Entwicklung oxidkeramischer Werkstoffe und Folien für thermoelektrische Multilayergeneratoren
(2016)
Calcium cobaltite is a promising oxide thermoelectric materials for applications between 600 °C and 900 °C in air to convert waste heat directly into electrical power. The solid-state reaction, well known for large scale powder synthesis of functional materials, is used for the production of thermoelectric oxides. As a high temperature process, the powder synthesis consumes a lot of energy. In different studies, different synthesis conditions were used for the preparation of calcium cobaltite. To the author’s knowledge, a systematic study of the synthesis conditions of calcium cobaltite and calcium manganate has not yet been published.
Therefore, the synthesis conditions for calcium cobaltite (temperature, dwell time, and particle size of raw materials) were studied with a statistical design of experiments (2³) and investigated regarding phase composition (XRD), densification, and thermoelectric properties.
This study showed that a higher energy input (elevated temperatures, longer dwell times, or repeated calcinations) during powder synthesis does not improve but deteriorate the thermoelectric properties of calcium cobaltite. The same correlation was determined for the shrinkage. As a higher energy input during powder synthesis leads to a larger grain size and therefore to a reduced sinter activity the shrinkage at a given sinter profile is minimize as well as the thermoelectric properties. These results can be used to minimize the energy demand for the powder synthesis of oxide thermoelectric materials.
In addition an increase of power factor by factor 10 can be achieved by applying pressure assisted sintering.
The development of competitive thermoelectric generators using oxide ceramics and multilayer technology requires the investigation of suitable sintering procedures. The sintering of Ca3Co4O9, which is the most promising p-type oxide regarding its figure of merit, is a special challenge, as the material starts to decompose at 926 °C. Pressure-assisted sintering (PAS), as known from large-scale production of low temperature co-fired ceramics, was used to sinter multilayers of Ca3Co4O9 green tape at 900 °C with different pressures and dwell times. In-situ shrinkage measurements, microstructural investigations and electric measurements were performed. Relative density increases from 57.4 % after free sintering for 24 h to 93.7 % after 2 h of PAS with 10 MPa axial load. The combination of tape casting and PAS induces a pronounced alignment of the anisotropic grains. In comparison to freely sintered multilayers, the electrical conductivity in the casting direction is thereby strongly increased by a factor of 5. With respect to dry-pressed bars, the improvement amounts to a factor of 15. This study shows that PAS is a proper technique to produce dense Ca3Co4O9 panels with good thermoelectric properties similar to hot-pressed tablets, even in large-scale production.
Influence of solid-state-synthesis conditions on properties of oxide thermoelectric materials
(2017)
Calcium cobaltite and calcium manganate are promising oxide thermoelectric materials for applications between 600 °C and 900 °C in air to convert waste heat directly into electrical power. The solid state reaction, well known for large scale powder synthesis of functional materials, is used for the production of thermoelectric oxides. As a high temperature process, the powder synthesis consumes a lot of energy. In different studies, different synthesis conditions were used for the preparation of calcium cobaltite and calcium manganate powder. To the author’s knowledge, a systematic study of the synthesis conditions of calcium cobaltite and calcium manganate has not yet been published.
Therefore, the synthesis conditions for calcium cobaltite (temperature, dwell time, and particle size of raw materials) were studied with a statistical design of experiments (2³) and investigated regarding phase composition (XRD), densification and thermoelectric properties. The gained knowledge was used to optimize the solid state reaction of calcium manganate.
This study showed that a higher energy input (elevated temperatures, longer dwell times, or repeated calcinations) during powder synthesis does not improve but deteriorate the thermoelectric properties of calcium cobaltite. The same correlation was determined for the densification. As a higher energy input during powder synthesis leads to a larger grain size and therefore to a reduced sinter activity the densification at a given sinter profile is minimize as well as the thermoelectric properties. These results can be used to minimize the energy demand for the powder synthesis of oxide thermoelectric materials.
Calciumcobaltit ist eines der vielversprechendsten thermoelektrischen Oxide, welche zur direkten Wärmerückgewinnung genutzt werden können. Calciumcobaltit weist sowohl eine anisotrope Partikelform als auch anisotrope thermoelektrische Eigenschaften auf. Durch gezielte Ausrichtung der Partikel mittels Foliengießens und druckunterstützter Sinterung kann diese Anisotropie gezielt auf ein Bauteil übertragen werden. Die Partikelmorphologie kann durch Dotierung und Kalzinierung beeinflusst werden. Verschiedene Calciumcobaltitpulver wurden druckgesintert und das Gefüge sowie die thermoelektrischen Eigenschaften untersucht. Die Dotierung mit Bismut führte zu einer Verschlechterung der elektrischen Leitfähigkeit bei druckgesinterten Proben im Gegensatz zu undotierten Pulvern.
Reaction sintering and sintering additives for cost-effective production of thermoelectric oxides
(2020)
Thermoelectric oxides attract much interest recently. Although their thermoelectric properties are inferior to non-oxides, they exhibit distinct advantages. Thermoelectric oxides are stable in air at higher temperatures, their raw materials are less toxic, and more abundant. To enhance attractivity of these materials for industrial applications, production costs need to be reduced.
Conventionally, the legs of thermoelectric generators are sintered from green bodies of previously synthesized powder. Reaction-sintering is a fabrication method without a powder synthesis step, as the final phase is formed during the sintering from a raw material mixture. Moreover, the reduction of chemical potential during reaction-sintering is effective as an additional driving force for sintering. We show that reaction-sintering increases the densification of CaMnO3 (n-type, Sm doped). Consequently, the electrical conductivities improved by about 100 % leading to superior power factors (PF = 230 µW/mK² for CaMnO3).
Another approach to reduce the production costs is to lower the sintering temperature by adding sinter additives. The addition of 4 wt% CuO to CaMnO3 lowers the sinter temperature from 1250 °C to 1050 °C. The achieved power factor PF = 264 µW/mK is more than two times higher as reported in literature for the same dopant.