Filtern
Erscheinungsjahr
Dokumenttyp
- Zeitschriftenartikel (130)
- Vortrag (31)
- Beitrag zu einem Tagungsband (27)
- Buchkapitel (10)
- Posterpräsentation (7)
- Beitrag zu einem Sammelband (4)
- Monografie (1)
- Video (1)
Sprache
- Englisch (211) (entfernen)
Schlagworte
- Laser-induced periodic surface structures (LIPSS) (71)
- Femtosecond laser ablation (39)
- Femtosecond laser (32)
- Surface functionalization (31)
- Laser processing (23)
- Laser ablation (19)
- Laser-induced periodic surface structures, LIPSS (12)
- Silicon (12)
- Nanostructures (11)
- Applications (10)
Organisationseinheit der BAM
- 6 Materialchemie (101)
- 6.2 Material- und Oberflächentechnologien (101)
- 9 Komponentensicherheit (15)
- 9.5 Tribologie und Verschleißschutz (15)
- 6.1 Oberflächen- und Dünnschichtanalyse (10)
- 4 Material und Umwelt (7)
- 4.1 Biologische Materialschädigung und Referenzorganismen (7)
- 6.7 Materialsynthese und Design (4)
- 6.6 Physik und chemische Analytik der Polymere (3)
- 5 Werkstofftechnik (1)
- 5.1 Mikrostruktur Design und Degradation (1)
Paper des Monats
- ja (3)
Ti:sapphire laser pulses of 130 fs and 800 nm were focused on 3.2-7m-thick TiN films by a 60-mm focal length lens in air. The morphology of the ablated areas generated by laser pulses at a fluence slightly above the ablation threshold was characterized in dependence on the pulse number by scanning electron microscopy (SEM) and atomic force microscopy (AFM). The cavity profiles, depths, diameters, and volumes were quantitatively evaluated by AFM. The polarization state of the laser light is discussed as a further parameter, in addition to fluence and pulse number, that influences and controls the ablation precision of these materials. It was observed that circularly polarized radiation enhances the average ablation rates and reduces the roughness in the cavities by a factor of 2-3 as compared to linearly polarized radiation of the same incident laser fluence. Special attention was paid to the interfacial region between the coating and substrate. Ultrashort-pulse laser drilling into the Si substrate revealed the generation of columnar features which even may surmount the original coating under laser conditions.
Chemical effects during the formation of femtosecond laser-induced periodic surface structures
(2019)
The processing of laser-induced periodic surface structures (LIPSS, ripples) on metals and semiconductors in ambient air is usually accompanied by superficial oxidation effects – a fact that is widely neglected in the current literature. In this contribution, chemical, structural, and mechanical alterations in the formation of femtosecond LIPSS are characterized by a variety of surface analytical techniques, including energy dispersive X-ray analyses (EDX), X-ray photoelectron spectroscopy (XPS), micro Raman spectroscopy (µ-RS), and depth-profiling Auger electron microscopy (AEM). Alternative routes of electrochemical and thermal oxidation allow to qualify the relevance of superficial oxidation effects on the tribological performance in oil lubricated reciprocating sliding tribological tests (RSTT). It is revealed that the fs-laser processing of near-wavelength sized LIPSS on metals leads to the formation of a few hundreds of nanometers thick graded oxide layers, consisting mainly of amorphous oxides. Regardless of reduced hardness and limited thickness, this nanostructured surface layer efficiently prevents a direct metal-to-metal contact in the RSTT and may also act as an anchor layer for specific wear-reducing additives contained in the used engine oil.
The chemical characteristics of two different types of laser-induced periodic surface structures (LIPSS), so-called high and low spatial frequency LIPSS (HSFL and LSFL), formed upon irradiation of titanium surfaces by multiple femtosecond laser pulses in air (30 fs, 790 nm, 1 kHz), are analyzed by various optical and electron beam based surface analytical techniques, including micro-Raman spectroscopy, energy dispersive X-ray analysis, X-ray photoelectron spectroscopy, and Auger electron spectroscopy. The latter method was employed in a high-resolution mode being capable of spatially resolving even the smallest HSFL structures featuring spatial periods below 100 nm. In combination with an ion sputtering technique, depths-resolved chemical information of superficial oxidation processes was obtained, revealing characteristic differences between the two different types of LIPSS. Our results indicate that a few tens of nanometer shallow HSFL are formed on top of a ∼150 nm thick graded superficial oxide layer without sharp interfaces, consisting of amorphous TiO2 and partially crystallized Ti2O3. The larger LSFL structures with periods close to the irradiation wavelength originate from the laser-interaction with metallic titanium. They are covered by a ∼200 nm thick amorphous oxide layer, which consists mainly of TiO2 (at the surface) and other titanium oxide species of lower oxidation states underneath.
Laser-induced periodic surface structures (LIPSS) and their combination with self-ordered microstructures forming hierarchical Spikes enable a large variety of different surface functionalizations for applications in the fields of optics, fluidics, tribology, or medicine. Moreover, high spatial frequency LIPSS (HSFL) provide an appealing and straightforward way for surface nanostructuring featuring spatial periods even below 100 nm – far beyond the optical diffraction limit. However, the imposed surface functionalities are usually caused by both, topographic and chemical surface alterations. For exploring these effects in detail, multi-method characterizations were performed here for HSFL and hierarchical Spikes processed on Ti-6Al-4V alloy upon irradiation with near-infrared ps-laser pulses (1030 nm wavelength, ~1 ps pulse duration, 1 – 400 kHz pulse repetition rate) under different laser and scan processing conditions. The following sample characterization involved morphological and topographical investigations by scanning electron microscopy (SEM), atomic force microscopy (AFM), stylus profilometry (SP), and white light interference microscopy (WLIM), as well as near-surface chemical analyses by X-ray photoelectron spectroscopy (XPS), hard X-ray photoelectron spectroscopy (HAXPES) and depth-profiling time-of-flight secondary ion mass spectrometry (TOF-SIMS). The results allow to qualify the laser ablation depth, the geometrical HSFL/Spikes characteristics and provide detailed insights into the depth extent and the nature of the ps-laser-induced near-surface oxidation arising from the laser-processing in ambient air and into the relevance of heat-accumulation effects at high pulse repetition rates. Moreover, the direct comparison of the HAXPES and XPS data reveals the role of surface-covering organic contaminants adsorbed from the ambient atmosphere without the uncertainties and potential sputter reduction potentially caused by ion-sputter depth profiling.
Laser-induced periodic surface structures (LIPSS) enable a large variety of different surface functionalizations for applications in the fields of optics, fluidics, tribology, or medicine. Moreover, high spatial frequency LIPSS (HSFL) provide an appealing and straightforward way for the generation of surface nanostructures featuring spatial periods even below 100 nm – far beyond the optical diffraction limit. However, the imposed surface functionalities are usually caused by both, topographic and chemical surface alterations. For exploring these effects in detail, multi-method characterization was performed here for HSFL processed on Ti-6Al-4V alloy upon irradiation with near-infrared ps-laser pulses (1030 nm wavelength, ~1 ps pulse duration, 1 – 400 kHz pulse repetition rate) under different scan processing conditions. The subsequent sample characterization involved morphological and topographical investigations by scanning electron microscopy (SEM), atomic force microscopy (AFM), stylus profilometry (SP), as well as near-surface chemical analyses by X-ray photoelectron spectroscopy (XPS), hard X-ray photoelectron spectroscopy (HAXPES) and depth-profiling time-of-flight secondary ion mass spectrometry (TOF-SIMS). The results allow to qualify the laser ablation depth, the geometrical HSFL characteristics and provide detailed insights into the depth extent and the nature of the ps-laser-induced near-surface oxidation arising from the laser-processing in ambient air and into the relevance of heat-accumulation effects at high pulse repetition rates. Moreover, the direct comparison of the HAXPES and XPS data reveals the role of surface-covering organic contaminants adsorbed from the ambient atmosphere without ion-sputter depth profiling. Furthermore, reduction of the oxides by sputtering can be avoided.
Commercial grade-1 titanium samples (Ti, 99.6%) were treated using three alternative methods, (i) femtosecond laser processing, (ii) thermal heat treatment, and (iii) electrochemical anodization, respectively, resulting in the formation of differently conditioned superficial titanium oxide layers. The laser processing (i) was carried out by a Ti:sapphire laser (pulse duration 30 fs, central wavelength 790 nm, pulse repetition rate 1 kHz) in a regime of generating laser-induced periodic surface structures (LIPSS). The experimental conditions (laser fluence, spatial spot overlap) were optimized in a sample-scanning setup for the processing of several square-millimeters large surface areas covered homogeneously by these nanostructures. The differently oxidized titanium surfaces were characterized by optical microscopy, micro Raman spectroscopy, variable angle spectroscopic ellipsometry, and instrumented indentation testing. The tribological performance was characterized in the regime of mixed friction by reciprocating sliding tests against a sphere of hardened steel in fully formulated engine oil as lubricant. The specific tribological performance of the differently treated surfaces is discussed with respect to possible physical and chemical mechanisms.
Laser ablation of single-crystalline indium phosphide (InP) was performed in air by means of linearly polarized Ti : sapphire femtosecond pulses (800 nm, 130 fs, 10 Hz). As a result of the irradiation with a variable number of laser pulses per spot (N /spl les/ 5), several morphological changes (crater formation, rim formation, ripple structures, and cones) were observed. These effects were explored using force modulation microscopy (FMM), a technique based on scanning force microscopy, allowing the simultaneous imaging of both topography and local stiffness at a high lateral resolution. The first laser pulse induces the formation of a protruding rim (height < 20 nm, width /spl ap/ 300 nm) bordering the ablated crater. A Fourier analysis of the multipulse generated topographies reveals the formation of wavelength-sized periodic ripples (modulation depth < 100 nm) with an orientation perpendicular to that of the electric field vector of the laser radiation. Besides these morphological alterations, material modifications were also observed in the irradiated regions by means of the FMM technique. Within the ablated craters, local stiffness variations were found revealing an inhomogeneous material composition/structure as a consequence of the femtosecond pulse laser treatment.
Structure formation on the surface of indium phosphide irradiated by femtosecond laser pulses
(2005)
Laser-induced periodic surface structures (LIPSS; ripples) with different spatial characteristics have been observed after irradiation of single-crystalline indium phosphide (c-InP) with multiple linearly polarized femtosecond pulses (130 fs, 800 nm) in air. With an increasing number of pulses per spot, N, up to 100, a characteristic evolution of two different types of ripples has been observed, i.e., (i) the growth of a grating perpendicular to the polarization vector consisting of nearly wavelength-sized periodic lines and (ii), in a specific pulse number regime (N = 530), the additional formation of equally oriented ripples with a spatial period close to half of the laser wavelength. For pulse numbers higher than 50, the formation of micrometer-spaced grooves has been found, which are oriented perpendicular to the ripples. These topographical surface alterations are discussed in the frame of existing LIPSS theories.
Laser ablation of single-crystalline indium phosphide (InP) was performed in air by means of linearly polarized Ti:sapphire femtosecond-pulses (800 nm, 130 fs, 10 Hz). As a result of the first laser pulses, several morphological changes (crater formation, rim formation, ripple structures and cones) were observed. These effects were explored using force modulation microscopy (FMM), a technique based on scanning force microscopy (SFM), allowing the simultaneous imaging of both topography and local stiffness at a high lateral resolution. The first laser pulse induces the formation of a protruding rim (height <20 nm, width ~300 nm) bordering the ablated crater. A Fourier-analysis of the multi-pulse generated topographies reveals the formation of wavelength-sized periodic ripples (modulation depth <100 nm) with an orientation perpendicular to that of the electric field vector of the laser radiation. Besides these morphological alterations, also material modifications were observed in the irradiated regions by means of the FFM technique. Within the ablated craters, local stiffness variations were found revealing an inhomogeneous material composition/structure as a consequence of the femtosecond pulse laser treatment.