Filtern
Erscheinungsjahr
Dokumenttyp
- Vortrag (68)
- Posterpräsentation (31)
- Beitrag zu einem Tagungsband (21)
- Zeitschriftenartikel (14)
- Buchkapitel (10)
- Beitrag zu einem Sammelband (4)
- Monografie (1)
- Video (1)
Referierte Publikation
- nein (150) (entfernen)
Schlagworte
Organisationseinheit der BAM
- 6 Materialchemie (59)
- 6.2 Material- und Oberflächentechnologien (59)
- 9 Komponentensicherheit (11)
- 9.5 Tribologie und Verschleißschutz (11)
- 6.1 Oberflächen- und Dünnschichtanalyse (8)
- 4 Material und Umwelt (5)
- 4.1 Biologische Materialschädigung und Referenzorganismen (5)
- 6.6 Physik und chemische Analytik der Polymere (1)
Paper des Monats
- ja (1)
A promising technology in photovoltaics is based on micro-concentrator solar cells, where the photovoltaic active area is realized as an array of sub-millimeter sized cells onto which the incident light is focused via microlenses. This approach allows to increase the cell efficiency and to realize much more compact modules compared to macroscopic concentrator devices. At the same time, expensive raw materials can be saved, which is of interest, for example, with respect to indium in the case of copper-indium-gallium-diselenide (CIGSe) thin film solar cells. Two methods to produce micro-sized precursors of CIGSe absorbers on molybdenum are presented using 30-fs laser pulses at 790 nm wavelength. On the one hand, a multi pulse surface structuring of the molybdenum film or the underlying glass substrate and a subsequent physical vapor deposition were used for a site-selective aggregation of indium droplets. On the other hand, a single pulse laser-induced forward transfer was utilized to selectively deposit combined copper-indium precursor pixels on the molybdenum back contact of the solar cell. Post-processing (selenization, isolation, contacting) of the laser-generated micro-sized precursors results in functional CIGSe solar cells.
The wetting behavior of material surfaces can be controlled by surface structures. We functionalized case-hardened alloyed carbon steel to modify the wetting behavior using ultrashort laser pulses (fs- to ps-range). The laser processing was performed by scanning the laser beam across the surface of initially polished flat sample material. An experimental study of the laser processing parameters (peak fluence, scan velocity, line overlap) rendered an assignment of different regimes associated with characteristic surface morphologies (laser-induced periodic surface structures, grooves, micro cones, etc.) possible. Analyzing the surface using optical as well as scanning electron microscopy allowed the identification of morphologies providing the optimum similarity to the natural skin of non-moisture havesting lizards. For mimicking skin structures of moisture-harvesting lizards, additionally a two-step laser processing strategy was established for realizing hierarchical microstructures. In this approach, micrometer-scaled capillaries (step 1) were superimposed by a laser-generated regular array of small dimples (step 2). Optical focus variation imaging measurements finally revealed the three dimensional topography of the laser processed surfaces derived from lizard skin structures. The functionality of these surfaces was analyzed in view of wetting and directional fluid transport properties. The results suggest possible applications of the laser-structured surfaces.
Der Vortrag gibt einen Überblick zu aktuellen Projekt- und Publikationsaktivitäten im BAM-Fachbereich 6.4 Technologien mit Nanowerkstoffen zum Thema “Laser-induzierte periodische Oberflächenstrukturen”. Die Herstellung solcher Mikro- und Nanostrukturen mittels ultrakurzer Laserpulse wird beschrieben, wodurch optische, chemische, mechanische oder biologische Oberflächenfunktionalsierungen vorgenommen werden können. Beispiele aus den Bereichen der Farbwirkung, der Benetzbarkeit mit Flüssigkeiten und der Reibungs- und Verschleissminderung werden erläutert.
Laser-induced periodic surface structures (LIPSS, ripples) are a universal phenomenon that can be observed on almost any material after the irradiation by linearly polarized laser beams, particularly when using ultrashort laser pulses with durations in the picosecond to femtosecond range. During the past few years significantly increasing research activities have been reported in the field of LIPSS, since their generation in a single-step process provides a simple way of nanostructuring and surface functionalization towards the control of optical, mechanical or chemical properties. In this contribution current applications of LIPSS are reviewed, including the colorization of technical surfaces, the control of surface wetting, the mimicry of the natural texture of animal integuments, the tailoring of surface colonization by bacterial biofilms, and the improvement of the tribological performance of nanostructured metal surfaces.
A procedure to fabricate CuInSe2 (CISe) micro-absorbers and solar cells for concentrator applications is presented. The micro-absorbers are developed from indium precursor islands, which are deposited on a molybdenum coated glass substrate (back contact), followed by deposition of copper on top and subsequent selenization as well as selective etching of copper selenides. In order to compare the properties of the locally grown absorbers to those of conventional large area CISe films, we systematically examine the compositional and morphological homogeneity of the micro absorbers and carry out photoluminescence measurements. Preliminary devices for micro-concentrator solar cell applications are fabricated by optimizing the copper to indium ratio and the size of the indium precursor islands. The resulting micro solar cells provide a characteristic I–V curve under standard illumination conditions (1 sun).
Ultrashort laser pulse micromachining features a high precision. By increasing the repetition rate of the applied laser to several 100 kHz, laser processing becomes quick and cost-effective and make
this method attractive for industrial applications. Upon exceeding a critical laser intensity, hard X-ray radiation is generated as a side effect. Even if the emitted X-ray dose per pulse is low, the accumulated X-ray dose becomes significant for high-repetition-rate laser systems so that radiation
safety must be considered.
Commercial grade-1 titanium samples (Ti, 99.5% purity) were treated using three alternative methods, i.e., fs-laser processing in air, thermal heat treatment in an oven, or anodization in an electrochemical bath, all resulting in the formation of differently conditioned superficial oxide layers. The laser processing was carried out by a Ti:sapphire laser (pulse duration 30 fs, central wavelength 790 nm, pulse repetition rate 1 kHz) in a regime of generating laser-induced periodic surface structures (LIPSS). The experimental conditions (laser fluence, spatial spot overlap) were optimized in a sample-scanning geometry for the processing of several square-millimetres large surface areas covered homogeneously by these nanostructures. The thermal processing in the oven was done at two different temperatures, while the electrochemical anodization was performed at room temperature, aiming to generate different polymorphs of titanium oxide at similar oxide layer thickness. The irradiated surface regions were characterized by optical and scanning electron microscopy, and micro Raman spectroscopy. The tribological performance of the differently treated titanium surfaces was characterized in the regime of mixed friction by reciprocating sliding tests against a sphere of hardened steel in un-additivated paraffin oil and fully formulated engine oil as lubricants. The specific tribological performance of the differently treated surfaces is discussed on the basis of possible physical and chemical mechanisms.
The processing of laser-induced periodic surface structures (LIPSS, ripples) on metals and semiconductors in ambient air is usually accompanied by superficial oxidation effects - widely neglected in the current literature. In this contribution, chemical, structural, and mechanical alterations in the formation of femtosecond LIPSS are characterized by a variety of surface analytical techniques, including energy dispersive X-ray analyses (EDX), X-ray photoelectron spectroscopy (XPS), micro Raman spectroscopy (µ-RS), and depth-profiling Auger electron microscopy (AEM). Alternative routes of electrochemical and thermal oxidation allow to qualify the relevance of superficial oxidation effects on the tribological performance in oil lubricated reciprocating sliding tribological tests (RSTT). It is revealed that the fs-laser processing of near-wavelength sized LIPSS on metals leads to the formation of a few hundreds of nanometer thick graded oxide layer, consisting mainly of amorphous oxides.
Regardless of its reduced hardness and limited thickness, this nanostructured surface layer can effciently prevent a direct metal-metal contact in the RSTT and may also act as an anchor layer for specific wear-reducing additives contained in the engine oil involved
Ultrashort laser pulse micromachining features a high precision. By increasing the repetition rate of the applied laser to several 100 kHz, laser processing becomes quick and cost-effective and make this method attractive for industrial applications. Upon exceeding a critical laser intensity, hard X-ray radiation is generated as a side effect. Even if the emitted X-ray dose per pulse is low, the accumulated X-ray dose becomes significant for high-repetition-rate laser systems so that radiation safety must be considered.
Antibiotic resistance is a growing global problem which poses a massive threat to human health. Although human activity contributes to the acceleration of the process, bacteria have a self-driven stabilisation mechanism to protect themselves from such and other external threats: biofilm formation. Nonetheless, it is the adhesion of a single bacterial cell to a surface that triggers the formation of such network of biomolecules and microorganisms, as well as its hazardous consequences. The main objective of this work was to quantify the adhesion force of a single E. coli cell on a Ti substrate via the AFM-related single-cell force spectroscopy, with both the cell and the substrate material being of high clinical relevance. A set of 25 x 25 force displacement curves was acquired with a maximum force of 3.2 nN without dwell time, yielding a topography map and an adhesion force map that showed to be correlated. A mean adhesion force of 0.85 ± 0.175 nN was measured and the presence of cell appendages on the bacterial cell wall was verified through individual force-displacement curves. Bacterial viability was assessed after the measurements via live/dead staining.
Laser-induced Periodic Surface Structures (LIPSS, ripples) are a universal phenomenon and can be generated in a contactless, single-step process on almost any type of solid upon irradiation with intense laser pulses. They represent a (quasi-)periodic modulation of the surface topography in the form of a linear grating and are typically formed in a “self-ordered” way in the focus of a laser beam. Thus, they are often accompanying laser material processing applications. The structural sizes of LIPSS typically range from several micrometers down to less than 100 nanometers – far beyond the optical diffraction limit – while their orientations exhibit a clear correlation with the local polarization direction of the laser radiation.
From a theoretical point of view, a controversial debate has emerged during the last decades, whether LIPSS originate from electromagnetic effects (seeded already during the laser irradiation) – or whether they emerge from matter-reorganization processes (distinctly after the laser irradiation). From a practical point of view, however, LIPSS represent a simple and robust way for the nanostructuring of solids that allows creating a wide range of different surface functionalities featuring applications in optics, tribology, medicine, energy technologies, etc.
This presentation reviews the currently existent theories of LIPSS. A focus is laid on the historic development of the fundamental ideas behind the LIPSS, their corresponding mathematical descriptions and numerical implementations, along with a comparison and critical assessment of the different approaches.
Fourth generation light sources, namely short wavelength, short pulse free electron lasers (FELs) are offering new and fascinating possibilities to resolve laser-induced structure formation at surfaces on the sub-micrometer to nanometer length scale and in temporal regimes ranging from picoseconds to several nanoseconds with sub-picosecond resolution. This unique spatio-temporal resolution allows to reveal early signatures of coherent/plasmonic electromagnetic scattering effects followed by the excitation of hydrodynamic capillary waves – providing new insights to the above-mentioned debate.
Finally, some unsolved scientific problems related to LIPSS are identified and the pending technological limitations are discussed. While the currently available laser and scanner technology already allows large area surface processing with rates at the m2/min level, industrial applications of LIPSS are sometimes limited by the complex interplay between the nanoscale surface topography and the specific surface chemistry. This typically manifests in difficulties to control the processing of LIPSS and in limitations to ensure the long-term stability of the created surface functions. Strategies for overcoming such limitations are outlined.
The performance of titanium alloy (Ti6Al4V) surfaces was investigated in lubricated reciprocating sliding tribological tests (RSTT). Special emphasis was laid on the effect of surface nanostructures in area of contact on the respective friction and wear behaviour. These so-called laser-induced periodic surface structures (LIPSS, ripples) were produced on the titanium alloy surface upon scan processing in air by an ultrashort pulsed femtosecond (fs) laser. As lubricant served two types of base oils, a pure polyalcylene-glycol, and an SAE 0W30 oil containing only antioxidants and temperature stabilizers. Tribological tests were carried out on polished as well as LIPSS covered areas using both types of base oil. A test metrics was established, combining the additive 2-ethylhexyl-zincdithiophosphate (ZDDP) or the ionic liquid [P6,6,6,14] [DEHP] (98% purity) with the respective base oils. The test metrics also considered the orientation of motion with respect to the orientation of the structures formed on the surface. Results are presented which show that the interplay between LIPSS and the local chemistry formed by the respective additives is beneficial for the tribological behaviour of the titanium alloy. Certain combinations of base oil, additive and LIPSS reduced friction and wear significantly in the tribological contact.
Laser-induced periodic surface structures (LIPSS) have gained remarkable attention as they represent a universal phenomenon that is often accompanying laser-processing. Such LIPSS enable a large variety of different surface functionalizations for applications in the fields of optics, fluidics, tribology, or medicine. Moreover, so-called “high spatial frequency LIPSS” (HSFL) provide an appealing and straightforward way for surface nanostructuring featuring spatial periods even below 100 nm – far beyond the optical diffraction limit. However, the imposed surface functionalities are usually caused by both, topographic and chemical surface alterations. For exploring these effects in detail, multi-method characterizations were performed here for HSFL on processed Ti- 6Al- 4V alloy upon irradiation with near-infrared ps-laser pulses (1030 nm wavelength, ~1 ps pulse duration, 1 – 400 kHz pulse repetition rate) under different laser and scan processing conditions. The sample characterization involved morphological and topographical investigations by scanning electron microscopy (SEM), atomic force microscopy (AFM), stylus profilometry (SP), and white light interference microscopy (WLIM), as well as near-surface chemical analyses by X-ray photoelectron spectroscopy (XPS), hard X-ray photoelectron spectroscopy (HAXPES) and depth-profiling time-of-flight secondary ion mass spectrometry (TOF-SIMS). The results allow to qualify the laser ablation depth, the geometrical HSFL characteristics and provide detailed insights into the depth extent and the nature of the ps-laser-induced near-surface oxidation. Significance for medical applications will be outlined.
Laser-induced periodic surface structures (LIPSS) and their combination with self-ordered microstructures forming hierarchical Spikes enable a large variety of different surface functionalizations for applications in the fields of optics, fluidics, tribology, or medicine. Moreover, high spatial frequency LIPSS (HSFL) provide an appealing and straightforward way for surface nanostructuring featuring spatial periods even below 100 nm – far beyond the optical diffraction limit. However, the imposed surface functionalities are usually caused by both, topographic and chemical surface alterations. For exploring these effects in detail, multi-method characterizations were performed here for HSFL and hierarchical Spikes processed on Ti-6Al-4V alloy upon irradiation with near-infrared ps-laser pulses (1030 nm wavelength, ~1 ps pulse duration, 1 – 400 kHz pulse repetition rate) under different laser and scan processing conditions. The following sample characterization involved morphological and topographical investigations by scanning electron microscopy (SEM), atomic force microscopy (AFM), stylus profilometry (SP), and white light interference microscopy (WLIM), as well as near-surface chemical analyses by X-ray photoelectron spectroscopy (XPS), hard X-ray photoelectron spectroscopy (HAXPES) and depth-profiling time-of-flight secondary ion mass spectrometry (TOF-SIMS). The results allow to qualify the laser ablation depth, the geometrical HSFL/Spikes characteristics and provide detailed insights into the depth extent and the nature of the ps-laser-induced near-surface oxidation arising from the laser-processing in ambient air and into the relevance of heat-accumulation effects at high pulse repetition rates. Moreover, the direct comparison of the HAXPES and XPS data reveals the role of surface-covering organic contaminants adsorbed from the ambient atmosphere without the uncertainties and potential sputter reduction potentially caused by ion-sputter depth profiling.
Surfaces of metallic copper and copper alloys effectively inactivate microorganisms and viruses. However, the exact inactivation mode is still under debate. Main factors are assumed to include direct contact with the metallic surface, influx of Cu(I)/Cu(II) ions and the generation of reactive oxygen species (ROS). Laser-induced periodic surface structures (LIPSS) are frequently reported to act antibacterial, mainly by prevention of bacterial adhesion due to a limited number of possible adhesion points or by increasing the overall surface of intrinsically antibacterial materials. In time-kill experiments with E. coli and S. aureus we analyzed the impact of LIPSS on the toxicity of metallic copper and brass. We also conducted ROS accumulation assays and conclude that the application of LIPSS is not generally straight forward to obtain or improve antibacterial surfaces. Thus, the antibacterial effects of LIPPS.
Irradiation of solid surfaces with intense ultrashort laser pulses represents a unique way of depositing energy into materials. It allows to realize states of extreme electronic excitation and/or very high temperature and pressure and to drive materials close to and beyond fundamental stability limits. As a consequence, structural changes and phase transitions often occur along unusual pathways and under strongly nonequilibrium conditions. Due to the inherent multiscale nature — both temporally and spatially—of these irreversible processes, their direct experimental observation requires techniques that combine high temporal resolution with the appropriate spatial resolution and the capability to obtain good quality data on a single pulse/event basis. In this respect, fourth-generation light sources, namely, short wavelength and short pulse free electron lasers (FELs), are offering new and fascinating possibilities. As an example, this talk will discuss the results of scattering experiments carried out at the FLASH free electron laser at DESY (Hamburg, Germany), which allowed us to resolve laser-induced structure formation at surfaces on the nanometer to submicron length scale and in temporal regimes ranging from picoseconds to several nanoseconds with sub-picosecond resolution. The current status and future perspectives in this field via exploiting the unique possibilities of these 4th-generation light sources will be discussed.
Unwanted X-ray emission in ultrashort pulse laser processing: From metallic to biological materials
(2023)
X-rays can be generated as an unwanted side effect during ultrashort pulse laser material processing of technical work pieces and even biological samples with laser intensities above 10^13 W/cm^2. First studies demonstrate the need to address this effect in industrial as well as in medical applications. This secondary hazard should be considered in work safety and risk assessment.
Laser-induced periodic surface structures (LIPSS) have gained remarkable attention as they represent a universal phenomenon that is often accompanying laser-processing. Such LIPSS enable a plethora of different surface functionalizations for applications in the fields of optics, fluidics, tribology, or medicine. Due to the inherent multiscale nature of processes involved in LIPSS formation, their in-situ observation requires experimental techniques that combine high temporal resolution with the appropriate spatial resolution. In this respect fourth generation light sources, namely short wavelength, short pulse free electron lasers (FELs) are offering new and fascinating possibilities. This work contribution will discuss the results of scattering experiments carried at the FLASH free electron laser at DESY (Hamburg, Germany), which allowed us to resolve laser-induced structure formation at surfaces on the nm to sub-µm length scale and in temporal regimes ranging from ps to several ns with sub-ps resolution. A ps-optical pump / fs-XUV scattering probe scheme was employed to 100 nm thick laser-excited silicon films, while recording snapshots of the transmitted XUV scattering patterns at various delay times after the laser pulse impact. On timescales ranging from hundred ps until several ns almost quantitative agreement was observed between certain features of the recorded scattering patterns and predictions of the first-principles theory of J.E. Sipe and coworkers. Other scattering features appearing with a delay of ~100 ps and lasting for ~1 ns are attributed to capillary surface waves being excited at the laser-melted film material while ablation proceeds. Our superior spatio-temporal resolution experiments allow to uniquely reveal and distinguish early signatures of coherent/plasmonic electromagnetic scattering effects, separately followed by hydrodynamic matter reorganization.