloy, the tool revealed severe wear. As a result, for this alloy no influence of the parameters on the machinability could be determined.