Filtern
Erscheinungsjahr
Dokumenttyp
- Zeitschriftenartikel (7)
- Beitrag zu einem Tagungsband (3)
- Vortrag (2)
- Forschungsbericht (1)
Schlagworte
- High throughput screening (2)
- Hydrogen detection (2)
- Hydrogen sensor (2)
- Long-term measurement (2)
- Low energy sensor (2)
- Activation (1)
- Alloy (1)
- Branddetektion (1)
- Brandfrüherkennung (1)
- Brandmelder (1)
Eingeladener Vortrag
- nein (2)
The silicon based semiconductor structure Si/SiO2/Si3N4/LaF3/Pt can be used as a potentiometric oxygen sensor working at room temperature. A thermal re-activation can be applied to overcome the earlier disadvantage of an increase in response time with continuous use. Using the Pt gate electrode as a resistive heater, very short electrical high-power pulses can be applied. A heating time as short as 300 ns was sufficient for the re-activation of the sensor. This way, only the sensitive thin layer system LaF3/Pt was heated, and the whole sensor was at room temperature immediately after heating. Impedance spectroscopy, X-ray photoelectron spectroscopy (XPS) and quadruple mass spectrometric (QMS)thermogravimetry (TG) were used to investigate the mechanism of deterioration in dynamic sensor behaviour and re-activation. The formation of hydrated carbonate and the desorption of CO2 and H2O have been shown to be the causes.
A silicon MIS-structure prepared with thin layers of the super-ionic conductor LaF3 and Pd is used to detect hydrogen. The sensor is able to detect hydrogen in a concentration range from below one ppm to the lower flammable limit in air which is 4 vol.-%. The chip operates at room temperature which results in an extremely low energy consumption compared to other hydrogen sensors. Only once per day a short heating pulse is necessary to reactivate the sensor chip. In cooperation with the BAM, a long-term experiment was carried out. The duration of the measurement was about three months, with a hydrogen exposure every two weeks. The sensor signal remained stable over the measured period.
A new high throughput screening method to characterise alloys used as gate metal of Metal/solid Electrolyte/Insulator/Semiconductor (MEIS) gas-sensors was developed. Samples with continuous gradients in alloy concentration for the system Pd1-x-yNiyCoy were analysed regarding H2 sensitivity. First results showed reduced poisoning effects of H2S for Ni concentrations between 4-11 at-% in Pd.
Ternary alloys have been studied as the gate metal of chemical sensors based on the field effect in silicon. The investigation of reduced poisoning of hydrogen sensors by H2S is presented in the alloy system PdxNiyCo1-x-y. A new method in high throughput screening of alloys is applied. Not singular sample compositions but a continuous gradient in alloy concentrations was produced on a semiconductor sample. A laser scanning system produces a photo current in the semiconductor to map the sensor signal and provide a quasi continuous alloy characterization. The new system is therefore called Continuous Gradient—High Throughput Screening Macroscope (CG-HTSM). Typically 625 alloys are characterized in 15 minutes. The resolution of our set-up allows distinguishing 100.000 alloy compositions.
A hydrogen sensor based on a silicon Metal/Solid Electrolyte/Insulator/Semiconductor (MEIS) structure with thin layers of the super-ionic conductor LaF3 and Pd gate metal was investigated in a hybrid structure on a resistance heater mounted on a ceramic substrate. The sensor was operated at room temperature, however, a short heating impulse once a day ensures a fast and reproducible dynamic behavior. The sensor was characterized in the concentration range typical for alarm levels up to 40% of the lower flammability limit and shows a logarithmic dependency of the sensor signal from the hydrogen concentration and a mean sensitivity of about 140 mV/decade. The response time (t90) is about 8 s. In a long term test for a period of three month, the sensor was exposed to hydrogen every two weeks. The sensor signal was shown to be stable in dynamic behavior, sensitivity and signal difference.
Characterization of Pd-Ni-Co alloy thin films by ED-EPMA with application of the STRATAGEM software
(2012)
Ternary thin film alloys based on Pd, Ni and Co on silicon wafers have been characterized in order to determine elemental composition and thickness. A broad variety of alloy compositions was obtained on one and the same substrate by magnetron dc-co-sputter deposition. Energy-dispersive electron probe X-ray microanalysis of these 'multi' alloy composition samples is performed in a non-destructive, precise and, if optimized, also in a time-saving way. The local thickness of the layers under study was in between 50 nm and 250 nm. Pure element bulk materials have been employed as reference specimens. The results attained in this study are compared to those obtained by other analytical methods as Auger electron spectroscopy and X-ray photo electron spectroscopy.
Forest fires start mostly in partial combustion. In this paper we present a hydrogen sensor to defect early stages of forest fires. First indoor experiments in a smoke density chamber with wood samples, proved that the sensor produce a strong signal change when the smouldering of wood starts, already before the CO concentration, measured in FTIR spectrometry, exceeds 10 ppm. In outdoor experiments we were able to detect forest fire in a distance of 110 m.
Durch die Verwendung von Grillgeräten in geschlossenen Räumen, wie Gartenlauben, Wohnungen oder Garagen kam es in den vergangenen Jahren zu einer Vielzahl von Unfällen mit schweren Vergiftungen und Todesfällen. Seit 2008 scheint das Auftreten von Kohlenmonoxid (CO) Intoxikationen innerhalb Deutschland wieder zu zunehmen. Die Hauptursachen sind dabei der unsachgemäße Gebrauch von Holzkohlegrills, schlecht gewartete Gasthermen und Kamine. Zum Schutz der Bevölkerung ist deshalb eine Aufklärung über mögliche Gefahren wichtig.
Im Rahmen dieser Arbeit wurden diese Gefahren bewertet. Es wurden verschiedene Brandszenarien mit Grillgeräten, mit unterschiedlichen Grillkohlearten und –mengen in geschlossenen Räumen realisiert und die entsprechenden Konzentrations-Zeit-Verläufe ermittelt. Bei den Brandversuchen wurden zudem notwendige Eingabeparameter für numerische Simulationen ermittelt, um die Verwendung von Holzkohlegrills in geschlossenen Räumen zu simulieren. Die Auswirkungen für Menschen beim Grillen in geschlossenen Räumen wurden quantifiziert, indem die Eintrittszeitpunkte der Handlungsunfähigkeit und des Todes mittels Fractional Effective Dose (FED)-Konzept bestimmt wurden. Die Ergebnisse zeigen deutlich, dass eine frühzeitige Detektion der toxischen Gase zur Warnung von Personen dringend notwendig ist. In den durchgeführten Brandversuchen zeigte sich, dass die gebräuchlichen Rauchmelder auf Streulichtbasis keine rechtzeitige Warnung ermöglichen. Deshalb sind für solche Brandszenarien andere Branddetektoren erforderlich. Entsprechende Versuche mit CO-Brandmeldern zeigten, dass das freigesetzte CO beim Grillen in geschlossenen Räumen frühzeitig detektiert werden kann und Personen somit rechtzeitig gewarnt werden können.
Zur frühzeitigen Erkennung von Schwelbränden wurde weiterhin ein neuer Wasserstoffdetektor getestet. Die Entstehung von Wasserstoff in einer sehr frühen Brandphase kann zur frühzeitigen Erkennung von Schwelbränden genutzt werden. Bei ersten Schwelbrandexperimenten mit Holzproben konnte Wasserstoff in einer geschlossenen Kammer (0,5 m3) nachgewiesen werden, noch bevor es zu einer erhöhten CO-Emission kam. Die Ergebnisse der Schwelbrandversuche werden vorgestellt und die Verwendbarkeit von CO- und Wasserstoff-Detektoren erörtert und diskutiert.