@article{SavelevGlavanBurdinetal., author = {Savelev, Dmitrii V. and Glavan, Gašper and Burdin, Dmitrii A. and Belyaeva, Inna A. and Fetisov, Leonid Y. and Shamonin (Chamonine), Mikhail and Fetisov, Yuri K.}, title = {Enhancement of magnetoelectric effect in polymer composites at low resonance frequencies by operation in the transverse-transverse mode}, series = {Journal of Magnetism and Magnetic Materials}, volume = {598}, journal = {Journal of Magnetism and Magnetic Materials}, publisher = {Elsevier}, issn = {1873-4766}, doi = {10.1016/j.jmmm.2024.172020}, abstract = {The resonant direct magnetoelectric (ME) effect for a series of multilayer heterostructures comprising a magnetoactive elastomer (MAE) of different thicknesses and a commercially available piezoelectric polyvinylidene fluoride-based vibration sensor has been investigated in detail. The specimens were rigidly fixed at one end as cantilevers. The cantilevers were operated in the transverse-transverse (T-T) mode, where both magnetic and electric fields were perpendicular to the plane of a non-deformed heterostructure. It is shown that the ME voltage coefficient of considered heterostructures in the T-T mode can be about 20-fold higher than in the conventional longitudinal-transverse (L-T) mode. The highest ME voltage coefficient reached about 150 V/(Oe·cm) at the first bending oscillation mode for the sample with MAE layer thickness of 4 mm. Mechanism of the resonant ME effect in T-T mode is explained using theory of critical bending of MAE cantilevers. Magnetic fields, when the ME voltage reaches its maximum, strongly depended on the MAE layer thickness, and could be associated with the critical field, where the structure commences to strongly bend. The non-monotonous dependence of the resonance frequency of the first oscillation mode on magnetic field strength was observed. The shift of the resonance frequency in the maximum magnetic field reached up to roughly 100 \% in comparison with zero field.}, language = {en} } @article{BurdinEkonomovChashinetal., author = {Burdin, Dmitrii A. and Ekonomov, Nikolai A. and Chashin, Dmitri V. and Fetisov, Leonid Y. and Fetisov, Yuri K. and Shamonin (Chamonine), Mikhail}, title = {Temperature Dependence of the Resonant Magnetoelectric Effect in Layered Heterostructures}, series = {Materials}, volume = {10}, journal = {Materials}, number = {10}, publisher = {MDPI}, doi = {10.3390/ma10101183}, url = {http://nbn-resolving.de/urn:nbn:de:bvb:898-opus4-32185}, abstract = {The dependence of the resonant direct magnetoelectric effect on temperature is studied experimentally in planar composite structures. Samples of rectangular shapes with dimensions of 5 mm x 20 mm employed ferromagnetic layers of either an amorphous (metallic glass) alloy or nickel with a thickness of 20-200 m and piezoelectric layers of single crystalline langatate material or lead zirconate titanate piezoelectric ceramics with a thickness of 500 m. The temperature of the samples was varied in a range between 120 and 390 K by blowing a gaseous nitrogen stream around them. It is shown that the effective characteristics of the magnetoelectric effectsuch as the mechanical resonance frequency f(r), the quality factor Q and the magnitude of the magnetoelectric coefficient (E) at the resonance frequencyare contingent on temperature. The interrelations between the temperature changes of the characteristics of the magnetoelectric effect and the temperature variations of the following material parametersYoung's modulus Y, the acoustic quality factor of individual layers, the dielectric constant epsilon, the piezoelectric modulus d of the piezoelectric layer as well as the piezomagnetic coefficients ((n)) of the ferromagnetic layerare established. The effect of temperature on the characteristics of the nonlinear magnetoelectric effect is observed for the first time. The results can be useful for designing magnetoelectric heterostructures with specified temperature characteristics, in particular, for the development of thermally stabilized magnetoelectric devices.}, language = {en} }