Produktion und Systeme
Refine
Document Type
Language
- English (7)
Has Fulltext
- yes (7) (remove)
Is part of the Bibliography
- no (7)
Keywords
- magnetoactive elastomer (2)
- magnetoelectric effect (2)
- magnetostriction (2)
- Applied Research (1)
- acoustic quality factor (1)
- composite structure (1)
- flexible composite (1)
- linear (1)
- low frequency (1)
- macroscopic deformation (1)
Institute
- Fakultät Elektro- und Informationstechnik (7) (remove)
Begutachtungsstatus
- peer-reviewed (6)
Significant deformations of bodies made from compliant magnetoactive elastomers (MAE) in magnetic fields make these materials promising for applications in magnetically controlled actuators for soft robotics. Reported experimental research in this context was devoted to the behaviour in the quasi-static magnetic field, but the transient dynamics are of great practical importance. This paper presents an experimental study of the transient response of apparent longitudinal and transverse strains of a family of isotropic and anisotropic MAE cylinders with six different aspect ratios in time-varying uniform magnetic fields. The time dependence of the magnetic field has a trapezoidal form, where the rate of both legs is varied between 52 and 757 kA/(s·m) and the maximum magnetic field takes three values between 153 and 505 kA/m. It is proposed to introduce four characteristic times: two for the delay of the transient response during increasing and decreasing magnetic field, as well as two for rise and fall times. To facilitate the comparison between different magnetic field rates, these characteristic times are further normalized on the rise time of the magnetic field ramp. The dependence of the normalized characteristic times on the aspect ratio, the magnetic field slew rate, maximum magnetic field values, initial internal structure (isotropic versus anisotropic specimens) and weight fraction of the soft-magnetic filler are obtained and discussed in detail. The normalized magnetostrictive hysteresis loop is introduced, and used to explain why the normalized delay times vary with changing experimental parameters.
Herein, the effect of an applied moderate (~240 mT) magnetic field on the work of adhesion (WoA) of mechanically soft (the shear modulus ~10 kPa) magnetoactive elastomer (MAE) samples with two different mass fractions (70 and 80 wt%) of carbonyl iron powder (CIP) is concerned. The unfilled elastomer sample is used for comparison. Due to some sedimentation of filling particles, the concentration of inclusions in thin (~10 μm) subsurface layers is different. It is shown that the WoA increases (up to 1.8-fold) on the particle-enriched side (PES) in the magnetic field and its value is higher for higher filler concentration. On the particle-depleted side (PDS), WoA does not depend on particle concentration and on the magnetic field. Adhesion and friction are coupled in MAEs. No statistically significant difference in the friction coefficient, determined from the extended Amontons´ law, depending on sample side, CIP concentration, or presence of magnetic field is found. However, the PDS in the magnetic field demonstrates significantly higher critical shear stress compared to that for the PES or PDS in the absence of magnetic field. Correlations between different surface properties are discussed. Obtained results are useful for the development of magnetically controllable soft robots.
The dependence of the resonant direct magnetoelectric effect on temperature is studied experimentally in planar composite structures. Samples of rectangular shapes with dimensions of 5 mm x 20 mm employed ferromagnetic layers of either an amorphous (metallic glass) alloy or nickel with a thickness of 20-200 m and piezoelectric layers of single crystalline langatate material or lead zirconate titanate piezoelectric ceramics with a thickness of 500 m. The temperature of the samples was varied in a range between 120 and 390 K by blowing a gaseous nitrogen stream around them. It is shown that the effective characteristics of the magnetoelectric effectsuch as the mechanical resonance frequency f(r), the quality factor Q and the magnitude of the magnetoelectric coefficient (E) at the resonance frequencyare contingent on temperature. The interrelations between the temperature changes of the characteristics of the magnetoelectric effect and the temperature variations of the following material parametersYoung's modulus Y, the acoustic quality factor of individual layers, the dielectric constant epsilon, the piezoelectric modulus d of the piezoelectric layer as well as the piezomagnetic coefficients ((n)) of the ferromagnetic layerare established. The effect of temperature on the characteristics of the nonlinear magnetoelectric effect is observed for the first time. The results can be useful for designing magnetoelectric heterostructures with specified temperature characteristics, in particular, for the development of thermally stabilized magnetoelectric devices.
In this work, the resonance enhancement of magnetoelectric (ME) coupling at the two lowest bending resonance frequencies was investigated in layered cantilever structures comprising a magnetoactive elastomer (MAE) slab and a commercially available piezoelectric polymer multilayer. A cantilever was fixed at one end in the horizontal plane and the magnetic field was applied horizontally. Five composite structures, each containing an MAE layer of different thicknesses from 0.85 to 4 mm, were fabricated. The fundamental bending resonance frequency in the absence of a magnetic field varied between roughly 23 and 55 Hz. It decreased with the increasing thickness of the MAE layer, which was explained by a simple theory. The largest ME voltage coefficient of about 7.85 V/A was measured in a sample where the thickness of the MAE layer was ≈2 mm. A significant increase in the bending resonance frequencies in the applied DC magnetic field of 240 kA/m up to 200% was observed. The results were compared with alternative designs for layered multiferroic structures. Directions for future research were also discussed.
The significant effect of an external dc magnetic field on the splashing behavior of ethanol drops impacting on the unstructured (flat) surface of soft magnetoactive elastomers (MAEs) is reported. The Weber number corresponding to the transition between the deposition and the splashing regime is reduced by ≈20% in a moderate magnetic field of ≈300 mT. Alongside this effect, a two-fold increase of the initial deceleration of the ejection sheet is observed for the softest sample. The main underlying mechanism for the observed phenomena is believed to be the magnetic-field-induced stiffening of the MAEs. Further possible mechanisms are magnetically induced changes in the surface roughness and magnetic-field-induced plasticity (magnetic shape memory effect). The potential application areas are magnetically regulable wetting and magneto-responsive surfaces for controlling the drop splashing.
Thermomechanical shape memory materials have certain disadvantages when it comes to 3D volumetric reproduction intended for rapid prototyping or robotic prehension. The need to constantly supply energy to counteract elastic retraction forces in order to maintain the required geometry, together with the inability to achieve conformal stability at elevated temperatures, limits the application of thermal shape memory polymers. Form removal also presents problems as most viscoelastic materials do not ensure demolding stability. This work demonstrates how magnetoactive boron−organo−silicon oxide polymers under the influence of an applied magnetic field can be used to achieve energy free sustainable volumetric shape memory effects over extended periods. The rheopectic properties of boron−organo−silicon oxide materials sustain form removal without mold distortion.
The Applied Research Conference which is held every year at another University of Applied Sciences in Bavaria is the main event for all students in the Master of Applied Research program. They come together to present their work in oral presentations and full papers, which are published in the proceedings, as well as poster presentations of the students after their 1st semester. For sure it is interesting for Professors and interested people to see the results of upcoming scientists and researchers. Due to the Corona pandemic, this year it is not possible to organize the conference as usual in presence. We have to refrain from face-to-face discussions, having together a cup of coffee. We as Professors at the OTH Regensburg wanted to give our students the chance to finish this semester successfully – despite all limitations due to the pandemic situation. Therefore we decided to organize the RARC 2020 – Regensburg Applied Research Conference 2020 – for the Master of Applied Research students of OTH Regensburg as an online conference. However, for a Technical University the situation is rather a challenge than a problem. Using a variety of online tools for teaching during this semester, we have enough experience to find a setup for RARC2020. We received 28 submissions for full papers, which were peer reviewed and 26 of them were accepted – you will find them in this proceedings, and they will be presented orally on July 31st, 2020. Additionally, there are 22 posters which will be presented on the same day. During the Plenary Opening Session, after a welcome by our President Prof. Dr. Wolfgang Baier we will have 3 Keynote speakers:
Prof. Dr. phil. habil. Karsten Weber: Erkenntnistheorie für Ingenieure
Prof. em. Georg Scharfenberg: 11 Years Master of Applied Research Alumnis
Veronika Fetzer: Entrepreneurship