Jerrycans made from three different types of high-density polyethylene (HDPE) were exposed outdoors, for one Berlin summer season. They were filled with a 55 percent nitric acid solution (HN03), pure water, or air, and half of them were protected from sunlight by an UV absorbing canvas. Thus, the separate effects of UV radiation and nitric acid could be compared to the combined impact. Combined impact was mainly affected by decomposition of nitric acid, resulting in presence of reactive nitrogen oxides, increased oxygen partial pressure, and UV radiation energy, simultaneously in vapour phase.
To investigate the degradation effects after the outdoor exposure, jerrycans were exposed to a so called hydraulic internal pressure test, similar to an approval test for dangerous goods packaging. After combined impact of UV radiation and nitric acid, internal pressure tests showed very fast failures, whereas after separate impacts no remarkable deteriorations were observed, compared to unaged jerrycans.
A new irradiation device for the exposure of plastic products is presented. Developed in the BAM division 3.1 "Dangerous Goods Packaging" it can be used for artificial UV irradiation of plastic Containers filled with hazardous liquids.
Present regulations and tests only investigate the exposure effects of UV and of media separately, but as the damaging effect is expected to be synergistic for at least some media, a combined test was looked for.
A chamber of 60 cm by 60 cm base area and 1 m height gives space for up to 40 cm wide objects. Two fluorescent UV lamp arrays are arranged on opposite walls, separated from the chamber by quartz glass panes. By continuously rotating the exposure object by means of a rotary disc that the object is placed on, spatial irradiation homogeneity is achieved over the exposure duration. The spectral irradiance of the chosen UVA 340 nm lamps gives the best match of global solar radiation in the short wavelength ränge. The close arrangement of the UVA lamps (15 each side) results in 60 W m'2 UV irradiance.
Constant temperature is adjusted to typically 40 °C by the control of the fan speed. This temperature is chosen, as it is the required temperature for three week storage of filled polyethylene Containers, for proving Chemical compatibility in the field of dangerous goods. To ensure homogeneity, an interiorfan provides for air circulation.
Transport und Lagerung flüssiger Chemikalien erfolgen häufig in HDPE-Behältern. Diese Behälter müssen Bauteilprüfungen bestehen, die mechanische und chemische Beanspruchungen kombinieren. UV-Beanspruchungen sind kein Bestandteil der Zulassungsprüfungen; gefordert wird aber eine ausreichende UV-Stabilisierung. Inwiefern diese UV-Stabilisierung aber abhängig vom jeweiligen Füllgut ist, soll hier untersucht werden.
Vorgestellt wird der experimentelle Aufbau zur kombinierten Beanspruchung von Kunststoffproben durch UV-Strahlung und flüssige Chemikalien. Aufgrund des Gefährdungspotenzials sind dabei entsprechende Sicherheitsvorgaben einzuhalten. Ziel ist die Bewertung synergistischer Effekte beider Einzelbeanspruchungen. Die Wirksamkeit verschiedener Stabilisierungskonzepte bei Beanspruchung durch 55 %-ige Salpetersäure wird beleuchtet. Es wird anschaulich gezeigt, dass nur pigmentiertes HDPE ausreichende Stabilität aufweist.