Self-Accelerating Decomposition Temperature (SADT) is a safety characteristic for the transport of self-reactive substances and organic peroxides. Its determination is time-consuming and in dependence on the test method also material-consuming. As shown previously, DSC measurements, which can be carried out fast and with a few milligram of material, supply a good correlation with SADT for technical pure, liquid organic peroxides. The approach is now applied for solid organic peroxides. Besides, the parameters, which are involved in the correlation, are discussed and their effect on the result is weighted qualitatively. In addition it was shown, that the method is inapplicable in an easy manner for diluted organic peroxides and pure self-reactive substances.
High and ultra-high molecular weight polyethylenes are high performance materials, which are predestined for a wide range of applications due to characteristics like high density, low weight, good dimensional stability, high chemical resistance, and high hydrogen content. These polymers are used in two demanding areas: as implant material in medical technology (only ultra-high molecular weight polyethylenes) and as a component for neutron shielding purposes in casks for storage and transport of radioactive waste. In the medical field (joint replacements) as well as during neutron radiation shielding application, high and ultra-high molecular weight polyethylenes are exposed to gamma irradiation: in the first case requested as sterilization process and for surface-crosslinking and in the second case existing as a side effect of inserting the radioactive material in the cask.
Given that polyethylene as shielding material has to withstand any type of degradation affecting safety relevant aspects to be applicable for long-term radiation shielding purposes for instance over a period of 40 years, the durability of the material is of special interest. High molecular weight polyethylene (HMW-PE; LUPOLEN 5261Z; Lyondell Basell) and ultra-high molecular weight polyethylene (UHMW-PE; GUR 4120; Ticona) were subjected to gamma radiation and afterwards thermally treated. The gamma doses used are in the range of 50 to 600 kGy and irradiation takes place at RT using a Co-60 source. The planned thermal treatment will take place at a temperature of 125 °C for periods of minimum 30 days and maximum of five years. With the applied conventional analytical techniques it is possible to detect structural changes of both types of polyethylene induced by gamma irradiation and certainly of thermal treatment. Through gamma irradiation melting temperature, crystallinity, and density, respectively increased. Furthermore both polyethylenes get oxidized and cross-linked. With regard to the special application as neutron radiation shielding material in casks for storage and transport of radioactive materials, the impact of irradiation lead to changes of material properties. A consolidated view indicates that the detected changes of the irradiated (U)HMW-PE are not safety relevant for long-term neutron radiation shielding purposes over a period of 40 years in Germany.
UV-curing coatings are nowadays widely used due to their unique advantages. High-quality coatings can be obtained at short curing times and low temperatures so that thermal stress to the substrate is minimised. Photocured Cycloaliphatic-Epoxy Oligosiloxane (CEO) resin was reported to be used as encapsulation material for organic electronics. However, further reinforcement of CEO film properties is desired to achieve requested device lifetime.
In this work we introduced Boehmite nanoparticles (BA) into CEO matrix in order to modify the film properties and study the main changes of the material behaviour with regard to its photocuring kinetics, thermal stability and glass transition. Particular interest was focused on the role of particle surface in nanocomposite properties. Hence, BA particles without (HP14) and with organic surface modifier (OS1) at different loadings (up to 10 wt%) were applied in this study. Morphology investigation with SEM operated in transmission mode showed good BA dispersion forming network-like structure. At the same time, distribution of particles differed for HP14 and OS1 as a result of different interaction in CEO-solvent-particles system. CEO structure obtained via non-hydrolytic sol-gel reaction was verified by 13C and 29Si NMR. In situ monitoring of film curing was performed using RT-IR spectroscopy. No significant modification of final convention degree with particle incorporation was observed in contrast to considerable decrease of curing efficiency reported previously for similar system by Esposito et al.,2008. Further, cured hybrid nanocomposite films were analysed by TGA and DSC, which revealed impact of surface modifier on film thermal properties.
The crystallization of ciprofloxacin - an antibacterial fluoroquinolone compound - with salicylic acid resulted in the isolation of five distinct solid forms of the drug, namely, an anhydrous salt, two polymorphic forms of the salt monohydrate, methanol and acetonitrile solvates, and the salt-cocrystal hydrate. The salicylate salts were investigated by different analytical techniques ranging from powder and single crystal X-ray diffractometry, differential scanning calorimetry, thermogravimetric analysis, variable temperature powder X-ray diffraction, dynamic vapor sorption analysis, dissolution, and solubility investigations. Real-time in situ Raman spectroscopy was used to investigate the mechanochemical formation pathways of the different solid polymorphs of ciprofloxacin salicylate. The mechanism of the phase transformation between the crystalline forms was evaluated under mechanochemical conditions. It was found that the formation pathway and kinetics of the grinding process depend on the form of the starting material and reaction conditions. The analysis of the solid-state thermal evolution of the hydrated salts revealed the two-step mechanism of dehydration process, which proceeds through a formation of the distinct intermediate crystalline products.
Carbon-fibre prepregs have found widespread use in lightweight applications. They are based on a carbon-fibre fabric impregnated with reactive epoxy resin. Prepreg materials are generally pre-cured so that they have a higher molecular weight than typical resins in order to reduce resin flow, which facilitates storage and later processing properties.
The measurements were carried out using commercially available materials and follow the published DMA investigations of the same material. TMDSC was used to find the correlation between curing conditions, the degree of cure and glass transition temperature. TMDSC has the advantage over standard DSC that it enables better determination of the glass transition temperature, which is often accompanied by an exothermic curing reaction, and thus overshadowed. The influence of the amplitude of temperature modulation was tested in preliminary experiments. For non-cured material a glass transition temperature of approximately 0 °C was determined; whereas for the totally cured material it was approximately 230 °C. The changes in degree of cure, temperature of actual glass transition and post-reaction are given as a function of curing time at 180 °C. The correlation between actual glass transition temperature and degree of cure is derived.
Carbon fibre prepregs have found widespread application in lightweight constructions. They are based on a carbon-fibre fabric impregnated with reactive epoxy resin. DMA measurements under temperature conditions similar to an autoclave programme were carried out using commercially available prepreg material with a high glass transition temperature. The characteristic of the temperature programme was a dynamic heating segment at 1.5 K/min followed by a longer isothermal segment at 180 °C. The courses of the storage modulus E', loss modulus E'' and tanδ were recorded. The measuring frequency was varied between 1 Hz and 33.3 Hz. Gelation and vitrification are assigned. The influence of the measuring frequency on the time to vitrification and the correlation with DSC are discussed. The reaction does not end even after 10 h curing at 180 °C, which is interpreted as the slow cessation of the reaction caused by vitrification.
EVA is a widely used material for the encapsulation of photovoltaic modules. It melts at elevated temperatures, and seals the module before it is crosslinked at temperatures above 130 °C by a peroxide-initiated crosslinking reaction. EVA has good optical properties necessary for application in solar modules. For process optimization and quality management, a method for the quick and reliable characterization of EVA crosslinking behaviour is of great value. Here, the practicability of ultrasound for online crosslinking monitoring is demonstrated. A sound velocity increase of about 8 m/s during the crosslinking reaction is found. The ultrasound results are compared with rheometer measurements performed with a curemeter typically used for the investigation of rubber crosslinking.
Two types of commercially applied Ethylene/Vinyl Acetate Copolymers (EVA) for encapsulation of photovoltaic modules were investigated by the thermal analysis methods of Differential Scanning Calorimetry (DSC) and Dynamic Mechanical Analysis (DMA) in the temperature range from -150 °C to 200 °C. Glass transition, crystal melting and cross-linking were analyzed. The aims of the investigations were to gain more information for incoming goods control and to get information about the whole temperature dependent material properties in the investigated temperature range, starting at very low temperatures up to the crosslinking temperature region.
Thermoanalytische Charakterisierung von Ethylen-Vinylacetat-Copolymer (EVA) für Photovoltaikmodule
(2011)
Das Ziel der Untersuchungen war mit Hilfe von DSC und DMA EVA-Folien im Anlieferungszustand hinsichtlich der Lage der Glasübergangstemperatur, des Schmelzverhaltens und der Temperaturabhängigkeit der Vernetzungsreaktion zu charakterisieren. Auf dieser Basis sollte die Lieferstabilität im Sinne einer Wareneingangskontrolle auf eine messtechnische Basis gestellt werden. In einem 2. Schritt sollte die vernetzte Folie dahingehend charakterisiert werden, ob infolge der Vernetzung eine Änderung der