Filtern
Dokumenttyp
- Zeitschriftenartikel (7)
- Vortrag (1)
- Posterpräsentation (1)
Sprache
- Englisch (9)
Schlagworte
- Fluoride (9) (entfernen)
Organisationseinheit der BAM
- 1 Analytische Chemie; Referenzmaterialien (5)
- 1.2 Biophotonik (3)
- 6 Materialchemie (3)
- 6.1 Oberflächen- und Dünnschichtanalyse (3)
- 4 Material und Umwelt (2)
- 6.3 Strukturanalytik (2)
- 1.1 Anorganische Spurenanalytik (1)
- 1.7 Organische Spuren- und Lebensmittelanalytik (1)
- 1.8 Umweltanalytik (1)
- 4.1 Biologische Materialschädigung und Referenzorganismen (1)
Paper des Monats
- ja (1)
Eingeladener Vortrag
- nein (1)
Alkaline earth metal fluoride nanoparticles have been investigated for application in wood protection. Sols of MgF2 and CaF2 were synthesized and their efficacy was tested against fungi and termites (Rehmer 2016, Krahl et al. 2016). The sols were characterized by XRD and SEM. The wood specimens were vacuum impregnated with nanoparticles and then exposed to fungi and termites according to EU certified test conditions. Our results show that wood impregnated with metal fluoride nanoparticles significantly reduce cellulose hydrolysis by fungi and termites. The wood samples were exposed to brown-rot fungi; Coniophora puteana and Poria placenta. Between the two fungi, the overall mass lost due to fungal degradation was lower for treated (MgF2 and CaF2) wood samples exposed to Coniophora puteana. Thus, the metal fluoride nanoparticles impregnated in the wood samples were more efficient in reducing cellulose degradation from Coniophora puteana than from Poria placenta. However the mass loss in samples treated with MgF2 was similar to those treated with CaF2, irrespective of type of fungi. Therefore, it is likely that fungal degradation in treated samples was dependent on the biocidal action of fluorides rather than on the differences in chemical and physical properties of MgF2 and CaF2, respectively. Conversely, for termite exposure, wood samples treated with MgF2 had lower cellulose degradation compared to those treated with CaF2. A possible explanation for this difference in results could be fungi and termites use separate mechanisms for cellulose hydrolysis which will be further investigated. Future experiments include testing the leaching potential of MgF2 and CaF2 nanoparticles from wood. The results from the leaching experiment will test if metal fluoride nanoparticles can provide long-term and environmentally safe protection to wood.
Improved Durability of Wood Treated with Nano Metal Fluorides against Brown-Rot and White-Rot Fungi
(2022)
Low-water soluble metal fluorides such as magnesium fluoride (MgF2) and calcium Fluoride (CaF2) were evaluated for decay protection of wood. Initially, the biocidal efficacy of nano metal fluorides (NMFs) against wood destroying fungi was assessed with an in-vitro agar test. The results from the test showed that agar medium containing MgF2 and CaF2 was more efficient in preventing fungal decay than stand-alone MgF2 or CaF2. These metal fluorides, in their nanoscopic form synthesized using fluorolytic sol-gel synthesis, were introduced into the sapwood of Scots pine and beech wood and then subjected to accelerated ageing by leaching (EN 84). MAS 19F NMR and X-ray micro CT images showed that metal fluorides were present in treated wood, unleached and leached. Decay resistance of Scots pine and beech wood treated with NMFs was tested against Wood destroying fungi Rhodonia placenta and Trametes versicolor in accordance with EN 113. Results revealed that mass losses were reduced to below 3% in wood treated with the combination of MgF2 and CaF2.
It is concluded that NMFs provide full protection to wood even after it has been leached and can be used as wood preservatives in outdoor environments.
We studied the dissolution behavior of β NaYF4:Yb(20%), Er(2%) UCNP of two different sizes in biologically relevant media i.e., water (neutral pH), phosphate buffered saline (PBS), and Dulbecco’s modified Eagle medium (DMEM) at different temperatures and particle concentrations. Special emphasis was dedicated to assess the influence of different surface functionalizations, particularly the potential of mesoporous and microporous silica shells of different thicknesses for UCNP stabilization and protection. Dissolution was quantified electrochemically using a fluoride ion selective electrode (ISE) and by inductively coupled plasma optical emission spectrometry (ICP OES). In addition, dissolution was monitored fluorometrically. These experiments revealed that a thick microporous silica shell drastically decreased dissolution. Our results also underline the critical influence of the chemical composition of the aqueous environment on UCNP dissolution. In DMEM, we observed the formation of a layer of adsorbed molecules on the UCNP surface that protected the UCNP from dissolution and enhanced their fluorescence. Examination of this layer by X ray photoelectron spectroscopy (XPS) and mass spectrometry (MS) suggested that mainly phenylalanine, lysine, and glucose are adsorbed from DMEM. These findings should be considered in the future for cellular toxicity studies with UCNP and other nanoparticles and the design of new biocompatible surface coatings.
For the first time, µ-X-ray fluorescence (µ-XRF) mapping combined with fluorine K-edge µ-X-ray absorption near-edge structure (µ-XANES) spectroscopy was applied to depict per- and polyfluoroalkyl substances (PFAS) contamination and inorganic fluoride in samples concentrations down to 100 µg/kg fluoride. To demonstrate the matrix tolerance of the method, several PFAS contaminated soil and sludge samples as well as selected consumer product samples (textiles, food contact paper and permanent baking sheet) were investigated. µ-XRF mapping allows for a unique element-specific visualisation at the sample surface and enables localisation of fluorine containing compounds to a depth of 1 µm. Manually selected fluorine rich spots were subsequently analysed via fluorine K-edge µ-XANES spectroscopy. To support spectral interpretation with respect to inorganic and organic chemical distribution and compound class determination, linear combination (LC) fitting was applied to all recorded µ-XANES spectra. Complementarily, solvent extracts of all samples were target-analysed via LC-MS/MS spectrometry. The detected PFAS sum values range from 20 to 1136 µg/kg dry weight (dw). All environmentally exposed samples revealed higher concentration of PFAS with a chain length >C8 (e.g. 580 µg/kg dw PFOS for Soil1), whereas the consumer product samples showed a more uniform distribution with regard to chain lengths from C4 to C8. Independent from quantified PFAS amounts via target analysis, µ-XRF mapping combined with µ-XANES spectroscopy was successfully applied to detect both point-specific concentration maxima and evenly distributed surface coatings of fluorinated organic contaminants in the corresponding samples.
The use of inorganic lanthanide-doped upconversion nanoparticles (UCNP) in bioimaging and cellular studies requires biocompatible particles. One possible cause of UCNP toxicity is the release of potentially harmful fluoride and lanthanide ions as revealed by dilution studies in aqueous environments, particularly under high dilution conditions. To address this issue, suitable surface coatings preventing such effects in combination with fast screening methods suited for online monitoring and in situ analyses are desired.
Here we present systematic studies of differently sized β-NaYF4:Yb,Er UCNP stabilized with different surface coatings and hydrophilic ligands varying in binding strength to the particle surface in various aqueous environments at different temperatures and UCNP concentrations. The concentration of the fluoride and lanthanide ions released upon particle dissolution was quantified electrochemically with a fluoride ion-sensitive electrode and inductively coupled plasma optical emission spectrometry (ICP-OES) and monitored fluorometrically, thereby exploiting the sensitivity of the upconversion luminescence to changes in size and surface chemistry. Moreover, changes in surface chemistry were determined with X-Ray photoelectron spectroscopy (XPS). Based upon our results, we could derive optimum screening parameters for UCNP stability studies and determine conditions and coating procedures and ligands for enhancing UCNP stability in aqueous environments.
Hydrogen production via formate photoreforming on TiO2 is characterized by marked dependence on the ratio between {101} and {001} surfaces for anatase nanoparticles. We observed higher rates of hydrogen Evolution with the increase of the {101} facets presence, owing to their reductive nature.
This helps the Pt photodeposition in the early stages of Irradiation and, then, the hydrogen ion reduction reaction. The selective photodeposition of 2 nm Pt nanoparticles on {101} facets was confirmed by transmission electron microscopy (TEM) micrographs. The results are confirmed also by experiments carried out without the use of Pt as cocatalyst and by photoelectrochemical measurements.
The work also explains the marginal effect of the fluorination on the H2 evolution.
Climate change may increase the overall susceptibility of peatlands to fire. Smoldering fires in peatlands can cause substantial emissions of greenhouse gases. It is, however, less clear how smoldering affects the soil pore water quality. In this study, soil samples were collected from agricultural fen and disturbed bog study sites in Germany and Lithuania to quantify the effect of peat burning on pore water composition. The samples were air dried and smoldered under ignition temperature (approximately 200 °C) with different durations (0, 2, 5, and 10 h). Pore water samples were extracted from the soil to determine dissolved organic carbon (DOC) concentrations, dissolved organic matter (DOM) fractions, fluoride, extractable organically bound fluorine (EOF), and sulfate concentrations. The results showed that soil smoldering changes the peat pore water chemistry and that changes differ between fens and bogs. The smoldering duration is likewise influential. For fen grasslands, 2 and 5 h of smoldering of peat caused a >10-fold increase in DOC (up to 1600 mg L−1) and EOF concentrations. The fluoride (up to 60 mg L−1) and sulfate concentrations substantially exceededWHOdrinking water guidelines. In contrast, the temperature treatment decreased theDOC concentrations of samples from raised bogs by 90 %. The fluoride concentrations decreased, but sulfate concentrations increased after smoldering of the bog samples. DOC, fluoride, and sulfate concentrations of bogs varied significantly between the smoldering duration treatments. For all peat samples, the extracted DOMwas dominated by humic-like substances before smoldering, but the fraction of low molecular weight substances increased after smoldering combustion. In conclusion, smoldering alters the biogeochemical processes in both peatland types and possibly impair the water quality of adjacent water resources especially in fen peat landscapes.
The measurement of biologically relevant anions, such as fluoride, is an important task in analytical chemistry, in particular, for dental health and osteoporosis. Although a large number of fluoride probes are known, the applicability under relevant conditions is limited to a few examples. To improve this situation, BODIPY-amidothiourea dyes with varying hydrogen-bond donating strengths were developed, the most H-acidic of which (1 c) could detect F- from an inorganic source (NaF) in 50?% aqueous solution (DMSO/water 1:1, v/v) with 0.01 ppm sensitivity through selective fluorescence quenching by a photoinduced electron-transfer (PET) process. Use of the probe and a reference dye with a test-strip assay and a portable and rapidly recording lateral-flow fluorescence reader made determination of F- in neat aqueous solutions, such as spiked water samples and toothpaste extracts, possible in a self-referenced manner, achieving a detection limit of 0.2 ppm.
We demonstrate the potential of time-resolved luminescence spectroscopy for the straightforward assessment and in situ monitoring of the stability of upconversion nanocrystals (UCNPs). Therefore, we prepared hexagonal NaYF4:Yb3+,Er3+ UCNPs with various coatings with a focus on phosphonate ligands of different valency, using different ligand exchange procedures, and studied their dissolution behaviour in phosphate-buffered saline (PBS) dispersions at 20 °C and 37 °C with various analytical methods. The amount of the released UCNPs constituting fluoride ions was quantified by potentiometry using a Fluoride ion-sensitive electrode and particle disintegration was confirmed by transmission electron microscopy studies of the differently aged UCNPs. In parallel, the luminescence features of the UCNPs were measured with special emphasis on the lifetime of the sensitizer emission to demonstrate its suitability as Screening parameter for UCNP stability and changes in particle composition. The excellent correlation between the changes in luminescence lifetime and fluoride concentration highlights the potential of our luminescence lifetime method for UCNP stability screening and thereby indirect monitoring of the release of potentially hazardous fluoride ions during uptake and dissolution in biological systems. Additionally, the developed in situ optical method was used to distinguish the dissolution dynamics of differently sized and differently coated UCNPs.