Filtern
Dokumenttyp
- Zeitschriftenartikel (8)
- Beitrag zu einem Tagungsband (5)
- Corrigendum (3)
- Vortrag (1)
Schlagworte
- Welding (5)
- Creep-resistant steel (3)
- High entropy alloy (3)
- Stress relief cracking (3)
- High Entropy Alloy (2)
- High-entropy alloy (2)
- Medium entropy alloy (2)
- Post weld heat treatment (2)
- Residual stresses (2)
- Austenitic stainless steel (1)
Organisationseinheit der BAM
- 9 Komponentensicherheit (14)
- 9.2 Versuchsanlagen und Prüftechnik (14)
- 9.0 Abteilungsleitung und andere (11)
- 9.4 Integrität von Schweißverbindungen (7)
- 5 Werkstofftechnik (1)
- 5.1 Mikrostruktur Design und Degradation (1)
- 6 Materialchemie (1)
- 6.2 Material- und Oberflächentechnologien (1)
- 8 Zerstörungsfreie Prüfung (1)
- 8.5 Röntgenbildgebung (1)
Eingeladener Vortrag
- nein (1)
For higher operational temperatures and pressures required in petrochemical plants, the modified 13CrMoV9-10 steel was developed providing high resistance against creep and compressed hydrogen. Extreme care during the welding procedure is necessary for this steel, attributed to low toughness, high strength in as-welded state, and increased susceptibility to stress relief cracking (SRC) during post-weld heat treatment (PWHT). Previous research of SRC in creep-resistant steels discussed mainly thermal and metallurgical factors. Few previous findings addressed the influences of welding procedure on crack formation during PWHT considering real-life manufacturing conditions. These investigations focus on effects of welding heat control on stresses during welding and subsequent PWHT operations close to realistic restraint and heat dissipation conditions using a special 3D testing facility, which was presented in parts I and II of this contribution. Part III addresses investigations on residual stress evolution affecting crack formation and discusses the transferability of results from large-scale testing to laboratory-scale. Experiments with test set-ups at different scales under diverse rigidity conditions and an assessment of the residual stresses of the weld-specimens using X-ray (surface near) and neutron diffraction analysis (bulk) were performed. This study aims to provide a way of investigating the SRC behaviour considering component-specific residual stresses via small-scale testing concepts instead of expensive weld mock-ups.
Hoch- und Mittelentropie-Legierungen (engl. High/Medium Entropy Alloys–HEA/MEA) sind relativ neue Werkstoffklassen. Im Gegensatz zu herkömmlichen Le-gierungen bestehen HEA aus fünf bzw. MEA aus drei oder vier Legierungselementen im äquiatomaren Gleichgewicht. Viele HEA weisen aufgrund hervorragender struktu-reller Eigenschaftskombinationen von sehr tiefen bis zu hohen Temperaturen enor-mes Anwendungspotential auf. Die Anwendung für reale Bauteile stellt jedoch die zentrale Frage der Eignung für die fügetechnische Verarbeitung. Dieser Aspekt findet in der weltweiten Materialforschung bisher kaum Beachtung. Anforderungen an die zuverlässige und sichere fügetechnische Verarbeitung dieser Werkstoffe sind von wesentlicher Bedeutung hinsichtlich wirtschaftlicher Bauteilfertigung für spätere po-tenzielle Anwendungsbereiche, bspw. in der Energietechnik. Das Rührreibschweißen (engl. Friction Stir Welding–FSW) stellt hierbei einen vielversprechenden Fügepro-zess dar, dessen Hauptvorteil in der Schweißprozesstemperatur unterhalb der Schmelztemperatur der zu fügenden Werkstoffe liegt. Dies bedingt die Vermeidung der Ausbildung von harten, versprödenden intermetallischen Phasen, wie sie z. B. beim konventionellen Schmelzschweißen von Eisen-Aluminium-Verbindungen auf-treten. Die vorliegende Arbeit stellt grundlegende Untersuchungen zur Schweißbar-keit einer CoCrFeMnNi-Legierung (HEA) und einer CoCrNi-Legierung (MEA) mit dem FSW-Prozess vor. Die Versuchsschweißungen werden mittels mikroskopischer Analysen hinsichtlich des Schweißnahtaufbaus sowie Schweißnahtfehlern charakte-risiert. FSW zeigt sich als grundlegend geeignet zur Verbindungsschweißung der HEA bzw. MEA. Anhand dieser Ergebnisse kann eine weitere Bewertung der Schweißbar-keit erfolgen.
High Entropy Alloys (HEAs) are a recent class of materials. In contrast to conventional alloys, HEAs consist of five alloying elements in equiatomic equilibrium. The high entropy effect is due, among other things, to the increased configuration entropy, which promotes solid solution formation. Many HEAs have enormous application potential due to excellent structural property combinations from very low to high temperatures. For the introduction of HEAs in real components, however, the question of the applicability of machining production technologies for component manufacture is of central importance. This has so far received Little attention in global materials research. Reliable and safe processing is essential for the demand of economical component production for potential areas of application, e.g. in power plant technology.
For metals, milling is the standard machining process. This article presents the results of machining analyses. It focuses on the surface integrity resulting from the milling process on a Co20Cr20Fe20Mn20Ni20-HEA. For this purpose, investigations were carried out using ball nose end milling tools for conventional milling process in comparison to an innovative hybrid process available at BAM Berlin, Ultrasonic-Assisted Milling (USAM). USAM promises a lower Degradation of the surface properties due to lower loads on the workpiece surface during machining.
For this purpose, basic milling parameters (cutting speed and tooth feed) were systematically varied and cutting forces were measured during the milling experiments. The subsequent Analysis of these forces allows an understanding of the mechanical loads acting on the tool and component surface. These loads cause topographical, mechanical and microstructural influences on the surface and consequently on the surface integrity. For their characterization, light and scanning electron microscopy were used, and the roughness and residual stresses via X-ray diffraction were measured. The results indicate significant advantages using USAM, especially due to reduced cutting forces compared to the conventional milling process. This causes lower mechanical loads on the tool and surface, combined with lower tensile residual stresses on and below the surface, and ultimately results in a significantly enhanced surface integrity.
High entropy alloys (HEA) are a new class of materials. In contrast to conventional alloys, HEA are single-phase alloys with at least five alloying elements. HEAs have enormous application potential due to (postulated) excellent structural property combinations from low to high temperatures. For HEA-application as structural materials in real components, a key issue is the suitability for joining processing. Requirements for the reliable and safe joining of these materials are crucial regarding economical component manufacture for future applications. In this context, friction stir welding (FSW) is a promising joining process due to the welding process temperature below the material melting point avoiding major issues, e. g. formation of (hard and brittle) intermetallic phases, which may have detrimental influences on the weld joint properties.
This study presents elementary research about the FSW process influences on a CoCrFeMnNi-HEA with focus on the microstructure and mechanical properties. For that purpose, the FSW joint of the HEA is compared to that of an austenitic stainless steel AISI 304. The microstructures of the welds were investigated and characterized by means of light microscopy, SEM, EBSD and XRD. Hardness and tensile testing were applied to determine influences on the mechanical properties. Generally, a comparable weldability of HEA and AISI 304 in terms of metallurgical characteristics and resulting mechanical properties exhibited. For the weld joints of both materials typical characteristics regarding FSW were observed within the weld metal and thermo-mechanically influenced zone: fine-grained stirred zone with increased hardness and reduced fracture elongation compared with the respective base material.
The new alloying concept of multi-element systems with defined entropy (HEA—high-entropy alloy; MEA—medium-entropy alloy) is gaining increasing importance in materials research. Significantly improved properties or combinations of properties are shown by some HEA/MEA systems. Thus, primarily the production and resulting microstructures of HEA, as well as its properties, have been investigated so far. Furthermore, processing is a main issue in transferring HEA systems from the laboratory to real components. Since welding is the most important joining process for metals, it is crucial to investigate the influence of welding to guarantee component integrity. Welding leads to residual stresses, which significantly affect the component integrity. Hence, the focus of this study is the residual stress formation and distribution in a CoCrFeMnNi HEA and ternary CoCrNi MEA using two different welding processes: tungsten inert gas (TIG) welding and solid-state friction stir welding (FSW). As a pathway for the application of HEA in this investigation, for the first time, residual stress analyses in realistic near-component specimens were performed. The residual stresses were determined by X-ray diffraction (XRD) on the surfaces of top and root weld side. The results were correlated with the local welding microstructures. The results show that both FSW and TIG generate significant tensile residual stresses on the weld surfaces in, and transverse to, the welding direction. In the case of FSW of the CoCrFeMnNi HEA, the longitudinal residual stresses are in the range of the yield strength of approx. 260 MPa in the weld zone.
Multielement-Legierungen (MPEA – multiple pricipal element alloys) stellen eine neue Klasse von Werkstoffen dar, die aus mindestens drei äquiatomaren Legierungselementen mit jeweils einem Gehalt von 5–35 Atom-% bestehen. Somit unterscheidet sich das Legierungskonzept fundamental von konventionellen bspw. Stahl- oder Al-basierten Legierungen. In jüngster Zeit lag der Schwerpunkt auf dem Legierungs-Design der MPEA und der Überprüfung bzw. Erreichung der gewünschten Eigenschaften bzw. -kombinationen. Hierzu werden die egierungselemente gezielt ausgewählt und die Mikrostrukturen ein- und zum Teil auch mehrphasig eingestellt. Ziel sind hochinnovative MPEA mit angepassten Eigenschaften für die industrielle Anwendung. Dabei sollen insbesondere die bei konventionellen Legierungen wesentlichen Zielkonflikte, wie bspw. der Trade-off zwischen Festigkeit und Duktilität, überwunden werden. Darüber hinaus sind mechanische Eigenschaften bei sehr hohen sowie kryogenen Temperaturen bei gleichzeitig höchster Korrosionsbeständigkeit von hohem Interesse. Die Herstellung von Bauteilen erfordert dazu werkstoff- und beanspruchungsgerechte Füge- bzw. Schweißverfahren. Der Schweißeignung von MPEA wurde bis Ende 2021 nur äußert wenig Aufmerksamkeit zuteil. Die Auswirkungen durch Schweißprozesse auf die Metallurgie und die gewünschten Eigenschaften sind bisher kaum bekannt und limitieren die potenzielle Anwendbarkeit als Funktions- oder Konstruktionswerkstoffe.
In einem interdisziplinären BAM-Forschungsprojekt werden aktuell grundlegende Untersuchungen zur Schweißverarbeitung und resultierender Mikrostruktur-Anwendungseigenschafts-Beziehung verschiedener MPEA durchgeführt. Insbesondere Wärmeeinflusszone und Schweißgut sind geprägt durch eine Mikrostruktur, die aus Ungleichgewichtszuständen resultiert. Im Falle von MPEA wurde dies bisher nicht systematisch untersucht. Dazu erfolgte im Rahmen des Projektes eine umfassende Literaturauswertung zum Schweißen von MPEA und Zusammenfassung in einer umfassenden, systematischen Datenbasis. Aus diesem Grund sollen in der vorliegenden Studie die bisher bedeutsamsten Erkenntnisse zur Schweißbarkeit von MPEA systematisch nach MPEA-Typ und Schweißverfahren geordnet und mit eigenen aktuellen Forschungsergebnissen verglichen werden. Durch WIG- und Rührreibschweißversuche an den MPEA-Systemen CoCrNiFeMn bzw. CoCrNi konnten im Projektverlauf bereits wesentliche Fragestellungen beantwortet werden. Dazu zählen Auftreten bzw. Verhinderung intermetallischer Phasen/Seigerungen oder deren Auswirkung auf die Eigenschaften der Schweißverbindung (bspw. Festigkeit oder Korrosionsbeständigkeit).
Influence of Surface Preparation on Cracking Phenomena in TIG-Welded High and Medium Entropy Alloys
(2022)
Multi-element systems with defined entropy (HEA—high entropy alloy or MEA—medium entropy alloy) are rather new material concepts that are becoming increasingly important in materials research and development. Some HEA systems show significantly improved properties or combinations of properties, e.g., the overcoming of the trade-off between high strength and ductility. Thus, the synthesis, the resulting microstructures, and properties of HEA have been primarily investigated so far. In addition, processing is crucial to achieve a transfer of potential HEA/MEA materials to real applications, e.g., highly stressed components. Since fusion welding is the most important joining process for metals, it is of vital importance to investigate the weldability of these materials. However, this has rarely been the subject of research to date. For that reason, in this work, the weldability depending on the surface preparation of a CoCrFeMnNi HEA and a CoCrNi MEA for TIG welding is investigated. The fusion welding of longer plates is described here for the first time for the CoCrNi alloy. The welds of both materials showed distinct formation of cracks in the heat affected Zone (HAZ). Optical and scanning electron microscopy analysis clearly confirmed an intergranular fracture topography. However, based on the results, the crack mechanism cannot be conclusively identified as either a liquid metal embrittlement (LME) or hot cracking-like liquid film separation.
The new multi-element alloying concept of systems with defined entropy (HEA — high-entropy alloy or MEA — medium-entropy alloy) is increasing in material research interest. Improved properties or combinations of properties are shown by several systems. Thus, the resulting microstructures and production of HEA/MEA as well as properties have been primarily investigated so far. Furthermore, processing is a key issue to transfer HEA/MEA systems to real components. Since welding is the most important joining process for metals, it is crucial to investigate the influence of welding to guarantee component integrity. Since most HEA are made of expensive alloying elements such as Co or Ni, they will not be used entirely as structural materials. Thus, it can be advantageous to weld conventional alloys such as austenitic stainless steels with the HEA and MEA to produce components that are both application-oriented and economically viable. Therefore, in this paper, first results of dissimilar metal welding, by tungsten inert gas (TIG) and friction stir welding (FSW), of a CoCrFeMnNi HEA as well as a CoCrNi MEA with a conventional AISI 304 austenitic stainless steel are presented. The focus is on the microstructure formation due to the two welding processes. The results of TIG welding show a dendritic microstructure, whereas in FSW both materials are stirred but still coexist.
Medium and High Entropy Alloys (MEA/HEA) are recently developed material classes, providing manifold applications, e.g., due to extraordinary structural properties. In that connection, the machinability as important issue for the processing of these materials was not in the scientific focus. This study focusses on experimental analysis of milling process conditions including ultrasonic assisted milling (USAM) and their effects on the resulting surface integrity of equiatomic CoCrFeNi-MEA specimens. For that reason, milling parameters (cutting speed, feed per cutting edge) were systematically varied for both conventional milling and USAM. The surface integrity was analyzed in terms of topography, defects, and residual stresses. Especially USAM leads to a decrease of occurring cutting forces and, hence, to an improvement of the surface integrity. Beneficial effects were observed in terms of lower tensile residual stresses at high cutting speed and feed per cutting edge.