Stone deterioration is the result of a complex interaction of external physical, chemical and biological forces with the mineralogical-petrophysical properties of the stone. With a better understanding of how these properties are linked to material behavior and durability, more effective measures for stone conservation can be developed. Studying these interactions in tuff is particularly complex due to the naturally high heterogeneity of tuff rocks.
The first aim of a current research project is to combine the results of recent and older studies on tuff deterioration. Furthermore, the literature overview is complemented by our own investigation of Weibern and Ettringen tuff, with a focus on pore structure characteristics.
Mixing and curing of geopolymers and related alkali-activated materials without storage and handling of highly alkaline solutions possesses advantages regarding safety and economic viability. One possible approach is to produce these materials from solid silica feedstocks and solid sodium aluminate, and subsequent mixing with water. We present a comparison between geopolymers and aluminosilicate gel-zeolite composites synthesized by this route from different silica feedstocks (by-product silica from chlorosilane production, microsilica, rice husk ash) and with different SiO2/Al2O3 ratios, using results from XRD, NMR, SEM, thermal analysis, mechanical and acid resistance testing. The use of rice husk ash favors formation of a fully amorphous geopolymer with high strength. Utilization of the other silica feedstocks leads to formation of aluminosilicate gel-zeolite composites, the amount and kind of zeolites depending on the feedstock and the SiO2/Al2O3 ratio. These composites show beneficial dehydration behavior, viz. no distinct dehydration step of thermal strain, with the phase assemblage after heating to 1000°C controlled by the starting composition. Mortars produced from both, the geopolymers as well as the composites, exhibit high resistance to sulfuric acid attack, making them promising materials for the construction and the repair of industrial and sewer structures.