Filtern
Dokumenttyp
Sprache
- Englisch (2)
Schlagworte
- Inclusions (2) (entfernen)
Organisationseinheit der BAM
On July 9, 2008 a high speed train derailed in Cologne main Station, Germany at a low speed because an axle was broken. Fortunately, the derailment happened at a low speed so that nobody was injured. The reason for the broken axle was investigated and it turned out that most likely large inclusions located shortly undemeath the surface in a T-transition were the origin of the final crack. Basing on that result, a systematic investigation on existing safety assessments of railway axles was performed. This results in an analysis of the production process of axles and in a critical review of existing of existing assessments. Improvements and future developments are outlined.
The paper provides an application of the IBESS approach to the investigation of the influence of various parameters of the global and local weld geometry as well as material defects on the fatigue strength of weldments. For this purpose, the global weld parameters, such as the weld toe radius, the flank angle, the excess weld metal, local secondary notches (in the present study as a measure of surface imperfections) and inclusions sizes have been determined as statistical distributions for different joint types and geometries and two steels of different strengths. The results are in line with literature data and reveal the potential of the theoretical approach to predict the correct trends. The combination with an advanced weld quality system has been demonstrated to be possible.