Filtern
Dokumenttyp
- Zeitschriftenartikel (7)
- Posterpräsentation (6)
- Corrigendum (1)
- Vortrag (1)
Sprache
- Englisch (15) (entfernen)
Schlagworte
- SAXS (12)
- Microwave synthesis (6)
- Silver nanoparticles (4)
- Digestion (3)
- Nanoparticles (3)
- Small-angle X-ray scattering (3)
- Zinc oxide (3)
- Small-angle scattering (2)
- Zinc oxide nanoparticles (2)
- Data analysis (1)
- Interlaboratory comparability (1)
- MOUSE (1)
- Methodology (1)
- Nanomaterials (1)
- Nanostructure quantification (1)
- Round Robin (1)
- Zinc (1)
- Zinc phosphate (1)
- digestion (1)
- nanoparticle (1)
- nanoparticles (1)
Organisationseinheit der BAM
Eingeladener Vortrag
- nein (1)
This paper reports the formation of zinc phosphate nanoparticles from the artificial digestion of zinc chloride. Initially, the formation of amorphous primary particles with a mean radius of 1.1 nm is observed, alongside the formation of larger, protein stabilized aggregates. These aggregates, with a radius of gyration of 37 nm, are observed after 5 minutes of exposure to artificial saliva and are shown to be colloidally stable for a minimum time of two weeks. The initially formed primary particles are thought to consist of amorphous zinc phosphate, which is then transformed into crystalline Zn3(PO4)2·4H2O over the course of two weeks. Our results demonstrate that the interaction of inorganic salts with bodily fluids can induce the formation of de novo nanoparticles, which in turn, provides insights into how zinc‐enriched foods may also facilitate the formation of nanoparticles upon contact with saliva. As such, this may be considered as an undesirable (bio)mineralization.
Zinc is an essential trace element and is ingested daily by humans, partly in dissolved form. The first contact is with saliva, in which many ions are dissolved whose solubility product with zinc can be low. This could result in compounds forming, possibly in nanoparticular form, which could have different effects on the organism than pure zinc ions.
In this study, we report on the saliva stage of the artificial digestion of zinc chloride as a model substance for zinc ions. To facilitate in situ measurements, the sample is continuously passed through a small-angle x-ray scattering (SAXS) system. This custom-made machine is capable of measuring over a wide q-range and thereby able to resolve structures from around 250 nm down to the crystal structure. It is thus an excellent tool for investigating both the particle size distribution and the atomic structure of the sample.
By curve fitting, we found that shortly after addition of zinc chloride to saliva, small particles with a mean radius of 1.9 ± 0.1 nm and a distribution width of 0.6 ± 0.1 nm formed. These particles are aggregated to compact mass fractals with a fractal aggregate size of 14.7 ± 0.1 nm and a fractal dimension of 2.96 ± 0.02. Approximately 7200 single particles form each mass fractal, whose radius of gyration was found to be 36 ± 1 nm. The growth of these structures continues over the course of several weeks. To determine the compound that was formed, infrared spectroscopy was used in addition to the SAXS measurements, and zinc phosphate was identified as the product.
A round-robin study has been carried out to estimate the impact of the human element in small-angle scattering data analysis. Four corrected datasets were provided to participants ready for analysis. All datasets were measured on samples containing spherical scatterers, with two datasets in dilute dispersions and two from powders. Most of the 46 participants correctly identified the number of populations in the dilute dispersions, with half of the population mean entries within 1.5% and half of the population width entries within 40%. Due to the added complexity of the structure factor, far fewer people submitted answers on the powder datasets. For those that did, half of the entries for the means and widths were within 44 and 86%, respectively. This round-robin experiment highlights several causes for the discrepancies, for which solutions are proposed.
Zinc oxide (ZnO) nanoparticles find manifold applications, most prominently in photovoltaics, where their unique optical properties are exploited. Particularly important are their band gap energy of 3.37 eV, which can be widely tuned through doping, and a large exciton binding energy of 60 mV. As a wide-bandgap II-VI semiconductor, the optical band gap energy and fluorescence energy become size-dependent when moving to particle radii of a few nanometers.
To gain a deeper insight into this issue, we report on a microwave-assisted, size-selective synthesis of pure ZnO nanoparticles. By hydrolysis of the metal precursor in presence of a strong base at temperatures exceeding the solvent’s boiling point, the reaction is dramatically accelerated, and narrowly dispersed, spherical particles are yielded within seconds – instead of hours at lower temperatures. The determination of their size distributions in high resolution using small-angle x-ray scattering (SAXS) allows for a precise mapping of the optical properties (UV/Vis absorption and fluorescence) to particle size.
We observed that the mean particle radii increase from 2.6 ± 0.1 nm with increasing synthesis temperature from 125 °C to 200 °C. This is accompanied by a red shift of the optical band gap and the fluorescence energies, the latter of which can be seen in Figure 1. Thus, undoped ZnO nanoparticles with narrow size distributions and pre-defined size as well as optical properties can be obtained through a microwave-assisted synthesis.
Zinc oxide (ZnO) as a wide-bandgap II-VI semiconductor finds application in areas like optoelectronics, photocatalysis as well as in detection systems. While band-gap engineering in macroscopic ZnO can be performed by alloying, the band-gap of ZnO nanoparticles is also dependent on their size. Since small-angle X-ray scattering (SAXS) provides a much higher resolution in terms of ultra-small nanoparticle size analysis compared to other techniques, it allows for a careful examination of the correlation between particle size and band-gap.
We report on the microwave-assisted synthesis of oleate-capped, photoluminescent zinc oxide nanoparticles with adjustable size as dispersions in organic solvents. The spherical particles were obtained by hydrolysis of the metal precursor in presence of a strong base at temperatures above the solvent’s boiling point. Hence, the reaction is dramatically accelerated and within seconds – instead of hours at lower temperatures –, narrowly dispersed particle systems are yielded. The particles’ sizes as derived from SAXS strongly depend on the reaction temperature and time. Choosing the right reaction conditions, the particle size and thus their band gap can be finely tuned. A size increase can be achieved both by increasing the reaction temperature and the reaction time.
See Figure 1 for an exemplary comparison of five-minute syntheses at different temperatures. Here, the yielded particles display diameters between 5.0 and 7.6 nm and corresponding band-gaps of 3.32 up to 3.41 eV. The size increase is accompanied by a red-shift of the UV/Vis absorption edges and fluorescence emission.
Furthermore, these particles can be transferred into water by coating with polysorbates.
Herein, a simple one-pot procedure is reported to obtain aqueous zinc oxide (ZnO) nanoparticle dispersions from ZnO nanoparticles dispersed in cyclohexane. In the process, polyoxyethylene (20) sorbitan monooleate (polysorbate 80, Tween 80) functions as a phase transfer agent and colloidal stabilizer. The particles grow in a defined manner during the transfer, presumably via coalescence. The final particle radii are tuneable in the range from 2.3 ± 0.1 nm to 5.7 ± 0.1 nm depending on the incubation time of the dispersion at 90 °C. Small-angle X-ray scattering is employed to determine the particle radius distributions before and after phase transfer. The larger ZnO particle radii are associated with a redshift of the optical bandgap and luminescence emission, as expected for semiconductor nanoparticles. The particles presented here exhibit a relative size distribution width of 20%, rendering them attractive for applications in, e.g., biology or catalysis. The latter application is demonstrated at the photocatalytic degradation of methylene blue dye.
We report on ultrasmall zinc oxide single-crystalline nanoparticles of narrow size distribution and long-term colloidal stability. These oleate-stabilized nanoparticles were synthesized using microwave-assisted synthesis for 5 min, corresponding to a 99% decrease in synthesis time, when compared to the conventional synthesis method. It was observed that the average particle radius increases from 2.6 ± 0.1 to 3.8 ± 0.1 nm upon increasing synthesis temperature from 125 to 200 °C. This change also corresponded to observed changes in the optical band gap and the fluorescence energy of the particles, from 3.44 ± 0.01 to 3.36 ± 0.01 eV and from 2.20 ± 0.01 to 2.04 ± 0.01 eV, respectively. Small-angle X-ray scattering, dynamic light scattering, and UV–vis and fluorescence spectroscopy were employed for particle characterization. Debye–Scherrer analysis of the X-ray diffraction (XRD) pattern reveals a linear increase of the crystallite size with synthesis temperature. The consideration of the convolution of a Lorentz function with a Gaussian function for data correction of the instrumental peak broadening has a considerable influence on the values for the crystallite size. Williamson–Hall XRD analyses in the form of the uniform deformation model, uniform stress deformation model, and uniform deformation energy density model revealed a substantial increase of strain, stress, and deformation energy density of the crystallites with decreasing size. Exponential and power law models were utilized for quantification of strain, stress, and deformation energy density.
Ever since increasing a reaction’s yield while shortening the reaction time is the main objective in synthesis optimization. Microwave reactors meet these demands. In literature however their usage is under discussion due to claims of the existence of non-thermal effects resulting from the microwave radiation. Especially for nano-reference-material syntheses it is of crucial importance to be aware of influences on the reaction pathway. Therefore, we compare ultra-small silver nanoparticles with mean radii of 3 nm, synthesized via conventional and microwave heating.
We employed a versatile one-pot polyol synthesis of poly(acrylic acid) (PAA) stabilized silver nanoparticles, which display superior catalytic properties. No microwave specific effects in terms of particle size distribution characteristics, as derived by small-angle X-ray scattering (SAXS) and dynamic light scattering (DLS), are revealed. Due to the microwave reactor’s characteristics of a closed system, syntheses can be carried out at temperatures beyond the solvent’s boiling point. Particle formation was accelerated by a factor of 30 by increasing the reaction temperature from 200 °C to 250 °C. The particle growth process follows a cluster coalescence mechanism.
A post-synthetic incubation step at 250 °C induces a further growth of the particles while the size distribution broadens. Thus, utilization of microwave reactors enables an enormous decrease of the reaction time as well as the opportunity of tuning the particles’ size. Possibly, decomposition of the stabilizing ligand at elevated temperatures results in reduced yields. A temperature of 250 °C and a corresponding reaction time of 30 s represent a compromise between short reaction times and high yields.
We report on etching of polyacrylic acid-stabilised silver nanoparticles in the presence of glutathione (GSH). The initial particles with a radius of 3.2 nm and consisting of ∼8100 silver atoms dissolve in a two-step reaction mechanism while in parallel smaller silver particles with a radius of 0.65 nm and consisting of 60 to 70 silver atoms were formed. The kinetics of the etching of the initial particles, accompanied by formation of smaller silver particles was interpreted based on in situ, time-resolved small-angle X-ray scattering (SAXS) experiments.
Zinc is an essential trace element and is ingested daily by humans, partly in dissolved form. The first contact is with saliva, in which many ions are dissolved whose solubility product with zinc can be low. This could result in compounds forming, possibly in nanoparticular form, which could have different effects on the organism than pure zinc ions. Available biopolymers, e.g. α-amylase, can in turn stabilise as-formed nanostructures.
In this study, we report on the saliva stage of the artificial digestion of zinc chloride as a model substance for zinc ions. To facilitate in situ measurements, the sample is continuously passed through a small-angle x-ray scattering (SAXS) system. This custom-made machine is capable of measuring over a wide q-range and thereby able to resolve structures from around 250 nm down to the crystal structure. It is thus an excellent tool for investigating both the particle size distribution and the atomic structure of the sample.
By curve fitting (see Figure 1), we found that shortly after addition of zinc chloride to saliva, small particles with a mean radius of 1.9 ± 0.1 nm and a distribution width of 0.6 ± 0.1 nm formed. These particles are aggregated to compact mass fractals with a fractal aggregate size of 14.7 ± 0.1 nm and a fractal dimension of 2.96 ± 0.02. Approximately 7200 single particles stick together by protein and form mass fractals, whose radii of gyration were found to be 36 ± 1 nm. To determine the compound that was formed, infrared spectroscopy was used in addition to the SAXS measurements, and zinc phosphate was identified as the product.