This contribution investigates laser-induced damage of thin film and bulk polymer
samples, with the focus on physical processes occurring close to the damage threshold. In-situ
real-time reflectivity (RTR) measurements with picosecond (ps) and nanosecond (ns) temporal
resolution were performed on thin polymer films on a timescale up to a few microseconds (µs).
A model for polymer thin film damage is presented, indicating that irreversible chemical
modification processes take place already below the fluence threshold for macroscopic damage.
On dye-doped bulk polymer filters (as used for laser goggles), transmission studies using fs-and
ps-laser pulses reveal the optical saturation behavior of the material and its relation to the
threshold of permanent damage. Implications of the sub-threshold processes for laser safety
applications will be discussed for thin film and bulk polymer damage.
Titanium and its alloys are known to allow the straightforward laser-based manufacturing of ordered surface nanostructures, so-called high spatial frequency laser-induced periodic surface structures (HSFL). These structures exhibit sub-100 nm spatial periods – far below the optical diffraction limit. The resulting surface functionalities are usually enabled by both, topographic and chemical alterations of the nanostructured surfaces. For exploring these effects, multi-method characterizations were performed here for HSFL processed on Ti–6Al–4V alloy upon irradiation with near-infrared ps-laser pulses (1030 nm, ≈1 ps pulse duration, 1–400 kHz) under different laser scan processing conditions, i.e., by systematically varying the pulse repetition frequency and the number of laser irradiation passes. The sample characterization involved morphological and topographical investigations by scanning electron microscopy (SEM), atomic force microscopy (AFM), tactile stylus profilometry, as well as near-surface chemical analyses hard X-ray photoelectron spectroscopy (HAXPES) and depth-profiling time-of-flight secondary ion mass spectrometry (ToF-SIMS). This provides a quantification of the laser ablation depth, the geometrical HSFL characteristics and enables new insights into the depth extent and the nature of the non-ablative laser-induced near-surface oxidation accompanying these nanostructures. This allows to answer the questions how the processing of HSFL can be industrially scaled up, and whether the latter is limited by heat-accumulation effects.