Intumescent coatings are used in civil engineering to improve the fire resistance of steel constructions. Due to the thin coating thickness and the profile-following application, the architectural appearance of the steel structure can be preserved. EN 13381-8 provides regulations to determine the contribution to the fire resistance of intumescent coatings applied to steel beams and columns. The scope of this standard excludes tension members and steel members with solid sections. For products that have already been successfully tested and assessed on beams and columns, EN 13381-10 offers the possibility based on unloaded fire tests to extend the scope of application of intumescent coatings to tension bars with solid sections. This approach contradicts the national safety level in Germany, where mechanically loaded testing is mandatory. Therefore, a new part of the test standard series EN 13381 is currently developed to enable the application of intumescent coatings on steel tension bars with solid section based on mechanically loaded fire tests. BAM has already carried out numerous fire tests on loaded steel tension members with intumescent coatings. Currently, in the BAM research project FIRESTEMIC, the influence of the steel bar orientation and the profile type on the thermal performance of intumescent coatings are investigated. Both questions concerning the thermal protection ability of intumescent coatings were analysed based on three different test sets, which were carried out in the tension furnace (Fig. 1a). The fire exposure corresponds to the standard temperature-time curve according to EN 1363-1.
This paper summarises the main findings from the fire tests conducted in the FIRESTEMIC project. The results serve as an experimental background for the proposal of the new standard. Regarding the bar orientation, a new test setup was developed and proposed for the new standard. The two tested commercial water-based intumescent coatings with applied dry film thickness from 1.5 mm to 2.5 mm showed only a slight dependence on the bar orientation. In terms of the steel profile type, circular and rectangular solid sections with identical section factor and applied dry film thickness were tested. It was observed that the circular solid bars with diameter 30 mm heat up faster compared to the solid rectangular bars with dimension 30×30 mm (Fig. 1b). Also at larger steel bars, i.e. diameter 40 mm and dimension 40×40 mm, the same trend occurred. Thus, it is recommended for the new test standard to allow a transfer of the test results from circular to rectangular solid sections. In addition, the paper will describe and explain the test and assessment procedure proposed for the newly developed standard.
Steel tension rod systems consist of tension rods, fork connectors and associated intersection or connecting plates. They are used for truss systems, bracings or suspensions owing to slender design and increased economic efficiency. In case of fire, beside the tension rods themselves, the connection parts require appropriate fire protection. The use of intumescent fire protection coatings prevents a rapid heating of the steel and helps to ensure the load-carrying capacity of the structures. Because the connection components of the tension rod systems feature surface curvature as well as a complex geometry, high demand is placed on the intumescence and thermal protection effectiveness of the reactive fire protection coatings. Experimental studies were carried out to investigate the performance of intumescent coatings applied to the components of tension rod systems. The examined aspects include the foaming and cracking behaviour of the intumescent coatings, the influence of different dry film thicknesses (DFT), the heating rate of the steel connecting parts in comparison to the tension rods, as well as the mounting orientation of the tension rods together with their associated fork connectors. The results show that a decrease in the surface curvature and/or an increase in the mass concentration of the steel components lead to a lower heating rate of the steel. Moreover, the performance of the intumescent coating on tension rod systems is influenced by the mounting orientation of the steel components.
For intumescent coatings durability is an important aspect. Due to ageing, which is caused by climatic conditions, the thermal protection performance of intumescent coatings can be reduced during the working life. The national German and the European procedures to assess the durability of intumescent coatings presume a working life of 10 years. For a longer period, additional investigations are required. However, the European assessment procedure does not provide specific information how to prove a durability of more than 10 years. In addition to this formal reason, also from a scientifical position, it is necessary to investigate the degradation of intumescent coatings in detail to propose a corresponding test concept for a durability of more than 10 years.
The presentation summarises the existing knowledge about the degradation behaviour and ageing of intumescent coatings. Furthermore, the results of different approaches from a recently conducted research project are presented. Starting from a water-based and an epoxy-based guide formulation, in a first approach a degradation of the intumescent coating was carried out directly during the production process, i.e. by reducing the concentration of functionally relevant chemical components. In another approach, the duration of the short-term weathering tests was significantly extended, i.e. by multiple repetition of the artificial weathering. The thermal protection performance of the intumescent coating was assessed by fire tests and tests with electrical heating source. In addition, small-scale tests were carried out to determine the thermal material properties of the intumescent coating and thermo-analytical methods were applied to characterise the degradation. Derived from this knowledge, possibilities to test and assess a working life for a period of more than 10 years are proposed.
Intumescent fire protection coatings are used to improve the fire resistance of steel members. Due to slender cross-sections typically used for tension members, high demands are placed on the effectiveness and reliability of the intumescent coatings. This paper describes real-scale fire tests of intumescent coatings applied to steel tension members with circular solid and hollow sections. First, the current regulations for the application of intumescent coatings on steel tension members are discussed. After that, a comparison between the foaming behaviour and failure mechanisms of intumescent coatings applied to steel tension members with different cross-sections and loading conditions is given. Next, the experimental setup and procedure of the performed fire tests are presented. In addition, the influences of various parameters on the performance of the intumescent coating are analysed, including the geometry of the steel profile, dry film thickness of the intumescent coating, load utilisation level as well as the orientation of the member. Based on the theoretical considerations and results of the fire tests, it is evidenced that mechanically loaded fire tests are essential to assess accurately the contribution of intumescent fire protection coatings to the fire resistance of steel tension members with circular solid sections.
Steel tension rod systems consist of tension rods, fork connectors and associated intersection or connecting plates. They are used for truss systems, bracings or suspensions owing to slender design and increased economic efficiency. In case of fire, beside the tension rods themselves, the connection parts require appropriate fire protection. The use of intumescent fire protection coatings prevents a rapid heating of the steel and helps to ensure the load-carrying capacity of the structures. Because the connection components of the tension rod systems feature surface curvature as well as a complex geometry, high demand is placed on the intumescence and thermal protection effectiveness of the reactive fire protection coatings. Experimental studies were carried out to investigate the performance of intumescent coatings applied to the components of tension rod systems. The examined aspects include the foaming and cracking behaviour of the intumescent coatings, the influence of different dry film thicknesses (DFT), the heating rate of the steel connecting parts in comparison to the tension rods, as well as the mounting orientation of the tension rods together with their associated fork connectors. The results show that a decrease in the surface curvature and/or an increase in the mass concentration of the steel components lead to a lower heating rate of the steel. Moreover, the performance of the intumescent coating on tension rod systems is influenced by the mounting orientation of the steel components.
Purpose – The purpose of this paper is to investigate the performance of intumescent coating on tension rod systems and their components. Steel tension rod systems consist of tension rods, fork end connectors and associated intersection or gusset plates. In case of fire, beside the tension rods themselves, the connection parts require appropriate fire protection. Intumescent fire protection coatings prevent a rapid heating of the steel and help secure the structural load-carrying capacity. Because the connection components of tension rod systems feature surface curvature and a complex geometry, high demand is placed on the intumescence and thermal protection performance of the coatings.
Design/methodology/approach – In this paper, experimental studies were carried out for steel tension rod systems with intumescent coating. The examined aspects include the foaming and cracking behaviour, the influence of different dry film thicknesses, the heating rate of the steel connecting parts in comparison to the tension rods, and the mounting orientation of the tension rods together with their fork end connectors.
Findings – The results show that a decrease in surface curvature and/or an increase inmass concentration of the steel components leads to a lower heating rate of the steel. Moreover, the performance of the intumescent coating on tension rod systems is influenced by themounting orientation of the steel components.
Originality/value – The findings based on fire tests contribute to a better understanding of the intumescent coating performance on connection components of tension rod systems. This subject has not been extensively studied yet.