Filtern
Erscheinungsjahr
Dokumenttyp
- Zeitschriftenartikel (85) (entfernen)
Schlagworte
- Microplastics (11)
- Microplastic (8)
- Flame retardance (7)
- Pyrolysis (7)
- Fire retardancy (6)
- Flame retardancy (6)
- Degradation (5)
- TED-GC/MS (5)
- Cone calorimeter (4)
- Mikroplastik (4)
Organisationseinheit der BAM
- 6 Materialchemie (17)
- 6.6 Physik und chemische Analytik der Polymere (17)
- 1 Analytische Chemie; Referenzmaterialien (7)
- 1.4 Prozessanalytik (4)
- 1.7 Organische Spuren- und Lebensmittelanalytik (4)
- 5 Werkstofftechnik (3)
- 5.3 Polymere Verbundwerkstoffe (3)
- 4 Material und Umwelt (1)
- 4.3 Schadstofftransfer und Umwelttechnologien (1)
- 6.1 Oberflächen- und Dünnschichtanalyse (1)
Paper des Monats
- ja (1)
A sedimented freshwater suspended organic matter fortified with particles of polyethylene (PE), polypropylene (PP), polystyrene (PS), and polyethylene terephthalate (PET) was employed in an interlaboratory comparison of thermoanalytical methods for microplastics identification and quantification. Three laboratories performed pyrolysis gas chromatography-mass spectrometry (Py-GC-MS), three others provided results using thermal extraction desorption followed by gas chromatography coupled to mass spectrometry (TED-GC-MS). One participant performed thermogravimetry-infrared spectroscopy (TGA-FTIR) and two participants used thermogravimetry coupled to mass spectrometry (TGA-MS). Further participants used differential scanning microscopy (DSC), a procedure based on micro combustion calorimetry (MCC) and a procedure based on elemental analysis.
Each participant employed a different combination of sample treatment, calibration and instrumental Settings for polymer identification and quantification. Though there is obviously room for improvements regarding the between-laboratory reproducibility and the harmonization of procedures it was seen that the participants Performing Py-GC-MS, TED-GC-MS, and TGA-FTIR were able to correctly identify all polymers and to report reasonable quantification results in the investigated concentration range (PE: 20.0 μg/mg, PP: 5.70 μg/mg; PS: 2.20 μg/mg, PET: 18.0 μg/mg). Although for the other methods limitations exists regarding the detection of specific polymers, they showed potential as alternative approaches for polymer quantification in solid environmental matrices.
Microplastic particles are currently detected in almost all environmental compartments. The results of detection vary widely, as a multitude of very different methods are used with very different requirements for analytical validity.
In this work four thermoanalytical methods are compared and their advantages and limitations are discussed. One of them is thermal extraction-desorption gas chromatography mass spectrometry (TED-GC/MS), an analysis method for microplastic detection that has become established in recent years. In addition, thermogravimetric analysis coupled with Fourier-transform infrared spectroscopy (TGA-FTIR) and mass spectrometry (TGA-MS) were applied, two methods that are less common in this field but are still used in other research areas. Finally, microscale combustion calorimeter (MCC) was applied, a method not yet used for microplastic detection.
The presented results are taken from a recently published interlaboratory comparison test by Becker et al. (2020). Here a reference material consisting of suspended matter and specified added polymer masses was examined, and only the results of the recoveries were presented. In the present paper, however, the results for the individual polymers are discussed in detail and individual perspectives for all instruments are shown.
It was found that TED-GC/MS is the most suitable method for samples with unknown matrix and unknown, variable kinds and contents of microplastic. TGA-FTIR is a robust method for samples with known matrix and with defined kinds of microplastic. TGA-MS may offer a solution for the detection of PVC particles in the future. MCC can be used as a very fast and simple screening method for the identification of a potential microplastic load of standard polymers in unknown samples.
The TED-GC-MS analysis is a two-step method. A sample is first decomposed in a thermogravimetric analyzer (TGA) and the gaseous decomposition products are then trapped on a solid-phase adsorber. Subsequently, the solid-phase adsorber is analyzed with thermal desorption gas chromatography mass spectrometry (TDU-GC-MS). This method is ideally suited for the analysis of polymers and their degradation processes. Here, a new entirely automated System is introduced which enables high sample throughput and reproducible automated fractioned collection of decomposition products. Strengths and limitations of the system configuration are elaborated via three examples focused on practical challenges in materials analysis and identification: i) separate analysis of the components of a wood-plastic-composite material, ii) quantitative determination of weight concentration of the constituents of a polymer blend and iii) quantitative analysis of model samples of microplastics in suspended particulate matter.
In this study, the thermal decomposition of 1,3,5-tris-(2,3-dibromopropyl)-1,3,5-triazine-2,4,6-trione (TDBPTAZTO) and 2,4,6-tris-(2,4,6-tribromo-phenoxy)-1,3,5-triazine (TTBP-TAZ) were investigated for the first time by thermogravimetric analysis. Both compounds were thermal degraded between 225 and 350 °C (TDBP-TAZTO) as well as 300 and 400 °C (TTBP-TAZ).
As a result, mass loss (%) of 98.5% for TTBP-TAZ and 95.4% for TDBP-TAZTO at 600 °C under N2 were observed. The major pyrolytic degradation products of TTBP-TAZ were formed in a single step and identified by FTIR analysis as 2,4,6-tribromophenol and further bromine-substituted aromatic compounds. In comparison, TDBP-TAZTO was pyrolytic degraded in two steps, whereby on the first step the release of hydrogen Bromide and 1,3,5-triallyl-1,3,5-triazine-2,4,6-trione could be detected. In the second minor step, isocyanic acid could be additionally identified.
Subsequently, the obtained products of the TGA-FTIR measurements were used for a targeted search for mass fragments in mass spectrometry measurements. For TTBP-TAZ, only the degradation product 1,3,5-tribromobenzene could be detected by MS/MS analyzes. No comparable thermal degradation products, except hydrogen bromide, were observed in the MS/MS spectra of TDBP-TAZTO. Therefore, the search of further mass fragments was not possible compared to the findings of the TGA-FTIR measurements.
In this work, a novel boehmite (BA)-embedded organic/inorganic nanocomposite coating based on cycloaliphatic epoxy oligosiloxane (CEOS) resin was fabricated applying UV-induced cationic polymerization. The main changes of the material behavior caused by the nanofiller were investigated with regard to its photocuring kinetics, thermal stability, and glass transition. The role of the particle surface was of particular interest, thus, unmodified nanoparticles (HP14) and particles modified with p-toluenesulfonic acid (OS1) were incorporated into a CEOS matrix in the concentration range of 1–10 wt.%. Resulting nanocomposites exhibited improved thermal properties, with the glass transition temperature (Tg) being shifted from 30 °C for unfilled CEOS to 54 °C (2 wt.% HP14) and 73 °C (2 wt.% OS1) for filled CEOS. Additionally, TGA analysis showed increased thermal stability of samples filled with nanoparticles. An attractive interaction between boehmite and CEOS matrix influenced the curing. Real-time infrared spectroscopy (RT-IR) experiments demonstrated that the epoxide conversion rate of nanocomposites was slightly increased compared to neat resin. The beneficial role of the BA can be explained by the participation of hydroxyl groups at the particle surface in photopolymerization processes and by the complementary contribution of p-toluenesulfonic acid surface modifier and water molecules introduced into the system with nanoparticles.
Reliable simulation of polymers on an atomistic length scale requires a realistic representation of the cured material. A molecular modelling method for the curing of epoxy systems is presented, which is developed with respect to efficiency while maintaining a well equilibrated system. The main criterion for bond formation is the distance between reactive groups and no specific reaction probability is prescribed. The molecular modelling is studied for three different mixing ratios with respect to the curing evolution of reactive Groups and the final curing stage. For the first time, the evolution of reactive groups during the curing process predicted by the molecular modelling is validated with near-infrared spectroscopy data, showing a good agreement between simulation results and experimental measurements. With the proposed method, deeper insights into the curing mechanism of epoxy systems can be gained and it allows us to provide reliable input data for molecular Dynamics simulations of material properties.
In this study, a method for the determination of tire and road wear particle (TRWP) contents in particulate samples from road Environment was developed. Zn was identified as the most suitable elemental marker for TRWP, due to its high concentration in tire tread and the possibility of separation from other Zn sources. The mean concentration of 21 tire samples was 8.7 ± 2.0 mg Zn/g. Before quantification in samples from road environment, TRWP were separated from the particulate matrix by density separation. Method development was conducted using shredded tread particles (TP) as a surrogate for TRWP.
Recovery of TP from spiked sediment was 95 ± 17% in a concentration range of 2 - 200 mg TP/g. TP determination was not affected by other Zn containing solids or spiked Zn-salts. By adjusting the density of the separation solution to 1.9 g/cm3, more than 90% of total TRWP were separated from the sample matrix. TRWP concentrations in particulate matter collected in two road runoff treatment Systems ranged from 0.38 to 150 mg TRWP/g. Differences in quantified TRWP contents of the two Systems indicate changes in particle dynamics due to ageing and aggregation processes. The developed method allows TRWP determination in road runoff and in environments that are influenced by road traffic. The validated separation procedure can also be applied for TRWP characterization in future studies.
A harmonization of sampling, sample preparation and detection is pivotal in order to obtain comparable data on microplastics (MP) in the environment. This paper develops and proposes a suitable sampling concept for waterbodies that considers different plastic specific properties and influencing factors in the environment.
Both artificial water including defined MP fractions and the discharge of a wastewater treatment plant were used to verify the derived sampling procedure, sample preparation and the subsequent analysis of MP using thermal extraction-desorption gas chromatography - mass spectrometry (TED-GC-MS).
A major finding of this paper is that an application of various particle size classes greatly improves the practical handling of the sampling equipment. Size classes also enable the TED-GC-MS to provide any data on the MP size distribution, a substantial sampling property affecting both the necessary sampling volume and the optimal sampling depth.
In the artificial water with defined MP fractions, the recovery rates ranged from 80 to 110%, depending on the different MP types and MP size classes. In the treated wastewater, we found both Polyethylene and polystyrene in different size classes and quantities.
Advanced wastewater treatment with powdered activated carbon (PAC) leads to a spread of PAC into different purification stages of wastewater treatment plants (WWTP) due to recirculation and filter back-wash. Currently, no methods for quantification of PAC in activated sludge are available. In this study, PAC containing activated sludge from four WWTP were examined by two-step thermogravimetric analysis (TGA) with heating up to 600°C in N2 and subsequently in synthetic air. Direct quantification of PAC according to temperature specific weight losses was possible for one WWTP. Quantification by combining specific mass losses was found to be an alternative direct method, with a detection limit of 1.2% PAC in dry sample mass.
Additionally, evolved gas analysis (EGA) by infrared-spectroscopy (FTIR) during TGA revealed interaction mechanisms between PAC and activated sludge. Aliphatic compounds from activated sludge were identified as major substances influenced by PAC. In derivative thermogravimetry (DTG), a typical double peak at approximately 300°C was found to be related to carbonylic species with increased evolution of acetic acid in aged activated sludge. TGA and EGA are promising tools to understand, control and optimise the application of PAC in advanced wastewater treatment.
Analysis of microplastic particles (MP) in environmental samples needs sophisticated techniques and is time intensive due to sample preparation and detection. An alternative to the most common (micro ) spectroscopic techniques, FTIR or Raman spectroscopy, are the thermoanalytical methods, where specific decomposition products can be analyzed as marker compounds for different kind of plastics types and mass contents. Thermal extraction desorption gas chromatography mass spectrometry (TED-GC-MS) allows the fast identification and quantification of MP in environmental samples without sample preparation. Whereas up to now only the analysis of thermoplastic polymers was realized, this is the first time that even the analysis of tire wear (TW) content in environmental samples is possible. Various marker compounds for TW were identified. They include characteristic decomposition products of elastomers, antioxidants and vulcanization agents. Advantages and drawbacks of these marker substances were evaluated. Environmental samples from street run off were exemplarily investigated and presented.
The occurrence of small particles consisting of organic polymers, so-called microplastic (MP), in aquatic Environments attracts increasing interest in both public and science. Recent sampling campaigns in surface Waters revealed substantial numbers of particles in the size range from a few micrometers to a few millimeters. In order to validate sample preparation, identification and quantification and to investigate the behavior of MP particles and potential toxic effects on organisms, defined MP model particles are needed. Many studies use spherical compounds that probably behave differently compared to irregularly shaped MP found in environmental samples.
However, preparation and handling of MP particles are challenging tasks and have been systematically investigated in the present study. Polystyrene (PS) as a commonly found polymer with a density slightly above that of water was selected as polymer type for milling and fractionation studies. A cryogenic ball mill proved to be practical and effective to produce particles in the size range from 1 to 200 μm. The yield of small particles increased with increasing pre-cooling and milling durations. Depending on the concentration and the size, PS particles do not completely disperse in water and particles partly creep vertically up along glass walls. Stabilized MP suspensions without use of surfactants that might harm organisms are needed for toxicological studies. The stabilization of PS particle suspensions with ozone treatment reduced the wall effect and increased the number of dispersed PS particles but increased the dissolved organic carbon concentration and changed the size Distribution of the particles.
Microplastics are increasingly entering marine, limnic and terrestrial ecosystems worldwide, where they sorb hydrophobic organic contaminants. Here, the sorption behavior of the fuel-related water contaminants benzene, toluene, ethyl benzene and xylene (BTEX) and four tertiary butyl ethers to virgin and via UV radiation aged polypropylene (PP) and polystyrene (PS) pellets was investigated. Changes in material properties due to aging were recorded using appropriate polymer characterization methods, such as differential scanning calorimetry, Fourier transform infrared spectroscopy, gel permeation chromatography, X-ray photoelectron spectroscopy, and microscopy.
Pellets were exposed to water containing BTEX and the ethers at 130-190 mg/L for up to two weeks.
Aqueous sorbate concentrations were determined by headspace gas chromatography. Sorption to the polymers was correlated with the sorbate's Kow and was significant for BTEX and marginal for the ethers.
Due to substantially lower glass transition temperatures, PP showed higher sorption than PS. Aging had no effect on the sorption behavior of PP. PS sorbed less BTEX after aging due to an oxidized surface layer.
The increasing pollution of terrestrial and aquatic ecosystems with plastic debris leads to the accumulation of microscopic plastic particles of still unknown amount. To monitor the degree of contamination analytical methods are urgently needed, which help to quantify microplastics (MP). Currently, time-costly purified materials enriched on filters are investigated both by micro-infrared spectroscopy and/or micro-Raman. Although yielding precise results, these techniques are time consuming, and are restricted to the analysis of a small part of the sample in the order of few micrograms. To overcome these problems, here we tested a macroscopic dimensioned NIR process-spectroscopic method in combination with chemometrics. For calibration, artificial MP/soil mixtures containing defined ratios of polyethylene, polyethylene terephthalate, polypropylene, and polystyrene with diameters < 125 µm were prepared and measured by a process FT-NIR spectrometer equipped with a fiber optic reflection probe. The resulting spectra were processed by chemometric models including support vector machine regression (SVR), and partial least squares discriminant analysis (PLS-DA). Validation of models by MP mixtures, MP-free soils and real-world samples, e.g. and fermenter residue, suggest a reliable detection and a possible classification of MP at levels above 0.5 to 1.0 mass% depending on the polymer. The benefit of the combined NIRS chemometric approach lies in the rapid assessment whether soil contains MP, without any chemical pre-treatment. The method can be used with larger sample volumes and even allows for an online prediction and thus meets the demand of a high-throughput method.
Non-isothermal heating rate kinetics was applied to two epoxy resin systems. In situ near-infrared (NIR) measurements were taken with a heatable NIR cell which allowed the cure to be monitored by characteristic absorption bands. An autocatalyzed reaction of the nth order was shown to describe the epoxy conversion curves. Differential Scanning Calorimetry (DSC) was used as a complementary method. The kinetic models developed by both NIR and DSC are in good accordance with experimental epoxy conversion in the in situ NIR setup for single and multiple cure temperature ramps.
A linear calibration curve of the characteristic absorption bands of epoxy normalized to aromatic vibrations was introduced. The curing degree of structural epoxies that were cured according to an industrial temperature cure profile was determined by NIR using the calibration curve. The epoxy conversions of the structural components showed good agreement with the experimental in situ NIR. Several degrees of cure for structural specimens were evaluated by NIR and residual reaction enthalpy by DSC. We present the non-destructive NIR spectroscopy as an alternative to determine fast and non-destructive epoxy conversion, particularly suitable for high degrees of cure on structural components.
In order to determine the relevance of microplastic particles in various environmental media, comprehensive investigations are needed. However, no analytical method exists for fast identification and quantification. At present, optical spectroscopy methods like IR and RAMAN imaging are used. Due to their time consuming procedures and uncertain extrapolation, reliable monitoring is difficult. For analyzing polymers Py-GC-MS is a standard method. However, due to a limited sample amount of about 0.5 mg it is not suited for analysis of complex sample mixtures like environmental samples. Therefore, we developed a new thermoanalytical method as a first step for identifying microplastics in environmental samples. A sample amount of about 20 mg, which assures the homogeneity of the sample, is subjected to complete thermal decomposition. The specific degradation products of the respective polymer are adsorbed on a solid-Phase adsorber and subsequently analyzed by thermal Desorption gas chromatography mass spectrometry. For certain identification, the specific degradation products for the respective polymer were selected first. Afterwards real environmental samples from the aquatic (three different rivers) and the terrestrial (bio gas plant) systems were screened for microplastics. Mainly polypropylene (PP), polyethylene (PE) and polystyrene (PS) were identified for the samples from the bio gas plant and PE and PS from the rivers. However, this was only the first step and quantification measurements will follow.
A first pilot study on the sorption of environmental pollutants on various microplastic materials
(2017)
With the drastic increase in plastic production, the input of plastic particles into the environment has become a recognised problem.
Xenobiotics are able to sorb to polymer materials, and this process is further enhanced where they Encounter microplastics (plastic fragments <5 mm). In this work we studied the sorption of metformin, a type-2 diabetes drug, and difenoconazole, a fungicide, onto the virgin polymer materials polyamide (PA), polypropylene (PP), and polystyrene (PS). Additionally, PP was cryo-milled and PA was treated with acid to investigate the influence of an increase in surface area and chemical modification. The material properties were also studied by dynamic scanning calorimetry (DSC), gel permeation chromatography (GPC) and Fourier transform infrared spectroscopy (FTIR). Sorption experiments were performed on the basis of a full factorial design examining the effect of agitation, pH value, and salinity. Experimental results showed that difenoconazole sorbs readily to all microplastics, whereas the more polar analyte metformin did not show any affinity to the materials used. For difenoconazole the governing factor in all cases is agitation, while both pH and salinity exhibited only a slight influence. The modification of polymers leads to enhanced sorption, indicating that an increase in surface area (cryo-milled PP) or inner volume (acid-treated PA) strongly favours adsorption. Moreover, long-term experiments demonstrated that the time until equilibrium is reached depends strongly on the particle size.
Avoiding aerial microfibre contamination of environmental samples is essential for reliable analyses when it comes to the detection of ubiquitous microplastics. Almost all laboratories have contamination problems which are largely unavoidable without investments in clean-air devices. Therefore, our study supplies an approach to assess background microfibre contamination of samples in the laboratory under particle-free air conditions. We tested aerial contamination of samples indoor, in a mobile laboratory, within a laboratory fume hood and on a clean bench with particles filtration during the examining process of a fish. The used clean bench reduced aerial microfibre contamination in our laboratory by 96.5%. This highlights the value of suitable clean-air devices for valid microplastic pollution data. Our results indicate, that pollution levels by microfibres have been overestimated and actual pollution levels may be many times lower. Accordingly, such clean-air devices are recommended for microplastic laboratory applications in future research work to significantly lower error rate
Discoloration Effects of High-Dose gamma-Irradiation and Long-Term Thermal Aging of (U) HMW-PE
(2017)
Two polyethylene types with ultra-high (UHMWPE) and high molecular weight (HMW-PE) used as neutron radiation shielding materials in casks for radioactive waste were irradiated with doses up to 600 kGy using a 60Co gammasource. Subsequently, thermal aging at 125∘C was applied for up to one year. Degradation effects in the materials were characterized using colorimetry, UV-Visspectroscopy, IR spectroscopy, and DSC. Both materials exhibited a yellowing upon irradiation.The discoloration of UHMW-PE disappeared again after thermal aging.Therefore, the yellowing is assumed to originate fromannealable color centers in the formof free radicals that are trapped in the crystalline regions of the polymer and recombine at elevated temperatures. For the antioxidantcontaining HMWPE, yellowing was observed after both irradiation and thermal aging. The color change was correlated mainly to decomposition products of the antioxidant in addition to trapped radicals as in UHMW-PE. Additionally, black spots appeared after thermal aging of HMW-PE.
n order to determine the relevance of microplastic particles in various environmental media, comprehensive investigations are needed. However, no analytical method exists for fast identification and quantification. At present, optical spectroscopy methods like IR and RAMAN imaging are used. Due to their time consuming procedures and uncertain extrapolation, reliable monitoring is difficult. For analyzing polymers Py-GC-MS is a standard method. However, due to a limited sample amount of about 0.5 mg it is not suited for analysis of complex sample mixtures like environmental samples. Therefore, we developed a new thermoanalytical method as a first step for identifying microplastics in environmental samples. A sample amount of about 20 mg, which assures the homogeneity of the sample, is subjected to complete thermal decomposition. The specific degradation products of the respective polymer are adsorbed on a solid-phase adsorber and subsequently analyzed by thermal desorption gas chromatography mass spectrometry. For certain identification, the specific degradation products for the respective polymer were selected first. Afterwards real environmental samples from the aquatic (three different rivers) and the terrestrial (bio gas plant) systems were screened for microplastics. Mainly polypropylene (PP), polyethylene (PE) and polystyrene (PS) were identified for the samples from the bio gas plant and PE and PS from the rivers. However, this was only the first step and quantification measurements will follow.
In recent years, an increasing trend towards investigating and monitoring the contamination of the environment by microplastics (MP) (plastic pieces < 5 mm) has been observed worldwide. Nonetheless, a reliable methodology that would facilitate and automate the monitoring of MP is still lacking. With the goal of selecting practical and standardized methods, and considering the challenges in microplastics detection, we present here a critical evaluation of two vibrational spectroscopies, Raman and Fourier transform infrared (FTIR) spectroscopy, and two extraction methods: thermal extraction desorption gas chromatography mass spectrometry (TED-GC-MS) and liquid extraction with subsequent size exclusion chromatography (SEC) using a soil with known contents of PE, PP, PS and PET as reference material. The obtained results were compared in terms of measurement time, technique handling, detection limits and requirements for sample preparation. The results showed that in designing and selecting the right methodology, the scientific question that determines what needs to be understood is significant, and should be considered carefully prior to analysis. Depending on whether the object of interest is quantification of the MP particles in the sample, or merely a quick estimate of sample contamination with plastics, the appropriate method must be selected. To obtain overall information about MP in environmental samples, the combination of several parallel approaches should be considered.
Central venous port devices made of two different polymeric materials, thermoplastic polyurethane (TPU)and silicone rubber (SiR), were compared due their material properties. Both naïve catheters as well as catheters after removal from patients were investigated. In lab experiments the influence of various chemo-therapeutic solutions on material properties was investigated, where as the samples after removal were compared according to the implanted time inpatient. The macroscopic,mechanical performance was assessed with dynamic, specially adapted tests for elasticity. The degradation status of the materials was determined with common tools of polymer characterisation, such as infrared spectroscopy, molecular weight measurements and various methods of thermal analysis. The surface morphology was an alysed using scanning electron microscopy. A correlation between material properties and clinical performance was proposed. The surface morphology and chemical composition of the polyurethane catheter materials can potentially result in increased susceptibility of the catheter to bloodstream infections and thrombotic complications. The higher mechanic failure,especially with increasing implantation time of the silicone catheters is related to the lower mechanical performance compared to the polyurethane material as well as loss of barium sulphate filler particles near the surface of the catheter. This results in preformed microscopic notches, which act as predetermined sites of fracture.
Due to the adsorption of biomolecules, the control of the biodistribution of nanoparticles is still one of the major challenges of nanomedicine. Poly(2-ethyl-2-oxazoline) (PEtOx) for surface modification of nanoparticles is applied and both protein adsorption and cellular uptake of PEtOxylated nanoparticles versus nanoparticles coated with poly(ethylene glycol) (PEG) and non-coated positively and negatively charged nanoparticles are compared. Therefore, fluorescent poly(organosiloxane) nanoparticles of 15 nm radius are synthesized, which are used as a scaffold for surface modification in a grafting onto approach.
With multi-angle dynamic light scattering, asymmetrical flow field-flow fractionation, gel electrophoresis, and liquid chromatography-mass spectrometry, it is demonstrated that protein adsorption on PEtOxylated nanoparticles is extremely low, similar as on PEGylated nanoparticles. Moreover, quantitative microscopy reveals that PEtOxylation significantly reduces the non-specific cellular uptake, particularly by macrophage-like cells. Collectively, studies demonstrate that PEtOx is a very effective alternative to PEG for stealth modification of the surface of nanoparticles.
Polyurethane versus silicone catheters for central venous port devices implanted at the forearm
(2016)
Purpose: We aimed to analyse short and long-term complications of polyurethane (PU) versus silicone catheters used in totally implantable venous-access ports (TIVAPs) implanted at the forearm.
Methods: Retrospective analysis of 698 consecutively implanted TIVAPs was performed. Primary end-points were defined as rates of major complications associated with either type of central venous port catheter. Technical success rate, device service interval as well as minor complications not requiring port explantation were defined as secondary end-points.
Results: A total of 698 port devices were implanted in 681 patients, 396 equipped with a PU catheter, 302 with a silicone catheter. The technical success rate was 99.9% with no major periprocedural complications. During follow-up a total of 211 complications in 146 patients were observed (1.0/1000 catheter days), 183 occurred associated with PU catheters (1.8/100 catheter days), 28 (0.3/1000 catheter days) with silicone catheters (log rank test p < 0.0001). Catheter-related bloodstream infections as well as thrombotic complications occurred significantly more frequently with PU catheters, while silicone catheters exhibited a trend towards a higher rate of mechanical failure such as disconnection or catheter rupture. Major complications requiring explantation of the device occurred more frequently with PU-based catheters (10.6%) compared to silicone catheter carrying ports (4.6%, log rank test p < 0.001).
Monitoring the ingestion of microplastics is challenging and suitable detection techniques are insufficiently used. Thus, misidentifying natural for synthetic microfibres cannot be avoided. As part of a framework to monitor the ingestion of microplastics in eelpout, this short report addresses the accurate identification of microfibres. We show that, following visual inspections, putatively synthetic microfibres are indeed of natural origin, as ascertained by spectrometric analyses. Consequently, we call for an inclusion of spectroscopic techniques in standardized microplastic monitoring schemes.
The cure behaviour of a specific ethylene vinyl acetate material as used for encapsulation of photovoltaic modules was analysed by rheometer, differential scanning calorimetry and Fourier transform infrared spectroscopy to test for a suitable replacement for the laborious determination of gel content. The results show that all applied methods are capable of describing the effects of the cross-linking process. Some provide results very similar to those yielded by analysis of the insoluble content, but the question remains as to whether indirect methods should be preferred over the direct measurement of physical properties, e.g. as performed by the curemeter. A material stored for one year was also tested to demonstrate the effect of extended storage on cure behaviour and how this is detected by different methods. This complements the other methods, which were clearly able to detect the different cure behaviour of the aged EVA, whereas determination of the gel content could not.
Sulphurous additives for polystyrene: Influencing decomposition behavior in the condensed phase
(2015)
The thermal decomposition behaviour of polystyrene (PS) containing sulphur and phosphorus additives was investigated, using thermogravimetry coupled with Fourier transform infrared spectroscopy (TGA-FTIR). It was found that the additives influence the decomposition process of the polymer in the condensed phase, resulting in a decrease in styrene monomer formation and an increase in styrene oligmer derivatives. Via reference measurements with binary mixtures it was found that the presence of sulphur additives influences the radicalic decomposition process of PS. In combination with quantum chemical calculations it was concluded that this is due to the formation of radicals that abstract hydrogen from the polymer matrix at lower temperatures, disfavouring the radicalic decomposition pathway leading to styrene.
The memory effect in polyolefinic products: A tool for confirming the steam sterilization process
(2015)
DSC-Messungen von dampfsterilisierten medizinischen Produkten aus Polyolefinen zeigen beim ersten Heizvorgang als auffällige Besonderheit eine zusätzliche Stufe, bekannt als Temperpeak. Das Ziel dieser Untersuchungen ist, dieses Phänomen nachzuvollziehen und zu verstehen, um es als Nachweis für die Dampfsterilisation nutzen zu können. Dafür wurden PP- und PE-Proben unter verschiedenen Bedingungen dampfsterilisiert und im Ofen thermisch behandelt. Anschließend wurden die Proben mittels DSC untersucht und die Einflüsse der thermischen Behandlung und der mechanischen Beanspruchung analysiert. Um den Einfluss unterschiedlicher Materialspezifikationen zu prüfen, wurden zusätzlich verschiedene Referenzmaterialien (PE und PP) untersucht und GPC-Messungen durchgeführt. Des Weiteren wurde die Beständigkeit des Signals gegenüber der Zeit und der Temperatureinflüssen betrachtet. Die Untersuchungen zeigen, dass sich ein stabiler Memory-Effekt erzeugen lässt.
Kunststoffe sind wichtige Werkstoffe und heutzutage aus Haushalt und Wirtschaft nicht mehr wegzudenken. Seit Anfang der 1970er-Jahre wird das Vorkommen von Kunststoffpartikeln in Küstengewässern beschrieben. Inzwischen ist Mikroplastik nicht nur im marinen Bereich, sondern auch in weiteren Umweltkompartimenten, Biota und technischen Einrichtungen der Wasserwirtschaft nachgewiesen worden, in dieser Arbeit wird ein Überblick über das Vorkommen von Mikroplastik in der aquatischen Umwelt und ersten bekannten Auswirkungen gegeben. Darüber hinaus werden die aktuellen Untersuchungsverfahren von Probenahme, Probenaufbereitung und Analytik betrachtet und offene fragen diskutiert. Zentral erscheint in diesem Zusammenhang die Entwicklung einer harmonisierten medienübergreifenden Untersuchungsmethodik, die eine Auswertung relevanter Stoffströme ermöglicht und auf notwendige Bewertungskonzepte abgestimmt ist.
Small polymer particles with a diameter of less than 5 mm called microplastics find their way into the environment from polymer debris and industrial production. Therefore a method is needed to identify and quantify microplastics in various environmental samples to generate reliable concentration values. Such concentration values, i.e. quantitative results, are necessary for an assessment of microplastic in environmental media. This was achieved by thermal extraction in thermogravimetric analysis (TGA), connected to a solid-phase adsorber. These adsorbers were subsequently analysed by thermal desorption gas chromatography mass spectrometry (TDS-GC-MS). In comparison to other chromatographic methods, like pyrolyse gas chromatography mass spectrometry (Py-GC-MS), the relatively high sample masses in TGA (about 200 times higher than used in Py-GC-MS) analysed here enable the measurement of complex matrices that are not homogenous on a small scale. Through the characteristic decomposition products known for every kind of polymer it is possible to identify and even to quantify polymer particles in various matrices. Polyethylene (PE), one of the most important representatives for microplastics, was chosen as an example for identification and quantification.
Using thermogravimetric analysis (TGA) with a solid-phase adsorber for thermal extraction, followed by subsequently analysing the adsorber with thermo-desorption gas chromatography mass spectrometry (TDS-GCMS) enables measurement of polymer degradation under oxidizing atmosphere, and the identification of certain complex hydrocarbon degradation products by chromatographic separation and defined mass patterns. This technique, thermal-extraction desorption gas chromatography mass spectrometry (TED-GCMS) was used to investigate the thermo-oxidative degradation of PA 66 and PA 66 doped with 2 wt% of metal oxide particles. In TGA pure PA 66 formed more residue under an oxidizing atmosphere than an inert one. In contrast to the measurements under inert atmosphere, several condensed aromatic species containing nitrogen could be identified in thermo-oxidative measurements. These degradation products were formed through condensation reactions of primary amides originating from imide hydrolysis. The formation of such highly condensed species also causes higher char formation. Four metal oxides have shown an impact on the thermo-oxidative degradation of PA 66: Fe2O3 on η-Al2O3 < pure Fe2O3 = Fe2O3 on γ-Al2O3 < pure ZnO. For ZnO even a char-stabilizing effect could be observed. A catalytic effect of these metal oxides causes more condensed cyclopentanone and pyridine derivates. Thus, more water is formed and released, resulting in increased hydrolysis of the imides and degradation at lower temperatures.
Near-infrared spectroscopy (NIR) turned out to be well suited for analyzing the degree of cure for epoxy systems. In contrast to dynamic scanning calorimetry (DSC), where the released heat of reaction determines the degree of epoxy conversion indirectly, NIR spectroscopy is able to determine the conversion directly by analyzing structural changes. Therefore, a new heatable NIR cell was equipped with an integrated thermocouple, which enables the real sample temperature to be controlled and monitored in situ during epoxy curing. Dynamic scans at different heating rates were used for kinetic modelling, to define kinetic parameters and to predict real curing processes. The kinetic models and their parameters were validated with an isothermal and a more complex multi-step curing scenario. Two available commercial epoxy systems based on DGEBA were used with an anhydride and with an amine hardener. NIR results were compared with DSC data. The simulated conversion predicted with a model fitted on the basis of NIR and DSC dynamic scans showed good agreement with the conversion measured in the isothermal curing validation test. Due to the proven reliability of NIR in measuring the reaction progress of curing, it can be considered a versatile measurement system for in situ monitoring of component production in the automotive, aerospace and wind energy sectors.
Polyglycerol (PG) coated polypropylene (PP) films were synthesized in a two-step approach that involved plasma bromination and subsequently grafting hyperbranched polyglycerols with very few amino functionalities. The influence of different molecular weights and density of reactive linkers were investigated for the grafted PGs. Longer bromination times and higher amounts of linkers on the surface afforded long-term stability. The protein adsorption and bacteria attachment of the PP-PG films were studied. Their extremely low amine content proved to be beneficial for preventing bacteria attachment.
The thermal molecular degradation of polyamide 66 (PA 66) doped with (partially supported) metal oxide particles (Fe2O3, ZnO, Al2O3) was investigated qualitatively and quantitatively using common analysis techniques like thermogravimetry coupled with IR-spectroscopic evolved gas analysis (TGA-FTIR). Using pyrolysis coupled with gas chromatography mass spectrometry (Py-GC-MS), qualitative conclusions were drawn about the complex hydrocarbon products. However, the combination of TGA with solid-phase extraction, followed by thermal desorption gas chromatography mass spectrometry (TED-GC-MS), allows qualitative and even semi-quantitative conclusions about the decomposition pathway of PA 66 in the presence of various metal oxide particles.
The investigations under inert conditions showed that the presence of metal particles increases the rate of decarboxylation and deamination reactions, as well as the formation rate of cyclopentanone and pyridine derivatives. These species are a consequence of various condensation reactions. The condensation reactions release a large amount of water, thus triggering the hydrolysis of PA 66. Molecular thermal degradation mechanisms were developed for the main decomposition as well as for the condensation reactions and supported by quantum chemical calculations. The catalytic effect of the metal oxides in PA 66 increases in the following order: PA 66 = PA 66 – Al2O3 < PA 66 – Fe2O3 < PA 66 – ZnO.
As polypeptoids become increasingly popular, they present a more soluble and processable alternative to natural and synthetic polypeptides; the breadth of their potential functionality slowly comes into focus. This report analyzes the ability of an alkyne-functionalized polypeptoid, poly(N-propargyl glycine), to crosslink upon heating. The crosslinking process is analyzed by thermal analysis (differential scanning calorimetry and thermogravimetric analysis), Fourier-transform infrared, electron paramagnetic resonance, and solid-state NMR spectroscopy. While a precise mechanism cannot be confidently assigned, it is clear that the reaction proceeds by a radical mechanism that exclusively involves the alkyne functionality, which, upon crosslinking, yields alkene and aromatic products.
Der Fänger im Spülgas
(2015)
After some months of operation, a number of PV modules develop a discolouration defect called 'snail trails', or 'snail traces', which appear as irregular dark stripes across the cells. Whereas these traces were soon identified as discoloured silver contacts along the cell edges or at micro cracks, the chemical and mechanistic reasons for this phenomenon have not yet been resolved in detail. In this work we show that silver nanoparticles accumulating within the encapsulation foil cause the brownish discolouration, and that certain additives of encapsulation and back sheet foils trigger the formation of these nanoparticles.
Two commercial polyethylene grades were exposed to water at elevated temperatures and enhanced oxygen pressure. To characterize their aging behavior laser-induced photoluminescence spectroscopy was applied. Additionally, aging characterization was performed by established methods such as tensile testing, infrared (IR) spectroscopy, high performance liquid chromatography (HPLC), differential scanning calorimetry (DSC) and UV–VIS spectroscopy. During the initial stages of aging, the overall concentration of phenolic antioxidants as well as oxidation onset temperatures decreased exponentially. Simultaneously, significant discoloration due to the formation of conjugated degradation products from phenolic antioxidants (e.g., quinone methides) was detected. After the consumption of antioxidants, photoluminescence started to grow continuously presumably due to the formation of photoluminescent unsaturated carbonyls. In the final stages of aging, embrittlement of the materials as characterized by the degradation of mechanical properties (i.e., loss in ductility) coincided with rising carbonyl index values as well as an increase in crystallinity due to chemicrystallization. Between integrated photoluminescence intensity and carbonyl index, a linear correlation was established. In the induction period, the photoluminescence method exhibited a significantly higher sensitivity to reflect aging induced material changes.
Cure monitoring of epoxy films by heatable in situ FTIR analysis: Correlation to composite parts
(2014)
The curing mechanism of an epoxy film containing dicyandiamide (DICY) and an epoxy formulation based on diglycidyl ether of Bisphenol A (DGEBA) polymer was studied as a function of various temperature programs. The investigation was performed in situ, using a thin film of the epoxy mixture on a silicon wafer substrate in a heatable transmission tool of a FTIR spectrometer. Based on these model-curing experiments, a major curing mechanism was proposed, taking into account the appearance, the decrease, and the development of characteristic bands at various temperatures. The conclusions of the model curing were correlated to FTIR measurements on a real, 50-mm-thick glass fiber reinforced component composite part from a technical process. It could be shown that characteristic bands that develop at curing temperatures above 150°C appear especially in the center of the thick sample. From the chemical or molecular point of view, this demonstrates the established technician's understanding that temperature control inside a large-scale fiber composite of, for example, aircraft, wind-turbine, automotive applications component is of major importance.
After several months of operation, many photovoltaic (PV) modules develop a discolouration defect called snail trails which appear as irregular dark traces across the cells. These traces are caused by silver nanoparticles accumulating within the encapsulation foil directly above the grid finger. In this work we systematically investigate combinations of encapsulation and back-sheet foils with respect to their susceptibility for snail trails. We can show that certain additive compositions within the encapsulation and back sheet foils are critical for the formation of the discolouring silver nanoparticles. We suggest a reaction model explaining the formation of snail trails from a chemical point of view. This fundamental understanding allows the rapid testing of foils for their snail trail sensitivity as well as the special design of resistant foils.
A flexible, sustainable, one-step thermal decomposition route for the synthesis of hierarchical, heteroatom doped carbon foams is presented. Task-specific semi-organic crystals combine functions for three different purposes: the carbon and heteroatom source, a foaming agent (CO2) and an in situ generable template (NaCl). Insights to the decomposition pathway were gained through FTIR/MS coupled TGA and an ultrafast out-of-furnace heating procedure and the products were analysed with (HR)SEM/TEM, EELS, FTIR, and N2 sorption. The resulting macroporous carbon foams are excellent supports for metallic nanoparticles due to their hierarchical structure, high surface area and tuneable heteroatom contents. This was demonstrated for catalytically active copper or the magnetic CoNi alloy for water purification.
The aim of this study is to investigate and compare three different factors, temperature, pretreatment and exposure media, on the oxidation and aging behavior of polypropylene (PP) bulk samples in the autoclave test under increased oxygen pressure. The aging of polypropylene, in this case syringe material, was accelerated under different conditions. The samples were aged at 75°, 80° and 85 °C under pure oxygen and at 75 °C under ultrapure water. Further samples treated with 15 kGy (e-beam) were aged at 75 °C under pure oxygen. All experiments were carried out at an oxygen partial pressure of 50 bar. The different courses of aging were evaluated and compared. Color and transparency were used to assess the visual changes; weight, geometry and tensile test for the changes in technical properties; and DSC, FTIR and TDS-GC-MS to improve our physico-chemical understanding of the aging processes.
The investigations showed that all factors tested influence oxidation/aging behaviour. Dry or wet exposure has no effect on aging during the induction time. However, after the point of maximum service time the degradation process of polymer changes significantly in the presence of water. The increase of aging temperature decreases the maximum service time; however a temperature higher than 80 °C changes the relative ratio of surface and bulk oxidation. The pretreatment with irradiation decreases the maximum service time further, because the irradiation partly damages the antioxidant, and the mobility of antioxidant fragments inside the polymer changes. These diffusion effects influence the relative ratio of bulk and surface oxidation of the polymer sample.
For analysis of the gaseous thermal decomposition products of polymers, the common techniques are thermogravimetry, combined with Fourier transformed infrared spectroscopy (TGA–FTIR) and mass spectrometry (TGA–MS). These methods offer a simple approach to the decomposition mechanism, especially for small decomposition molecules. Complex spectra of gaseous mixtures are very often hard to identify because of overlapping signals. In this paper a new method is described to adsorb the decomposition products during controlled conditions in TGA on solid-phase extraction (SPE) material: twisters. Subsequently the twisters were analysed with thermal desorption gas chromatography mass spectrometry (TDS–GC–MS), which allows the decomposition products to be separated and identified using an MS library. The thermoplastics polyamide 66 (PA 66) and polybutylene terephthalate (PBT) were used as example polymers. The influence of the sample mass and of the purge gas flow during the decomposition process was investigated in TGA. The advantages and limitations of the method were presented in comparison to the common analysis techniques, TGA–FTIR and TGA–MS.
Glass fiber reinforced polyamide (PA) 6T/DT flame retarded with aluminum diethylphosphinate (AlPi) was tested to assess its flame retardant properties. Models for the decomposition of PA 6T/DT with and without AlPi are presented. Thermal decomposition was measured by performing TGA with Fourier transform infrared (FTIR) spectroscopy and FTIR spectroscopy in the condensed phase. Fire behavior was studied using a cone calorimeter and flammability was tested with UL 94 and the limiting oxygen index. AlPi works as an effective flame retardant for glass fiber reinforced PA 6T/DT materials, acting in the gas phase. Also observed was condensed-phase action, which occurs especially under oxidative conditions before the samples ignite.
Combinations of different common flame retardants in wood–plastic composites (WPCs) are tested to identify synergistic or antagonistic effects with the goal of improving the fire performance of WPCs. Flame retardants investigated are expandable graphite (EG), ammonium polyphosphate (APP), and red phosphorus (RP) and combinations of two of them are used. The fire behavior is studied by cone calorimetric measurements. Additional thermogravimetry is used for further investigations. The fire tests show that EG has the highest potential for flame retardancy, but due to its expansion it cracks the formed residue layer. Combinations of EG with RP or with high amounts of APP are able to suppress this cracking.
A new flame retardant based on an ammonium phosphonate is studied with respect to its thermal decomposition and its mode of action in wood-plastic composites (WPCs). The measurements are carried out by means of fire tests (cone calorimeter) and pyrolysis investigations (thermogravimetry, infrared spectroscopy). The flame retardant acts mainly in the condensed phase by increasing the amount of residue formed by the wood part in the WPC. Additional flame dilution is achieved by the release of water, ammonia and carbon dioxide during the decomposition of the flame retardant.
In this study, we investigated the basic knowledge necessary to develop flame-retarded woodplastic composite (WPC) materials by focusing on decking boards. Therefore, the respective effects of geometry, material composition, and moisture were studied by performing cone calorimetric measurements. Using hollow-shaped geometries removes combustible material and reduces the fire load but simultaneously increases fire propagation. The best results were achieved by using high-wood contents. The addition of talc can reduce the intensity of burning. Moisture also has a positive effect on burning behavior. Apart from the well-known mechanism of water, a change was observed in the resultant residue.
The reactivity of the flame retardant and its decomposition temperature control the condensed-phase action in bisphenol A polycarbonate/acrylonitrile–butadiene–styrene/polytetrafluoroethylene (PC/ABSPTFE) blends. Thus, to increase charring in the condensed phase of PC/ABSPTFE + aryl phosphate, two halogen-free flame retardants were synthesized: 3,3,5-trimethylcyclohexylbisphenol bis(diphenyl phosphate) (TMC-BDP) and bisphenol A bis(diethyl phosphate) (BEP). Their performance is compared to bisphenol A bis(diphenyl phosphate) (BDP) in PC/ABSPTFE blend. The comprehensive study was carried out using thermogravimetry (TG); TG coupled with Fourier transform infrared spectrometer (TG-FTIR); the Underwriters Laboratory burning chamber (UL 94); limiting oxygen index (LOI); cone calorimeter at different irradiations; tensile, bending and heat distortion temperature tests; as well as rheological studies and differential scanning calorimeter (DSC). With respect to pyrolysis, TMC-BDP works as well as BDP in the PC/ABSPTFE blend by enhancing the cross-linking of PC, whereas BEP shows worse performance because it prefers cross-linking with itself rather than with PC. As to its fire behavior, PC/ABSPTFE + TMC-BDP presents results very similar to PC/ABSPTFE + BDP; the blend PC/ABSPTFE + BEP shows lower flame inhibition and higher total heat evolved (THE). The UL 94 for the materials with TMC-BDP and BDP improved from HB to V0 for specimens of 3.2 mm thickness compared to PC/ABSPTFE and PC/ABSPTFE + BEP; the LOI increased from around 24% up to around 28%, respectively. BEP works as the strongest plasticizer in PC/ABSPTFE, whereas the blends with TMC-BDP and BDP present the same rheological properties. PC/ABSPTFE + TMC-BDP exhibits the best mechanical properties among all flame-retarded blends.
Heterogeneous, gradual or structured morphology of fire residues plays an important role in fire retardancy of polymers. A scanning electron microscope with an attached energy dispersive X-ray spectrometer (SEM/EDX) is highlighted as a powerful tool for the advanced characterization of such complex fire residues, since it offers high resolution in combination with both good depth of field and analysis of chemical composition. Two examples are presented: First, comprehensive SEM/EDX investigation on a complex structured fire residue of glass fibre reinforced polyamide 6,6 (PA 66-GF) flame retarded by diethylaluminium phosphinate, melamine polyphosphate and some zinc borate. A multilayered surface crust (thickness ~ 24 µm) covers a rather hollow area stabilized by GF glued together. The resulting efficient thermal insulation results in self-extinguishing before pyrolysis is completed, even under forced-flaming combustion. Second, sophisticated, quasi online SEM/EDX imaging of the formation of residual protection layer in layered silicate epoxy resin nanocomposites (LSEC). Burning specimens were quenched in liquid nitrogen for subsequent analyses. Different zones were distinguished in the condensed phase characterized by distinct processes such as melting and ablation of organic material, as well as agglomeration, depletion, exfoliation and reorientation of the LS.