Filtern
Erscheinungsjahr
Dokumenttyp
Sprache
- Englisch (420) (entfernen)
Schlagworte
- Laser beam welding (94)
- Welding simulation (26)
- Resistance spot welding (22)
- Solidification cracking (21)
- Laser metal deposition (20)
- Additive manufacturing (19)
- Microstructure (16)
- Numerical simulation (16)
- Mechanical properties (15)
- Laser welding (14)
Organisationseinheit der BAM
- 9 Komponentensicherheit (182)
- 9.3 Schweißtechnische Fertigungsverfahren (177)
- 9.6 Additive Fertigung metallischer Komponenten (3)
- 5 Werkstofftechnik (2)
- 5.2 Metallische Hochtemperaturwerkstoffe (2)
- 7 Bauwerkssicherheit (2)
- 7.7 Modellierung und Simulation (2)
- 9.0 Abteilungsleitung und andere (2)
- 5.5 Materialmodellierung (1)
Eingeladener Vortrag
- nein (25)
Fusion welding processes are widely used for joining metal structures, such as pipes, ships, and cars. In general, these joining processes offer a very good compromise between reliability, safety, cost and maintenance which are important issues in the current economical context. The negative heat effects of welding, i.e. distortions and residual stresses of the welded parts, are well known and many researches in this field have already been done in the last decades in order to minimize them. On the experimental side, many sophisticated procedures have become state of the art to deal with this problem. On the computational side, the improvement of the simulation algorithms and the computing power enables the simulations of many physical phenomena occurring during the welding process. The implementation of welding simulation techniques is nevertheless not an easy task and often associated with expert knowledge which hinders their global application in an industrial environment. This paper is focused on the industrial requirements of a welding simulation software with special respect to the needs of the automotive industry. The necessary information to run a welding simulation and the expectations of a weld specialist without deep knowledge in numerical methods are investigated. These expectations are tested on an automotive welded assembly with a commercially available welding simulation software designed especially for the needs of the automotive industry. A welding experiment is done and the measured temperature distributions and distortions serve as reference to validate the simulation results. The result quality of the simulations of temperature fields and distortions is in best agreement with experimental data. The workflow is well adapted for the considered industrial requirements and the time-tosolution as well as the computational costs are acceptable, whereas the efficient calibration of the heat input model is still a point which will be further investigated in current and future research works.
Evaluating innovative process technologies has become highly important within the last decades. As standard tools different Life Cycle Assessment methods have been established, which are continuously improved. While those are designed for evaluating single processes they run into difficulties when it comes to assessing environmental impacts of process innovations at macroeconomic level. In this paper we develop a multi-step evaluation framework building on multi regional inputeoutput data that allows estimating macroeconomic impacts of new process technologies, considering the network characteristics of the global economy.
Our procedure is as follows: i) we measure differences in material usage of process alternatives, ii) we identify where the standard processes are located within economic networks and virtually replace those by innovative process technologies, iii) we account for changes within economic systems and evaluate impacts on emissions.
Within this paper we exemplarily apply the methodology to two recently developed innovative technologies: longitudinal large diameter steel pipe welding and turning of high-temperature resistant materials. While we find the macroeconomic impacts of very specific process innovations to be small, its conclusions can significantly differ from traditional process based approaches. Furthermore, information gained from the methodology provides relevant additional insights for decision makers extending the picture gained from traditional process life cycle assessment.
Due to rapid, localized heating and cooling, distortions accumulate in additive manufactured laser metal deposition (LMD) components, leading to a loss of dimensional accuracy or even cracking. Numerical welding simulations allow the prediction of these deviations and their optimization before conducting experiments. To assess the viability of the simulation tool for the use in a predictive manner, comprehensive systems as well as to choose the optimal product matches, product analysis methods are needed. Indeed, most of the known methods aim to analyze a product or one product family on the physical level. Different product families, however, may differ largely in terms of the number and nature of components. This fact impedes an efficient comparison and choice of appropriate product family combinations for the production system. A new methodology is proposed to analyze existing products in view of their functional and physical architecture. The aim is to Cluster these products in new assembly oriented product families for the optimization.
Hot crack assessment during production and processing of metallic materials is an essential prerequisite for the safety of welded structures. The hot cracking investigations presented here were carried out as part of a study aimed at the development of Cr/Ni low transformation temperature filler materials. Low transformation temperature alloys open up the possibility for welding high strength steels. The externally loaded Modified Varestraint Transvarestraint hot cracking test was employed in the experiments described. The hot cracking resistance was evaluated with the help of light microscopy applied at the specimen surface. The proportionality between hot cracking susceptibility and Cr/Ni alloy content was explained by the altered solidification kinetics and by the enlarged solidification interval. The internal crack paths and the three-dimensional structure of the crack net in the material volume were examined using X-ray computer tomography. The total crack lengths for different material depths and circumjacent rectangular volumes, respectively, were be determined. An increasing hot cracking susceptibility with increasing Cr/Ni alloy content was also be established for the specimen volume.
A numerical framework for simulation of the steady-state thermal behaviour in keyhole mode welding has been developed. It is based on the equivalent heat source concept and consists of two parts: computational thermo-fluid dynamics and heat conduction. The solution of the thermo-fluid dynamics problem by the finite element method for a bounded domain results in a weld pool interface geometry being the input data for a subsequent heat conduction problem solved for a workpiece by a proposed boundary element method. The main physical phenomena, such as keyhole shape, thermo-capillary and natural convection and temperature-dependent material properties are taken into consideration. The developed technique is applied to complete-penetration keyhole laser beam welding of a 15 mm thick low-alloyed steel plate at a welding speed of 33 mm/s and a laser power of 18 kW. The fluid flow of the molten metal has a strong influence on the weld pool geometry. The thermo-capillary convection is responsible for an increase of the weld pool size near the plate surfaces and a bulge formation near the plate middle plane. The numerical and experimental molten pools, cross-sectional weld dimensions and thermal cycles of the heat affected zone are in close agreement.
Offshore wind energy plays an important role for the desired transition towards a carbon dioxide free industry within the next decades. However, the grounding of the offshore wind plants governs the overall installation process besides bureaucratic bottlenecks.
The application of lightweight principles in steel construction, e.g. the usage dissolved load-bearing structures, so called Jackets foundations, offer great potential in reducing the resource consumption, especially with respect to the needed amount of steel.
In this context this paper focuses on a fully digitalization of the welding manufacturing and as well as testing chain to enable a fully automated manufacturing as well as quality assessment of tubular nodes as key element of Jackets foundation structures. Furthermore, the relationship between the seam shape geometry and resulting fatigue strength is evaluated by numerical methods incorporating bionic principles. It is shown that tubular nodes can be welded fully automatically taking geometry tolerances into account. Moreover, the seam shape could be manufactured as requested by the numerical models which offers great potential for an extended lifetime. Subsequently, the improvements in resource efficiency and reduction of carbon dioxide emissions are evaluated by a life-cycle-assessment.
In additive manufacturing (AM) Laser Metal Deposition (LMD), parts are built by welding layers of powder feedstock onto a substrate. Applications for steel powders include forging tools and structural components for various industries. For large parts, the choice of tool-paths influences the build-rate, the part performance and the distortions in a highly geometry-dependent manner. With weld-path lengths in the range of hundreds of meters, a reliable, automated tool path generation is essential for the usability of LMD processes.
In this contribution, automated tool-path generation approaches are shown and their results are discussed for arbitrary geometries. The investigated path strategies are the classical approaches: “Zig-zag-” and “contour-parallel-strategies”. After generation, the tool-paths are automatically formatted into g-code for experimental build-up and ASCII for a numerical simulation model. Finally, the tool paths are discussed in regards to volume-fill, microstructure and porosity for the experimental samples.
This work presents a part of the IGF project 18737N “Welding distortion simulation” (FOSTA P1140)
In additive manufacturing (AM) directed energy deposition (DED), parts are built by welding layers of powder or wire feedstock onto a substrate with applications for steel powders in the fields of forging tools, spare parts, and structural components for various industries. For large and bulky parts, the choice of toolpaths influences the build rate, the mechanical performance, and the distortions in a highly geometry-dependent manner. With weld-path lengths in the range of hundreds of meters, a reliable, automated tool-path generation is essential for the usability of DED processes. This contribution presents automated tool-path generation approaches and discusses the results for arbitrary geometries. Socalled “zig-zag” and “contour-parallel” processing strategies are investigated and the tool-paths are automatically formatted into machine-readable g-code for experimental validation to build sample geometries. The results are discussed in regard to volume-fill, microstructure, and porosity in dependence of the path planning according to photographs and metallographic cross-sections.
To increase the competitiveness of jacket substructures compared to monopiles a changeover from an individual towards a serial jacket production based on automated manufactured tubular joints combined with standardized pipes has to be achieved. Therefore, this paper addresses fatigue tests of automatically welded tubular X-joints focusing on the location of the technical fatigue crack. The detected location of the technical crack is compared to numerical investigations predicting the most fatigue prone notch considering the structural stress approach as well as the notch stress approach. Besides, the welding process of the automated manufactured tubular X-joints is presented.
To increase the competitiveness of jacket substructures compared to monopiles a changeover from an individual towards a serial jacket production based on automated manufactured tubular joints combined with standardized pipes has to be achieved. Therefore, this paper ad-dresses the welding process of automated manufactured tubular X-joints. Additionally, fatigue tests of the automatically welded tubular joints are presented focusing on the location of the technical fatigue crack. The detected location of the technical crack is compared to numerical investigations predicting the most fatigue prone notch con-sidering the structural stress approach as well as the notch stress ap-proach.
To increase the competitiveness of jacket substructures compared to monopiles a changeover from an individual towards a serial jacket production based on automated manufactured tubular joints combined with standardized pipes has to be achieved. Therefore, this paper addresses fatigue tests of automatically welded tubular X-joints focusing on the location of the technical fatigue crack. The detected location of the technical crack is compared to numerical investigations predicting the most fatigue prone notch considering the structural stress approach as well as the notch stress approach. Besides, the welding process of the automated manufactured tubular X-joints is presented.
The present work deals with the development of a strategy for the prevention of end crater defects in high-power laser welding of thick-walled circumferential welds. A series of experiments were performed to understand the influence of the welding parameters on the formation of end crater defects such as pores, cracks, excessive root-side drop-through and shrinkage cavities in the overlap area. An abrupt switch-off of the laser power while closing the circumferential weld leads to a formation of a hole which passes through the whole welded material thickness. A laser power ramp causes solidification cracks which are initiated on the transition from full-penetration mode to partial penetration. Strategies with a reduction of the welding speed shows a creation of inadmissible root sagging. Defocusing the laser beam led to promising results in terms of avoiding end crater defects. Cracks and pores in the overlap area could be effectively avoided by using defocusing techniques. A strategy for avoiding of end crater imperfections was tested on flat specimens of steel grade S355J2 with a wall thickness of 10 mm and then transferred on the 9.5 mm thick pipe sections made of high-strength steel X100Q.
The present work deals with the development of a strategy for the prevention of end crater defects in high-power laser welding of thick-walled circumferential welds. A series of experiments were performed to understand the influence of the welding Parameters on the formation of end crater defects such as pores, cracks, root excess weld metal and shrinkage cavities in the overlap area. An abrupt switch-off of the laser power while closing the circumferential weld leads to a formation of a hole which passes through the whole welded material thickness. A laser power ramp-down causes solidification cracks which are initiated on the transition from full-penetration mode to partial penetration. Defocusing the laser beam led to promising results in terms of avoiding end crater defects. Cracks and pores in the overlap area could be effectively avoided by using defocusing techniques.
A strategy for avoiding of end crater imperfections was tested on flat specimens of steel grade S355J2 with a wall thickness of between 8 mm and 10 mm and then transferred on the 10 mm thick pipe sections made of high-strength pipeline steel API5L-X100Q.
Liquid metal embrittlement (LME) cracking can occur during resistance spot welding (RSW) in zinc-coated advanced high-strength steels (AHSS) for automotive production. In this study, a methodological variation of hold time is performed to investigate the process-related crack influence factors. A combination of numerical and experimental investigations confirms, that the extent of heat dissipation and re-heating of the sheet surface can be influenced and thus the degree of crack formation can be controlled in a targeted manner by the parameterisation of the hold time. The temperature and stress history of crack-free and crack-afflicted spot welds are analysed and a conclusion on the borders defining the LME active region is derived.
Laser metal deposition (LMD) has been applied as a coating technology for many years. Today, the technologies capacity to produce 3D depositions leads to a new field of application as additive manufacturing method. In this paper, 3D laser metal deposition of titanium alloy Ti-6Al-4V is studied with special regard to the demands of additive manufacturing. Therefore, only the coaxial LMD powder nozzle is used to create the shielding gas atmosphere, which ensures high geometric flexibility. Furthermore, specimen with high aspect ratio and hundreds of layers are manufactured, which represent typical features in additive manufacturing. The presented study contains the following steps: First, cylindrical specimens are manufactured with a standard shell-core build-up strategy and mechanical properties as well as fracture mechanisms are determined. Based on the results, experiments are conducted to improve the build-up strategy and new tensile test specimens are built with the improved strategy. The improved strategy incorporates variable track overlap ratios to achieve a constant growth in the shell and core area. As blanks, lean cylinders comprising more than 240 layers and a height of more than 120mm are manufactured. The specimens are analyzed by X-ray inspection for material defects. Fractured surfaces are observed via scanning electron microscopy and the composition of the surfaces is determined using energy dispersive X-ray spectroscopy. The tensile test results prove mechanical properties close to ASTM F1108 specification for wrought material.
Laser metal deposition (LMD) has been applied as coating technology for many years. Today, the technologies capacity to produce 3D depositions leads to a new field of application as additive manufacturing method. In this paper, 3D laser metal deposition of titanium alloy Ti-6Al-4V is studied with special regard to the demands of additive manufacturing. Therefore, only the powder nozzle is used to create the shielding gas atmosphere, which ensures high geometric flexibility. Furthermore, specimen with high aspect ratio and hundreds of layers are manufactured, which represent typical features in additive manufacturing.
Build-up strategies for generating components of cylindrical shape with laser metal deposition
(2015)
Laser Metal Deposition LMD) as additive manufacturing process offers the potential to produce near net shape components. This reduces the amount of material and post-processing. The components are composed of individual layers. Already mall irregularities within a layer can add up over multiple layers and lead to error propagation. This paper deals with the issue of build-up strategies to minimize irregularities and prevent error propagation. Different travel paths and the influence of a changing starting point regarding to error propagation are discussed. Different deposition rates between core and peripheral area are detected and successfully compensated by adjusting the build-up sequence. Stainless steel and titanium alloy Ti-6Al-4V are used in the experiments. The results are intended to illustrate the potential of an adjusted build-up strategy and provide basic information on the way to an automated deposition process. This paper is of interest for engineers in industry or science using LMD as additive manufacturing process.
Laser Metal Deposition (LMD) as a technology for additive manufacturing allows the production of large components outside of closed working chambers. Industrial applications require a stable process as well as a constant deposition of the filler material in order to ensure uniform volume growth and reproducible mechanical properties. This paper deals with the influence of travel path strategies on temperature profile and material deposition. Meandering and spiral hatching strategies are used in the center as well as in the edge of a specimen. The temperature is measured with thermocouples attatched to the backside of the specimen. The tests are carried out on the materials S235JR and 316L. The results show a strong dependence of the maximum temperatures on the travel path strategy and the welding position on the component.