Laser ablation inductively coupled plasma mass spectrometry (LA-ICP-MS) was utilized for spatially resolved bioimaging of the distribution of silver and gold nanoparticles in individual fibroblast cells upon different incubation experiments. High spatial resolution was achieved by optimization of scan speed, ablation frequency, and laser energy. Nanoparticles are visualized with respect to cellular substructures and are found to accumulate in the perinuclear region with increasing incubation time. On the basis of matrix-matched calibration, we developed a method for quantification of the number of metal nanoparticles at the single-cell level. The results provide insight into nanoparticle/cell interactions and have implications for the development of analytical methods in tissue diagnostics and therapeutics.
Polyethylene (PE) frits were used to quantify sulphur in copper and its alloys by isotope dilution combined with LA-ICP-MS as an alternative approach to conventional sample preparation: the copper samples were spiked, the spiked samples were dissolved, the resulting solutions were absorbed in the PE frits and finally the PE frits were analysed by LA-ICP-MS. A prerequisite for such a support material is a low sulphur blank and thus PE was selected for this purpose. The absorption efficiency of the PE frits was studied for varying sulphur amounts ranging from 2 mg S to 80 mg S showing that more than 99.5% of the loaded sulphur was absorbed by the frit. The so prepared PE frits were measured by LA-ICP-MS and yielded a good linearity (R2 ¼ 0.999) for the sulphur ion intensities corresponding to sulphur amounts up to 40 mg S; the associated sensitivity is approximately 3.4 x 10⁴ cps μg⁻¹ for ³²S. For the validation of the developed procedure the reference materials BAM-M376a, BAM-228 and BAM-227 were applied such that 2 μg S, 5 μg S and 11 μg S were absorbed in the PE frits, respectively. These samples were pre-quantified for the adsorbed sulphur amount by external calibration LA-ICP-MS yielding sulphur amounts of 0.9 μg, 5.1 μg and 8.5 μg (quantified for ³²S only), respectively. Relative Standard deviations of the isotope ratios were below 5% in average (n ¼ 3 lines) in all cases (except for the pure spike solution). These samples were then analysed by LA-ICP-IDMS and the measurement results were validated by comparing them with the results obtained by conventional ICP-IDMS. The obtained relative expanded measurement uncertainties ranged between 10% and 26%. Pearson's coefficient was used to express the correlation between both techniques; the obtained value was 0.999 demonstrating a strong correlation. Contrary to most published LA-ICP-IDMS procedures, the developed procedure enables SI-traceability for the measurement results. The metrological traceability to the SI for the sulphur mass fractions in copper was established by an unbroken chain of comparisons, each accompanied by an uncertainty budget. Thus, the measurement results are considered reliable, acceptable and comparable within the stated measurement uncertainty. The metrological traceability chain from the kg down to mass fraction in the samples obtained by LA-ICP-IDMS is presented as well.
Quantification of metals in single cells by LA-ICP-MS comparison of single spot analysis and imaging
(2018)
LA-ICP-MS is increasingly used for single cell analysis in two different detection modes using either the imaging mode with subcellular resolution or alternatively single spot analysis of cells with a larger laser spot size. This study compares the analytical figures of merit of both detection modes (signal to noise, precision, accuracy, throughput), as well as ease of operation and data evaluation. Adherent 3T3 fibroblast cells were stained with two metal dyes (mDOTA-Ho, Ir-DNA-intercalator) and several dozen cells were measured using both modes. We found a ten times higher throughput for single spot analysis, which has as well a straightforward data analysis, shortening the total analysis time further. The signal to noise ratio for single spot analysis was found to be slightly better compared to the signal to noise of pixels in imaging. The mean metal intensity per single cell differed by only 10% between both modes and obtained distributions were found to show no statistically significant differences. Using matrix matched calibration based on standards spotted onto nitrocellulose membrane, we achieved detection limits (10 σ) of 12 fg for Ir and 30 fg for Ho and quantified 57 ± 35 fg Ir and 1,192 ± 707 fg Ho per single cell. Compared to a conventional ICP-MS measurement of a digest of ~60,000 cells, 54 % of Ir content and 358 % Ho content was found using quantitative LA-ICP-MS. The difference might be a consequence of the two metal dyes binding to different structures of the cell and therefore might behave differently in sample preparation for conventional and LA-ICP-MS.
LA-ICP-MS is increasingly used for single cell analysis in two different detection modes using either the imaging mode with subcellular resolution or alternatively single spot analysis of cells with a larger laser spot size. This study compares the analytical figures of merit of both detection modes (signal to noise, precision, accuracy, throughput), as well as ease of operation and data evaluation. Adherent 3T3 fibroblast cells were stained with two metal dyes (mDOTA-Ho, Ir-DNA-intercalator) and several dozen cells were measured using both modes. We found a ten times higher throughput for single spot analysis, which has as well a straightforward data analysis, shortening the total analysis time further. The signal to noise ratio for single spot analysis was found to be slightly better compared to the signal to noise of pixels in imaging. The mean metal intensity per single cell differed by only 10% between both modes and obtained distributions were found to show no statistically significant differences. Using matrix matched calibration based on standards spotted onto nitrocellulose membrane, we achieved detection limits (10s) of 12 fg for Ir and 30 fg for Ho and quantified 57 +/-35 fg Ir and 1192 +/- 707 fg Ho per single cell.
Compared to a conventional ICP-MS measurement of a digest of about 60000 cells, 54% of Ir content and 358% Ho content was found using quantitative LA-ICP-MS. The difference might be a consequence of the two metal dyes binding to different structures of the cell and therefore might behave differently in sample preparation for conventional and LA-ICP-MS.
The quantification of the sulphur mass fraction in pure copper and copper alloys by GDMS and LA-ICP-MS revealed a lack of traceability mainly due to a lack of suitable certified reference materials for calibrating the instruments. Within this study GDMS and LA-ICP-MS were applied as routine analytical tools to quantify sulphur in copper samples by applying reference materials as calibrators, which were characterized for their sulphur mass fraction by IDMS beforehand. Different external calibration strategies were applied including a matrix cross type calibration. Both techniques with all calibration strategies were validated by using certified reference materials (others than those used for calibration) and good agreement with the reference values was achieved except for the matrix cross type calibration, for which the agreement was slightly worse. All measurement results were accompanied by an uncertainty statement. For GDMS, the relative expanded (k = 2) measurement uncertainty ranged from 3% to 7%, while for LA-ICP-MS it ranged from 11% to 33% when applying matrix-matched calibration in the sulphur mass fraction range between 25 mg kg-1 and 1300 mg kg-1. For cross-type calibration the relative expanded (k = 2) measurement uncertainty need to be increased to at least 12% for GDMS and to at least 54% for LA-ICP-MS to yield metrological compatibility with the reference values. The so obtained measurement results are traceable to the international system of units (SI) via IDMS reference values, which is clearly illustrated by the unbroken chain of calibrations in the metrological traceability scheme.
Solution-doped metal powder pellets as well as aspirated liquids were used as calibration samples to analyze pure copper and zinc certified reference materials (CRMs) by femtosecond laser ablation ICP-MS. It was demonstrated that calibration by copper pellets resulted in relative deviations up to 20%, whereas fs-LA-ICP-MS among copper-based CRMs led to inaccuracies in the same range unless nominal mass fractions were chosen to be <3 mg/kg. Calibration by zinc pellets generally provided better accuracy. Depending on the analyte considered, deviations below 10% were obtained even for mass fractions close to the limit of quantification. Our data, therefore, indicate solution-doped metal powder pellets to be suitable as calibration samples for fs-LA-ICP-MS of metals. Furthermore, the utilization of liquid standards for calibration was found to result in stronger deviations of up to 50% for both copper and zinc samples which, in addition, turned out to be dependent on the plasma conditions.
A micro-droplet generator (µDG) sample introduction system was coupled to a sector field ICP-MS instrument to investigate the analytical figures of merit with respect to single cell analysis. The sector field instrument was operated for the first time in a fast scanning mode (E-scan) with the shortest time resolution of 100 µs to measure the single droplet time resolved and using the original detector in a pulse counting mode without modification of the existing electronics. For reduction of the droplet diameter a triple pulse mode of the droplet generator was applied and a droplet diameter down to 23 µm has been achieved for this investigation with a 100% transport efficiency of droplets. Signal duration times of single droplets of less than 500 µs have been measured. Overall detection efficiencies in the range of 10-3 counts per atom have been achieved and absolute limits of detection range between 120 ag for Fe and 1.1 ag for Mg as a mean value from 1000 droplet events.
We have applied a micro droplet generator (µDG) for sample introduction of single selenized yeast cells into a sector field ICP-MS, which was operated in a fast scanning mode with sampling rates of up to 10 kHz, to measure single cells time resolved with 100 µs integration time. Selenized yeast cells have been used as a model system for preliminary investigation. The single cells to be measured have been embedded into droplets and it will be shown that the time duration of a single cell event always is about 400 to 500 µs, and thus comparable to the time duration of a droplet without a cell. A fixed droplet generation rate of 50 Hz produced equidistant signals in time of each droplet event and was advantageous to separate contribution from background and blank from the analytical signal. Open vessel digestion and a multielement analysis were performed with washed yeast cells and absolute amounts per single cell were determined for Na (0.91 fg), Mg (9.4 fg), Fe (5.9 fg), Cu (0.54 fg), Zn (1.2 fg) and Se (72 fg). Signal intensities from single cells have been measured for the elements Cu, Zn and Se, and histograms were calculated for about 1000 cell events. The mean elemental sensitivities measured here range from 0.7 counts per ag (Se) to 10 counts per ag (Zn) with RSD's from 49% (Zn) to 69% (Se) for about 1000 cell events.
Three methods for direct solid sampling of bulk material namely IR laser ablation, glow discharge and spark OES, were compared with respect to analytical figures of merit obtained for elemental analysis with atomic spectrometry. Matrices investigated were copper, pressed doped copper powder, and magnesium alloys. For the vast majority of analytes, statistical equivalence regarding precision (usually ≤ 5%) and the performance of the calibrations between the compared methods was demonstrated.
In this work, different calibration strategies for the determination of trace elements in pure copper metal by nanosecond laser ablation ICP-MS were investigated. In addition to certified reference materials (CRMs), pellets of doped copper powder were used for calibration. The micro homogeneity of the CRMs as well as the solution-doped pellets was sufficient to use them as calibration samples in combination with a laser spot size of 200 µm. In contrast, pellets doped with analytes in solid form showed a significant heterogeneity. For most of the investigated analytes and copper CRMs the measured mass fractions were within ± 20% of their certified values when other copper CRMs were used as calibration samples. When solution-doped powder pellets were used as calibration samples a systematic trend towards mass fractions below the certified values was observed for nearly all elements determined in the analysed CRMs. Thermal fractionation effects during the ablation of the solution-doped pellets were suspected as the extent of the fractionation depends on the irradiance, whereas fractionation is reduced at higher irradiance.