Filtern
Erscheinungsjahr
Dokumenttyp
- Zeitschriftenartikel (15)
- Vortrag (5)
- Posterpräsentation (2)
- Beitrag zu einem Sammelband (1)
- Beitrag zu einem Tagungsband (1)
- Sonstiges (1)
- Forschungsdatensatz (1)
Sprache
- Englisch (26)
Schlagworte
- EDS (26) (entfernen)
Organisationseinheit der BAM
Eingeladener Vortrag
- nein (5)
Determination of the efficiency of an energy dispersive X-ray spectrometer up to 50 keV with a SEM
(2009)
Both electron and polychromatic photon excitations (micro-focus X-ray source) at a scanning electron microscope (SEM) are used to determine the efficiency of an energy dispersive X-ray spectrometer up to 50 keV by means of a calibrated X-ray spectrometer and reference materials (RM) specially selected for this purpose.
The accurate knowledge of the properties of polycapillary X-ray semi-lenses has a significant influence on the quantitative results in a widespread field of applications involving microfocus X-ray beams. A routine procedure for the characterisation of a polycapillary X-ray semi-lens with a scanning electron microscope (SEM) having attached an energy dispersive spectrometer (EDS) is presented in this paper. A key issue of the procedure consists of fitting the semi-lens in front of the EDS for spectra acquisition. Relevant semi-lens parameters such as focal distance, full width at half maximum (FWHM) of the acceptance area, and transmission are determined in parallelising mode of the semi-lens. Special attention has been paid to the calculation of the transmission.
In order to bridge the gap between lab-scale and industrial-scale production of graphene it is necessary to develop processes, equipment and measurement procedures to control the material features. One of the crucial reasons of graphene’s limited commercialization is the lack of standard procedures to properly characterize and define the material chemical and structural properties down to the nanometer level. This leads to many issues regarding material synthesis repeatability, inappropriateness choice of measurands and measurement reproducibility which heavily affect the consistency of the material performance.
In our study, a comparative analysis is performed on two different series (G5 and G6) of industrial graphene powders, each series produced with four types of functionalization: raw graphene, oxygen-functionalized, nitrogen-functionalized and fluorine-functionalized. All the 8 sample variants were analyzed from a chemical and morphological point of view in the form of powders prepared as slightly pressed in metallic sample holders.
The results of the comparative chemical analyses XPS and EDS show a good agreement in the concentration values for all the elements present in the samples, despite the different analysis volumes addressed by the two techniques. For this reason, the samples can be considered homogeneous in both lateral and vertical direction.
A clear influence of the morphology on the composition is evident. Therefore, such correlative measurements of morphology and composition are necessary for a comprehensive characterization of industrial graphene flakes.
Nanosafety is becoming increasingly important as nanomaterials are widely used in industrial processes and consumer products. For nanotoxicity measurements prior sterilization of the samples is necessary, but as structure activity relationships are made with properties of pristine particles, the question arises, if the sterilization process has an impact on the physico-chemical properties of nanoparticles and thus on the biological behavior.
This question will be addressed in this talk. For this purpose, results from SEM and EDS measurements are combined with those of a novel lab-based HAXPES spectrometer in order to obtain a more complete picture. At the end, an influence of sterilization will be evident, which indicates a restructuring of the nanoparticles owing to sterilization.
For test laboratories operating under accreditation schemes like ISO/IEC 17025 (ISO/IEC 17025), as the international reference for testing and calibration laboratories wanting to demonstrate their capacity to deliver reliable results, a periodical control of the critical instrumental parameters of an Energy-Dispersive X-ray Spectrometer (EDS) is required.
This periodical check of an EDS is specified with exact procedures and materials in the ISO 15632:2021 ”Microbeam Analysis – Selected instrumental performance parameters for the specification and checking of energy-dispersive X-ray spectrometers for use in electron probe microanalysis” (ISO 15632). The EDS check can be simplified to the acquisition of only one 10 kV spectrum from a dedicated test material, EDS-TM002, which is made available by BAM since 2009 (https://webshop.bam.de/webshop_en/). The optional BAM software “EDX spectrometer check” is destined to automatically evaluate this spectrum and determine the performance of the EDS in terms of energy resolution and calibration, as well as possible alteration of low-energy efficiency due to detector contamination. Nearly 200 laboratories have the EDS-TM and associated software package in use.
Practical examples based on various types of artifacts occurred in the EDS spectra and a long-term (>10 years) meticulous observation of the own spectrometers will be discussed. Different types of EDS spectrometers are considered, e.g. Si(Li) and SDD, of various window types (AP, the recent one Si3N4 or even windowless), and with different front contact layers (Au and Ni) (Hodoroaba and Procop, 2014). Evaluation of other parameters or effects such as the deadtime at different count rates or pileup effects is also explained with examples.
The conversion of solar energy into electricity and solar fuels is of crucial importance for a green and sustainable future. Water splitting using semiconductor photo-catalysts is considered a sustainable method to produce clean hydrogen (H2) fuel. Nevertheless, H2 photo-production efficiency remains still low, although extensive research works to understand better the mechanisms of the Hydrogen Evolution Reaction (HER) and the Oxygen Evolution Reaction (OER) are being carried out. In this respect, TiO2 is a key photoactive material, usually employed with a co-catalyst deposited onto the surface to enhance charge carriers’ separation and catalyze surface charge transfer reactions. The deposition of a co-catalyst on the TiO2 nanoparticle surface represents one successful way to enhance the activity of the photocatalyst through a modification of its surface and redox properties. In this context, high-resolution scanning electron microscopy coupled with elemental analysis by energy-dispersive X-ray spectroscopy (EDS) is fundamental for studying and understanding the effect of the nanoparticle morphology on the functional properties of shape-controlled TiO2 crystals (bipyramides, platelets, and elongated particles). Different types of metal-semiconductor combinations, TiO2 shapes and dopant metals (Ag, Pt, etc) and metal concentrations will be discussed.