Grouting is a universal repair and strengthening technique, which is constantly used for structural remediation of concrete components, trenches, mine subsidence, dam joints, restoration of masonry structures, and geological stabilizations. Having an extremely small particle size of only few microns, ultrafine cements are ideal for grouting applications due to their superior permeability and compressive strength properties of the hardened cement paste compared to that of the less-expensive, but coarser ordinary Portland cements. Supplementary cementitious materials (SCMs) are often used to replace ultrafine cement in order to modify certain properties and to reduce costs. The aim of this experimental study is to investigate the effect of three supplementary materials: microsilica (MS), fly ash (FA), and metakaolin (MK) on the workability, and mechanical properties of an ultrafine cement based grout with a constant water-binder ratio and constant superplasticizer content. Maximum percentages of replacement with ultrafine cement were 6% by volume of cement for MS and 16% for FA, and MK. In general, results suggest that the workability is improved by addition of FA, whereas is reduced, when modified with MS and MK. The compressive strength of grout after cement replacement remains comparable to that of pure cement grout. However, there is a tendency of the MS to positively affect the compressive strength opposite to FA, whereas flexural strength is positively affected by FA. Based on the results, it is evident that grouts with Hägerman cone flow more than 500 mm and compressive strength of more than 90 MPa after 28 days can be produced.
Synopsis: The paper presents the results of a study on the influence of agitation on the structural build-up of fresh cement pastes using a penetration test. It first presents results about the influence of the penetrating shape’s geometry on the influence on the cement paste specimen. Then, results are shown for the load-deflection curves depending upon time and agitation before testing. Based on the observation of the force required to penetrate the sample, conclusions on the structural build-up can be made. The observations were made over the course of time with samples that were left at rest and partly agitated before testing at different time steps. The setup allows to identify the contribution of the chemical reaction to the structural build-up process. The presence of superplasticizer obviously reduces the load that cement paste can withstand, while the loss of thixotropy is found notably lower than that of neat cement pates
Synopsis: Lately, there has been rising attention to superplasticizers (SP) based on polyphosphate esters. However, the influence of the molecular structure of the polyphosphate polymers on time-dependent properties such as structural build-up has not been examined yet intensively. To investigate this effect, three comb polyphosphate superplasticizers with different charge densities were synthesised by free radical polymerisation. Our findings indicate that SP with the lowest and medium charge densities extend the induction period more strongly than the SP with the highest charge density. The reduction of the structural build-up rate is linearly dependent on the dosage and concentration of the functional group of polyphosphate SP in the cementitious system. This study proposes a mathematical equation expressing the relationship between the structural build-up rate during the induction period and the molecular structure of the polyphosphate SP.
Structural build-up describes the stability and early-age strength development of fresh mortar used in 3D printing. lt is influenced by several factors, i.e. the composition of the print able material, the printing regime, and the ambient conditions. The existing modelling approaches for structural build-up usually define the model parameters for a specific material composition with out considering the influence of the ambient conditions. The goal of this contribution is to explicitly include the temperature dependency in the modelling approach. Temperature changes have signifi cant impact on the structural build-up process: an increase of the temperature leads to a faster dissol ution of cement phases and accelerates hydration. The proposed extended model includes temperature dependency using the Arrhenius theory. The new model parameters are successfully calibrated based on Viskomat measurement data using Bayesian inference. Furthermore, a higher impact of the temperature in the re-flocculation as in the structuration stage is observed.
Superplasticizer and Shrinkage Reducing Admixture Dosages for Microfine Cement in Grout Systems
(2019)
Grouts have numerous applications including crack repair as maintenance in construction industries. Microfine cements are intensively used for high strength mortar and grout products. They are ideal for injection grouting in structural repair. Such grouts should have suitable rheological properties to be injectable, especially those used in repair and rehabilitation. The use of superplasticizers (SP) in these products is thus becoming increasingly crucial to achieve favorable workability and viscosity properties. A difficulty in such grouts is the plastic shrinkage due to finer particles used. It is thus necessary to determine optimum SP and shrinkage reducing admixture (SRA) dosages for a microfine cement based grout. In this study, a saturation dosage was decided from two Polycarboxylate ether (PCE) based SPs in relation to neat cement using slump flow and rheological parameters. A range of grout mixtures was formulated containing micro silica (MS) and fly ash (FA), and tested for suitable rheological and mechanical parameters. Based on the results, a grout mixture with MS and FA was selected to determine optimum SRA content. According to the results, a SP dosage of 3% by weight of neat cement is sufficient to achieve saturation. The grout material including MS and FA can produce comparable properties to neat cement grout. MS is found to improve compressive strength within the range considered, whereas a higher FA content provides favourable rheological properties. Finally, a SRA dosage of 4%, which could reduce the shrinkage by about 43% after 28d days, is determined for the grout system.
Während für die Bauwirtschaft in den meisten Ländern der nördlichen Halbkugel die Instandhaltung bestehender Strukturen und Infrastruktur im Vordergrund steht, geht es in vielen Ländern der Südhalbkugel in der Hauptsache um die Schaffung von Bauwerken und Infrastruktur zur Verwirklichung angemessener Lebensbedingungen, was wiederum das schnelle Wirtschaftswachstum weiter befeuert.
Beton ist als Massenbaustoff, trotz landläufig anderer Bewertung, aufgrund seines im Vergleich zu anderen Baustoffen günstigen CO2-Footprints und der globalen Verfügbarkeit hierbei aktuell ohne Alternative. Allerdings ist Beton nach Wasser das am zweithäufigsten genutzte Produkt auf Erden [1] und die globale Nachfrage und Produktion steigt dramatisch. Dies hat Konsequenzen für das globale Klima, denn gerade die als Bindemittel eingesetzten Portlandzemente verursachen bei ihrer Herstellung selbst unter modernsten Produktionsbedingungen große Mengen an CO2.
Deshalb müssen für zukünftige nachhaltigere Technologien neuartige Betone entwickelt werden, die bei gleicher oder verbesserter Leistungsfähigkeit, einen geringeren Bedarf an Portlandzement aufweisen.
Um den CO2-Ausstoß, der mit der Betonherstellung verbunden ist zu minimieren, müssen Anteile an Portlandzement im Bindemittel reduziert und durch nachhaltigere Ersatzstoffe ausgetauscht werden. Darüber hinaus muss das eingesetzte Bindemittel im Beton so effizient wie möglich ausgenutzt werden. Das heißt, ein Bauteil oder Bauwerk sollte gerade so viel Bindemittel enthalten, wie für die Tragfähigkeit und Dauerhaftigkeit erforderlich ist. Hierfür erscheint der Einsatz von leistungsfähigen bauchemischen Produkten unumgänglich. Diese können zum einen die veränderten Verarbeitungseigenschaften, die Zementersatzstoffe mit sich bringen, ausgleichen und gleichzeitig helfen, den Gesamtwassergehalt zu minimieren, so dass das Bindemittel seine maximale Leistungsfähigkeit erzielt. Fließmittel sind aktuell die wichtigsten Zusatzmittel für Beton. Sie reduzieren den Wasserbedarf und ermöglichen, Zement im Beton effizienter auszunutzen. Darüber hinaus sind Stabilisierer wichtig zur Erhöhung der Robustheit, insbesondere im Hinblick auf die bautechnischen Herausforderungen der Zukunft – vom Pumpen über weite Distanzen, dem Spritzen, dem Betonieren bei extremen Klimabedingungen bis hin zum 3D-Druck.
Sustainability means meeting the needs of today without compromising the needs of the next generations. How can we meet the needs of the next generations, if we do not even know what these needs are? If we do not listen to the next generation and learn from them? Do we even meet the needs of today for everyone on earth?
In this paper, we demonstrate the value of 1H NMR relaxometry for studying the hydration of clinker-reduced, more climate-friendly cementitious binders. The results were obtained on typical CEM I cements and sister samples containing two different reactive agricultural ashes as well as non-reactive biochars as supplementary cementitious materials. The findings prove that time-resolved NMR measurements provide valuable additional information when combined with classical heat flow calorimetry.
Influence of the hydroxypropylation of starch on its performance as viscosity modifying agent
(2022)
Synopsis: Starch is a commonly used viscosity modifying agent (VMA). The performance of starch as VMA depends on its origin (e.g. potato, corn, cassava, etc.) and corresponding molecular properties, such as molecular weight, ratio between amylose and amylopectin etc. Depending upon the application, the efficiency of starch can be enhanced by hydroxypropylation. The maximum degree of substitution (DoS) cannot be greater than 3.0, which is the number of hydroxy groups per glucose monomer in the polymer. In the current research three potato starches exhibiting the DoS of 0.4, 0.6 and 0.8 were utilised. The influence of the modified starch on the rheological properties and hydration of cement paste, as well as the viscosity of the pore solution were investigated. Our findings show that the starch with the highest DoS increases the dynamic yield stress the most, while the plastic viscosity is less dependent on the DoS. Additionally, starch with the highest DoS retards hydration to lower degree than other starches.
The presence of polycarboxylate ether (PCE) based superplasticizers (SPs) has an enormous influence on the early hydration of cement. The hydration is retarded and the timing of formation and the morphology of hydrates is affected. This short paper presents experimental results about the influence of delayed addition time of PCE SPs on hydration of cement and alite pastes, investigated by isothermal heat flow calorimetry. For cement as well as for alite pastes the hydration is retarded with SP, whereby the high charge PCE has a stronger retarding effect than the low charge PCE. The retardation caused by PCE is much more pronounced for alite than for cement mixes. If PCE is added later to the mix, the induction period is shortened and the hydration is accelerated compared to simultaneous addition. This applies for cement and alite pastes. With delayed PCE addition the alite shows a clearly less retarded setting and main hydration than after simultaneous addition. It is obvious that for alite pastes there is less retardation the later the addition of SP.