Filtern
Dokumenttyp
- Vortrag (31) (entfernen)
Sprache
- Englisch (31)
Referierte Publikation
- nein (31) (entfernen)
Schlagworte
- Ageing (31) (entfernen)
Organisationseinheit der BAM
- 3 Gefahrgutumschließungen; Energiespeicher (14)
- 3.3 Sicherheit von Transportbehältern (6)
- 3.4 Sicherheit von Lagerbehältern (6)
- 7 Bauwerkssicherheit (3)
- 8 Zerstörungsfreie Prüfung (3)
- 3.1 Sicherheit von Gefahrgutverpackungen und Batterien (2)
- 7.5 Technische Eigenschaften von Polymerwerkstoffen (2)
- 8.5 Röntgenbildgebung (2)
- 9 Komponentensicherheit (2)
- 9.6 Additive Fertigung metallischer Komponenten (2)
Eingeladener Vortrag
- nein (31)
As a Federal institute for materials research and testing it is part of our tasks to evaluate the safety of casks designed for transport and/or storage of radioactive material. This includes the investigation of elastomeric seals and polymeric neutron shielding materials used in the containers.
In this contribution we would like to present our research focused on the long term performance and associated changes of material properties of elastomeric seals (e.g. EPDM, FKM) and neutron shielding materials ((Ultra) High Molecular Weight Polyethylene) employed in storage casks. Our approach comprises accelerated ageing investigations at elevated temperatures and to some extent investigations of irradiated materials.
As the requirements for the extended use of cables in nuclear power plants and for the long term use of cask components are to a certain extent similar, our work might be of interest for the workshop on “Cables ageing in nuclear power plants; R&D current status and forecast”.
BAM is the federal institute for materials research and testing in Germany. One of our tasks is to evaluate the safety of casks designed for transport and/or storage of radioactive waste. As elastomeric seals are used in the containers as safety-relevant parts, it is our goal to be able to evaluate the service lifetime of the seals with regard to the requirements for long-term safety (40 years and more) of the containers. For this reason, an accelerated ageing programme with selected rubbers often used for seals (HNBR, EPDM and FKM) was started. Ageing was performed at four different temperatures (75 °C, 100 °C, 125 °C and 150 °C) for up to 2 years. For assessing properties related to the sealability, O-rings were aged in compression by 25 % (corresponding to the compression during service) between plates. For comparison, uncompressed O-rings were aged as well. The aged materials were characterized with conventional polymer analysis methods such as hardness and tensile tests, but also with more seal-specific methods such as compression stress relaxation (CSR, reflecting the loss of sealing force of a compressed seal over time), and compression set (CS, representing the recovery behaviour of a seal after release from compression). CS is chosen as the property for lifetime prediction as it is both sensitive to degradation and related to the seal performance. CS data is extrapolated to 60 °C, which yields lifetimes of approximately 5 years for HNBR and 64 years for EPDM for a criterion of 85 % CS respectively, and approx. 40 years for FKM for a criterion of 65 % CS (the highest value measured so far).
The ageing of polymers, including elastomers, is an undesirable but inevitable process leading to a limited lifetime of rubber products such as seals. In order to investigate the degradation of material properties of elastomers used as seals, an ageing programme was started with hydrogenated acrylonitrile butadiene rubber (HNBR), ethylene propylene diene rubber (EPDM) and fluorocarbon rubber (FKM) [1-3]. Sheets of 2 mm thickness were aged at four different temperatures (75 °C, 100 °C, 125 °C and 150 °C) for time periods of 1 day up to 1 year. The aged samples were examined using standard analytical methods such as hardness, dynamic-mechanical analysis (DMA), thermogravimetric analysis (TGA), mass loss, density and tensile tests. Additionally, DMA equipment was used to investigate relaxation and recovery behaviour which is more sensitive to degradation effects and can help to correctly interpret data from hardness and DMA measurements. The results show e.g. an increase in hardness and glass transition temperature for HNBR and, less pronounced, for EPDM. This confirms ageing mechanisms described in the literature, e.g. dominant crosslinking reactions in HNBR and both chain scissions and crosslinking for EPDM. FKM, which is very heat resistant, exhibits only minor degradation. Where possible, shift factors for time-temperature data sets were determined. The values obtained from different methods are compared and discussed.
BAM is the federal institute for materials research and testing in Germany. One of our tasks is to evaluate the safety of casks designed for transport and/or storage of radioactive waste. As elastomeric seals are used in the containers as safety-relevant parts, it is our goal to be able to evaluate the service lifetime of the seals with regard to the requirements for long-term safety (40 years and more) of the containers. For this reason, an accelerated ageing programme with selected rubbers often used for seals (HNBR, EPDM and FKM) was started. Ageing was performed at four different temperatures (75 °C, 100 °C, 125 °C and 150 °C) for up to 2 years. For assessing properties related to the sealability, O-rings were aged in compression by 25 % (corresponding to the compression during service) between plates. For comparison, uncompressed O-rings were aged as well. The aged materials were characterized with conventional polymer analysis methods such as hardness and tensile tests, but also with more seal-specific methods such as compression stress relaxation (CSR, reflecting the loss of sealing force of a compressed seal over time), and compression set (CS, representing the recovery behaviour of a seal after release from compression). CS is chosen as the property for lifetime prediction as it is both sensitive to degradation and related to the seal performance. CS data is extrapolated to 60 °C, which yields lifetimes of approximately 5 years for HNBR and 64 years for EPDM for a criterion of 85 % CS respectively, and approx. 40 years for FKM for a criterion of 65 % CS (the highest value measured so far).
The Bundesanstalt für Materialforschung und –prüfung (BAM) and Sandia National Laboratories (SNL) entered into a Memorandum of Understanding (MOU) in September 2012 to foster technical collaborations in the areas associated with the backend of the commercial nuclear fuel cycle. Specifically, the focus is on packaging, transportation, and storage of commercial spent nuclear fuel. The institutes meet about twice each year, alternating between institutes. This provides the opportunity for staff members from the host organization more exposure to technical issues that are of concern internationally and to collaborate with technical experts working on similar problems.
Since 2012, the focus of the meetings has been on technical issues associated with extended dry storage and subsequent transportation of commercial spent fuel. Topics range from hydride effects on cladding integrity, spent fuel response during Normal Conditions of Transport (NCT), finite element analyses of fuel and cask response to accident conditions, bolt and seal behavior over extended periods of time, and corrosion associated with bolts, metallic seals, and stainless steel canisters.
This MOU has provided an effective leverage for technical collaboration. For example, SNL is funding (through DOE), Savannah River National Laboratories (SRNL) to look at bolt and seal degradation issues. SRNL has an MOU with BAM to collaborate on bolt and seal degradation during extended storage. Likewise, Sandia and BAM are collaborating with the EC Joint Research Center on an International Nuclear Energy Research Initiative (I-NERI) to investigate spent fuel behavior when subjected to mechanical loadings. This important work will provide insight into failure mechanisms, as well as spent fuel release fractions, given a breach of the cladding wall.
This presentation provides an overview of high ranked technical issues associated with extended storage and subsequent transportation, as well as the work underway at BAM and SNL that are addressing these issues.
Characterisation of degradation and determination of end-of-lifetime criterion for O-ring seals
(2017)
The ageing of polymers, including elastomers, is an undesirable but inevitable process leading to a limited lifetime of rubber products such as seals. Independent of the application, as e.g. automotive, piping or container applications, a long lifetime or at least a timely exchange of a seal before occurence of critical failure is desired.
In order to investigate the degradation of material properties and to determine the lifetime of elastomers used as seals, an ageing programme was started with hydrogenated acrylonitrile butadiene rubber (HNBR), ethylene propylene diene rubber (EPDM) and fluorocarbon rubber (FKM) [1-3]. Both O-ring seals (uncompressed and compressed by 25 %) with a cord diameter of 10 mm as well as sheets with a thickness of 2 mm were aged at 75 °C, 100 °C, 125 °C and 150 °C for up to two years. The changes of material properties during ageing were characterised for each material using the sheets by means of e.g. dynamic-mechanical analysis and tensile tests, while sealing properties such as compression stress relaxation (CSR), compression set (CS) and leakage rate were determined on O-rings. The experimental results indicate that while material properties, CSR and CS show considerable degradation effects, the static leakage rate stays constant or even decreases before failure occurs quite suddenly at advanced degradation levels. This reveals that static leakage rate has only limited sensitivity for the degradation of the seal material.
Our approach to determine a suitable end of lifetime criterion, which involves a partial decompression of the seal during the leakage test, is presented and discussed.
Elastomer seals are widely used as barrier seals in containers for low and intermediate level radioactive waste and in some countries for spent fuel transportation casks. Depending on the area of use, the rubber materials have to demonstrate proper sealing performance with regard to mechanical, thermal and environmental conditions as well as irradiation during the entire operation period.
In Germany the low and intermediate level radioactive waste is planned to be disposed in the Konrad repository in standardized containers. Many of these containers use an elastomer seal between lid and container body. Depending on the radiactive inventory and a possible containment of the waste in inner barrels and/or concrete structures, such containers may require a specific leak tightness. In such cases, specified leakage rates are shall not be exceeded by the the seals to keep potential activity releases from the inventories well below defined limits.
Generally, all waste containers have to fulfill the waste acceptance criteria for the Konrad repository as defined by the reports BfS SE-IB-29/08 and SE-IB-30/08. From these criteria several requirements for seal performance are derived. The seals have to:
- ensure full functionality until final container disposal,
- maintain its function in case of a thermal or mechanical accident,
- ensure encapsulation also at -20 °C.
This combination of requirements is challenging especially as a seal exchange, which is typical for many other applications, is hardly possible and thus a sound understanding of how to perform safety evaluation of containers is required. Therefore BAM has initiated investigations on elastomer seal behaviour. This work focuses on low temperature behaviour and sealing performance concerning static conditions as well as partial loss of compression and ageing of elastomer seals. Concerning ageing, property changes caused by long-term thermooxidative conditions as well as gamma irradiation are investigated.
This contribution presents an overview and explanation of the aims of the ongoing research and gives an update of the most relevant results.
Elastomer seals are widely used as barrier seals in containers for low and intermediate level radioactive waste. In addition, they are also used in waste fuel storage and transportation casks as auxiliary seals. Depending on the area of use, the rubber materials have to demonstrate proper sealing performance with respect to mechanical, thermal and environmental conditions as well as irradiation during the entire operation period. A fundamental understanding of the structure property relationship and their changes during aging can help to evaluate the long-term sealing performance.
In the present study, specific materials are investigated to study the structure-property and seal performance-correlation. Fluoro-elastomer (FKM), silicone rubber (VMQ) and ethylene propylene diene rubber (EPDM) were chosen as base rubbers. Comparable mechanical properties for these seals, especially in terms of a comparable compression behavior were achieved by careful control of base rubber formulation, i.e., by opting for the right filler and its concentration, amount of crosslinking chemicals, and with the assistance of process oils. Moreover, with the same rubber, similar mechanical properties were achieved by varying the filler concentration and crosslinking degree, which shall enable to correlate the particular influence on the structure property dependency of the seals in detail. The materials are investigated under pristine and aged conditions to evaluate the influence of aging, e.g. on the stress relaxation or recovery behavior. These values appear to be suitable parameters to judge the expected sealing performance.
Due to the electrically conducting nature of some fillers used to reinforce rubbers (such as carbon blacks, carbon nanotubes (CNTs), Graphene, etc.) it is possible to obtain current information about mechanical and visco-elastic properties by monitoring the electrical conductivity or resistivity. A simple relation that relates electrical resistance with mechanical stress was derived and the stress values were theoretically predicted from the electrical resistance values, which showed good correlation with experimental results.
Elastomer seals are widely used as barrier seals in containers for low and intermediate level radioactive waste. In addition, they are also used in waste fuel storage and transportation as auxiliary seals. Depending on the area of use, the rubber materials have to demonstrate proper sealing performance with regard to mechanical, thermal and environmental conditions as well as irradiation during the entire operation period. A fundamental understanding of the structure property relationship can help to understand the performance of rubber seals in aged conditions. The present study focuses on the investigation of specific materials to study the structure-property and seal performance-correlation. Fluoro-elastomer (FKM), silicone rubber (VMQ) and ethylene propylene diene rubber (EPDM) were chosen as the prime candidates. Mechanical properties for these seals were achieved by careful control of base rubber formulation, i.e., by opting for the right filler and its concentration, amount of crosslinking chemicals, and with the assistance of process oils. Moreover, with the same rubber, similar mechanical properties were achieved by varying the filler concentration and crosslinking degree, which enables us to understand the structure property dependency of the seals in detail. The materials are investigated in the pristine and under aged conditions to evaluate the influence of ageing on e.g. the stress relaxation or recovery behavior. These values appear to be suitable parameters to judge the expected seal performance. Due to the electrically conducting nature of fillers used to reinforce rubbers (such as carbon blacks, carbon nanotubes (CNTs), Graphene, etc.) it is possible to obtain current information about mechanical and visco-elastic properties by monitoring the electrical conductivity or resistivity. A simple relation that bridges electrical resistance and the mechanical stress was derived and the stress values were theoretically predicted from the electrical resistance values, which showed good correlation with experimental results.