Filtern
Erscheinungsjahr
Dokumenttyp
Schlagworte
- Nanoparticle (183) (entfernen)
Organisationseinheit der BAM
- 1 Analytische Chemie; Referenzmaterialien (73)
- 1.2 Biophotonik (48)
- 6 Materialchemie (33)
- 1.1 Anorganische Spurenanalytik (27)
- 6.5 Synthese und Streuverfahren nanostrukturierter Materialien (16)
- 6.6 Physik und chemische Analytik der Polymere (8)
- 6.3 Strukturanalytik (6)
- 1.8 Umweltanalytik (5)
- 4 Material und Umwelt (5)
- 4.2 Material-Mikrobiom Wechselwirkungen (5)
Paper des Monats
- ja (1)
Eingeladener Vortrag
- nein (50)
To enhance the biological effects of radiation damage in cancerous cells, we present an alternative approach to the use of gold nanoparticles (AuNP), focusing on the synthesis and characterization of highly monodisperse, spherical radioactive gold nanoparticles 198AuNP. The size of the AuNP size was optimized with the help of Geant4/TOPAS particle scattering simulations, and energy deposition per nm3 per decay for varying radii (2–10 nm) was evaluated. This work is the foundation for ongoing experimental work to evaluate cell death induced by 198AuNP which aims for the use of radioactive gold nanoparticles in cancer treatment.
Dose enhancement by gold nanoparticles (AuNP) was shown to increase the biological effectiveness of radiation damage in biomolecules and tissue. Most of the current studies focus on external beam therapy on combination with AuNP. Here we present a Monte-Carlo study (Geant4) to characterise radioactive AuNP. Radioactive 198 Au emits beta and gamma rays and is considered for applications with solid tumours. To effectively apply 198 AuNP their energy deposit characteristics have to be determined in terms of intrinsic and extrinsic properties e.g. AuNP diameter, AuNP density, and their clustering behaviour. After each decay process, the energy deposit, inelastic scattering events, kinetic energy spectrum of secondary particles within the AuNP themselves and in a spherical target volume of water up to 1 μm radius were determined. Simulations were performed for AuNP radii ranging from 2.5 nm to 20 nm radius, different cluster sizes and densities. The results show an increase of the energy deposit in the vicinity of the AuNP up to 150 nm. This effect nearly vanishes for distances up to one micron. For the case of AuNP clusters and the same activity, the enhancement of the energy deposit increases with the relative gold mass percentage and therefore can be adjusted by changing AuNP radius or clustering behaviour.
Using atomic force microscopy (AFM) and small angle X-ray scattering (SAXS), we show a full comparison between structuring of nanoparticles in confinement and in bulk in order to explain the effect of confinement on characteristic lengths and the scaling law of the characteristic lengths. Three different-sized particle suspensions are used to check the generalization and the correlation between the characteristic lengths and the system parameters, like particle diameter and Debye length. The two characteristic lengths obtained from AFM force curves, the oscillatory wavelength λ, which is related to the average particle distance, and the decay length ξ, which measures how far particle correlates to obtain periodic oscillations, are in good agreement with the mean particle distance 2π/qmax and the correlation length 2/Δq in bulk, respectively, obtained from the structure peaks of SAXS diagrams. Although confinement causes layering of nanoparticles parallel to the confining surfaces, the characteristic lengths in the direction perpendicular to the confining surfaces follow the bulk behavior. The wavelength scales as ρ-1/3 with the particle number density ρ irrespective of the particle size and the ionic strength and shows a pure volume effect. Upon comparing with literature results, the λ = ρ-1/3 scaling law can be applied more generally for charged particles, as long as the repulsive interaction is sufficiently long-ranged, than the previous expression of λ = 2(R + κ-1), which only approaches the value of average particle distance under specific conditions. The decay length ξ is controlled both by the particle size and the ionic strength of the suspensions, and ξ = R + κ-1 is proposed in the paper. In addition, the interaction strength, the force amplitude and maximum scattering intensity, increases linearly with particle concentration. On the other hand, the Monte Carlo (MC) simulations and approximate hypernetted chain (HNC) closure calculation based on Derjaguin-Landau-Verwey-Overbeek (DLVO) potential are employed to study the characteristic lengths from the theoretical point of view. The experimental wavelengths are in good agreement with the theoretical counterparts and the experimental decay lengths show the same qualitative behavior as theoretical ones on the particle size and ionic strength.
Comprehensive Characterization of APTES Surface Modifications of Hydrous Boehmite Nanoparticles
(2020)
Hydrous boehmite (γ-AlOOH) nanoparticles (BNP) show great potential as nanoscale filler for the fabrication of fiber reinforced nanocomposite materials. Notably, the particle−matrix interaction has been demonstrated to be decisive for improving the matrix-dominant mechanical properties in the past years. Tailoring the surface properties of the nanofiller enables to selectively design the interaction and thus to exploit the benefits of the nanocomposite in an optimal way. Here, an extensive study is presented on the binding of (3-aminopropyl)triethoxysilane (APTES), a common silane surface modifier, on BNP in correlation to different process parameters (concentration, time, temperature, and pH). Furthermore, a comprehensive characterization of the modified BNP was performed by using elemental analysis (EA), thermogravimetric analysis (TGA) coupled with mass spectrometry (TGA-MS), and Kaiser’s test (KT). The results show an increasing monolayer formation up to a complete surface coverage with rising APTES concentration, time, and temperature, resulting in a maximal grafting density of 1.3 molecules/nm². Unspecific multilayer formation was solely observed under acidic conditions. Comparison of TGA-MS results with data recorded from EA, TGA, and KT verified that TGA-MS is a convenient and highly suitable method to elucidate the ligand binding in detail.
Whilst a decisive role of the particle-matrix interphase on the mechanical properties of nanoparticle-filled polymers has been demonstrated in the last years, the arbitrary design of this interphase remains a very challenging goal. In principle, this could be realized via an appropriate surfacemodification of the nanofiller prior to its incorporation in the polymer. For most systems, such as for boehmite nanofillers, however, the interaction of organic modifiers with the particle surface has not been studied in detail, and only single studies are known rather than systematic investiga- tions on the effects of different chemical functions anchored on the particle surface. In this chapter, we present an extensive study on the binding of APTES, a common silane surface modifier, with boehmite, and show that thermogravimetric analysis (TGA) coupled with mass spectrometry (MS) is a convenient and highly suitable method to elucidate the ligand binding in detail. Furthermore, a two-step coupling strategy is presented, demonstrating that based on APTES anchored to the parti- cle surface, the condensation of various carboxylic acids can be utilized to enable highly diverse chemical properties of the nanofillers, which leads to very different particle-matrix interactions in the nanocomposites.
We synthesized a generation of water-soluble, atomically precise gold nanoclusters (Au NCs) with anisotropic Surface containing a short dithiol pegylated chain (AuMHA/TDT). The AuMHA/TDT exhibit a high brightness (QY ∼ 6%) in the shortwave infrared (SWIR) spectrum with a detection above 1250 nm.
Furthermore, they show an extended half-life in blood (t1/2ß = 19.54 ± 0.05 h) and a very weak accumulation in organs. We also developed a non-invasive, whole-body vascular imaging system in the SWIR window with high-resolution, benefiting from a series of Monte Carlo image processing. The imaging process enabled to improve contrast by 1 order of magnitude and enhance the spatial Resolution by 59%. After systemic administration of these nanoprobes in mice, we can quantify vessel complexity in depth (>4 mm), allowing to detect very subtle vascular disorders non-invasively in bone morphogenetic protein 9 (Bmp9)-deficient mice. The combination of these anisotropic surface charged Au NCs plus an improved SWIR imaging device allows a precise mapping at high-resolution and an in depth understanding of the organization of the vascular network in live animals.
Two sets of polystyrene nanoparticles (PSNPs) with comparable core sizes but different carboxyl group densities were made and separated using asymmetric flow field flow fractionation (AF4), capillary electrophoresis (CE), and the off-line hyphenation of both methods. Our results revealed the significant potential of two-dimensional off-line AF4-CE hyphenation to improve the separation and demonstrated for the first time, the applicability of CE to determine the functional group density of nanoparticles (NPs). Compared to the result acquired with conductometric titration, the result obtained with synthesized 100 nm sized PSNPs revealed only a slight deviation of 1.7%. Commercial 100 nm sized PSNPs yielded a deviation of 4.6 %. For 60 nm sized PSNPs, a larger deviation of 10.6 % between both methods was observed, which is attributed to the lower separation resolution.
Nowadays, different nanoparticles have been developed for commercial applications. However, since data on toxicity are barely available, their increasing application in cosmetic products, food and their release in the environment might cause severe problems. Since a range of physical, chemical, and biological characteristics of NPs are closely related to particle size and surface functionalization, precise separation and surface groups quantification is essential to acquire an in-depth understanding of their properties.
In this work, the performance of asymmetrical flow field flow fractionation (AF4) and capillary electrophoresis (CE) for the separation of nanoparticles (NPs) with different sizes, coatings, and coating densities was investigated and optimized.
For the first time, a two-dimensional off-line hyphenation of both techniques (AF4-CE) was developed. The results clearly demonstrated, that AF4-CE hyphenation can significantly improve the separation resolution and reduce the peak broadening in CE. Also, for the first time, CE was employed to determine the coating density of NPs and the results were in good agreement with the values acquired with conductometric titration.
The successful off-line coupling of asymmetrical flow field flow fractionation (AF4) and capillary electrophoresis (CE) for Separation of nanoparticles (NPs) with different surface coatings was shown.
Two mixtures of polystyrene nanoparticles (PS-NPs) with comparable core sizes (20 nm and 50 nm) but different coatings (no coating/carboxyl-coated) were studied. Separation in either method resulted in non-baseline resolved or non-separated peaks. In contrast, two-dimensional off-line coupling of AF4 and CE resulted in clearly separated regions in their 2 D plots and can obviouly improve separation resolution.
High sensitizer and activator concentrations have been increasingly examined to improve the performance of multi-color emissive upconversion (UC) nanocrystals (UCNC) like NaYF4:Yb,Er and first strategies were reported to reduce concentration quenching in highly doped UCNC. UC luminescence (UCL) is, however, controlled not only by dopant concentration, yet by an interplay of different parameters including size, crystal and shell quality, and excitation power density (P). Thus, identifying optimum dopant concentrations requires systematic studies of UCNC designed to minimize additional quenching pathways and quantitative spectroscopy. Here, we quantify the dopant concentration dependence of the UCL quantum yield (ΦUC) of solid
NaYF4:Yb,Er/NaYF4:Lu upconversion core/shell nanocrystals of varying Yb3+ and Er3+ concentrations (Yb3+ series: 20%‒98% Yb3+; 2% Er3+; Er3+ series: 60% Yb3+; 2%‒40% Er3+). To circumvent other luminescence quenching processes, an elaborate synthesis yielding OH-free UCNC with record ΦUC of ~9% and ~25 nm core particles with a thick surface shell were used. High Yb3+ concentrations barely reduce ΦUC from ~9% (20% Yb3+) to ~7% (98% Yb3+) for an Er3+ concentration of 2%, thereby allowing to strongly increase the particle absorption cross section and UCNC brightness. Although an increased Er3+ concentration reduces ΦUC from ~7% (2% Er3+) to 1% (40%) for 60% Yb3+. Nevertheless, at very high P (> 1 MW/cm2) used for microscopic studies, highly Er3+-doped UCNC display a high brightness because of reduced saturation. These findings underline the importance of synthesis control and will pave the road to many fundamental studies of UC materials.