Additive manufacturing (AM) offers a range of novel applications. However, the manufacturing process is complex and the production of defect-free parts with a high reliability is still a challenge. Thermography is a valuable tool for process surveillance, especially in metal AM processes. The high process temperatures allow one to use cameras usually operating in the visible spectral range. Here, we compare the results of first measurements during the manufacturing process of a commercial laser metal deposition (LMD) setup using a MWIR camera with those from a VIS high-speed camera with band pass filter in the NIR range.
Additive manufacturing (AM) opens the route to a range of novel applications.However, the complexity of the manufacturing process poses a challenge for the production of defect-free parts with a high reliability. Since process dynamics and resulting microstructures of AM parts are strongly influenced by the involved temperature fields, thermography is a valuable tool for process surveillance. The high process temperatures in metal AM processes allow one to use cameras usually operating in the visible spectral range to detect the thermally emitted radiation from the process. In our work, we compare the results of first measurements during the manufacturing processes of a commercial laser metal deposition (LMD) setup and a laser beam melting (LBM) setup using a MWIR camera with those from a VIS high-speed camera with band pass filter in the NIR range.
Additive manufacturing (AM) opens the route to a range of novel applications. However, the complexity of the manufacturing process poses a challenge to produce defect-free parts with a high reliability. Since process dynamics and resulting microstructures of AM parts are strongly influenced by the involved temperature fields and cooling rates, thermography is a valuable tool for process monitoring. Another approach to monitor the energy input into the part during process is the use of optical tomography.
Common visual camera systems reach much higher spatial resolution than infrared thermography cameras, whereas infrared thermography provides a much higher temperature dynamic. Therefore, the combined application increases the depth of information. Here, we present first measurement results using a laser beam melting setup that allows simultaneous acquisition of thermography and optical tomography from the same point of view using a beam splitter. A high-resolution CMOS camera operating in the visible spectral range is equipped with a near infrared bandpass filter and images of the build plate are recorded with long-term exposure during the whole layer exposing time. Thus, areas that reach higher maximum temperature or are at elevated temperature for an extended period of time appear brighter in the images. The used thermography camera is sensitive to the mid wavelength infrared range and records thermal videos of each layer exposure at an acquisition rate close to 1 kHz.
As a next step, we will use computer tomographic data of the built part as a reference for defect detection.
This research was funded by BAM within the focus area Materials.
The main solidification parameters, namely the crystal axis, the growth rate, and the cross-sectional area of the columnar crystal control the primary microstructure and thus the final weld seam properties.
Limited understanding of solidification parameters due to complexities in experimental and theoretical weld pool boundary determination and
its mathematical description.
Application of local Lamé curves for efficient weld pool boundary reconstruction Derivation of general analytical solutions for the main solidification parameters of a two-dimensional columnar crystal growth during laser beam welding of thin steel sheets.
The Lamé curves approximation technique was successfully applied for the reconstruction of the rear part of the two-dimensional steady-state weld pool boundary. General analytical expressions for the main solidification parameters, namely the crystal axis, the growth rate and the cross-sectional area of the crystal were derived.
The derived expressions and herewith obtained results were verified and validated by comparing them to known theoretical solutions and experimental measurements. Dimensionless analysis of the influence of the size and shape of the rear weld pool boundary on the solidification parameters was provided.
The derived general solutions and the analysis provided allow for critical welding parameters to be estimated and adapted accordingly to improve the welding process.
Despite of the significant advances in additive manufacturing (AM) process optimization there is still a lack of experimental results and understanding regarding the mechanical behavior and its relationship with the microstructural features of AM-parts, especially in loading conditions typical for safety-relevant applications. Within the scope of the presented ongoing investigations, a basic microstructural characterization, tensile tests at room and elevated temperature (400°C) as well as a characterization of the fatigue behavior of additively manufactured Ti-6Al-4V in the low cycle fatigue regime are carried out in the as-built state. After failure, different techniques are used to describe the failure mechanisms of the specimens. The AM-Specimens are provided by the Fraunhofer institute for production systems and design technology and investigated at the BAM following the philosophy of the TF-Project AGIL.
The motivation and the measurement setup for large fast-scanning piezoresistive cantilevers are presented. The theory behind the measurements of mechanical properties through contact resonance is explained. Results of such measurements on two kinds of polymer are compared to results from force distance curves. Noise, time-dependency and dependency of the results on the vibration mode are identified as challenges of contact resonance.
The geometry of the melt pool in laser beam welding plays a major role to understand the dynamics of the melt and its solidification behavior. In this study, a butt configuration of 20 mm thick structural steel and transparent quartz glass was used to observe the weld pool geometry in the partial penetration mode by means of a high-speed camera. The observations show that the dimensions of the weld pool vary depending on the depth. The areas close to the weld pool surface take a teardrop-shape. A bulge-region and its temporal evolution were observed approximately in the weld pool root. Additionally, a 3D transient thermal-fluid numerical simulation was performed to obtain the weld pool shape and to understand the formation mechanism of the observed bulging effect. The model considers the local temperature field, the effects of phase transition, thermo-capillary convection, natural convection and temperature-dependent material properties. The numerical results showed good accordance and were furthermore used to improve the understanding of the experimentally observed bulging effect.
Influence of deposition hatch length on residual stress in selective laser melted Inconel 718
(2018)
The present study aims to evaluate the bulk residual stresses in SLM parts by using neutron diffraction measurements performed at E3 line -BER II neutron reactor- of Helmholtz-Zentrum für Materialien und Energie (HZB) Berlin. Together with microstructure characterization and distortion measurements, it is possible to describe the stress state throughout the whole sample. The sample was measured in as-build condition (on a build plate) and after releasing from the build plate. The used material is the nickel based superalloy 718. This alloy is widely used in aerospace and chemical industries due to its superior corrosion and heat resistant properties.
Obtained results indicated different residual stress states for each of the transversal, longitudinal and normal component. The normal and transversal component exhibits a rather compressive behavior while the longitudinal was tensile in the center part of the sample and became compressive towards the tip. As expected, the absolute values of all stress components decreased after releasing the sample from the building plate. A surface scan utilizing a coordinate-measuring machine (CMM) allowed us to present top surface distortion before and after releasing. The top surface showed a distortion around ±80µm after releasing. Microstructure evolution in the scanning-building cross-section is largely dominated by columnar grains. In addition, many small random orientated grains are prominent in the regions of a laser overlap during SLM.
In summary, for the sample of superalloy 718 manufactured by SLM, a small distortion occurred when removing the sample from the build plate whereby the residual stress state decreases. Moreover, the observed columnar grains in the building direction could give a reason for the lowest stress values in that normal direction. However, the most important parameter controlling the residual stresses is the temperature gradient. Hence, future investigations are planned for a different scan strategy to distribute the laser impact in a more homogenous manner.
Laser implantation aims at reducing friction and wear on highly stressed surfaces in forming processes. Especially the hot stamping process that is used as a resource efficient process for manufacturing geometrical complex and high-strength structures, exhibits severe wear and high friction during the forming operation. The laser implantation process addresses this problem by combining two different approaches (surface modification and surface structuring) in surface technology by creating elevated, highly wear-resistant micro-features to influence the tribological performance. Pure TiB2 implants have shown to reduce tool-sided wear significally and improve the part formability by reducing local necking in deep drawing tests. Within the scope of this work, TiB2-TiC and TiB2-TaC hard material mixtures are implanted on X38CrMoV5-3 hot work tool steel. The aim is to investigate how the implant material properties can be influenced by the application of different mixing ratios of hard material mixtures under the specific variation of the process parameters. Distinct implant formations are tested on a novel test apparatus to examine the influence on the tribological properties.
From the analyses of the implant properties by hardness measurements, light microscopic images, EDX and XRD analyses process parameter ranges are identified to produce defect-free dome- and ring-shaped implants. The specific process parameters (pulse power, pulse duration, mixing ratio and coating thickness) can be used for the determination of the implant geometry (height, width and depth). The tribological tests exhibit improved friction and wear properties. Based on these results, a tribosystem manufactured by this additive surface treatment technology shows great potential to enhance the effectiveness of the hot stamping process.
Entwicklung einer Bohrlochsonde für Ultraschalluntersuchungen an Abschlussbauwerken in Endlagern
(2021)
Für die Qualitätssicherung von Abschlusswerken für Endlager wird eine Ultraschall-Bohrlochsonde entwickelt. Mithilfe dieser Sonde, die aus einer Vielzahl von einzelnen koppelmittelfreien Ultraschall-Punktkontaktprüfköpfen besteht, soll die Rissfreiheit der Versuchsbauwerke überprüft werden.
Ein erster Prototyp der Sonde wurde mit einem kommerziellen Ultraschallgerät betrieben und bestand aus 12 Transversalwellen-Punktkontaktprüfköpfen von denen jeweils sechs als Sender und sechs als Empfänger parallelgeschaltet waren. Um den erzeugten Schalldruck der Bohrlochsonde zu steigern, wurde bei der Neuentwicklung die Prüfkopfanzahl erhöht und zusätzlich die laufzeitgesteuerte Anregung der einzelnen Prüfköpfe vorgesehen. Für die Anregung der Prüfköpfe mit programmierten Zeitverzögerungen wurde ein neuartiger mehrkanaliger Sender für bipolare Rechtecksignale entwickelt.
Durch die Entwicklung der Bohrlochsonde soll eine dynamische Anpassung der Prüfkopf-Apertur sowie eine Fokussierung des Schallfeldes in Abhängigkeit der zu untersuchenden Tiefe erfolgen. Mithilfe entsprechender Anregungsfunktionen kann das Schallfeld der Bohrlochsonde unterschiedlich geformt werden, z. B. ist auch ein Schwenken des fokussierten Schallbündels möglich. Dadurch wird das erfasste Prüfvolumen begrenzt und auf diese Weise das Signal-Störverhältnis der Empfangssignale verbessert. In Kombination mit SAFT-Rekonstruktionsrechnungen wird durch eine optimierte Abstrahlcharakteristik der Sonde mit einem hohen Schalldruck unter verschiedenen Winkeln eine verbesserte Signalqualität und damit eine erhöhte Aussagesicherheit der Ergebnisse in der Objektabbildung erwartet.
Für die konventionelle Fertigung hat sich das bestehende System der Qualitätsinfrastruktur (QI) bewährt. Die additive Fertigung vergrößert den gestalterischen Spielraum von möglichen Bauteilgeometrien und Prozessfehlern jedoch erheblich. Hier gerät die QI an ihre Grenzen, sodass die Fertigung und Zulassung sicherheits-relevanter Bauteile sehr zeit- und kostenintensive Versuche erfordern. Eine moderne digitale QI erlaubt eine effizientere Qualitätssicherung für additiv gefertigte Bauteile. Dies erfordert eine durchgängig digitale Abbildung des physischen Materialflusses.
In Hinblick auf den austenitischen Stahl AISI 316L erzeugt das pulverbettbasierte selektive Laserstrahlschmelzen, als ein additives Fertigungsverfahren, kristallographisch texturierte und Multiskalige Mikrostruktur. Einerseits können diese Mikrostrukturen zu einer Verbesserung der statischen mechanischen Eigenschaften führen (z. B. zu einer höheren Streckgrenze). Andererseits stehen diesen Verbesserungen der mechanischen Eigenschaften hohe Eigenspannungen gegenüber, die sich nachteilig auf das Ermüdungsverhalten auswirken können. Zur Reduzierung der Eigenspannungen und der daraus resultierenden negativen Auswirkungen auf die Ermüdungseigenschaften, werden Bauteile nach der Herstellung typischerweise wärmebehandelt. In dieser Studie wurde eine niedrige Wärmebehandlungstemperatur von 450°C höher temperierten Behandlungen bei 800 °C und 900 °C gegenübergestellt. Diese Wärmebehandlungstemperaturen bilden die oberen und die untere Grenze ein Spannungsarmglühendes Materials, ohne die prozessinduzierte Mikrostruktur signifikant zu verändern. Zusätzlich bieten diese Temperaturen den Vorteil, dass sie eine übermäßige intergranulare Ausscheidung von Karbiden und TCP-Phasen vermeiden, die zu einer Sensibilisierung des Werkstoffes gegen korrosive Umgebungen führen würden. Die Auswirkungen der Wärmebehandlung auf das Gefüge wurden mittels Rasterelektronenmikroskopie (BSE und EBSD) untersucht. Die Relaxation der Eigenspannungen wurde vor und nach den jeweiligen Wärmebehandlungen bei 800°C und 900°C mittels Neutronenbeugung charakterisiert. Die Ergebnisse zeigen, dass die Proben nach der Wärmebehandlung bei 900 °C nahezu spannungsfrei sind, was mit der Auflösung der zellularen Substruktur korreliert.
The WelDX research project aims to foster the exchange of scientific data inside the welding community by developing and establishing a new open source file format suitable for documentation of experimental welding data and upholding associated quality standards. In addition to fostering scientific collaboration inside the national and international welding community an associated advisory committee will be established to oversee the future development of the file format. The proposed file format will be developed with regards to current needs of the community regarding interoperability, data quality and performance and will be published under an appropriate open source license.
By using the file format objectivity, comparability and reproducibility across different institutes and experimental setups can be improved.
The long-term global goals of achieving almost net zero carbon emissions in the next decades are closely linked to the development of highly efficient components in plant, process and energy engineering, and their sustainable and resource-saving production. Plant components must increasingly withstand tribological loads in addition to high thermal, mechanical, and corrosive stresses. Such combined stresses demand high-performance alloys economically tailored to the application for wear protection and components produced as semi-finished products, via additive manufacturing (AM) or claddings via deposition welding. For instance, the protection of special components made of less cost-intensive materials, e.g., steel in process engineering for screw machines or exhaust gas separation, is feasible applying cost-intensive Ni- or Co-based hard-phase claddings.
Today an increasing number of above-mentioned applications demand precise finishing machining of components to ensure defined compact surfaces with a high integrity and complex contours. Contour milling is standard process for finishing machining of metals. Especially, the desired properties of wear resistant materials (e.g., high strength, hard precipitations) imply significant challenges for milling processes and tools, leading frequently to uneconomic milling conditions due to intolerable high tool wear and surface defects. Inhomogeneous, anisotropic weld structures due to cladding or AM of wear resistance alloys lead to further deteriorations of milling processes due to unstable milling conditions and process forces during chip removal.
To tackle these challenges, already several approaches exist, (1) to enhance machinability of the claddings by alloy modifications to specifically influence solidification and hard phases morphology (precipitation shape, size, distribution) and (2) to achieve significant improvements of the machining situation (e.g., increase of tool life and surfaces integrity) by means of modern hybrid machining processes such as ultrasonic-assisted milling. This contribution shows a comprehensive overview of recent results with these promising approaches for additively welded Ni- CoCr-alloys.
The mechanical behavior of normal strength and high-strength concretes under tension can be significantly improved by the incorporation of steel fibers. This improvement comprises not only an enhancement in strength and ductility, but also in energy absorption capacity, which makes steel fiber reinforced high-strength concrete potentially suitable for seismic design applications. Force transfer controlled processes between steel fibers and concrete matrix, i.e. fiber debonding and fiber pull-out during crack opening are the main mechanisms contributing to the high-energy dissipation characteristic of this composite material.
In order to gain more information on the material efficiency under tension, a comparative study on different ultra-high performance fiber reinforced concretes (UHPFCs) subjected to direct tensile loading at moderate strain rates is presented. The experimental approach considered three UHPFC mixtures, incorporating two volumetric fractions of high-strength smooth steel fibers. The stiffness modification of the concrete matrix was realized by the addition of a copolymer. The direct tensile tests were conducted on small sized dumbbell shaped specimens at nominal strain rates of 0.000025 1/s and 0.01 1/s, representing quasi-static and seismic loading conditions, respectively. For a detailed analysis of crack formation and crack propagation during load application, classical tensile tests were accompanied by non-destructive measuring technique using digital image correlation (DIC). Furthermore, relevant material parameters, such as such as first and post cracking stresses, strain capacity, and energy absorption capacity are determined and discussed.