Filtern
Erscheinungsjahr
Dokumenttyp
- Zeitschriftenartikel (64)
- Beitrag zu einem Tagungsband (11)
- Sonstiges (1)
- Posterpräsentation (1)
Schlagworte
- Computed tomography (8)
- Electron tomography (8)
- Fuel cell (8)
- Neutron tomography (8)
- Radiography (8)
- Neutron imaging (7)
- Tomography (7)
- Water transport (7)
- Polymer electrolyte membrane fuel cell (PEMFC) (6)
- DIRECTT (5)
Organisationseinheit der BAM
Paper des Monats
- ja (1)
Neutron Bragg-edge imaging was applied for the visualization of a γ-Austenite to α'-martensite phase transformation. In the present study, a super martensitic
stainless steel sample was heated until complete austenitization and was subsequently cooled down to room temperature. The martensitic phase Transformation started at Ms = 190 °C. Using a monochromatic neutron beam with λ = 0.390 nm, the transmitted intensity was significantly reduced during cooling below Ms, since the emerging martensitic phase has a higher attenuation coefficient than the austenitic phase at this wavelength. The phase Transformation process was visualized by filming the transmission images from a scintillator screen with a CCD camera with a temporal resolution of 30 s and a spatial
resolution of 100 µm.
Herein, we present a detailed investigation of the electrochemically triggered formation and dissolution processes of α- and β-sulfur crystals on a monolithic carbon cathode using operando high-resolution synchrotron radiography (438 nm/pixel).
The combination of visual monitoring with the electrical current response during cyclic voltammetry provides valuable insights into the sulfur formation and dissolution mechanism. Our observations show that the crystal growth process is mainly dictated by a rapid equilibrium between long-chain polysulfides on one side and solid sulfur/short-chain polysulfides on the other side, which is consistent with previous studies in this field. The high temporal and spatial resolution of synchrotron imaging enables the observation of different regimes during the sulfur formation and dissolution process. The appearance of short-chain polysulfides after the first anodic CV peak initiates a rapid dissolution process of α-sulfur crystals on the cathode. The increase in the long-chain lithium polysulfide concentration at the cathode surface during charge results in an increased crystal growth rate, which in turn produces imperfections in α- and β-sulfur crystals. There are strong indications that these defects are fluid inclusions, which may trap dissolved polysulfides and therefore reduce the electrochemical cell capacity.
A strategy to mitigate typical reconstruction artefacts in missing wedge computed tomography is presented. These artefacts appear as elongations of reconstructed details along the mean direction (i.e. the symmetry centre of the projections). Although absent in standard computed tomography applications, they are most prominent in advanced electron tomography and also in special topics of X-ray and Neutron tomography under restricted geometric boundary conditions. We investigate the Performance of the DIRECTT (Direct Iterative Reconstruction of Computed Tomography Trajectories) algorithm to reduce the directional artefacts in standard procedures. In order to be sensitive to the anisotropic nature of missing wedge artefacts, we investigate isotropic substructures of metal foam as well as circular disc models. Comparison is drawn to filtered backprojection and algebraic techniques. Reference is made to reconstructions of complete data sets. For the purpose of assessing the reconstruction Quality, Fourier transforms are employed to visualize the missing wedge directly. Deficient reconstructions of disc models are evaluated by a length-weighted boundary orientations. The DIRECTT results are assessd at different signal-to-noise ratios by means of local and integral evaluation Parameters.
The potentials of incoherent X-ray scattering (Compton) computed tomography (CT) are investigated. The imaging of materials of very different atomic number or density at once is generally a perpetual challenge for X-ray tomography or radiography. In a basic laboratory set-up for simultaneous perpendicular Compton scattering and direct beam attenuation tomography are conducted by single channel photon counting line scans. This results in asymmetric distortions of the projection profiles of the scattering CT data set. In a first approach, corrections of Compton scattering data by taking advantage of rotational symmetry yield tomograms without major geometric artefacts. A cylindrical sample composed of PE, PA, PVC, glass and wood demonstrates similar Compton contrast for all the substances, while the conventional absorption tomogram only reveals the two high order materials. Comparison to neutron tomography
reveals astonishing similarities except for the glass component (without hydrogen). Therefore, Compton CT offers the potential to replace neutron tomography, which requires much more efforts.
In various kinds of radiography, deficient transmission imaging may occur due to backlighting inside the detector itself arising from light or radiation scattering. The related intensity mismatches barely disturb the high resolution contrast, but its long range nature results in reduced attenuation levels which are often disregarded. Based on X-ray observations and an empirical formalism, a procedure is developed for a first order correction of detector backlighting. A backlighting factor is modeled as a function of the relative detector coverage by the sample projection. Different cases of sample transmission are regarded at different backlight factors and detector coverage. The additional intensity of backlighting may strongly affect the values of materials’ attenuation up to a few 10%. The presented scenario provides a comfortable procedure for corrections of X-ray or neutron transmission imaging data.
The understanding of dynamic processes in Li-metal batteries is an important consideration to enable the full capacity of cells to be utilised. These processes, however, are generally not directly observable using X-ray techniques due to the low attenuation of Li; and are challenging to visualise using neutron imaging due to the low temporal resolution of the technique. In this work, complementary X-ray and neutron imaging are combined to track the dynamics of Li within a primary Li/SOCl2 cell. The temporal challenges posed by neutron imaging are overcome using the golden ratio imaging method which enables the identification of Li diffusion in operando. This combination of techniques has enabled an improved understanding of the processes which limit rate performance in Li/SOCl2 cells and may be applied beyond this chemistry to other Li-metal cells.
Spectral neutron tomography
(2021)
Combined three-dimensional (3D) mapping of (micro-)structures with elemental and crystalline phase variations is of significant importance for the characterization of materials. Neutron wavelength selective imaging is a spectral imaging technique that exploits unique contrast differences e.g. for mapping dissimilar elemental, isotope, or phase compositions, and has the particular advantage of being applicable to sample volumes on the meso- and macroscale. While being mostly applied as radiography (2D) so far, we herein report that the extension to tomography allows for the display of the full spectral information for every voxel and in 3D. The development is supported by example data from a continuous as well as a pulsed neutron source. As a practical example, we collected 4D data sets (3D + spectral) of plastically deformed metastable stainless steel and herein demonstrate an improved quantification strategy for crystalline phase fractions. These exemplary results illustrate that localized phase transformations can be quantified even in complex geometries within centimeter-sized samples, and we will discuss the limits and future prospects of the technique that is not limited to crystalline materials.
In this investigation, synchrotron X-ray imaging was used to investigate the water distribution inside newly developed gas diffusion media in polymer electrolyte membrane fuel cells. In-situ radiography was used to reveal the relationship between the structure of the microporous layer (MPL) and the water flow in a newly developed MPL equipped with randomly arranged holes. A strong influence of these holes on the overall water transport was found. This contribution provides a brief overview to some of our recent activities on this research field.
The water management in proton exchange membrane fuel cells (PEMFC) is strongly influenced by the design of the gas diffusion layers (GDL). Limiting current measurements in small-scale cells operating at high stoichiometries are useful to determine the oxygen transport resistance. The oxygen transport resistance increases, once water condenses inside the GDL. In this study a new electrochemical method for voltage loss estimation of GDL induced oxygen transport losses are presented. This new method, referred to as “transient limiting current” (TLC), is compared with the literature method. TLC allows a direct estimation of oxygen transport resistance at an arbitrarily conditioned state. This study also presents a case study of liquid water visualization of a PEM fuel cell with varying GDLs types.
With the help of quasi in-situ synchrotron X-ray computed tomography and time resolved radiography measurements we investigate appearance and distribution of liquid water inside the GDLs under limiting current conditions.
Die Computer-gestützte Laminografie (CL) wurde als komplementäre Methode zur Computertomografie für die dreidimensionale Bildgebung von lateral ausgedehnten Objekten entwickelt. Ursprünglich für medizinische Zwecke verwendet, wurde diese Methode kürzlich als zerstörungsfreie nicht-invasive Methode nicht nur in der Materialforschung, sondern auch mit steigendem Interesse für kunsthandwerkliche und historische Objekte eingesetzt. Hier wird die Computer-gestützten Laminografie mit polychromatischer Neutronenstrahlung an einer historischen Tsuba eingesetzt, einem Stichblatt eines japanischen Schwerts. Eine Analyse der Lötstellen gibt Rückschlüsse auf das Herstellungsverfahren. Zudem wurden unterschiedliche Materialsysteme gefunden, vermutlich um dem Tsuba lokal eine höhere Stabilität zu verleihen. Die Messungen wurden an der Imaging-Beamline CONRAD-2 an der Neutronenquelle BER 2 des Helmholtz-Zentrums Berlins (HZB) durchgeführt.