Semiconductor quantum dots (QDs) possess unique electronic and optical properties, making them promising candidates for applications in lightemitting diodes, solar cells, bioimaging, and photocatalysis. Precise control over their size, shape, and chemical and electronic structure is crucial to ensure the desired functional properties and optimize device performance. However, challenges in QD synthesis and post-synthesis modification persist, especially in large-scale production. This study addresses the classification of QDs synthesized in a tubular flow reactor consisting of a mixture of the desired InP/ZnS core−shell QDs and QDs made from the shell material, i.e., here ZnS QDs formed as a byproduct during the formation step of the ZnS shell. The homogeneous nucleation of ZnS nanoparticles from the shelling material introduces a heterogeneity in size and composition and affects the optical properties of the resulting QDs. To address this issue, we developed a size-selective agglomeration (SSA) technique by incrementally introducing ethanol as a poor solvent and classified the synthesized QDs into 13 distinct fractions. These 13 fractions are sorted into three distinct groups: (i) larger InP/ZnS QDs, (ii) a combination of smaller InP/ZnS QDs and larger ZnS QDs, and (iii) predominant ZnS QDs with some very tiny InP/ZnS QDs. The comprehensive characterization of the fractions was conducted using UV−visible absorption spectroscopy, photoluminescence spectroscopy, high-resolution scanning transmission electron microscopy, energy-dispersive X-ray spectroscopy, total reflection X-ray fluorescence, and analytical ultracentrifugation. We could demonstrate that our method effectively separated unwanted ZnS QDs from the target InP/ZnS QDs. In addition, the fractions enriched in smaller InP/ZnS QDs exhibited a higher photoluminescence quantum yield compared to the fractions with larger QDs. This demonstrates the efficacy of SSA in finetuning the composition of QD mixtures produced on a larger scale to improve their functional properties. This approach provides fundamental understanding toward the development of a scalable two-dimensional classification process for such ultrasmall nanoparticles by particle size and composition.
The inter-instrument, inter-laboratory, and long-term comparability of fluorescence data requires the correction of the measured emission and excitation spectra for the wavelength- and polarization-dependent spectral irradiance of the excitation channel at the sample position and the spectral responsivity of the emission channel employing procedures that guarantee traceability to the respective primary standards. In this respect the traceability chain of fluorometry is discussed from a radiometrists point of view. This involves, in a first step, the realization of the spectral radiance scale, based on the blackbody radiator and electron storage ring, and the spectral responsivity scale, based on the cryogenic radiometer and their control via key comparisons of the national metrology institutes. In a second step, the characterization including state-of-the art uncertainties of the respective source and detector transfer standards such as tungsten strip lamps, integrating sphere radiators, and trap detectors used to disseminate these radiometric quantities to users of spectroscopic techniques is presented.
Aggregation-induced emission (AIE) has been meanwhile observed for many dye classes and particularly for fluorophores containing propeller-like groups. Herein, we report on the AIE characteristics of a series of four hydrophobic pyrrolidinylvinylquinoxaline (PVQ) derivatives with phenyl, pyrrolyl, indolyl, and methoxythienyl substituents used to systematically vary the torsion angle between this substituent at the quinoxaline C2 position and the planar PVQ moiety. These molecules, which are accessible via four- or five-component one-pot syntheses, were spectroscopically studied in organic solvents and solvent−water mixtures, as dye aggregates, solids, and entrapped in polystyrene particles (PSP). Steady-state and time-resolved fluorescence measurements revealed a strong fluorescence enhancement for all dyes in ethanol−water mixtures of high water content, accompanying the formation of dye aggregates with sizes of a few hundred nm, overcoming polarity and H-bonding-induced fluorescence quenching of the chargetransfer-type emission of these PVQ dyes. The size and shape of these dye aggregates and the size of the AIE effect are controlled by the water content and the substituent-dependent torsion angle that influences the nucleation process and the packing of the molecules during aggregation. Staining of 1 μm-sized carboxy-functionalized PSP with the PVQ dyes resulted also in a considerable increase in the fluorescence quantum yield and lifetime, reflecting the combined influence of the restricted molecular motion and the reduced polarity of the dye microenvironment.
Starting from trivalent 10-alkoxy-10H-9-oxa-10-phosphaphenanthrenes, a broad range of DOPO derivatives was synthesized via transesterification with aliphatic alcohols and subsequent Michaelis-Arbuzov rearrangement using catalytic amounts of p-toluenesulfonic acid methylester. Due to the considerable differences in the nature of the alcohols employed, several procedures for processing them are presented.
10-Ethyl-9-oxa-10-phosphaphenanthrene-10-oxide (1) can be nitrated using acetic anhydride and fuming nitric acid. The nitro group is reduced using palladium on charcoal and hydrogen. These reaction conditions are used for the synthesis of an analogous DOPO-based diaminic hardener (7). An evaluation of the curing behavior, mechanical properties and flammability of a neat resin made of DGEBA and 7 (DGEBA + 7) and of a carbon fiber-reinforced resin made of DGEBA, 4,4-diaminodiphenylsulfon (DDS) and 7 (DGEBA + DDS + 7) shows the potential of this hardener to lead to flame-retardant systems while keeping relevant properties on a high level; especially when compared to a similar system (DGEBA + DDS + 1).
AbstractThe next generation of adhesives requires effective debonding capabilities that can be triggered on demand to enable advanced circular repair and recycling strategies. A new class of lignin‐inspired, two‐component (2K) structural adhesives offers bonding strengths of up to 20 MPa and clean, on‐command electrochemical debonding within 5–30 min. The debonding is induced by a distinct electrochemical oxidation of thiol‐catechol connectivities (TCCs) within the entire adhesive network, enforcing rapid and clean adhesive failure on the cathodic substrate side. The TCC‐functionalities are formed during curing by a thiol‐quinone Michael‐type polyaddition, reacting polyester‐based trithiols with tris‐quinones as lignin‐inspired minimal building blocks. The structural adhesive can be fine‐tuned by adjusting the formulation. The addition of carbon black and ionic liquids facilitates the desired electrochemical transformation of TCC‐catechols to TCC‐quinones. Applying only 9 V for 5–30 min, leads to clean debonding with 72–86% loss of shear strength. A comprehensive study of curing, bonding, and debonding behavior by rheological, spectroscopic, and electrochemical investigations reveals the debonding mechanism by correlating catechol oxidation to adhesive performance. The electrochemical debonding capability of TCC‐structural adhesives is demonstrated in a functional prototype, where on‐command detachment of a cover glass from a display device is achieved within 6.5 min.
The need for the traceable characterization of fluorescence instruments is emphasized from a chemists point of view, focusing on spectral fluorescence standards for the determination of the wavelength- and polarization-dependent relative spectral responsivity and relative spectral irradiance of fluorescence measuring systems, respectively. In a first step, major sources of error of fluorescence measurements and instrument calibration are revealed to underline the importance of this issue and to illustrate advantages and disadvantages of physical and chemical transfer standards for generation of spectral correction curves. Secondly, examples for sets of traceable chemical emission and excitation standards are shown that cover a broad spectral region and simple procedures for the determination of corrected emission spectra with acceptable uncertainties are presented. With proper consideration of the respective measurement principle and geometry, these dye-based characterization procedures can be not only applied to spectrofluorometers but also to other types of fluorescence measuring systems and even to Raman spectrometers.
InP/ZnS core/shell quantum dots (QDs), recognized as highly promising heavy-metal-free emitters, are increasingly being utilized in lighting and display applications. Their synthesis in a tubular flow reactor enables production in a highly efficient, scalable, and reproducible manner, particularly when combined with a single-source shell precursor, such as zinc diethyldithiocarbamate (Zn(S2CNEt2)2). However, the photoluminescence quantum yield (PLQY) of QDs synthesized with this route remains significantly lower compared with those synthesized in batch reactors involving multiple steps for the shell growth. Our study identifies the formation of absorbing, yet nonemissive ZnS nanoparticles during the ZnS shell formation process as a main contributing factor to this discrepancy. By varying the shelling conditions, especially the shelling reaction temperature and InP core concentration, we investigated the formation of pure ZnS nanoparticles and their impact on the optical properties, particularly PLQY, of the resultant InP/ZnS QDs through ultraviolet−visible (UV−vis) absorption, steady-state and time-resolved photoluminescence (PL) spectroscopy, scanning transmission electron microscopy (STEM), and analytical ultracentrifugation (AUC) measurements. Our results suggest that process conditions, such as lower shelling temperatures or reduced InP core concentrations (resulting in a lower external surface area), encourage homogeneous nucleation of ZnS. This reduces the availability of shell precursors necessary for effective passivation of the InP core surfaces, ultimately resulting in lower PLQYs. These findings explain the origin of persistently underperforming PLQY of InP/ZnS QDs synthesized from this synthesis route and suggest further optimization strategies to improve their emission for lighting and display applications.
Knowledge of the structure–property relationships of functional nanomaterials, including, for example, their size- and composition-dependent photoluminescence (PL) and particle-to-particle variations, is crucial for their design and reproducibility. Herein, the Angstrom-resolution capability of an analytical ultracentrifuge combined with an in-line multiwavelength emission detection system (MWE-AUC) for measuring the sedimentation coefficient-resolved spectrally corrected PL spectra of dispersed nanoparticles is demonstrated. The capabilities of this technique are shown for giant-shell CdSe/CdS quantum dots (g-QDs) with a PL quantum yield (PL QY) close to unity capped with oleic acid and oleylamine ligands. The MWE-AUC PL measurements are calibrated and validated with certified fluorescence standards. The spectrally corrected and size-dependent PL spectra of the g-QDs derived from a single MWE-AUC experiment are then analyzed and compared with the results of single-particle spectroscopic studies, yielding the PL spectra, decay kinetics, and blinking behavior of individual g-QDs. This study underlines the vast potential of MWE-AUC with in-line optical detection for the characterization of advanced nanomaterials with a complex structure.
Colloids provide manifold opportunities for targeted product design due to their tunable properties with respect to size, shape, composition, surface, and spectral characteristics. However, the determination of structure-property relationships is quite challenging as most particulate samples exhibit polydispersity of their disperse properties. Analytical ultracentrifugation (AUC) is a fractionating technique and highly accurate method for the multidimensional analysis of nanoparticles as it permits the differentiation of spectral information linked to hydro- and thermodynamic properties of the particles.
So far, characterization capabilities for fluorescent nanoparticles by AUC were limited, as the formerly commercially available fluorescence detector could not provide any spectral information. Using a multiwavelength emission detector developed in our group, it is possible to extract spectra of fluorescent particles and biomolecules alongside their sedimentation and diffusion coefficients within a single centrifugation experiment.
In our contribution, we will highlight that even narrowly distributed core/shell CdSe/CdS quantum dots still show size- and structure-dependent shifts of their fluorescence spectra, which can be resolved with our AUC system in an ensemble measurement. Thereby, we can link spectral changes of only a few nanometers to particle sizes retrieved with Angstrom size resolution. Single-particle measurements not only supported the results obtained with the AUC system but also provided deeper insights into the photophysical processes of individual QDs, clearly demonstrating the complementary nature of the techniques used. With our novel multiwavelength emission detector and the established extinction-based detector for AUC, a comprehensive platform for the holistic characterization of fluorescent colloids is now available.