TY - JOUR A1 - Hornberger, Helga A1 - Striegl, Birgit A1 - Trahanofsky, M. A1 - Kneissl, F. A1 - Kronseder, Matthias T1 - Degradation and bioactivity studies of Mg membranes for dental surgery JF - Materials Letter X N2 - Bioresorbable materials are under investigation due to their promising properties for applications as implant material. This study is about the degradation and bioactivity behaviour of magnesium foils, which allegorize dental membranes. The degradation behaviour including pitting corrosion during immersion tests can be precisely observed using micro-computed tomography. Using the bioactivity test according to Kokubo, it is shown that magnesium has strong Ca-phosphate layer formation correlated with high degradation. Therefore, magnesium foils appear to hold a great potential for bone implant application. KW - Magnesium KW - Dental membrane KW - Bioactivity KW - Corrosion rate Y1 - 2019 U6 - https://doi.org/10.1016/j.mlblux.2019.100007 VL - 2 IS - June SP - 1 EP - 5 PB - Elsevier ER - TY - JOUR A1 - Hornberger, Helga A1 - Kissel, Hannah A1 - Striegl, Birgit A1 - Kronseder, Matthias A1 - Vollnhals, Florian A1 - Christiansen, Silke H. T1 - Bioactivity and corrosion behavior of magnesium barrier membranes JF - Materials and Corrosion N2 - In the current research, magnesium and its alloys have been intensively studied as resorbable implant materials. Magnesium materials combine their good mechanical properties with bioactivity, which make them interesting for guided bone regeneration and for the application as barrier membranes. In this study, the in vitro degradation behavior of thin magnesium films was investigated in cell medium and simulated body fluid. Three methods were applied to evaluate corrosion rates: measurements of (i) the gaseous volume evolved during immersion, (ii) volume change after immersion, and (iii) polarization curves. In this comparison, measurements of H2 development in Dulbecco's modified Eagle's medium showed to be the most appropriate method, exhibiting a corrosion rate of 0.5 mm·year−1. Observed oxide and carbon contamination have a high impact on controlled degradation, suggesting that surface treatment of thin foils is necessary. The bioactivity test showed positive results; more detailed tests in this area are of interest. Y1 - 2022 U6 - http://nbn-resolving.de/urn/resolver.pl?urn:nbn:de:bvb:898-opus4-24499 N1 - Corresponding author: Helga Hornberger VL - 73 IS - 1 SP - 8 EP - 19 PB - Wiley ER -