Schlagworte
- Compression set (20)
- Ageing (18)
- Elastomer (16)
- Seal (15)
- Rubber (12)
- Aging (10)
- Metal seal (10)
- Storage (9)
- O-ring (8)
- Compression (7)
Organisationseinheit der BAM
- 3 Gefahrgutumschließungen; Energiespeicher (38)
- 3.4 Sicherheit von Lagerbehältern (38)
- 3.3 Sicherheit von Transportbehältern (2)
- 9 Komponentensicherheit (2)
- 5 Werkstofftechnik (1)
- 5.2 Metallische Hochtemperaturwerkstoffe (1)
- 9.5 Tribologie und Verschleißschutz (1)
- 9.6 Additive Fertigung metallischer Komponenten (1)
Paper des Monats
- ja (2)
Eingeladener Vortrag
- nein (32)
Casks for the transport and storage of heat generating radioactive waste in Germany are normally provided with screwed lid systems, which are in most cases equipped with double jacket metal seals with an inner spring wire to provide long term resistance to the seal compression force. Preservation of the high sealing quality of those seals under operational and accidental stress conditions is essentially important to the safety of those casks. Relative displacements of the lid system surfaces caused by specific impact scenarios cannot be excluded and have to be evaluated with respect to a possible increase in the leakage rate.
To get representative data for such metal sealed lid systems, BAM has developed a special conceptualised flange system placed in an appropriate testing machine for relevant mechanical loading of the metal seals under static and cyclic conditions. Furthermore, the flange system enables continuous measurement of the standard helium leakage rate during each test.
The primary aim of the investigation is to identify the correlation between variation of installation conditions (axial displacements) caused by external loads and the standard helium leakage rate. An essential parameter in this case is the useable resilience ru of a metal seal under relevant stress conditions. The useable resilience ru is the vertical difference in the cross-section between the seal's assembling status and the point where the leakage rate, by means of external load relieving, exceeds the quality criterion of 10-8 Pa m3 s-1. Load relieving can instantly occur due to modification of the seal groove dimension caused by accident impacts and deformation of the lid system. Furthermore, component specific basis data for the development of finite element calculation models should be collected. In the tests, seals are subjected to static and cyclic loads. All tests are performed at ambient temperature.
This paper presents the test configuration, different test series and results of the current experiments. Typical load-displacement-leakage rate correlations are presented and discussed.
The special properties of high molecular weight polyethylene (HMW-PE) and ultra high molecular
weight polyethylene (UHMW-PE) result basically from their extreme chain lengths and their high
degree of crystallinity. As high-performance polymers, they are used for a variety of applications.
UHMW-PE in particular is often utilized for endoprothesis (due to its excellent slip and wear
properties) and due to its high hydrogen content as a neutron moderator in casks for storage and
transport of radioactive materials.
To prepare the material for instance for its use as a total joint replacement, it is exposed to radiation
for several reasons, such as sterilization and crosslinking, leading to partial improvement of the
mechanical properties (e.g. fracture toughness, crack propagation resistance, wear resistance) and
better chemical stability.
To be applicable for long term radiation shielding purposes for instance over a period of 40 years,
PE has to withstand any type of degradation affecting safety relevant aspects.
The scope of our investigation comprises an estimation of the radiation impact on the molecular and
supra molecular structure of two types of PE and to what extent these changes are detectable by
thermo-analytical (TA) methods, such as Differential Scanning Calorimetry (DSC), Thermo
Mechanical Analysis (TMA), Dynamic Mechanical Analysis (DMA) and Thermo Gravimetric
Analysis (TGA). Additionally FT-IR spectroscopy as well as density and gas sorption
measurements were carried out.
Due to the poor solubility of HMW-PE and UHMW-PE, some classical analytical techniques are
not applicable. But TA-methods represent a feasible approach to detect structural and
morphological features of these materials as well as changes caused by external influences, such as
thermal treatment and/or irradiation. With the combination of the applied TA-techniques it is
possible to distinguish between crosslinking and degradation.
Die Messung des dynamischen Speichermoduls mit der Dynamisch-Mechanischen-Analyse ermöglicht einen schnellen Überblick über das temperaturabhängige Verhalten von elastomeren Dichtungsmaterialien. Ein direkter Rückschluss von der so ermittelten Glasübergangstemperatur Tg auf die Versagenstemperatur einer Dichtung ist aber ohne zusätzliche Messungen bisher nicht möglich.
Mit den Ergebnissen des Druckverformungsrestes DVR und des DVRDMA ist eine ge-nauere Beschreibung der Tieftemperatureigenschaften und dadurch der Funktion von elastomeren Dichtungsmaterialien möglich. Messungen ergeben beispielsweise, dass sich das EPDM bei einer Temperatur von -40 °C laut der Dynamisch Mechanischen Analyse noch im gummielastischen Bereich befindet. Die DVRDMA-Werte zeigen eine Rückstellung um mehr als 40 % der Ausgangsdeformation in wenigen Minuten.
Mit derart detailliert bestimmten Eigenschaften lassen sich Rückschlüsse auf einsatzspezifische Anforderungen wie z. B. die Dichtwirkung in Abhängigkeit von Betriebstemperatur und mechanischer Belastungsgeschwindigkeit ziehen, so dass je nach Einsatzbedingungen für die Dichtungen eine geeignete Materialauswahl getrof-fen werden kann.